-1.000000000000000e-01 0.000000000000000e+00 1.989460077488630e+20 -1.000000000000000e-01 1.500000000000000e-03 1.970990306122682e+20 -1.000000000000000e-01 3.000000000000000e-03 1.922933441521983e+20 -1.000000000000000e-01 4.500000000000001e-03 1.847100798725102e+20 -1.000000000000000e-01 6.000000000000000e-03 1.746461934347441e+20 -1.000000000000000e-01 7.500000000000000e-03 1.624953590587235e+20 -1.000000000000000e-01 9.000000000000001e-03 1.487229735775812e+20 -1.000000000000000e-01 1.050000000000000e-02 1.338374369370652e+20 -1.000000000000000e-01 1.200000000000000e-02 1.183600782975821e+20 -1.000000000000000e-01 1.350000000000000e-02 1.027960634580709e+20 -1.000000000000000e-01 1.500000000000000e-02 8.760837871553451e+19 -1.000000000000000e-01 1.650000000000000e-02 7.319658405394838e+19 -1.000000000000000e-01 1.800000000000000e-02 5.988151766568749e+19 -1.000000000000000e-01 1.950000000000000e-02 4.789656735254094e+19 -1.000000000000000e-01 2.100000000000000e-02 3.738555168406800e+19 -1.000000000000000e-01 2.250000000000000e-02 2.840671941130736e+19 -1.000000000000000e-01 2.400000000000000e-02 2.094191931689198e+19 -1.000000000000000e-01 2.550000000000000e-02 1.490964897485222e+19 -1.000000000000000e-01 2.700000000000000e-02 1.018048684406722e+19 -1.000000000000000e-01 2.850000000000000e-02 6.593363326920686e+18 -1.000000000000000e-01 3.000000000000000e-02 3.971232721333878e+18 -1.000000000000000e-01 3.150000000000000e-02 2.134950742656438e+18 -1.000000000000000e-01 3.300000000000000e-02 9.145050393635727e+17 -1.000000000000000e-01 3.450000000000000e-02 1.571393327240981e+17 -1.000000000000000e-01 3.600000000000000e-02 -2.676990436821914e+17 -1.000000000000000e-01 3.750000000000000e-02 -4.663232592512207e+17 -1.000000000000000e-01 3.900000000000000e-02 -5.211733384089526e+17 -1.000000000000000e-01 4.050000000000000e-02 -4.929396506924289e+17 -1.000000000000000e-01 4.200000000000000e-02 -4.237699314480733e+17 -1.000000000000000e-01 4.350000000000000e-02 -3.409466885452108e+17 -1.000000000000000e-01 4.500000000000000e-02 -2.605426141272108e+17 -1.000000000000000e-01 4.650000000000000e-02 -1.907107610842099e+17 -1.000000000000000e-01 4.800000000000000e-02 -1.344150515701492e+17 -1.000000000000000e-01 4.950000000000000e-02 -9.153405899109366e+16 -1.000000000000000e-01 5.100000000000000e-02 -6.036525437524065e+16 -1.000000000000000e-01 5.250000000000000e-02 -3.861519378892229e+16 -1.000000000000000e-01 5.400000000000000e-02 -2.398729718557711e+16 -1.000000000000000e-01 5.550000000000000e-02 -1.448064263583584e+16 -1.000000000000000e-01 5.700000000000000e-02 -8.499465336697928e+15 -1.000000000000000e-01 5.850000000000000e-02 -4.851879721633672e+15 -1.000000000000000e-01 6.000000000000000e-02 -2.693860462767418e+15 -1.000000000000000e-01 6.150000000000000e-02 -1.454575802458284e+15 -1.000000000000000e-01 6.300000000000000e-02 -7.635830073261291e+14 -1.000000000000000e-01 6.450000000000000e-02 -3.894906779856507e+14 -1.000000000000000e-01 6.600000000000000e-02 -1.928843124487357e+14 -1.000000000000000e-01 6.750000000000000e-02 -9.262530954421184e+13 -1.000000000000000e-01 6.900000000000001e-02 -4.305656431123582e+13 -1.000000000000000e-01 7.050000000000001e-02 -1.932548094046387e+13 -1.000000000000000e-01 7.200000000000001e-02 -8.344024680144258e+12 -1.000000000000000e-01 1.200000000000000e-01 0.000000000000000e+00 -9.800000000000000e-02 0.000000000000000e+00 1.989460077445473e+20 -9.800000000000000e-02 1.500000000000000e-03 1.970990306063843e+20 -9.800000000000000e-02 3.000000000000000e-03 1.922933441443586e+20 -9.800000000000000e-02 4.500000000000001e-03 1.847100798623015e+20 -9.800000000000000e-02 6.000000000000000e-03 1.746461934217524e+20 -9.800000000000000e-02 7.500000000000000e-03 1.624953590425654e+20 -9.800000000000000e-02 9.000000000000001e-03 1.487229735579411e+20 -9.800000000000000e-02 1.050000000000000e-02 1.338374369137346e+20 -9.800000000000000e-02 1.200000000000000e-02 1.183600782704965e+20 -9.800000000000000e-02 1.350000000000000e-02 1.027960634273397e+20 -9.800000000000000e-02 1.500000000000000e-02 8.760837868145851e+19 -9.800000000000000e-02 1.650000000000000e-02 7.319658401702109e+19 -9.800000000000000e-02 1.800000000000000e-02 5.988151762657865e+19 -9.800000000000000e-02 1.950000000000000e-02 4.789656731206177e+19 -9.800000000000000e-02 2.100000000000000e-02 3.738555164312148e+19 -9.800000000000000e-02 2.250000000000000e-02 2.840671937082819e+19 -9.800000000000000e-02 2.400000000000000e-02 2.094191927778313e+19 -9.800000000000000e-02 2.550000000000000e-02 1.490964893792494e+19 -9.800000000000000e-02 2.700000000000000e-02 1.018048680999121e+19 -9.800000000000000e-02 2.850000000000000e-02 6.593363296189521e+18 -9.800000000000000e-02 3.000000000000000e-02 3.971232694248290e+18 -9.800000000000000e-02 3.150000000000000e-02 2.134950719325809e+18 -9.800000000000000e-02 3.300000000000000e-02 9.145050197234769e+17 -9.800000000000000e-02 3.450000000000000e-02 1.571393165660199e+17 -9.800000000000000e-02 3.600000000000000e-02 -2.676990566738548e+17 -9.800000000000000e-02 3.750000000000000e-02 -4.663232694598815e+17 -9.800000000000000e-02 3.900000000000000e-02 -5.211733462486940e+17 -9.800000000000000e-02 4.050000000000000e-02 -4.929396565763068e+17 -9.800000000000000e-02 4.200000000000000e-02 -4.237699357638058e+17 -9.800000000000000e-02 4.350000000000000e-02 -3.409466916388833e+17 -9.800000000000000e-02 4.500000000000000e-02 -2.605426162945311e+17 -9.800000000000000e-02 4.650000000000000e-02 -1.907107625680969e+17 -9.800000000000000e-02 4.800000000000000e-02 -1.344150525630538e+17 -9.800000000000000e-02 4.950000000000000e-02 -9.153405964039030e+16 -9.800000000000000e-02 5.100000000000000e-02 -6.036525479020210e+16 -9.800000000000000e-02 5.250000000000000e-02 -3.861519404810218e+16 -9.800000000000000e-02 5.400000000000000e-02 -2.398729734378341e+16 -9.800000000000000e-02 5.550000000000000e-02 -1.448064273021480e+16 -9.800000000000000e-02 5.700000000000000e-02 -8.499465391722368e+15 -9.800000000000000e-02 5.850000000000000e-02 -4.851879752985653e+15 -9.800000000000000e-02 6.000000000000000e-02 -2.693860480225772e+15 -9.800000000000000e-02 6.150000000000000e-02 -1.454575811959311e+15 -9.800000000000000e-02 6.300000000000000e-02 -7.635830123793324e+14 -9.800000000000000e-02 6.450000000000000e-02 -3.894906806122386e+14 -9.800000000000000e-02 6.600000000000000e-02 -1.928843137830128e+14 -9.800000000000000e-02 6.750000000000000e-02 -9.262531020662527e+13 -9.800000000000000e-02 6.900000000000001e-02 -4.305656463263233e+13 -9.800000000000000e-02 7.050000000000001e-02 -1.932548109286287e+13 -9.800000000000000e-02 7.200000000000001e-02 -8.344024750768217e+12 -9.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -9.600000000000000e-02 0.000000000000000e+00 1.989460077370114e+20 -9.600000000000000e-02 1.500000000000000e-03 1.970990305961103e+20 -9.600000000000000e-02 3.000000000000000e-03 1.922933441306693e+20 -9.600000000000000e-02 4.500000000000001e-03 1.847100798444758e+20 -9.600000000000000e-02 6.000000000000000e-03 1.746461933990671e+20 -9.600000000000000e-02 7.500000000000000e-03 1.624953590143511e+20 -9.600000000000000e-02 9.000000000000001e-03 1.487229735236467e+20 -9.600000000000000e-02 1.050000000000000e-02 1.338374368729961e+20 -9.600000000000000e-02 1.200000000000000e-02 1.183600782232013e+20 -9.600000000000000e-02 1.350000000000000e-02 1.027960633736789e+20 -9.600000000000000e-02 1.500000000000000e-02 8.760837862195708e+19 -9.600000000000000e-02 1.650000000000000e-02 7.319658395254094e+19 -9.600000000000000e-02 1.800000000000000e-02 5.988151755828919e+19 -9.600000000000000e-02 1.950000000000000e-02 4.789656724137954e+19 -9.600000000000000e-02 2.100000000000000e-02 3.738555157162317e+19 -9.600000000000000e-02 2.250000000000000e-02 2.840671930014595e+19 -9.600000000000000e-02 2.400000000000000e-02 2.094191920949367e+19 -9.600000000000000e-02 2.550000000000000e-02 1.490964887344478e+19 -9.600000000000000e-02 2.700000000000000e-02 1.018048675048978e+19 -9.600000000000000e-02 2.850000000000000e-02 6.593363242528652e+18 -9.600000000000000e-02 3.000000000000000e-02 3.971232646953104e+18 -9.600000000000000e-02 3.150000000000000e-02 2.134950678587299e+18 -9.600000000000000e-02 3.300000000000000e-02 9.145049854291498e+17 -9.600000000000000e-02 3.450000000000000e-02 1.571392883517778e+17 -9.600000000000000e-02 3.600000000000000e-02 -2.676990793590983e+17 -9.600000000000000e-02 3.750000000000000e-02 -4.663232872856167e+17 -9.600000000000000e-02 3.900000000000000e-02 -5.211733599379679e+17 -9.600000000000000e-02 4.050000000000000e-02 -4.929396668503722e+17 -9.600000000000000e-02 4.200000000000000e-02 -4.237699432996723e+17 -9.600000000000000e-02 4.350000000000000e-02 -3.409466970408639e+17 -9.600000000000000e-02 4.500000000000000e-02 -2.605426200789726e+17 -9.600000000000000e-02 4.650000000000000e-02 -1.907107651591692e+17 -9.600000000000000e-02 4.800000000000000e-02 -1.344150542968028e+17 -9.600000000000000e-02 4.950000000000000e-02 -9.153406077415216e+16 -9.600000000000000e-02 5.100000000000000e-02 -6.036525551478223e+16 -9.600000000000000e-02 5.250000000000000e-02 -3.861519450066614e+16 -9.600000000000000e-02 5.400000000000000e-02 -2.398729762003352e+16 -9.600000000000000e-02 5.550000000000000e-02 -1.448064289501355e+16 -9.600000000000000e-02 5.700000000000000e-02 -8.499465487802659e+15 -9.600000000000000e-02 5.850000000000000e-02 -4.851879807730553e+15 -9.600000000000000e-02 6.000000000000000e-02 -2.693860510710475e+15 -9.600000000000000e-02 6.150000000000000e-02 -1.454575828549420e+15 -9.600000000000000e-02 6.300000000000000e-02 -7.635830212029249e+14 -9.600000000000000e-02 6.450000000000000e-02 -3.894906851986247e+14 -9.600000000000000e-02 6.600000000000000e-02 -1.928843161128455e+14 -9.600000000000000e-02 6.750000000000000e-02 -9.262531136329083e+13 -9.600000000000000e-02 6.900000000000001e-02 -4.305656519383513e+13 -9.600000000000000e-02 7.050000000000001e-02 -1.932548135897264e+13 -9.600000000000000e-02 7.200000000000001e-02 -8.344024874087431e+12 -9.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -9.400000000000000e-02 0.000000000000000e+00 1.989460077239723e+20 -9.400000000000000e-02 1.500000000000000e-03 1.970990305783333e+20 -9.400000000000000e-02 3.000000000000000e-03 1.922933441069831e+20 -9.400000000000000e-02 4.500000000000001e-03 1.847100798136324e+20 -9.400000000000000e-02 6.000000000000000e-03 1.746461933598154e+20 -9.400000000000000e-02 7.500000000000000e-03 1.624953589655328e+20 -9.400000000000000e-02 9.000000000000001e-03 1.487229734643081e+20 -9.400000000000000e-02 1.050000000000000e-02 1.338374368025073e+20 -9.400000000000000e-02 1.200000000000000e-02 1.183600781413677e+20 -9.400000000000000e-02 1.350000000000000e-02 1.027960632808308e+20 -9.400000000000000e-02 1.500000000000000e-02 8.760837851900325e+19 -9.400000000000000e-02 1.650000000000000e-02 7.319658384097256e+19 -9.400000000000000e-02 1.800000000000000e-02 5.988151744012965e+19 -9.400000000000000e-02 1.950000000000000e-02 4.789656711907986e+19 -9.400000000000000e-02 2.100000000000000e-02 3.738555144791144e+19 -9.400000000000000e-02 2.250000000000000e-02 2.840671917784628e+19 -9.400000000000000e-02 2.400000000000000e-02 2.094191909133414e+19 -9.400000000000000e-02 2.550000000000000e-02 1.490964876187640e+19 -9.400000000000000e-02 2.700000000000000e-02 1.018048664753596e+19 -9.400000000000000e-02 2.850000000000000e-02 6.593363149680609e+18 -9.400000000000000e-02 3.000000000000000e-02 3.971232565119439e+18 -9.400000000000000e-02 3.150000000000000e-02 2.134950608098487e+18 -9.400000000000000e-02 3.300000000000000e-02 9.145049260905431e+17 -9.400000000000000e-02 3.450000000000000e-02 1.571392395333884e+17 -9.400000000000000e-02 3.600000000000000e-02 -2.676991186108011e+17 -9.400000000000000e-02 3.750000000000000e-02 -4.663233181290355e+17 -9.400000000000000e-02 3.900000000000000e-02 -5.211733836241724e+17 -9.400000000000000e-02 4.050000000000000e-02 -4.929396846273279e+17 -9.400000000000000e-02 4.200000000000000e-02 -4.237699563387916e+17 -9.400000000000000e-02 4.350000000000000e-02 -3.409467063877742e+17 -9.400000000000000e-02 4.500000000000000e-02 -2.605426266270960e+17 -9.400000000000000e-02 4.650000000000000e-02 -1.907107696424359e+17 -9.400000000000000e-02 4.800000000000000e-02 -1.344150572966647e+17 -9.400000000000000e-02 4.950000000000000e-02 -9.153406273587162e+16 -9.400000000000000e-02 5.100000000000000e-02 -6.036525676850493e+16 -9.400000000000000e-02 5.250000000000000e-02 -3.861519528372611e+16 -9.400000000000000e-02 5.400000000000000e-02 -2.398729809802210e+16 -9.400000000000000e-02 5.550000000000000e-02 -1.448064318016066e+16 -9.400000000000000e-02 5.700000000000000e-02 -8.499465654047956e+15 -9.400000000000000e-02 5.850000000000000e-02 -4.851879902454268e+15 -9.400000000000000e-02 6.000000000000000e-02 -2.693860563457386e+15 -9.400000000000000e-02 6.150000000000000e-02 -1.454575857254865e+15 -9.400000000000000e-02 6.300000000000000e-02 -7.635830364701639e+14 -9.400000000000000e-02 6.450000000000000e-02 -3.894906931343326e+14 -9.400000000000000e-02 6.600000000000000e-02 -1.928843201440961e+14 -9.400000000000000e-02 6.750000000000000e-02 -9.262531336464000e+13 -9.400000000000000e-02 6.900000000000001e-02 -4.305656616487015e+13 -9.400000000000000e-02 7.050000000000001e-02 -1.932548181941563e+13 -9.400000000000000e-02 7.200000000000001e-02 -8.344025087463545e+12 -9.