Re: fused silica

From: Don Kendall (donk@stout.chtm.unm.edu)
Date: Fri Mar 12 1999 - 18:56:13 EST


Hello Silke, I got this message circuitously, but I hope the labnetwork
group forwards you the message. I didn't see an email address in my copy.
        The person most likely to know this info is Dr. Caroline Matzke at
Sandia Labs. I don't have her email address, but her phone is :
505-844-7193, and her FAX number is 505-844-8985. She is actually
working on a single crystal quartz system, but will know about the fused
quartz work. Good Luck.
Don L. Kendall, U. New Mexico
         
> >>>>
>
> <excerpt>Date: Fri, 12 Mar 1999 12:26:01 -0600
>
> From: "Silke Lieber"
>
> To: labnetwork@mtl.mit.edu
>
>
> Dear Sirs and madams,
>
>
> hopefully you can help me .
>
>
> I am working at the university of Texas, Dallas.
>
> And I discovered a page on the web about microfabricated Fused Silica
> Flow Chambers for
>
> Flow Cytometry.
>
> I need to contact this people who designed this thing. Could you help me
> finding the adress
>
> how I can contact this people?
>
>
> Thank you very much.
>
> Sincerely
>
> Silke Lieber
>
> </excerpt>
>
>
>
>
> Professor Steven R. J. Brueck
>
> Center for High Technology Materials
>
> University of New Mexico
>
> 1313 Goddard SE
>
> Albuquerque, NM 87106
>
> voice: 505-272-7800;
>
> fax: 505-272-7801;
>
> email: brueck@chtm.unm.edu
>



This archive was generated by hypermail 2b29 : Tue Mar 09 2004 - 07:49:02 EST