Hello
We are starting a new process for cleaning glass substrates for thin
film deposition. Will a standard RCA process etch the glass? Should
there be any steps we eliminate or adjust? Does anyone have any
experience or advice before we start?
Please send replies directly to me at
hannah.dayan@nrc.ca
thanks