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -9.200000000000000e-02 0.000000000000000e+00 1.989460077016162e+20 -9.200000000000000e-02 1.500000000000000e-03 1.970990305478540e+20 -9.200000000000000e-02 3.000000000000000e-03 1.922933440663721e+20 -9.200000000000000e-02 4.500000000000001e-03 1.847100797607500e+20 -9.200000000000000e-02 6.000000000000000e-03 1.746461932925168e+20 -9.200000000000000e-02 7.500000000000000e-03 1.624953588818316e+20 -9.200000000000000e-02 9.000000000000001e-03 1.487229733625696e+20 -9.200000000000000e-02 1.050000000000000e-02 1.338374366816513e+20 -9.200000000000000e-02 1.200000000000000e-02 1.183600780010604e+20 -9.200000000000000e-02 1.350000000000000e-02 1.027960631216390e+20 -9.200000000000000e-02 1.500000000000000e-02 8.760837834248464e+19 -9.200000000000000e-02 1.650000000000000e-02 7.319658364968392e+19 -9.200000000000000e-02 1.800000000000000e-02 5.988151723754023e+19 -9.200000000000000e-02 1.950000000000000e-02 4.789656690939196e+19 -9.200000000000000e-02 2.100000000000000e-02 3.738555123580255e+19 -9.200000000000000e-02 2.250000000000000e-02 2.840671896815838e+19 -9.200000000000000e-02 2.400000000000000e-02 2.094191888874471e+19 -9.200000000000000e-02 2.550000000000000e-02 1.490964857058776e+19 -9.200000000000000e-02 2.700000000000000e-02 1.018048647101734e+19 -9.200000000000000e-02 2.850000000000000e-02 6.593362990488771e+18 -9.200000000000000e-02 3.000000000000000e-02 3.971232424812212e+18 -9.200000000000000e-02 3.150000000000000e-02 2.134950487242480e+18 -9.200000000000000e-02 3.300000000000000e-02 9.145048243520297e+17 -9.200000000000000e-02 3.450000000000000e-02 1.571391558322260e+17 -9.200000000000000e-02 3.600000000000000e-02 -2.676991859094810e+17 -9.200000000000000e-02 3.750000000000000e-02 -4.663233710113622e+17 -9.200000000000000e-02 3.900000000000000e-02 -5.211734242351567e+17 -9.200000000000000e-02 4.050000000000000e-02 -4.929397151066589e+17 -9.200000000000000e-02 4.200000000000000e-02 -4.237699786949048e+17 -9.200000000000000e-02 4.350000000000000e-02 -3.409467224134415e+17 -9.200000000000000e-02 4.500000000000000e-02 -2.605426378541263e+17 -9.200000000000000e-02 4.650000000000000e-02 -1.907107773291836e+17 -9.200000000000000e-02 4.800000000000000e-02 -1.344150624400529e+17 -9.200000000000000e-02 4.950000000000000e-02 -9.153406609932133e+16 -9.200000000000000e-02 5.100000000000000e-02 -6.036525891806471e+16 -9.200000000000000e-02 5.250000000000000e-02 -3.861519662631506e+16 -9.200000000000000e-02 5.400000000000000e-02 -2.398729891755344e+16 -9.200000000000000e-02 5.550000000000000e-02 -1.448064366905725e+16 -9.200000000000000e-02 5.700000000000000e-02 -8.499465939082445e+15 -9.200000000000000e-02 5.850000000000000e-02 -4.851880064862024e+15 -9.200000000000000e-02 6.000000000000000e-02 -2.693860653894162e+15 -9.200000000000000e-02 6.150000000000000e-02 -1.454575906471547e+15 -9.200000000000000e-02 6.300000000000000e-02 -7.635830626464812e+14 -9.200000000000000e-02 6.450000000000000e-02 -3.894907067404343e+14 -9.200000000000000e-02 6.600000000000000e-02 -1.928843270558431e+14 -9.200000000000000e-02 6.750000000000000e-02 -9.262531679603652e+13 -9.200000000000000e-02 6.900000000000001e-02 -4.305656782975014e+13 -9.200000000000000e-02 7.050000000000001e-02 -1.932548260886433e+13 -9.200000000000000e-02 7.200000000000001e-02 -8.344025453305784e+12 -9.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -9.000000000000001e-02 0.000000000000000e+00 1.989460076636346e+20 -9.000000000000001e-02 1.500000000000000e-03 1.970990304960715e+20 -9.000000000000001e-02 3.000000000000000e-03 1.922933439973766e+20 -9.000000000000001e-02 4.500000000000001e-03 1.847100796709063e+20 -9.000000000000001e-02 6.000000000000000e-03 1.746461931781805e+20 -9.000000000000001e-02 7.500000000000000e-03 1.624953587396285e+20 -9.000000000000001e-02 9.000000000000001e-03 1.487229731897222e+20 -9.000000000000001e-02 1.050000000000000e-02 1.338374364763244e+20 -9.000000000000001e-02 1.200000000000000e-02 1.183600777626872e+20 -9.000000000000001e-02 1.350000000000000e-02 1.027960628511820e+20 -9.000000000000001e-02 1.500000000000000e-02 8.760837804259049e+19 -9.000000000000001e-02 1.650000000000000e-02 7.319658332469643e+19 -9.000000000000001e-02 1.800000000000000e-02 5.988151689335339e+19 -9.000000000000001e-02 1.950000000000000e-02 4.789656655314528e+19 -9.000000000000001e-02 2.100000000000000e-02 3.738555087544273e+19 -9.000000000000001e-02 2.250000000000000e-02 2.840671861191170e+19 -9.000000000000001e-02 2.400000000000000e-02 2.094191854455787e+19 -9.000000000000001e-02 2.550000000000000e-02 1.490964824560027e+19 -9.000000000000001e-02 2.700000000000000e-02 1.018048617112320e+19 -9.000000000000001e-02 2.850000000000000e-02 6.593362720031744e+18 -9.000000000000001e-02 3.000000000000000e-02 3.971232186438965e+18 -9.000000000000001e-02 3.150000000000000e-02 2.134950281915648e+18 -9.000000000000001e-02 3.300000000000000e-02 9.145046515046275e+17 -9.000000000000001e-02 3.450000000000000e-02 1.571390136291602e+17 -9.000000000000001e-02 3.600000000000000e-02 -2.676993002457496e+17 -9.000000000000001e-02 3.750000000000000e-02 -4.663234608551438e+17 -9.000000000000001e-02 3.900000000000000e-02 -5.211734932306916e+17 -9.000000000000001e-02 4.050000000000000e-02 -4.929397668891455e+17 -9.000000000000001e-02 4.200000000000000e-02 -4.237700166765497e+17 -9.000000000000001e-02 4.350000000000000e-02 -3.409467496400528e+17 -9.000000000000001e-02 4.500000000000000e-02 -2.605426569281522e+17 -9.000000000000001e-02 4.650000000000000e-02 -1.907107903884895e+17 -9.000000000000001e-02 4.800000000000000e-02 -1.344150711783494e+17 -9.000000000000001e-02 4.950000000000000e-02 -9.153407181361309e+16 -9.000000000000001e-02 5.100000000000000e-02 -6.036526257003300e+16 -9.000000000000001e-02 5.250000000000000e-02 -3.861519890729014e+16 -9.000000000000001e-02 5.400000000000000e-02 -2.398730030988618e+16 -9.000000000000001e-02 5.550000000000000e-02 -1.448064449966214e+16 -9.000000000000001e-02 5.700000000000000e-02 -8.499466423338302e+15 -9.000000000000001e-02 5.850000000000000e-02 -4.851880340782694e+15 -9.000000000000001e-02 6.000000000000000e-02 -2.693860807540616e+15 -9.000000000000001e-02 6.150000000000000e-02 -1.454575990087627e+15 -9.000000000000001e-02 6.300000000000000e-02 -7.635831071184152e+14 -9.000000000000001e-02 6.450000000000000e-02 -3.894907298563543e+14 -9.000000000000001e-02 6.600000000000000e-02 -1.928843387984711e+14 -9.000000000000001e-02 6.750000000000000e-02 -9.262532262576566e+13 -9.000000000000001e-02 6.900000000000001e-02 -4.305657065827762e+13 -9.000000000000001e-02 7.050000000000001e-02 -1.932548395008854e+13 -9.000000000000001e-02 7.200000000000001e-02 -8.344026074848979e+12 -9.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -8.800000000000001e-02 0.000000000000000e+00 1.989460075996939e+20 -8.800000000000001e-02 1.500000000000000e-03 1.970990304088977e+20 -8.800000000000001e-02 3.000000000000000e-03 1.922933438812252e+20 -8.800000000000001e-02 4.500000000000001e-03 1.847100795196577e+20 -8.800000000000001e-02 6.000000000000000e-03 1.746461929856998e+20 -8.800000000000001e-02 7.500000000000000e-03 1.624953585002351e+20 -8.800000000000001e-02 9.000000000000001e-03 1.487229728987403e+20 -8.800000000000001e-02 1.050000000000000e-02 1.338374361306646e+20 -8.800000000000001e-02 1.200000000000000e-02 1.183600773613950e+20 -8.800000000000001e-02 1.350000000000000e-02 1.027960623958780e+20 -8.800000000000001e-02 1.500000000000000e-02 8.760837753773028e+19 -8.800000000000001e-02 1.650000000000000e-02 7.319658277759254e+19 -8.800000000000001e-02 1.800000000000000e-02 5.988151631392813e+19 -8.800000000000001e-02 1.950000000000000e-02 4.789656595341774e+19 -8.800000000000001e-02 2.100000000000000e-02 3.738555026879090e+19 -8.800000000000001e-02 2.250000000000000e-02 2.840671801218415e+19 -8.800000000000001e-02 2.400000000000000e-02 2.094191796513261e+19 -8.800000000000001e-02 2.550000000000000e-02 1.490964769849638e+19 -8.800000000000001e-02 2.700000000000000e-02 1.018048566626299e+19 -8.800000000000001e-02 2.850000000000000e-02 6.593362264727779e+18 -8.800000000000001e-02 3.000000000000000e-02 3.971231785146806e+18 -8.800000000000001e-02 3.150000000000000e-02 2.134949936255851e+18 -8.800000000000001e-02 3.300000000000000e-02 9.145043605226981e+17 -8.800000000000001e-02 3.450000000000000e-02 1.571387742357886e+17 -8.800000000000001e-02 3.600000000000000e-02 -2.676994927264442e+17 -8.800000000000001e-02 3.750000000000000e-02 -4.663236121036820e+17 -8.800000000000001e-02 3.900000000000000e-02 -5.211736093820111e+17 -8.800000000000001e-02 4.050000000000000e-02 -4.929398540629627e+17 -8.800000000000001e-02 4.200000000000000e-02 -4.237700806171827e+17 -8.800000000000001e-02 4.350000000000000e-02 -3.409467954750019e+17 -8.800000000000001e-02 4.500000000000000e-02 -2.605426890385383e+17 -8.800000000000001e-02 4.650000000000000e-02 -1.907108123733268e+17 -8.800000000000001e-02 4.800000000000000e-02 -1.344150858889342e+17 -8.800000000000001e-02 4.950000000000000e-02 -9.153408143340267e+16 -8.800000000000001e-02 5.100000000000000e-02 -6.036526871798065e+16 -8.800000000000001e-02 5.250000000000000e-02 -3.861520274722362e+16 -8.800000000000001e-02 5.400000000000000e-02 -2.398730265382458e+16 -8.800000000000001e-02 5.550000000000000e-02 -1.448064589795340e+16 -8.800000000000001e-02 5.700000000000000e-02 -8.499467238564342e+15 -8.800000000000001e-02 5.850000000000000e-02 -4.851880805284490e+15 -8.800000000000001e-02 6.000000000000000e-02 -2.693861066198491e+15 -8.800000000000001e-02 6.150000000000000e-02 -1.454576130852070e+15 -8.800000000000001e-02 6.300000000000000e-02 -7.635831819851995e+14 -8.800000000000001e-02 6.450000000000000e-02 -3.894907687711134e+14 -8.800000000000001e-02 6.600000000000000e-02 -1.928843585667321e+14 -8.800000000000001e-02 6.750000000000000e-02 -9.262533243988961e+13 -8.800000000000001e-02 6.900000000000001e-02 -4.305657541999445e+13 -8.800000000000001e-02 7.050000000000001e-02 -1.932548620798771e+13 -8.800000000000001e-02 7.200000000000001e-02 -8.344027121192955e+12 -8.800000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -8.600000000000001e-02 0.000000000000000e+00 1.989460074930339e+20 -8.600000000000001e-02 1.500000000000000e-03 1.970990302634821e+20 -8.600000000000001e-02 3.000000000000000e-03 1.922933436874720e+20 -8.600000000000001e-02 4.500000000000001e-03 1.847100792673584e+20 -8.600000000000001e-02 6.000000000000000e-03 1.746461926646207e+20 -8.600000000000001e-02 7.500000000000000e-03 1.624953581009004e+20 -8.600000000000001e-02 9.000000000000001e-03 1.487229724133502e+20 -8.600000000000001e-02 1.050000000000000e-02 1.338374355540657e+20 -8.600000000000001e-02 1.200000000000000e-02 1.183600766919952e+20 -8.600000000000001e-02 1.350000000000000e-02 1.027960616363805e+20 -8.600000000000001e-02 1.500000000000000e-02 8.760837669556745e+19 -8.600000000000001e-02 