Researchers find unexpected magnetic effect

May 9, 2016

Combining two thin-film materials yields surprising room-temperature magnetism.

MIT-Proximity-Coupling_0.jpg
Arrows indicate the spin direction in the ferromagnetic insulator (EuS, shown in red) and topological insulator (Bi2Se3, shown in blue) at the interface between the two materials. Image: Ferhat Katmis