New technique produces highly conductive graphene wafers

April 6, 2017

"Now we can really produce single-domain graphene at wafer scale."--Jeehwan Kim

MIT-Single-Domain_0.jpg
Researchers at MIT have found a way to make graphene with fewer wrinkles, and to iron out the wrinkles that do appear. They found each wafer exhibited uniform performance, meaning that electrons flowed freely across each wafer, at similar speeds, even across previously wrinkled regions.