1.650000000000000e-02 7.319658186496255e+19 -8.600000000000001e-02 1.800000000000000e-02 5.988151534738252e+19 -8.600000000000001e-02 1.950000000000000e-02 4.789656495300566e+19 -8.600000000000001e-02 2.100000000000000e-02 3.738554925682833e+19 -8.600000000000001e-02 2.250000000000000e-02 2.840671701177208e+19 -8.600000000000001e-02 2.400000000000000e-02 2.094191699858699e+19 -8.600000000000001e-02 2.550000000000000e-02 1.490964678586639e+19 -8.600000000000001e-02 2.700000000000000e-02 1.018048482410016e+19 -8.600000000000001e-02 2.850000000000000e-02 6.593361505230254e+18 -8.600000000000001e-02 3.000000000000000e-02 3.971231115746964e+18 -8.600000000000001e-02 3.150000000000000e-02 2.134949359656962e+18 -8.600000000000001e-02 3.300000000000000e-02 9.145038751325571e+17 -8.600000000000001e-02 3.450000000000000e-02 1.571383749010852e+17 -8.600000000000001e-02 3.600000000000000e-02 -2.676998138055974e+17 -8.600000000000001e-02 3.750000000000000e-02 -4.663238644030239e+17 -8.600000000000001e-02 3.900000000000000e-02 -5.211738031352985e+17 -8.600000000000001e-02 4.050000000000000e-02 -4.929399994785612e+17 -8.600000000000001e-02 4.200000000000000e-02 -4.237701872772525e+17 -8.600000000000001e-02 4.350000000000000e-02 -3.409468719327821e+17 -8.600000000000001e-02 4.500000000000000e-02 -2.605427426022249e+17 -8.600000000000001e-02 4.650000000000000e-02 -1.907108490464746e+17 -8.600000000000001e-02 4.800000000000000e-02 -1.344151104278217e+17 -8.600000000000001e-02 4.950000000000000e-02 -9.153409748027896e+16 -8.600000000000001e-02 5.100000000000000e-02 -6.036527897343940e+16 -8.600000000000001e-02 5.250000000000000e-02 -3.861520915265869e+16 -8.600000000000001e-02 5.400000000000000e-02 -2.398730656377390e+16 -8.600000000000001e-02 5.550000000000000e-02 -1.448064823045835e+16 -8.600000000000001e-02 5.700000000000000e-02 -8.499468598451823e+15 -8.600000000000001e-02 5.850000000000000e-02 -4.851881580125020e+15 -8.600000000000001e-02 6.000000000000000e-02 -2.693861497668523e+15 -8.600000000000001e-02 6.150000000000000e-02 -1.454576365662777e+15 -8.600000000000001e-02 6.300000000000000e-02 -7.635833068713015e+14 -8.600000000000001e-02 6.450000000000000e-02 -3.894908336852489e+14 -8.600000000000001e-02 6.600000000000000e-02 -1.928843915423846e+14 -8.600000000000001e-02 6.750000000000000e-02 -9.262534881093720e+13 -8.600000000000001e-02 6.900000000000001e-02 -4.305658336306642e+13 -8.600000000000001e-02 7.050000000000001e-02 -1.932548997441404e+13 -8.600000000000001e-02 7.200000000000001e-02 -8.344028866610792e+12 -8.600000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -8.400000000000001e-02 0.000000000000000e+00 1.989460073167371e+20 -8.400000000000001e-02 1.500000000000000e-03 1.970990300231269e+20 -8.400000000000001e-02 3.000000000000000e-03 1.922933433672201e+20 -8.400000000000001e-02 4.500000000000001e-03 1.847100788503366e+20 -8.400000000000001e-02 6.000000000000000e-03 1.746461921339138e+20 -8.400000000000001e-02 7.500000000000000e-03 1.624953574408462e+20 -8.400000000000001e-02 9.000000000000001e-03 1.487229716110562e+20 -8.400000000000001e-02 1.050000000000000e-02 1.338374346010142e+20 -8.400000000000001e-02 1.200000000000000e-02 1.183600755855544e+20 -8.400000000000001e-02 1.350000000000000e-02 1.027960603810186e+20 -8.400000000000001e-02 1.500000000000000e-02 8.760837530356933e+19 -8.400000000000001e-02 1.650000000000000e-02 7.319658035649033e+19 -8.400000000000001e-02 1.800000000000000e-02 5.988151374979399e+19 -8.400000000000001e-02 1.950000000000000e-02 4.789656329943979e+19 -8.400000000000001e-02 2.100000000000000e-02 3.738554758417082e+19 -8.400000000000001e-02 2.250000000000000e-02 2.840671535820620e+19 -8.400000000000001e-02 2.400000000000000e-02 2.094191540099847e+19 -8.400000000000001e-02 2.550000000000000e-02 1.490964527739417e+19 -8.400000000000001e-02 2.700000000000000e-02 1.018048343210203e+19 -8.400000000000001e-02 2.850000000000000e-02 6.593360249868363e+18 -8.400000000000001e-02 3.000000000000000e-02 3.971230009306160e+18 -8.400000000000001e-02 3.150000000000000e-02 2.134948406605439e+18 -8.400000000000001e-02 3.300000000000000e-02 9.145030728385857e+17 -8.400000000000001e-02 3.450000000000000e-02 1.571377148468361e+17 -8.400000000000001e-02 3.600000000000000e-02 -2.677003445124395e+17 -8.400000000000001e-02 3.750000000000000e-02 -4.663242814247636e+17 -8.400000000000001e-02 3.900000000000000e-02 -5.211741233871562e+17 -8.400000000000001e-02 4.050000000000000e-02 -4.929402398337891e+17 -8.400000000000001e-02 4.200000000000000e-02 -4.237703635740574e+17 -8.400000000000001e-02 4.350000000000000e-02 -3.409469983086826e+17 -8.400000000000001e-02 4.500000000000000e-02 -2.605428311368267e+17 -8.400000000000001e-02 4.650000000000000e-02 -1.907109096629620e+17 -8.400000000000001e-02 4.800000000000000e-02 -1.344151509877751e+17 -8.400000000000001e-02 4.950000000000000e-02 -9.153412400391635e+16 -8.400000000000001e-02 5.100000000000000e-02 -6.036529592453097e+16 -8.400000000000001e-02 5.250000000000000e-02 -3.861521974010476e+16 -8.400000000000001e-02 5.400000000000000e-02 -2.398731302646957e+16 -8.400000000000001e-02 5.550000000000000e-02 -1.448065208582027e+16 -8.400000000000001e-02 5.700000000000000e-02 -8.499470846189128e+15 -8.400000000000001e-02 5.850000000000000e-02 -4.851882860847131e+15 -8.400000000000001e-02 6.000000000000000e-02 -2.693862210838767e+15 -8.400000000000001e-02 6.150000000000000e-02 -1.454576753777820e+15 -8.400000000000001e-02 6.300000000000000e-02 -7.635835132936376e+14 -8.400000000000001e-02 6.450000000000000e-02 -3.894909409808347e+14 -8.400000000000001e-02 6.600000000000000e-02 -1.928844460473383e+14 -8.400000000000001e-02 6.750000000000000e-02 -9.262537587039241e+13 -8.400000000000001e-02 6.900000000000001e-02 -4.305659649204909e+13 -8.400000000000001e-02 7.050000000000001e-02 -1.932549619988276e+13 -8.400000000000001e-02 7.200000000000001e-02 -8.344031751585352e+12 -8.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -8.200000000000000e-02 0.000000000000000e+00 1.989460070280015e+20 -8.200000000000000e-02 1.500000000000000e-03 1.970990296294776e+20 -8.200000000000000e-02 3.000000000000000e-03 1.922933428427176e+20 -8.200000000000000e-02 4.500000000000001e-03 1.847100781673462e+20 -8.200000000000000e-02 6.000000000000000e-03 1.746461912647321e+20 -8.200000000000000e-02 7.500000000000000e-03 1.624953563598218e+20 -8.200000000000000e-02 9.000000000000001e-03 1.487229702970742e+20 -8.200000000000000e-02 1.050000000000000e-02 1.338374330401243e+20 -8.200000000000000e-02 1.200000000000000e-02 1.183600737734464e+20 -8.200000000000000e-02 1.350000000000000e-02 1.027960583250104e+20 -8.200000000000000e-02 1.500000000000000e-02 8.760837302378095e+19 -8.200000000000000e-02 1.650000000000000e-02 7.319657788594288e+19 -8.200000000000000e-02 1.800000000000000e-02 5.988151113329352e+19 -8.200000000000000e-02 1.950000000000000e-02 4.789656059126066e+19 -8.200000000000000e-02 2.100000000000000e-02 3.738554484472377e+19 -8.200000000000000e-02 2.250000000000000e-02 2.840671265002707e+19 -8.200000000000000e-02 2.400000000000000e-02 2.094191278449800e+19 -8.200000000000000e-02 2.550000000000000e-02 1.490964280684672e+19 -8.200000000000000e-02 2.700000000000000e-02 1.018048115231365e+19 -8.200000000000000e-02 2.850000000000000e-02 6.593358193860242e+18 -8.200000000000000e-02 3.000000000000000e-02 3.971228197198199e+18 -8.200000000000000e-02 3.150000000000000e-02 2.134946845715561e+18 -8.200000000000000e-02 3.300000000000000e-02 9.145017588565935e+17 -8.200000000000000e-02 3.450000000000000e-02 1.571366338223884e+17 -8.200000000000000e-02 3.600000000000000e-02 -2.677012136941343e+17 -8.200000000000000e-02 3.750000000000000e-02 -4.663249644151334e+17 -8.200000000000000e-02 3.900000000000000e-02 -5.211746478896317e+17 -8.200000000000000e-02 4.050000000000000e-02 -4.929406334830656e+17 -8.200000000000000e-02 4.200000000000000e-02 -4.237706523096521e+17 -8.200000000000000e-02 4.350000000000000e-02 -3.409472052847580e+17 -8.200000000000000e-02 4.500000000000000e-02 -2.605429761371340e+17 -8.200000000000000e-02 4.650000000000000e-02 -1.907110089395061e+17 -8.200000000000000e-02 4.800000000000000e-02 -1.344152174161048e+17 -8.200000000000000e-02 4.950000000000000e-02 -9.153416744383136e+16 -8.200000000000000e-02 5.100000000000000e-02 -6.036532368671026e+16 -8.200000000000000e-02 5.250000000000000e-02 -3.861523708002501e+16 -8.200000000000000e-02 5.400000000000000e-02 -2.398732361095111e+16 -8.200000000000000e-02 5.550000000000000e-02 -1.448065840005957e+16 -8.200000000000000e-02 5.700000000000000e-02 -8.499474527491055e+15 -8.200000000000000e-02 5.850000000000000e-02 -4.851884958389742e+15 -8.200000000000000e-02 6.000000000000000e-02 -2.693863378855593e+15 -8.200000000000000e-02 6.150000000000000e-02 -1.454577389425343e+15 -8.200000000000000e-02 6.300000000000000e-02 -7.635838513682611e+14 -8.200000000000000e-02 6.450000000000000e-02 -3.894911167075292e+14 -8.200000000000000e-02 6.600000000000000e-02 -1.928845353145275e+14 -8.200000000000000e-02 6.750000000000000e-02 -9.262542018785975e+13 -8.200000000000000e-02 6.900000000000001e-02 -4.305661799445024e+13 -8.200000000000000e-02 7.050000000000001e-02 -1.932550639583845e+13 -8.200000000000000e-02 7.200000000000001e-02 -8.344036476542480e+12 -8.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -8.000000000000000e-02 0.000000000000000e+00 1.989460065594417e+20 -8.000000000000000e-02 1.500000000000000e-03 1.970990289906641e+20 -8.000000000000000e-02 3.000000000000000e-03 1.922933419915558e+20 -8.000000000000000e-02 4.500000000000001e-03 1.847100770589904e+20 -8.000000000000000e-02 6.000000000000000e-03 1.746461898542253e+20 -8.000000000000000e-02 7.500000000000000e-03 1.624953546055368e+20 -8.000000000000000e-02 9.000000000000001e-03 1.487229681647461e+20 -8.000000000000000e-02 1.050000000000000e-02 1.338374305071144e+20 -8.000000000000000e-02 1.200000000000000e-02 1.183600708327602e+20 -8.000000000000000e-02 1.350000000000000e-02 1.027960549885234e+20 -8.000000000000000e-02 1.500000000000000e-02 8.760836932414358e+19 -8.000000000000000e-02 1.650000000000000e-02 7.319657387674196e+19 -8.000000000000000e-02 1.800000000000000e-02 5.988150688724025e+19 -8.000000000000000e-02 1.950000000000000e-02 4.789655619643138e+19 -8.000000000000000e-02 2.100000000000000e-02 3.738554039915296e+19 -8.000000000000000e-02 2.250000000000000e-02 2.840670825519780e+19 -8.000000000000000e-02 2.400000000000000e-02 2.094190853844473e+19 -8.000000000000000e-02 2.550000000000000e-02 1.490963879764580e+19 -8.000000000000000e-02 2.700000000000000e-02 1.018047745267627e+19 -8.000000000000000e-02 2.850000000000000e-02 6.593354857373165e+18 -8.000000000000000e-02 3.000000000000000e-02 3.971225256511955e+18 -8.000000000000000e-02 3.150000000000000e-02 2.134944312705669e+18 -8.000000000000000e-02 3.300000000000000e-02 9.144996265284696e+17 -8.000000000000000e-02 3.450000000000000e-02 1.571348795374392e+17 -8.000000000000000e-02 3.600000000000000e-02 -2.677026242009628e+17 -8.000000000000000e-02 3.750000000000000e-02 -4.663260727709425e+17 -8.000000000000000e-02 3.900000000000000e-02 -5.211754990515091e+17 -8.000000000000000e-02 4.050000000000000e-02 -4.929412722965562e+17 -8.000000000000000e-02 4.200000000000000e-02 -4.237711208693679e+17 -8.000000000000000e-02 4.350000000000000e-02 -3.409475411652413e+17 -8.000000000000000e-02 4.500000000000000e-02 -2.605432114434282e+17 -8.000000000000000e-02 4.650000000000000e-02 -1.907111700453420e+17 -8.000000000000000e-02 4.800000000000000e-02 -1.344153252159044e+17 -8.000000000000000e-02 4.950000000000000e-02 -9.153423793806416e+16 -8.000000000000000e-02 5.100000000000000e-02 -6.036536873913566e+16 -8.000000000000000e-02 5.250000000000000e-02 -3.861526521922313e+16 -8.000000000000000e-02 5.400000000000000e-02 -2.398734078743283e+16 -8.000000000000000e-02 5.550000000000000e-02 -1.448066864679822e+16 -8.000000000000000e-02 5.700000000000000e-02 -8.499480501502630e+15 -8.000000000000000e-02 5.850000000000000e-02 -4.851888362278932e+15 -8.000000000000000e-02 6.000000000000000e-02 -2.693865274311652e+15 -8.000000000000000e-02 6.150000000000000e-02 -1.454578420953249e+15 -8.000000000000000e-02 6.300000000000000e-02 -7.635843999952835e+14 -8.000000000000000e-02 6.450000000000000e-02 -3.894914018765614e+14 -8.000000000000000e-02 6.600000000000000e-02 -1.928846801771962e+14 -8.000000000000000e-02 6.750000000000000e-02 -9.262549210618323e+13 -8.000000000000000e-02 6.900000000000001e-02 -4.305665288851650e+13 -8.000000000000000e-02 7.050000000000001e-02 -1.932552294182096e+13 -8.000000000000000e-02 7.200000000000001e-02 -8.344044144196246e+12 -8.