Sandwiched between superconductors, graphene adopts exotic electronic states

May 12, 2017

Platform may be used to explore avenues for quantum computing.

MIT-Graphene-Semiconductors_0.jpg
MIT physicists have found that a flake of graphene, when brought in close proximity with two superconducting materials, can inherit some of those materials' superconducting qualities. As graphene is sandwiched between superconductors, its electronic state changes dramatically, even at its center. Pictured is the experimental concept and device schematic.