Note: This data was digitized from the CV_PLOT image and may contain error. VG(V) CGG(1e-12) -3.0 1.75 -2.5 1.71 -2.2 1.68 -2.0 1.65 -1.8 1.61 -1.6 1.57 -1.5 1.545 -1.4 1.50 -1.3 1.45 -1.2 1.365 -1.1 1.255 -1.0 1.105 -0.9 0.93 -0.8 0.79 -0.7 0.71 -0.6 0.65 -0.5 0.595 -0.4 0.56 -0.3 0.53 -0.2 0.505 -0.1 0.49 0.0 0.475 0.1 0.46 0.2 0.46 0.3 0.51 0.4 0.785 0.5 1.20 0.6 1.43 0.7 1.52 0.8 1.56 0.9 1.59 1.0 1.60 1.2 1.62 1.5 1.63 1.75 1.635 2.0 1.63 2.5 1.62 3.0 1.60