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -7.800000000000001e-02 0.000000000000000e+00 1.989460058060281e+20 -7.800000000000001e-02 1.500000000000000e-03 1.970990279634934e+20 -7.800000000000001e-02 3.000000000000000e-03 1.922933406229426e+20 -7.800000000000001e-02 4.500000000000001e-03 1.847100752768261e+20 -7.800000000000001e-02 6.000000000000000e-03 1.746461875862217e+20 -7.800000000000001e-02 7.500000000000000e-03 1.624953517847603e+20 -7.800000000000001e-02 9.000000000000001e-03 1.487229647361006e+20 -7.800000000000001e-02 1.050000000000000e-02 1.338374264341987e+20 -7.800000000000001e-02 1.200000000000000e-02 1.183600661043273e+20 -7.800000000000001e-02 1.350000000000000e-02 1.027960496236684e+20 -7.800000000000001e-02 1.500000000000000e-02 8.760836337536642e+19 -7.800000000000001e-02 1.650000000000000e-02 7.319656743020669e+19 -7.800000000000001e-02 1.800000000000000e-02 5.988150005986175e+19 -7.800000000000001e-02 1.950000000000000e-02 4.789654912983071e+19 -7.800000000000001e-02 2.100000000000000e-02 3.738553325096319e+19 -7.800000000000001e-02 2.250000000000000e-02 2.840670118859713e+19 -7.800000000000001e-02 2.400000000000000e-02 2.094190171106623e+19 -7.800000000000001e-02 2.550000000000000e-02 1.490963235111053e+19 -7.800000000000001e-02 2.700000000000000e-02 1.018047150389913e+19 -7.800000000000001e-02 2.850000000000000e-02 6.593349492518157e+18 -7.800000000000001e-02 3.000000000000000e-02 3.971220528079042e+18 -7.800000000000001e-02 3.150000000000000e-02 2.134940239789909e+18 -7.800000000000001e-02 3.300000000000000e-02 9.144961978830275e+17 -7.800000000000001e-02 3.450000000000000e-02 1.571320587609237e+17 -7.800000000000001e-02 3.600000000000000e-02 -2.677048922045380e+17 -7.800000000000001e-02 3.750000000000000e-02 -4.663278549352587e+17 -7.800000000000001e-02 3.900000000000000e-02 -5.211768676646504e+17 -7.800000000000001e-02 4.050000000000000e-02 -4.929422994672522e+17 -7.800000000000001e-02 4.200000000000000e-02 -4.237718742830269e+17 -7.800000000000001e-02 4.350000000000000e-02 -3.409480812392922e+17 -7.800000000000001e-02 4.500000000000000e-02 -2.605435898007007e+17 -7.800000000000001e-02 4.650000000000000e-02 -1.907114290930859e+17 -7.800000000000001e-02 4.800000000000000e-02 -1.344154985509966e+17 -7.800000000000001e-02 4.950000000000000e-02 -9.153435128822227e+16 -7.800000000000001e-02 5.100000000000000e-02 -6.036544118051618e+16 -7.800000000000001e-02 5.250000000000000e-02 -3.861531046523021e+16 -7.800000000000001e-02 5.400000000000000e-02 -2.398736840610235e+16 -7.800000000000001e-02 5.550000000000000e-02 -1.448068512288993e+16 -7.800000000000001e-02 5.700000000000000e-02 -8.499490107326108e+15 -7.800000000000001e-02 5.850000000000000e-02 -4.851893835512167e+15 -7.800000000000001e-02 6.000000000000000e-02 -2.693868322082163e+15 -7.800000000000001e-02 6.150000000000000e-02 -1.454580079583274e+15 -7.800000000000001e-02 6.300000000000000e-02 -7.635852821519829e+14 -7.800000000000001e-02 6.450000000000000e-02 -3.894918604098852e+14 -7.800000000000001e-02 6.600000000000000e-02 -1.928849131069799e+14 -7.800000000000001e-02 6.750000000000000e-02 -9.262560774618689e+13 -7.800000000000001e-02 6.900000000000001e-02 -4.305670899591380e+13 -7.800000000000001e-02 7.050000000000001e-02 -1.932554954668862e+13 -7.800000000000001e-02 7.200000000000001e-02 -8.344056473286615e+12 -7.800000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -7.600000000000001e-02 0.000000000000000e+00 1.989460046056975e+20 -7.600000000000001e-02 1.500000000000000e-03 1.970990263270160e+20 -7.600000000000001e-02 3.000000000000000e-03 1.922933384424828e+20 -7.600000000000001e-02 4.500000000000001e-03 1.847100724375010e+20 -7.600000000000001e-02 6.000000000000000e-03 1.746461839728627e+20 -7.600000000000001e-02 7.500000000000000e-03 1.624953472907293e+20 -7.600000000000001e-02 9.000000000000001e-03 1.487229592736194e+20 -7.600000000000001e-02 1.050000000000000e-02 1.338374199452729e+20 -7.600000000000001e-02 1.200000000000000e-02 1.183600585710386e+20 -7.600000000000001e-02 1.350000000000000e-02 1.027960410764388e+20 -7.600000000000001e-02 1.500000000000000e-02 8.760835389783835e+19 -7.600000000000001e-02 1.650000000000000e-02 7.319655715965569e+19 -7.600000000000001e-02 1.800000000000000e-02 5.988148918255541e+19 -7.600000000000001e-02 1.950000000000000e-02 4.789653787139816e+19 -7.600000000000001e-02 2.100000000000000e-02 3.738552186254375e+19 -7.600000000000001e-02 2.250000000000000e-02 2.840668993016458e+19 -7.600000000000001e-02 2.400000000000000e-02 2.094189083375988e+19 -7.600000000000001e-02 2.550000000000000e-02 1.490962208055953e+19 -7.600000000000001e-02 2.700000000000000e-02 1.018046202637106e+19 -7.600000000000001e-02 2.850000000000000e-02 6.593340945288584e+18 -7.600000000000001e-02 3.000000000000000e-02 3.971212994790334e+18 -7.600000000000001e-02 3.150000000000000e-02 2.134933750864115e+18 -7.600000000000001e-02 3.300000000000000e-02 9.144907354018079e+17 -7.600000000000001e-02 3.450000000000000e-02 1.571275647299719e+17 -7.600000000000001e-02 3.600000000000000e-02 -2.677085055635581e+17 -7.600000000000001e-02 3.750000000000000e-02 -4.663306942603716e+17 -7.600000000000001e-02 3.900000000000000e-02 -5.211790481244578e+17 -7.600000000000001e-02 4.050000000000000e-02 -4.929439359446106e+17 -7.600000000000001e-02 4.200000000000000e-02 -4.237730746136041e+17 -7.600000000000001e-02 4.350000000000000e-02 -3.409489416794895e+17 -7.600000000000001e-02 4.500000000000000e-02 -2.605441925954575e+17 -7.600000000000001e-02 4.650000000000000e-02 -1.907118418051787e+17 -7.600000000000001e-02 4.800000000000000e-02 -1.344157747066100e+17 -7.600000000000001e-02 4.950000000000000e-02 -9.153453187648091e+16 -7.600000000000001e-02 5.100000000000000e-02 -6.036555659334823e+16 -7.600000000000001e-02 5.250000000000000e-02 -3.861538255068438e+16 -7.600000000000001e-02 5.400000000000000e-02 -2.398741240787101e+16 -7.600000000000001e-02 5.550000000000000e-02 -1.448071137242290e+16 -7.600000000000001e-02 5.700000000000000e-02 -8.499505411221258e+15 -7.600000000000001e-02 5.850000000000000e-02 -4.851902555408775e+15 -7.600000000000001e-02 6.000000000000000e-02 -2.693873177757518e+15 -7.600000000000001e-02 6.150000000000000e-02 -1.454582722094878e+15 -7.600000000000001e-02 6.300000000000000e-02 -7.635866875945940e+14 -7.600000000000001e-02 6.450000000000000e-02 -3.894925909402687e+14 -7.600000000000001e-02 6.600000000000000e-02 -1.928852842082182e+14 -7.600000000000001e-02 6.750000000000000e-02 -9.262579198260295e+13 -7.600000000000001e-02 6.900000000000001e-02 -4.305679838561862e+13 -7.600000000000001e-02 7.050000000000001e-02 -1.932559193327900e+13 -7.600000000000001e-02 7.200000000000001e-02 -8.344076115861424e+12 -7.600000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -7.400000000000001e-02 0.000000000000000e+00 1.989460027109047e+20 -7.400000000000001e-02 1.500000000000000e-03 1.970990237437398e+20 -7.400000000000001e-02 3.000000000000000e-03 1.922933350004981e+20 -7.400000000000001e-02 4.500000000000001e-03 1.847100679554585e+20 -7.400000000000001e-02 6.000000000000000e-03 1.746461782689619e+20 -7.400000000000001e-02 7.500000000000000e-03 1.624953401966358e+20 -7.400000000000001e-02 9.000000000000001e-03 1.487229506507699e+20 -7.400000000000001e-02 1.050000000000000e-02 1.338374097021199e+20 -7.400000000000001e-02 1.200000000000000e-02 1.183600466792970e+20 -7.400000000000001e-02 1.350000000000000e-02 1.027960275841316e+20 -7.400000000000001e-02 1.500000000000000e-02 8.760833893700000e+19 -7.400000000000001e-02 1.650000000000000e-02 7.319654094698378e+19 -7.400000000000001e-02 1.800000000000000e-02 5.988147201208430e+19 -7.400000000000001e-02 1.950000000000000e-02 4.789652009929680e+19 -7.400000000000001e-02 2.100000000000000e-02 3.738550388525043e+19 -7.400000000000001e-02 2.250000000000000e-02 2.840667215806322e+19 -7.400000000000001e-02 2.400000000000000e-02 2.094187366328877e+19 -7.400000000000001e-02 2.550000000000000e-02 1.490960586788762e+19 -7.400000000000001e-02 2.700000000000000e-02 1.018044706553271e+19 -7.400000000000001e-02 2.850000000000000e-02 6.593327452981412e+18 -7.400000000000001e-02 3.000000000000000e-02 3.971201103048762e+18 -7.400000000000001e-02 3.150000000000000e-02 2.134923507711141e+18 -7.400000000000001e-02 3.300000000000000e-02 9.144821125522755e+17 -7.400000000000001e-02 3.450000000000000e-02 1.571204706364391e+17 -7.400000000000001e-02 3.600000000000000e-02 -2.677142094643837e+17 -7.400000000000001e-02 3.750000000000000e-02 -4.663351763029158e+17 -7.400000000000001e-02 3.900000000000000e-02 -5.211824901091668e+17 -7.400000000000001e-02 4.050000000000000e-02 -4.929465192208651e+17 -7.400000000000001e-02 4.200000000000000e-02 -4.237749694063807e+17 -7.400000000000001e-02 4.350000000000000e-02 -3.409502999352079e+17 -7.400000000000001e-02 4.500000000000000e-02 -2.605451441426168e+17 -7.400000000000001e-02 4.650000000000000e-02 -1.907124932956156e+17 -7.400000000000001e-02 4.800000000000000e-02 -1.344162106345715e+17 -7.400000000000001e-02 4.950000000000000e-02 -9.153481694572307e+16 -7.400000000000001e-02 5.100000000000000e-02 -6.036573877932653e+16 -7.400000000000001e-02 5.250000000000000e-02 -3.861549634183531e+16 -7.400000000000001e-02 5.400000000000000e-02 -2.398748186726410e+16 -7.400000000000001e-02 5.550000000000000e-02 -1.448075280886250e+16 -7.400000000000001e-02 5.700000000000000e-02 -8.499529569324477e+15 -7.400000000000001e-02 5.850000000000000e-02 -4.851916320281067e+15 -7.400000000000001e-02 6.000000000000000e-02 -2.693880842728122e+15 -7.400000000000001e-02 6.150000000000000e-02 -1.454586893455663e+15 -7.400000000000001e-02 6.300000000000000e-02 -7.635889061688417e+14 -7.400000000000001e-02 6.450000000000000e-02 -3.894937441256662e+14 -7.400000000000001e-02 6.600000000000000e-02 -1.928858700134613e+14 -7.400000000000001e-02 6.750000000000000e-02 -9.262608281067727e+13 -7.400000000000001e-02 6.900000000000001e-02 -4.305693949255219e+13 -7.400000000000001e-02 7.050000000000001e-02 -1.932565884301771e+13 -7.400000000000001e-02 7.200000000000001e-02 -8.344107122826978e+12 -7.