New chip fabrication approach

January 29, 2016

Depositing different materials within a single chip layer could lead to more efficient computers.

MIT-In-Plane_0.jpg
Researchers used the MIT and Tim the Beaver logos to show photoluminescence emissions from a monolayer of molybdenum disulfide inlayed onto graphene. The arrow indicates the graphene-MoS2 lateral heterostructure, which could potentially form the basis for ultrathin computer chips. Image courtesy of the researchers.