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -7.200000000000001e-02 0.000000000000000e+00 1.989459997473676e+20 -7.200000000000001e-02 1.500000000000000e-03 1.970990197033850e+20 -7.200000000000001e-02 3.000000000000000e-03 1.922933296170865e+20 -7.200000000000001e-02 4.500000000000001e-03 1.847100609453519e+20 -7.200000000000001e-02 6.000000000000000e-03 1.746461693478166e+20 -7.200000000000001e-02 7.500000000000000e-03 1.624953291011695e+20 -7.200000000000001e-02 9.000000000000001e-03 1.487229371642637e+20 -7.200000000000001e-02 1.050000000000000e-02 1.338373936813897e+20 -7.200000000000001e-02 1.200000000000000e-02 1.183600280801036e+20 -7.200000000000001e-02 1.350000000000000e-02 1.027960064815850e+20 -7.200000000000001e-02 1.500000000000000e-02 8.760831553760772e+19 -7.200000000000001e-02 1.650000000000000e-02 7.319651558967016e+19 -7.200000000000001e-02 1.800000000000000e-02 5.988144515673168e+19 -7.200000000000001e-02 1.950000000000000e-02 4.789649230296871e+19 -7.200000000000001e-02 2.100000000000000e-02 3.738547576799329e+19 -7.200000000000001e-02 2.250000000000000e-02 2.840664436173513e+19 -7.200000000000001e-02 2.400000000000000e-02 2.094184680793616e+19 -7.200000000000001e-02 2.550000000000000e-02 1.490958051057400e+19 -7.200000000000001e-02 2.700000000000000e-02 1.018042366614042e+19 -7.200000000000001e-02 2.850000000000000e-02 6.593306350434817e+18 -7.200000000000001e-02 3.000000000000000e-02 3.971182503855352e+18 -7.200000000000001e-02 3.150000000000000e-02 2.134907486980946e+18 -7.200000000000001e-02 3.300000000000000e-02 9.144686260460964e+17 -7.200000000000001e-02 3.450000000000000e-02 1.571093751701545e+17 -7.200000000000001e-02 3.600000000000000e-02 -2.677231306097011e+17 -7.200000000000001e-02 3.750000000000000e-02 -4.663421864095215e+17 -7.200000000000001e-02 3.900000000000000e-02 -5.211878735207493e+17 -7.200000000000001e-02 4.050000000000000e-02 -4.929505595756268e+17 -7.200000000000001e-02 4.200000000000000e-02 -4.237779329434797e+17 -7.200000000000001e-02 4.350000000000000e-02 -3.409524243053560e+17 -7.200000000000001e-02 4.500000000000000e-02 -2.605466324031500e+17 -7.200000000000001e-02 4.650000000000000e-02 -1.907135122545771e+17 -7.200000000000001e-02 4.800000000000000e-02 -1.344168924445838e+17 -7.200000000000001e-02 4.950000000000000e-02 -9.153526280623374e+16 -7.200000000000001e-02 5.100000000000000e-02 -6.036602372600370e+16 -7.200000000000001e-02 5.250000000000000e-02 -3.861567431607159e+16 -7.200000000000001e-02 5.400000000000000e-02 -2.398759050473141e+16 -7.200000000000001e-02 5.550000000000000e-02 -1.448081761722968e+16 -7.200000000000001e-02 5.700000000000000e-02 -8.499567353633145e+15 -7.200000000000001e-02 5.850000000000000e-02 -4.851937849131191e+15 -7.200000000000001e-02 6.000000000000000e-02 -2.693892831070608e+15 -7.200000000000001e-02 6.150000000000000e-02 -1.454593417642683e+15 -7.200000000000001e-02 6.300000000000000e-02 -7.635923761140364e+14 -7.200000000000001e-02 6.450000000000000e-02 -3.894955477570447e+14 -7.200000000000001e-02 6.600000000000000e-02 -1.928867862379647e+14 -7.200000000000001e-02 6.750000000000000e-02 -9.262653767824820e+13 -7.200000000000001e-02 6.900000000000001e-02 -4.305716018984305e+13 -7.200000000000001e-02 7.050000000000001e-02 -1.932576349271628e+13 -7.200000000000001e-02 7.200000000000001e-02 -8.344155619049827e+12 -7.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -7.000000000000001e-02 0.000000000000000e+00 1.989459951549560e+20 -7.000000000000001e-02 1.500000000000000e-03 1.970990134422951e+20 -7.000000000000001e-02 3.000000000000000e-03 1.922933212747438e+20 -7.000000000000001e-02 4.500000000000001e-03 1.847100500822197e+20 -7.000000000000001e-02 6.000000000000000e-03 1.746461555232649e+20 -7.000000000000001e-02 7.500000000000000e-03 1.624953119072061e+20 -7.000000000000001e-02 9.000000000000001e-03 1.487229162650524e+20 -7.000000000000001e-02 1.050000000000000e-02 1.338373688550470e+20 -7.000000000000001e-02 1.200000000000000e-02 1.183599992580746e+20 -7.000000000000001e-02 1.350000000000000e-02 1.027959737802632e+20 -7.000000000000001e-02 1.500000000000000e-02 8.760827927700500e+19 -7.000000000000001e-02 1.650000000000000e-02 7.319647629499686e+19 -7.000000000000001e-02 1.800000000000000e-02 5.988140354063927e+19 -7.000000000000001e-02 1.950000000000000e-02 4.789644922870433e+19 -7.000000000000001e-02 2.100000000000000e-02 3.738543219640485e+19 -7.000000000000001e-02 2.250000000000000e-02 2.840660128747074e+19 -7.000000000000001e-02 2.400000000000000e-02 2.094180519184375e+19 -7.000000000000001e-02 2.550000000000000e-02 1.490954121590070e+19 -7.000000000000001e-02 2.700000000000000e-02 1.018038740553770e+19 -7.000000000000001e-02 2.850000000000000e-02 6.593273649112963e+18 -7.000000000000001e-02 3.000000000000000e-02 3.971153681826353e+18 -7.000000000000001e-02 3.150000000000000e-02 2.134882660638206e+18 -7.000000000000001e-02 3.300000000000000e-02 9.144477268348442e+17 -7.000000000000001e-02 3.450000000000000e-02 1.570921812067407e+17 -7.000000000000001e-02 3.600000000000000e-02 -2.677369551613027e+17 -7.000000000000001e-02 3.750000000000000e-02 -4.663530495416705e+17 -7.000000000000001e-02 3.900000000000000e-02 -5.211962158634158e+17 -7.000000000000001e-02 4.050000000000000e-02 -4.929568206655324e+17 -7.000000000000001e-02 4.200000000000000e-02 -4.237825253551143e+17 -7.000000000000001e-02 4.350000000000000e-02 -3.409557163114482e+17 -7.000000000000001e-02 4.500000000000000e-02 -2.605489386691962e+17 -7.000000000000001e-02 4.650000000000000e-02 -1.907150912727682e+17 -7.000000000000001e-02 4.800000000000000e-02 -1.344179490037320e+17 -7.000000000000001e-02 4.950000000000000e-02 -9.153595372891437e+16 -7.000000000000001e-02 5.100000000000000e-02 -6.036646529038833e+16 -7.000000000000001e-02 5.250000000000000e-02 -3.861595011182714e+16 -7.000000000000001e-02 5.400000000000000e-02 -2.398775885354978e+16 -7.000000000000001e-02 5.550000000000000e-02 -1.448091804678042e+16 -7.000000000000001e-02 5.700000000000000e-02 -8.499625905658287e+15 -7.000000000000001e-02 5.850000000000000e-02 -4.851971211069470e+15 -7.000000000000001e-02 6.000000000000000e-02 -2.693911408669496e+15 -7.000000000000001e-02 6.150000000000000e-02 -1.454603527775060e+15 -7.000000000000001e-02 6.300000000000000e-02 -7.635977532752296e+14 -7.000000000000001e-02 6.450000000000000e-02 -3.894983427339424e+14 -7.000000000000001e-02 6.600000000000000e-02 -1.928882060548689e+14 -7.000000000000001e-02 6.750000000000000e-02 -9.262724255861755e+13 -7.000000000000001e-02 6.900000000000001e-02 -4.305750219089530e+13 -7.000000000000001e-02 7.050000000000001e-02 -1.932592566193409e+13 -7.000000000000001e-02 7.200000000000001e-02 -8.344230770671219e+12 -7.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -6.800000000000000e-02 0.000000000000000e+00 1.989459881040215e+20 -6.800000000000000e-02 1.500000000000000e-03 1.970990038293644e+20 -6.800000000000000e-02 3.000000000000000e-03 1.922933084663729e+20 -6.800000000000000e-02 4.500000000000001e-03 1.847100334035683e+20 -6.800000000000000e-02 6.000000000000000e-03 1.746461342978140e+20 -6.800000000000000e-02 7.500000000000000e-03 1.624952855085469e+20 -6.800000000000000e-02 9.000000000000001e-03 1.487228841775609e+20 -6.800000000000000e-02 1.050000000000000e-02 1.338373307380553e+20 -6.800000000000000e-02 1.200000000000000e-02 1.183599550063275e+20 -6.800000000000000e-02 1.350000000000000e-02 1.027959235724646e+20 -6.800000000000000e-02 1.500000000000000e-02 8.760822360448377e+19 -6.800000000000000e-02 1.650000000000000e-02 7.319641596413170e+19 -6.800000000000000e-02 1.800000000000000e-02 5.988133964559575e+19 -6.800000000000000e-02 1.950000000000000e-02 4.789638309486431e+19 -6.800000000000000e-02 2.100000000000000e-02 3.738536529900103e+19 -6.800000000000000e-02 2.250000000000000e-02 2.840653515363073e+19 -6.800000000000000e-02 2.400000000000000e-02 2.094174129680024e+19 -6.800000000000000e-02 2.550000000000000e-02 1.490948088503553e+19 -6.800000000000000e-02 2.700000000000000e-02 1.018033173301647e+19 -6.800000000000000e-02 2.850000000000000e-02 6.593223441314448e+18 -6.800000000000000e-02 3.000000000000000e-02 3.971109430079246e+18 -6.800000000000000e-02 3.150000000000000e-02 2.134844543646493e+18 -6.800000000000000e-02 3.300000000000000e-02 9.144156393433249e+17 -6.800000000000000e-02 3.450000000000000e-02 1.570657825475490e+17 -6.800000000000000e-02 3.600000000000000e-02 -2.677581806122024e+17 -6.800000000000000e-02 3.750000000000000e-02 -4.663697281931515e+17 -6.800000000000000e-02 3.900000000000000e-02 -5.212090242343314e+17 -6.800000000000000e-02 4.050000000000000e-02 -4.929664335962224e+17 -6.800000000000000e-02 4.200000000000000e-02 -4.237895762896017e+17 -6.800000000000000e-02 4.350000000000000e-02 -3.409607706752847e+17 -6.800000000000000e-02 4.500000000000000e-02 -2.605524795823582e+17 -6.800000000000000e-02 4.650000000000000e-02 -1.907175156098498e+17 -6.800000000000000e-02 4.800000000000000e-02 -1.344195711861340e+17 -6.800000000000000e-02 4.950000000000000e-02 -9.153701453333360e+16 -6.800000000000000e-02 5.100000000000000e-02 -6.036714324388983e+16 -6.800000000000000e-02 5.250000000000000e-02 -3.861637355335614e+16 -6.800000000000000e-02 5.400000000000000e-02 -2.398801732700203e+16 -6.800000000000000e-02 5.550000000000000e-02 -1.448107224075065e+16 -6.800000000000000e-02 5.700000000000000e-02 -8.499715803194971e+15 -6.800000000000000e-02 5.850000000000000e-02 -4.852022433141858e+15 -6.800000000000000e-02 6.000000000000000e-02 -2.693939931685967e+15 -6.800000000000000e-02 6.150000000000000e-02 -1.454619050312395e+15 -6.800000000000000e-02 6.300000000000000e-02 -7.636060090707285e+14 -6.800000000000000e-02 6.450000000000000e-02 -3.895026339866800e+14 -6.800000000000000e-02 6.600000000000000e-02 -1.928903859631116e+14 -6.800000000000000e-02 6.750000000000000e-02 -9.262832479289905e+13 -6.800000000000000e-02 6.900000000000001e-02 -4.305802728037027e+13 -6.800000000000000e-02 7.050000000000001e-02 -1.932617464756988e+13 -6.800000000000000e-02 7.200000000000001e-02 -8.344346154308668e+12 -6.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -6.600000000000000e-02 0.000000000000000e+00 1.989459773784305e+20 -6.600000000000000e-02 1.500000000000000e-03 1.970989892065703e+20 -6.600000000000000e-02 3.000000000000000e-03 1.922932889828068e+20 -6.600000000000000e-02 4.500000000000001e-03 1.847100080326907e+20 -6.600000000000000e-02 6.000000000000000e-03 1.746461020105326e+20 -6.600000000000000e-02 7.500000000000000e-03 1.624952453519942e+20 -6.600000000000000e-02 9.000000000000001e-03 1.487228353673908e+20 -6.600000000000000e-02 1.050000000000000e-02 1.338372727560578e+20 -6.600000000000000e-02 1.200000000000000e-02 1.183598876923929e+20 -6.600000000000000e-02 1.350000000000000e-02 1.027958471984301e+20 -6.600000000000000e-02 1.500000000000000e-02 8.760813891773810e+19 -6.600000000000000e-02 1.650000000000000e-02 7.319632419130515e+19 -6.600000000000000e-02 1.800000000000000e-02 5.988124245108795e+19 -6.600000000000000e-02 1.950000000000000e-02 4.789628249479152e+19 -6.600000000000000e-02 2.100000000000000e-02 3.738526353742643e+19 -6.600000000000000e-02 2.250000000000000e-02 2.840643455355793e+19 -6.600000000000000e-02 2.400000000000000e-02 2.094164410229243e+19 -6.600000000000000e-02 2.550000000000000e-02 1.490938911220899e+19 -6.600000000000000e-02 2.700000000000000e-02 1.018024704627080e+19 -6.600000000000000e-02 2.850000000000000e-02 6.593147067279843e+18 -6.600000000000000e-02 3.000000000000000e-02 3.971042116144660e+18 -6.600000000000000e-02 3.150000000000000e-02 2.134786561649068e+18 -6.600000000000000e-02 3.300000000000000e-02 9.143668291731882e+17 -6.600000000000000e-02 3.450000000000000e-02 1.570256259947764e+17 -6.600000000000000e-02 3.600000000000000e-02 -2.677904678936504e+17 -6.600000000000000e-02 3.750000000000000e-02 -4.663950990706460e+17 -6.600000000000000e-02 3.900000000000000e-02 -5.212285078004803e+17 -6.600000000000000e-02 4.050000000000000e-02 -4.929810563903481e+17 -6.600000000000000e-02 4.200000000000000e-02 -4.238003018806548e+17 -6.600000000000000e-02 4.350000000000000e-02 -3.409684591653196e+17 -6.600000000000000e-02 4.500000000000000e-02 -2.605578658735792e+17 -6.600000000000000e-02 4.650000000000000e-02 -1.907212034115389e+17 -6.600000000000000e-02 4.800000000000000e-02 -1.344220387831721e+17 -6.600000000000000e-02 4.950000000000000e-02 -9.153862818531240e+16 -6.600000000000000e-02 5.100000000000000e-02 -6.036817451882553e+16 -6.600000000000000e-02 5.250000000000000e-02 -3.861701767516481e+16 -6.600000000000000e-02 5.400000000000000e-02 -2.398841050616883e+16 -6.600000000000000e-02 5.550000000000000e-02 -1.448130679426557e+16 -6.600000000000000e-02 5.700000000000000e-02 -8.499852551624113e+15 -6.600000000000000e-02 5.850000000000000e-02 -4.852100350048092e+15 -6.600000000000000e-02 6.000000000000000e-02 -2.693983319723511e+15 -6.600000000000000e-02 6.150000000000000e-02 -1.454642662556681e+15 -6.600000000000000e-02 6.300000000000000e-02 -7.636185674467135e+14 -6.600000000000000e-02 6.450000000000000e-02 -3.895091616635504e+14 -6.600000000000000e-02 6.600000000000000e-02 -1.928937019497209e+14 -6.600000000000000e-02 6.750000000000000e-02 -9.262997104310145e+13 -6.600000000000000e-02 6.900000000000001e-02 -4.305882602484662e+13 -6.600000000000000e-02 7.050000000000001e-02 -1.932655339426116e+13 -6.600000000000000e-02 7.200000000000001e-02 -8.344521671144301e+12 -6.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -6.400000000000000e-02 0.000000000000000e+00 1.989459612141154e+20 -6.400000000000000e-02 1.500000000000000e-03 1.970989671688616e+20 -6.400000000000000e-02 3.000000000000000e-03 1.922932596195297e+20 -6.400000000000000e-02 4.500000000000001e-03 1.847099697967692e+20 -6.400000000000000e-02 6.000000000000000e-03 1.746460533510426e+20 -6.400000000000000e-02 7.500000000000000e-03 1.624951848328891e+20 -6.400000000000000e-02 9.000000000000001e-03 1.487227618065990e+20 -6.400000000000000e-02 1.050000000000000e-02 1.338371853725960e+20 -6.400000000000000e-02 1.200000000000000e-02 1.183597862449628e+20 -6.400000000000000e-02 1.350000000000000e-02 1.027957320967117e+20 -6.400000000000000e-02 1.500000000000000e-02 8.760801128810593e+19 -6.400000000000000e-02 1.650000000000000e-02 7.319618588238794e+19 -6.400000000000000e-02 1.800000000000000e-02 5.988109597126772e+19 -6.400000000000000e-02 1.950000000000000e-02 4.789613088251515e+19 -6.400000000000000e-02 2.100000000000000e-02 3.738511017467487e+19 -6.400000000000000e-02 2.250000000000000e-02 2.840628294128157e+19 -6.400000000000000e-02 2.400000000000000e-02 2.094149762247220e+19 -6.400000000000000e-02 2.550000000000000e-02 1.490925080329178e+19 -6.400000000000000e-02 2.700000000000000e-02 1.018011941663863e+19 -6.400000000000000e-02 2.850000000000000e-02 6.593031965561527e+18 -6.400000000000000e-02 3.000000000000000e-02 3.970940668714555e+18 -6.400000000000000e-02 3.150000000000000e-02 2.134699178187274e+18 -6.400000000000000e-02 3.300000000000000e-02 9.142932683814474e+17 -6.400000000000000e-02 3.450000000000000e-02 1.569651068896953e+17 -6.400000000000000e-02 3.600000000000000e-02 -2.678391273836670e+17 -6.400000000000000e-02 3.750000000000000e-02 -4.664333349921851e+17 -6.400000000000000e-02 3.900000000000000e-02 -5.212578710775971e+17 -6.400000000000000e-02 4.050000000000000e-02 -4.930030940990948e+17 -6.400000000000000e-02 4.200000000000000e-02 -4.238164661957461e+17 -6.400000000000000e-02 4.350000000000000e-02 -3.409800463286644e+17 -6.400000000000000e-02 4.500000000000000e-02 -2.605659834409972e+17 -6.400000000000000e-02 4.650000000000000e-02 -1.907267612207266e+17 -6.400000000000000e-02 4.800000000000000e-02 -1.344257576473209e+17 -6.400000000000000e-02 4.950000000000000e-02 -9.154106008663178e+16 -6.400000000000000e-02 5.100000000000000e-02 -6.036972873182171e+16 -6.400000000000000e-02 5.250000000000000e-02 -3.861798841773938e+16 -6.400000000000000e-02 5.400000000000000e-02 -2.398900305830959e+16 -6.400000000000000e-02 5.550000000000000e-02 -1.448166028498718e+16 -6.400000000000000e-02 5.700000000000000e-02 -8.500058642336128e+15 -6.400000000000000e-02 5.850000000000000e-02 -4.852217776996135e+15 -6.400000000000000e-02 6.000000000000000e-02 -2.694048708932048e+15 -6.400000000000000e-02 6.150000000000000e-02 -1.454678248078705e+15 -6.400000000000000e-02 6.300000000000000e-02 -7.636374939138380e+14 -6.400000000000000e-02 6.450000000000000e-02 -3.895189993895299e+14 -6.400000000000000e-02 6.600000000000000e-02 -1.928986994041387e+14 -6.400000000000000e-02 6.750000000000000e-02 -9.263245207252528e+13 -6.400000000000000e-02 6.900000000000001e-02 -4.306002979602613e+13 -6.400000000000000e-02 7.050000000000001e-02 -1.932712419551840e+13 -6.400000000000000e-02 7.200000000000001e-02 -8.344786188915020e+12 -6.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -6.200000000000001e-02 0.000000000000000e+00 1.989459370791165e+20 -6.200000000000001e-02 1.500000000000000e-03 1.970989342642768e+20 -6.200000000000001e-02 3.000000000000000e-03 1.922932157771116e+20 -6.200000000000001e-02 4.500000000000001e-03 1.847099127065728e+20 -6.200000000000001e-02 6.000000000000000e-03 1.746459806973774e+20 -6.200000000000001e-02 7.500000000000000e-03 1.624950944715887e+20 -6.200000000000001e-02 9.000000000000001e-03 1.487226519727079e+20 -6.200000000000001e-02 1.050000000000000e-02 1.338370549000249e+20 -6.200000000000001e-02 1.200000000000000e-02 1.183596347734284e+20 -6.200000000000001e-02 1.350000000000000e-02 1.027955602379089e+20 -6.200000000000001e-02 1.500000000000000e-02 8.760782072382842e+19 -6.200000000000001e-02 1.650000000000000e-02 7.319597937283033e+19 -6.200000000000001e-02 1.800000000000000e-02 5.988087726170450e+19 -6.200000000000001e-02 1.950000000000000e-02 4.789590450966261e+19 -6.200000000000001e-02 2.100000000000000e-02 3.738488118818132e+19 -6.200000000000001e-02 2.250000000000000e-02 2.840605656842903e+19 -6.200000000000001e-02 2.400000000000000e-02 2.094127891290898e+19 -6.200000000000001e-02 2.550000000000000e-02 1.490904429373417e+19 -6.200000000000001e-02 2.700000000000000e-02 1.017992885236114e+19 -6.200000000000001e-02 2.850000000000000e-02 6.592860106758721e+18 -6.200000000000001e-02 3.000000000000000e-02 3.970789197180153e+18 -6.200000000000001e-02 3.150000000000000e-02 2.134568705616154e+18 -6.200000000000001e-02 3.300000000000000e-02 9.141834344902845e+17 -6.200000000000001e-02 3.450000000000000e-02 1.568747455892871e+17 -6.200000000000001e-02 3.600000000000000e-02 -2.679117810488064e+17 -6.200000000000001e-02 3.750000000000000e-02 -4.664904251885444e+17 -6.200000000000001e-02 3.900000000000000e-02 -5.213017134956395e+17 -6.200000000000001e-02 4.050000000000000e-02 -4.930359986838156e+17 -6.200000000000001e-02 4.200000000000000e-02 -4.238406011946015e+17 -6.200000000000001e-02 4.350000000000000e-02 -3.409973471652593e+17 -6.200000000000001e-02 4.500000000000000e-02 -2.605781038110366e+17 -6.200000000000001e-02 4.650000000000000e-02 -1.907350596062520e+17 -6.200000000000001e-02 4.800000000000000e-02 -1.344313102971838e+17 -6.200000000000001e-02 4.950000000000000e-02 -9.154469116751752e+16 -6.200000000000001e-02 5.100000000000000e-02 -6.037204933301464e+16 -6.200000000000001e-02 5.250000000000000e-02 -3.861943783708029e+16 -6.200000000000001e-02 5.400000000000000e-02 -2.398988780011018e+16 -6.200000000000001e-02 5.550000000000000e-02 -1.448218808329557e+16 -6.200000000000001e-02 5.700000000000000e-02 -8.500366357143125e+15 -6.200000000000001e-02 5.850000000000000e-02 -4.852393107608077e+15 -6.200000000000001e-02 6.000000000000000e-02 -2.694146341802002e+15 -6.200000000000001e-02 6.150000000000000e-02 -1.454731380953712e+15 -6.200000000000001e-02 6.300000000000000e-02 -7.636657530921455e+14 -6.200000000000001e-02 6.450000000000000e-02 -3.895336881347019e+14 -6.200000000000001e-02 6.600000000000000e-02 -1.929061611218775e+14 -6.200000000000001e-02 6.750000000000000e-02 -9.263615650676614e+13 -6.200000000000001e-02 6.900000000000001e-02 -4.306182715124198e+13 -6.200000000000001e-02 7.050000000000001e-02 -1.932797646099406e+13 -6.200000000000001e-02 7.200000000000001e-02 -8.345181141380217e+12 -6.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -6.000000000000000e-02 0.000000000000000e+00 1.989459013778971e+20 -6.000000000000000e-02 1.500000000000000e-03 1.970988855908211e+20 -6.000000000000000e-02 3.000000000000000e-03 1.922931509240824e+20 -6.000000000000000e-02 4.500000000000001e-03 1.847098282570298e+20 -6.000000000000000e-02 6.000000000000000e-03 1.746458732258812e+20 -6.000000000000000e-02 7.500000000000000e-03 1.624949608064233e+20 -6.000000000000000e-02 9.000000000000001e-03 1.487224895030980e+20 -6.000000000000000e-02 1.050000000000000e-02 1.338368619010562e+20 -6.000000000000000e-02 1.200000000000000e-02 1.183594107121588e+20 -6.000000000000000e-02 1.350000000000000e-02 1.027953060191761e+20 -6.000000000000000e-02 1.500000000000000e-02 8.760753883539235e+19 -6.000000000000000e-02 1.650000000000000e-02 7.319567389765420e+19 -6.000000000000000e-02 1.800000000000000e-02 5.988055373991150e+19 -6.000000000000000e-02 1.950000000000000e-02 4.789556965210056e+19 -6.000000000000000e-02 2.100000000000000e-02 3.738454246444253e+19 -6.000000000000000e-02 2.250000000000000e-02 2.840572171086698e+19 -6.000000000000000e-02 2.400000000000000e-02 2.094095539111598e+19 -6.000000000000000e-02 2.550000000000000e-02 1.490873881855804e+19 -6.000000000000000e-02 2.700000000000000e-02 1.017964696392505e+19 -6.000000000000000e-02 2.850000000000000e-02 6.592605888025866e+18 -6.000000000000000e-02 3.000000000000000e-02 3.970565135910609e+18 -6.000000000000000e-02 3.150000000000000e-02 2.134375706647462e+18 -6.000000000000000e-02 3.300000000000000e-02 9.140209648804666e+17 -6.000000000000000e-02 3.450000000000000e-02 1.567410804239678e+17 -6.000000000000000e-02 3.600000000000000e-02 -2.680192525451000e+17 -6.000000000000000e-02 3.750000000000000e-02 -4.665748747316566e+17 -6.000000000000000e-02 3.900000000000000e-02 -5.213665665248585e+17 -6.000000000000000e-02 4.050000000000000e-02 -4.930846721395604e+17 -6.000000000000000e-02 4.200000000000000e-02 -4.238763024140108e+17 -6.000000000000000e-02 4.350000000000000e-02 -3.410229390853974e+17 -6.000000000000000e-02 4.500000000000000e-02 -2.605960326285474e+17 -6.000000000000000e-02 4.650000000000000e-02 -1.907473348288099e+17 -6.000000000000000e-02 4.800000000000000e-02 -1.344395239446029e+17 -6.000000000000000e-02 4.950000000000000e-02 -9.155006237205630e+16 -6.000000000000000e-02 5.100000000000000e-02 -6.037548203640306e+16 -6.000000000000000e-02 5.250000000000000e-02 -3.862158186195538e+16 -6.000000000000000e-02 5.400000000000000e-02 -2.399119653690907e+16 -6.000000000000000e-02 5.550000000000000e-02 -1.448296881849777e+16 -6.000000000000000e-02 5.700000000000000e-02 -8.500821538181498e+15 -6.000000000000000e-02 5.850000000000000e-02 -4.852652461945885e+15 -6.000000000000000e-02 6.000000000000000e-02 -2.694290763292663e+15 -6.000000000000000e-02 6.150000000000000e-02 -1.454809976707532e+15 -6.000000000000000e-02 6.300000000000000e-02 -7.637075549223892e+14 -6.000000000000000e-02 6.450000000000000e-02 -3.895554161702976e+14 -6.000000000000000e-02 6.600000000000000e-02 -1.929171987201703e+14 -6.000000000000000e-02 6.750000000000000e-02 -9.264163621780375e+13 -6.000000000000000e-02 6.900000000000001e-02 -4.306448585337416e+13 -6.000000000000000e-02 7.050000000000001e-02 -1.932923715783204e+13 -6.000000000000000e-02 7.200000000000001e-02 -8.345765366997989e+12 -6.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -5.800000000000000e-02 0.000000000000000e+00 1.989458490593149e+20 -5.800000000000000e-02 1.500000000000000e-03 1.970988142619915e+20 -5.800000000000000e-02 3.000000000000000e-03 1.922930558847925e+20 -5.800000000000000e-02 4.500000000000001e-03 1.847097044999022e+20 -5.800000000000000e-02 6.000000000000000e-03 1.746457157310839e+20 -5.800000000000000e-02 7.500000000000000e-03 1.624947649259449e+20 -5.800000000000000e-02 9.000000000000001e-03 1.487222514109606e+20 -5.800000000000000e-02 1.050000000000000e-02 1.338365790694730e+20 -5.800000000000000e-02 1.200000000000000e-02 1.183590823601265e+20 -5.800000000000000e-02 1.350000000000000e-02 1.027949334726947e+20 -5.800000000000000e-02 1.500000000000000e-02 8.760712574016591e+19 -5.800000000000000e-02 1.650000000000000e-02 7.319522623708746e+19 -5.800000000000000e-02 1.800000000000000e-02 5.988007963281369e+19 -5.800000000000000e-02 1.950000000000000e-02 4.789507893292691e+19 -5.800000000000000e-02 2.100000000000000e-02 3.738404607955523e+19 -5.800000000000000e-02 2.250000000000000e-02 2.840523099169333e+19 -5.800000000000000e-02 2.400000000000000e-02 2.094048128401817e+19 -5.800000000000000e-02 2.550000000000000e-02 1.490829115799129e+19 -5.800000000000000e-02 2.700000000000000e-02 1.017923386869862e+19 -5.800000000000000e-02 2.850000000000000e-02 6.592233341544457e+18 -5.800000000000000e-02 3.000000000000000e-02 3.970236783878281e+18 -5.800000000000000e-02 3.150000000000000e-02 2.134092875064225e+18 -5.800000000000000e-02 3.300000000000000e-02 9.137828727430620e+17 -5.800000000000000e-02 3.450000000000000e-02 1.565451999455012e+17 -5.800000000000000e-02 3.600000000000000e-02 -2.681767473423812e+17 -5.800000000000000e-02 3.750000000000000e-02 -4.666986318591892e+17 -5.800000000000000e-02 3.900000000000000e-02 -5.214616058147369e+17 -5.800000000000000e-02 4.050000000000000e-02 -4.931560009691560e+17 -5.800000000000000e-02 4.200000000000000e-02 -4.239286209962161e+17 -5.800000000000000e-02 4.350000000000000e-02 -3.410604429297951e+17 -5.800000000000000e-02 4.500000000000000e-02 -2.606223065297838e+17 -5.800000000000000e-02 4.650000000000000e-02 -1.907653236328651e+17 -5.800000000000000e-02 4.800000000000000e-02 -1.344515606871794e+17 -5.800000000000000e-02 4.950000000000000e-02 -9.155793363838426e+16 -5.800000000000000e-02 5.100000000000000e-02 -6.038051251371965e+16 -5.800000000000000e-02 5.250000000000000e-02 -3.862472383703446e+16 -5.800000000000000e-02 5.400000000000000e-02 -2.399311443369049e+16 -5.800000000000000e-02 5.550000000000000e-02 -1.448411295193447e+16 -5.800000000000000e-02 5.700000000000000e-02 -8.501488586169449e+15 -5.800000000000000e-02 5.850000000000000e-02 -4.853032534432691e+15 -5.800000000000000e-02 6.000000000000000e-02 -2.694502406697464e+15 -5.800000000000000e-02 6.150000000000000e-02 -1.454925155361798e+15 -5.800000000000000e-02 6.300000000000000e-02 -7.637688136840821e+14 -5.800000000000000e-02 6.450000000000000e-02 -3.895872576601760e+14 -5.800000000000000e-02 6.600000000000000e-02 -1.929333738397654e+14 -5.800000000000000e-02 6.750000000000000e-02 -9.264966649568012e+13 -5.800000000000000e-02 6.900000000000001e-02 -4.306838206555861e+13 -5.800000000000000e-02 7.050000000000001e-02 -1.933108465414295e+13 -5.800000000000000e-02 7.200000000000001e-02 -8.346621524196977e+12 -5.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -5.600000000000001e-02 0.000000000000000e+00 1.989457731042385e+20 -5.600000000000001e-02 1.500000000000000e-03 1.970987107082163e+20 -5.600000000000001e-02 3.000000000000000e-03 1.922929179086430e+20 -5.600000000000001e-02 4.500000000000001e-03 1.847095248317675e+20 -5.600000000000001e-02 6.000000000000000e-03 1.746454870832717e+20 -5.600000000000001e-02 7.500000000000000e-03 1.624944805505648e+20 -5.600000000000001e-02 9.000000000000001e-03 1.487219057535342e+20 -5.600000000000001e-02 1.050000000000000e-02 1.338361684602095e+20 -5.600000000000001e-02 1.200000000000000e-02 1.183586056651810e+20 -5.600000000000001e-02 1.350000000000000e-02 1.027943926171276e+20 -5.600000000000001e-02 1.500000000000000e-02 8.760652601673780e+19 -5.600000000000001e-02 1.650000000000000e-02 7.319457633238622e+19 -5.600000000000001e-02 1.800000000000000e-02 5.987939133356501e+19 -5.600000000000001e-02 1.950000000000000e-02 4.789436651659714e+19 -5.600000000000001e-02 2.100000000000000e-02 3.738332543785516e+19 -5.600000000000001e-02 2.250000000000000e-02 2.840451857536356e+19 -5.600000000000001e-02 2.400000000000000e-02 2.093979298476950e+19 -5.600000000000001e-02 2.550000000000000e-02 1.490764125329006e+19 -5.600000000000001e-02 2.700000000000000e-02 1.017863414527051e+19 -5.600000000000001e-02 2.850000000000000e-02 6.591692485977357e+18 -5.600000000000001e-02 3.000000000000000e-02 3.969760088932775e+18 -5.600000000000001e-02 3.150000000000000e-02 2.133682265800738e+18 -5.600000000000001e-02 3.300000000000000e-02 9.134372153166084e+17 -5.600000000000001e-02 3.450000000000000e-02 1.562608245653759e+17 -5.600000000000001e-02 3.600000000000000e-02 -2.684053951545328e+17 -5.600000000000001e-02 3.750000000000000e-02 -4.668782999938640e+17 -5.600000000000001e-02 3.900000000000000e-02 -5.215995819642623e+17 -5.600000000000001e-02 4.050000000000000e-02 -4.932595547443404e+17 -5.600000000000001e-02 4.200000000000000e-02 -4.240045760725907e+17 -5.600000000000001e-02 4.350000000000000e-02 -3.411148902646711e+17 -5.600000000000001e-02 4.500000000000000e-02 -2.606604504566823e+17 -5.600000000000001e-02 4.650000000000000e-02 -1.907914394205701e+17 -5.600000000000001e-02 4.800000000000000e-02 -1.344690353904908e+17 -5.600000000000001e-02 4.950000000000000e-02 -9.156936098618125e+16 -5.600000000000001e-02 5.100000000000000e-02 -6.038781566056878e+16 -5.600000000000001e-02 5.250000000000000e-02 -3.862928529392110e+16 -5.600000000000001e-02 5.400000000000000e-02 -2.399589879806680e+16 -5.600000000000001e-02 5.550000000000000e-02 -1.448577398208674e+16 -5.600000000000001e-02 5.700000000000000e-02 -8.502456993162429e+15 -5.600000000000001e-02 5.850000000000000e-02 -4.853584316104640e+15 -5.600000000000001e-02 6.000000000000000e-02 -2.694809666380320e+15 -5.600000000000001e-02 6.150000000000000e-02 -1.455092369439717e+15 -5.600000000000001e-02 6.300000000000000e-02 -7.638577479351047e+14 -5.600000000000001e-02 6.450000000000000e-02 -3.896334845014561e+14 -5.600000000000001e-02 6.600000000000000e-02 -1.929568565564680e+14 -5.600000000000001e-02 6.750000000000000e-02 -9.266132469327837e+13 -5.600000000000001e-02 6.900000000000001e-02 -4.307403850886359e+13 -5.600000000000001e-02 7.050000000000001e-02 -1.933376681251732e+13 -5.600000000000001e-02 7.200000000000001e-02 -8.347864476178791e+12 -5.600000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -5.400000000000001e-02 0.000000000000000e+00 1.989456638657451e+20 -5.400000000000001e-02 1.500000000000000e-03 1.970985617773096e+20 -5.400000000000001e-02 3.000000000000000e-03 1.922927194715217e+20 -5.400000000000001e-02 4.500000000000001e-03 1.847092664332867e+20 -5.400000000000001e-02 6.000000000000000e-03 1.746451582422815e+20 -5.400000000000001e-02 7.500000000000000e-03 1.624940715622578e+20 -5.400000000000001e-02 9.000000000000001e-03 1.487214086294668e+20 -5.400000000000001e-02 1.050000000000000e-02 1.338355779224934e+20 -5.400000000000001e-02 1.200000000000000e-02 1.183579200831217e+20 -5.400000000000001e-02 1.350000000000000e-02 1.027936147593446e+20 -5.400000000000001e-02 1.500000000000000e-02 8.760566349527261e+19 -5.400000000000001e-02 1.650000000000000e-02 7.319364164027839e+19 -5.400000000000001e-02 1.800000000000000e-02 5.987840142246829e+19 -5.400000000000001e-02 1.950000000000000e-02 4.789334192034532e+19 -5.400000000000001e-02 2.100000000000000e-02 3.738228901188632e+19 -5.400000000000001e-02 2.250000000000000e-02 2.840349397911173e+19 -5.400000000000001e-02 2.400000000000000e-02 2.093880307367277e+19 -5.400000000000001e-02 2.550000000000000e-02 1.490670656118223e+19 -5.400000000000001e-02 2.700000000000000e-02 1.017777162380532e+19 -5.400000000000001e-02 2.850000000000000e-02 6.590914628194386e+18 -5.400000000000001e-02 3.000000000000000e-02 3.969074506873497e+18 -5.400000000000001e-02 3.150000000000000e-02 2.133091728084586e+18 -5.400000000000001e-02 3.300000000000000e-02 9.129400912491784e+17 -5.400000000000001e-02 3.450000000000000e-02 1.558518362583829e+17 -5.400000000000001e-02 3.600000000000000e-02 -2.687342361447350e+17 -5.400000000000001e-02 3.750000000000000e-02 -4.671366984747341e+17 -5.400000000000001e-02 3.900000000000000e-02 -5.217980190855593e+17 -5.400000000000001e-02 4.050000000000000e-02 -4.934084856510058e+17 -5.400000000000001e-02 4.200000000000000e-02 -4.241138145660225e+17 -5.400000000000001e-02 4.350000000000000e-02 -3.411931963518627e+17 -5.400000000000001e-02 4.500000000000000e-02 -2.607153090034293e+17 -5.400000000000001e-02 4.650000000000000e-02 -1.908289991129548e+17 -5.400000000000001e-02 4.800000000000000e-02 -1.344941674863823e+17 -5.400000000000001e-02 4.950000000000000e-02 -9.158579578312763e+16 -5.400000000000001e-02 5.100000000000000e-02 -6.039831903700110e+16 -5.400000000000001e-02 5.250000000000000e-02 -3.863584557536554e+16 -5.400000000000001e-02 5.400000000000000e-02 -2.399990326734195e+16 -5.400000000000001e-02 5.550000000000000e-02 -1.448816287352152e+16 -5.400000000000001e-02 5.700000000000000e-02 -8.503849754857780e+15 -5.400000000000001e-02 5.850000000000000e-02 -4.854377887797594e+15 -5.400000000000001e-02 6.000000000000000e-02 -2.695251566862152e+15 -5.400000000000001e-02 6.150000000000000e-02 -1.455332856512133e+15 -5.400000000000001e-02 6.300000000000000e-02 -7.639856530608701e+14 -5.400000000000001e-02 6.450000000000000e-02 -3.896999678853005e+14 -5.400000000000001e-02 6.600000000000000e-02 -1.929906293695138e+14 -5.400000000000001e-02 6.750000000000000e-02 -9.267809149811289e+13 -5.400000000000001e-02 6.900000000000001e-02 -4.308217359837061e+13 -5.400000000000001e-02 7.050000000000001e-02 -1.933762428925154e+13 -5.400000000000001e-02 7.200000000000001e-02 -8.349652088124986e+12 -5.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -5.200000000000000e-02 0.000000000000000e+00 1.989455082325985e+20 -5.200000000000000e-02 1.500000000000000e-03 1.970983495939949e+20 -5.200000000000000e-02 3.000000000000000e-03 1.922924367562203e+20 -5.200000000000000e-02 4.500000000000001e-03 1.847088982904517e+20 -5.200000000000000e-02 6.000000000000000e-03 1.746446897393167e+20 -5.200000000000000e-02 7.500000000000000e-03 1.624934888726293e+20 -5.200000000000000e-02 9.000000000000001e-03 1.487207003719612e+20 -5.200000000000000e-02 1.050000000000000e-02 1.338347365776517e+20 -5.200000000000000e-02 1.200000000000000e-02 1.183569433276778e+20 -5.200000000000000e-02 1.350000000000000e-02 1.027925065377774e+20 -5.200000000000000e-02 1.500000000000000e-02 8.760443465253200e+19 -5.200000000000000e-02 1.650000000000000e-02 7.319230997531956e+19 -5.200000000000000e-02 1.800000000000000e-02 5.987699108647763e+19 -5.200000000000000e-02 1.950000000000000e-02 4.789188216807601e+19 -5.200000000000000e-02 2.100000000000000e-02 3.738081240570384e+19 -5.200000000000000e-02 2.250000000000000e-02 2.840203422684243e+19 -5.200000000000000e-02 2.400000000000000e-02 2.093739273768211e+19 -5.200000000000000e-02 2.550000000000000e-02 1.490537489622340e+19 -5.200000000000000e-02 2.700000000000000e-02 1.017654278106471e+19 -5.200000000000000e-02 2.850000000000000e-02 6.589806406627241e+18 -5.200000000000000e-02 3.000000000000000e-02 3.968097751429542e+18 -5.200000000000000e-02 3.150000000000000e-02 2.132250383242922e+18 -5.200000000000000e-02 3.300000000000000e-02 9.122318337435871e+17 -5.200000000000000e-02 3.450000000000000e-02 1.552691466299680e+17 -5.200000000000000e-02 3.600000000000000e-02 -2.692027391095198e+17 -5.200000000000000e-02 3.750000000000000e-02 -4.675048413096924e+17 -5.200000000000000e-02 3.900000000000000e-02 -5.220807343869389e+17 -5.200000000000000e-02 4.050000000000000e-02 -4.936206689657378e+17 -5.200000000000000e-02 4.200000000000000e-02 -4.242694477126384e+17 -5.200000000000000e-02 4.350000000000000e-02 -3.413047597977316e+17 -5.200000000000000e-02 4.500000000000000e-02 -2.607934665098245e+17 -5.200000000000000e-02 4.650000000000000e-02 -1.908825107728844e+17 -5.200000000000000e-02 4.800000000000000e-02 -1.345299734284249e+17 -5.200000000000000e-02 4.950000000000000e-02 -9.160921059856862e+16 -5.200000000000000e-02 5.100000000000000e-02 -6.041328329980718e+16 -5.200000000000000e-02 5.250000000000000e-02 -3.864519207229906e+16 -5.200000000000000e-02 5.400000000000000e-02 -2.400560847375993e+16 -5.200000000000000e-02 5.550000000000000e-02 -1.449156635043921e+16 -5.200000000000000e-02 5.700000000000000e-02 -8.505834036023911e+15 -5.200000000000000e-02 5.850000000000000e-02 -4.855508497125493e+15 -5.200000000000000e-02 6.000000000000000e-02 -2.695881146786938e+15 -5.200000000000000e-02 6.150000000000000e-02 -1.455675480788839e+15 -5.200000000000000e-02 6.300000000000000e-02 -7.641678807405621e+14 -5.200000000000000e-02 6.450000000000000e-02 -3.897946874104451e+14 -5.200000000000000e-02 6.600000000000000e-02 -1.930387458255292e+14 -5.200000000000000e-02 6.750000000000000e-02 -9.270197932842902e+13 -5.200000000000000e-02 6.900000000000001e-02 -4.309376373970452e+13 -5.200000000000000e-02 7.050000000000001e-02 -1.934312007396337e+13 -5.200000000000000e-02 7.200000000000001e-02 -8.352198916293100e+12 -5.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -5.000000000000000e-02 0.000000000000000e+00 1.989452885859048e+20 -5.000000000000000e-02 1.500000000000000e-03 1.970980501374553e+20 -5.000000000000000e-02 3.000000000000000e-03 1.922920377571475e+20 -5.000000000000000e-02 4.500000000000001e-03 1.847083787266039e+20 -5.000000000000000e-02 6.000000000000000e-03 1.746440285361641e+20 -5.000000000000000e-02 7.500000000000000e-03 1.624926665166395e+20 -5.000000000000000e-02 9.000000000000001e-03 1.487197008007081e+20 -5.000000000000000e-02 1.050000000000000e-02 1.338335491788440e+20 -5.000000000000000e-02 1.200000000000000e-02 1.183555648224655e+20 -5.000000000000000e-02 1.350000000000000e-02 1.027909424930454e+20 -5.000000000000000e-02 1.500000000000000e-02 8.760270037387151e+19 -5.000000000000000e-02 1.650000000000000e-02 7.319043058258305e+19 -5.000000000000000e-02 1.800000000000000e-02 5.987500066448799e+19 -5.000000000000000e-02 1.950000000000000e-02 4.788982200437354e+19 -5.000000000000000e-02 2.100000000000000e-02 3.737872845589678e+19 -5.000000000000000e-02 2.250000000000000e-02 2.839997406313997e+19 -5.000000000000000e-02 2.400000000000000e-02 2.093540231569248e+19 -5.000000000000000e-02 2.550000000000000e-02 1.490349550348689e+19 -5.000000000000000e-02 2.700000000000000e-02 1.017480850240421e+19 -5.000000000000000e-02 2.850000000000000e-02 6.588242361895176e+18 -5.000000000000000e-02 3.000000000000000e-02 3.966719246217296e+18 -5.000000000000000e-02 3.150000000000000e-02 2.131062984435258e+18 -5.000000000000000e-02 3.300000000000000e-02 9.112322624905032e+17 -5.000000000000000e-02 3.450000000000000e-02 1.544467906401822e+17 -5.000000000000000e-02 3.600000000000000e-02 -2.698639422621676e+17 -5.000000000000000e-02 3.750000000000000e-02 -4.680244051575134e+17 -5.000000000000000e-02 3.900000000000000e-02 -5.224797334597834e+17 -5.000000000000000e-02 4.050000000000000e-02 -4.939201255053661e+17 -5.000000000000000e-02 4.200000000000000e-02 -4.244890944063283e+17 -5.000000000000000e-02 4.350000000000000e-02 -3.414622104601042e+17 -5.000000000000000e-02 4.500000000000000e-02 -2.609037710191147e+17 -5.000000000000000e-02 4.650000000000000e-02 -1.909580323403201e+17 -5.000000000000000e-02 4.800000000000000e-02 -1.345805067303284e+17 -5.000000000000000e-02 4.950000000000000e-02 -9.164225617341437e+16 -5.000000000000000e-02 5.100000000000000e-02 -6.043440252100353e+16 -5.000000000000000e-02 5.250000000000000e-02 -3.865838288154290e+16 -5.000000000000000e-02 5.400000000000000e-02 -2.401366029147214e+16 -5.000000000000000e-02 5.550000000000000e-02 -1.449636971314359e+16 -5.000000000000000e-02 5.700000000000000e-02 -8.508634472865093e+15 -5.000000000000000e-02 5.850000000000000e-02 -4.857104137939342e+15 -5.000000000000000e-02 6.000000000000000e-02 -2.696769679544256e+15 -5.000000000000000e-02 6.150000000000000e-02 -1.456159030027499e+15 -5.000000000000000e-02 6.300000000000000e-02 -7.644250605779779e+14 -5.000000000000000e-02 6.450000000000000e-02 -3.899283660706681e+14 -5.000000000000000e-02 6.600000000000000e-02 -1.931066530850407e+14 -5.000000000000000e-02 6.750000000000000e-02 -9.273569247413384e+13 -5.000000000000000e-02 6.900000000000001e-02 -4.311012102784490e+13 -5.000000000000000e-02 7.050000000000001e-02 -1.935087633262312e+13 -5.000000000000000e-02 7.200000000000001e-02 -8.355793281623920e+12 -5.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -4.800000000000000e-02 0.000000000000000e+00 1.989449815202412e+20 -4.800000000000000e-02 1.500000000000000e-03 1.970976314977775e+20 -4.800000000000000e-02 3.000000000000000e-03 1.922914799571960e+20 -4.800000000000000e-02 4.500000000000001e-03 1.847076523773243e+20 -4.800000000000000e-02 6.000000000000000e-03 1.746431041754034e+20 -4.800000000000000e-02 7.500000000000000e-03 1.624915168645164e+20 -4.800000000000000e-02 9.000000000000001e-03 1.487183034019810e+20 -4.800000000000000e-02 1.050000000000000e-02 1.338318891975498e+20 -4.800000000000000e-02 1.200000000000000e-02 1.183536376747781e+20 -4.800000000000000e-02 1.350000000000000e-02 1.027887559614590e+20 -4.800000000000000e-02 1.500000000000000e-02 8.760027585557420e+19 -4.800000000000000e-02 1.650000000000000e-02 7.318780319508111e+19 -4.800000000000000e-02 1.800000000000000e-02 5.987221805829953e+19 -4.800000000000000e-02 1.950000000000000e-02 4.788694189940206e+19 -4.800000000000000e-02 2.100000000000000e-02 3.737581509799592e+19 -4.800000000000000e-02 2.250000000000000e-02 2.839709395816847e+19 -4.800000000000000e-02 2.400000000000000e-02 2.093261970950402e+19 -4.800000000000000e-02 2.550000000000000e-02 1.490086811598496e+19 -4.800000000000000e-02 2.700000000000000e-02 1.017238398410691e+19 -4.800000000000000e-02 2.850000000000000e-02 6.586055830308845e+18 -4.800000000000000e-02 3.000000000000000e-02 3.964792098529825e+18 -4.800000000000000e-02 3.150000000000000e-02 2.129403003141051e+18 -4.800000000000000e-02 3.300000000000000e-02 9.098348637634392e+17 -4.800000000000000e-02 3.450000000000000e-02 1.532971385170599e+17 -4.800000000000000e-02 3.600000000000000e-02 -2.707883030228338e+17 -4.800000000000000e-02 3.750000000000000e-02 -4.687507544371005e+17 -4.800000000000000e-02 3.900000000000000e-02 -5.230375334112849e+17 -4.800000000000000e-02 4.050000000000000e-02 -4.943387651831244e+17 -4.800000000000000e-02 4.200000000000000e-02 -4.247961600699507e+17 -4.800000000000000e-02 4.350000000000000e-02 -3.416823261892190e+17 -4.800000000000000e-02 4.500000000000000e-02 -2.610579765151171e+17 -4.800000000000000e-02 4.650000000000000e-02 -1.910636113491952e+17 -4.800000000000000e-02 4.800000000000000e-02 -1.346511521911061e+17 -4.800000000000000e-02 4.950000000000000e-02 -9.168845382473946e+16 -4.800000000000000e-02 5.100000000000000e-02 -6.046392715241454e+16 -4.800000000000000e-02 5.250000000000000e-02 -3.867682360799380e+16 -4.800000000000000e-02 5.400000000000000e-02 -2.402491671745165e+16 -4.800000000000000e-02 5.550000000000000e-02 -1.450308480514730e+16 -4.800000000000000e-02 5.700000000000000e-02 -8.512549478288684e+15 -4.800000000000000e-02 5.850000000000000e-02 -4.859334840788432e+15 -4.800000000000000e-02 6.000000000000000e-02 -2.698011846663610e+15 -4.800000000000000e-02 6.150000000000000e-02 -1.456835030951386e+15 -4.800000000000000e-02 6.300000000000000e-02 -7.647845975057580e+14 -4.800000000000000e-02 6.450000000000000e-02 -3.901152485856012e+14 -4.800000000000000e-02 6.600000000000000e-02 -1.932015873057949e+14 -4.800000000000000e-02 6.750000000000000e-02 -9.278282338826119e+13 -4.800000000000000e-02 6.900000000000001e-02 -4.313298848582259e+13 -4.800000000000000e-02 7.050000000000001e-02 -1.936171956760459e+13 -4.800000000000000e-02 7.200000000000001e-02 -8.360818197579029e+12 -4.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -4.600000000000001e-02 0.000000000000000e+00 1.989445563050528e+20 -4.600000000000001e-02 1.500000000000000e-03 1.970970517782890e+20 -4.600000000000001e-02 3.000000000000000e-03 1.922907075327944e+20 -4.600000000000001e-02 4.500000000000001e-03 1.847066465509413e+20 -4.600000000000001e-02 6.000000000000000e-03 1.746418241487460e+20 -4.600000000000001e-02 7.500000000000000e-03 1.624899248612349e+20 -4.600000000000001e-02 9.000000000000001e-03 1.487163683267401e+20 -4.600000000000001e-02 1.050000000000000e-02 1.338295905059591e+20 -4.600000000000001e-02 1.200000000000000e-02 1.183509690192945e+20 -4.600000000000001e-02 1.350000000000000e-02 1.027857281190442e+20 -4.600000000000001e-02 1.500000000000000e-02 8.759691845640287e+19 -4.600000000000001e-02 1.650000000000000e-02 7.318416486880756e+19 -4.600000000000001e-02 1.800000000000000e-02 5.986836478991145e+19 -4.600000000000001e-02 1.950000000000000e-02 4.788295361766566e+19 -4.600000000000001e-02 2.100000000000000e-02 3.737178076861466e+19 -4.600000000000001e-02 2.250000000000000e-02 2.839310567643208e+19 -4.600000000000001e-02 2.400000000000000e-02 2.092876644111593e+19 -4.600000000000001e-02 2.550000000000000e-02 1.489722978971139e+19 -4.600000000000001e-02 2.700000000000000e-02 1.016902658493558e+19 -4.600000000000001e-02 2.850000000000000e-02 6.583027987894027e+18 -4.600000000000001e-02 3.000000000000000e-02 3.962123443046311e+18 -4.600000000000001e-02 3.150000000000000e-02 2.127104311550305e+18 -4.600000000000001e-02 3.300000000000000e-02 9.078997885225126e+17 -4.600000000000001e-02 3.450000000000000e-02 1.517051352355006e+17 -4.600000000000001e-02 3.600000000000000e-02 -2.720683296802269e+17 -4.600000000000001e-02 3.750000000000000e-02 -4.697565808200592e+17 -4.600000000000001e-02 3.900000000000000e-02 -5.238099578128790e+17 -4.600000000000001e-02 4.050000000000000e-02 -4.949184846716355e+17 -4.600000000000001e-02 4.200000000000000e-02 -4.252213752583620e+17 -4.600000000000001e-02 4.350000000000000e-02 -3.419871357538044e+17 -4.600000000000001e-02 4.500000000000000e-02 -2.612715155942288e+17 -4.600000000000001e-02 4.650000000000000e-02 -1.912098139484097e+17 -4.600000000000001e-02 4.800000000000000e-02 -1.347489798757798e+17 -4.600000000000001e-02 4.950000000000000e-02 -9.175242692671582e+16 -4.600000000000001e-02 5.100000000000000e-02 -6.050481196369599e+16 -4.600000000000001e-02 5.250000000000000e-02 -3.870235976491788e+16 -4.600000000000001e-02 5.400000000000000e-02 -2.404050427366765e+16 -4.600000000000001e-02 5.550000000000000e-02 -1.451238366024518e+16 -4.600000000000001e-02 5.700000000000000e-02 -8.517970858683957e+15 -4.600000000000001e-02 5.850000000000000e-02 -4.862423850223992e+15 -4.600000000000001e-02 6.000000000000000e-02 -2.699731961897151e+15 -4.600000000000001e-02 6.150000000000000e-02 -1.457771136463238e+15 -4.600000000000001e-02 6.300000000000000e-02 -7.652824733043197e+14 -4.600000000000001e-02 6.450000000000000e-02 -3.903740378063192e+14 -4.600000000000001e-02 6.600000000000000e-02 -1.933330493262907e+14 -4.600000000000001e-02 6.750000000000000e-02 -9.284808884417131e+13 -4.600000000000001e-02 6.900000000000001e-02 -4.316465464588022e+13 -4.600000000000001e-02 7.050000000000001e-02 -1.937673494949797e+13 -4.600000000000001e-02 7.200000000000001e-02 -8.367776548308960e+12 -4.600000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -4.400000000000000e-02 0.000000000000000e+00 1.989439730706913e+20 -4.400000000000000e-02 1.500000000000000e-03 1.970962566224833e+20 -4.400000000000000e-02 3.000000000000000e-03 1.922896480587564e+20 -4.400000000000000e-02 4.500000000000001e-03 1.847052669376908e+20 -4.400000000000000e-02 6.000000000000000e-03 1.746400684364606e+20 -4.400000000000000e-02 7.500000000000000e-03 1.624877412350552e+20 -4.400000000000000e-02 9.000000000000001e-03 1.487137141356309e+20 -4.400000000000000e-02 1.050000000000000e-02 1.338264375707894e+20 -4.400000000000000e-02 1.200000000000000e-02 1.183473086336371e+20 -4.400000000000000e-02 1.350000000000000e-02 1.027815750648127e+20 -4.400000000000000e-02 1.500000000000000e-02 8.759231337498678e+19 -4.400000000000000e-02 1.650000000000000e-02 7.317917446169389e+19 -4.400000000000000e-02 1.800000000000000e-02 5.986307956353842e+19 -4.400000000000000e-02 1.950000000000000e-02 4.787748320406005e+19 -4.400000000000000e-02 2.100000000000000e-02 3.736624719506208e+19 -4.400000000000000e-02 2.250000000000000e-02 2.838763526282646e+19 -4.400000000000000e-02 2.400000000000000e-02 2.092348121474290e+19 -4.400000000000000e-02 2.550000000000000e-02 1.489223938259773e+19 -4.400000000000000e-02 2.700000000000000e-02 1.016442150351949e+19 -4.400000000000000e-02 2.850000000000000e-02 6.578874933662535e+18 -4.400000000000000e-02 3.000000000000000e-02 3.958463057388866e+18 -4.400000000000000e-02 3.150000000000000e-02 2.123951376380652e+18 -4.400000000000000e-02 3.300000000000000e-02 9.052455974132733e+17 -4.400000000000000e-02 3.450000000000000e-02 1.495215090557912e+17 -4.400000000000000e-02 3.600000000000000e-02 -2.738240419656137e+17 -4.400000000000000e-02 3.750000000000000e-02 -4.711361940705544e+17 -4.400000000000000e-02 3.900000000000000e-02 -5.248694318508439e+17 -4.400000000000000e-02 4.050000000000000e-02 -4.957136404773199e+17 -4.400000000000000e-02 4.200000000000000e-02 -4.258046096198614e+17 -4.400000000000000e-02 4.350000000000000e-02 -3.424052191539859e+17 -4.400000000000000e-02 4.500000000000000e-02 -2.615644104198491e+17 -4.400000000000000e-02 4.650000000000000e-02 -1.914103485998669e+17 -4.400000000000000e-02 4.800000000000000e-02 -1.348831624467760e+17 -4.400000000000000e-02 4.950000000000000e-02 -9.184017381888053e+16 -4.400000000000000e-02 5.100000000000000e-02 -6.056089045631015e+16 -4.400000000000000e-02 5.250000000000000e-02 -3.873738571080286e+16 -4.400000000000000e-02 5.400000000000000e-02 -2.406188450336014e+16 -4.400000000000000e-02 5.550000000000000e-02 -1.452513817128687e+16 -4.400000000000000e-02 5.700000000000000e-02 -8.525406941447359e+15 -4.400000000000000e-02 5.850000000000000e-02 -4.866660802465856e+15 -4.400000000000000e-02 6.000000000000000e-02 -2.702091309204776e+15 -4.400000000000000e-02 6.150000000000000e-02 -1.459055119056946e+15 -4.400000000000000e-02 6.300000000000000e-02 -7.659653705323446e+14 -4.400000000000000e-02 6.450000000000000e-02 -3.907289987061692e+14 -4.400000000000000e-02 6.600000000000000e-02 -1.935133654807342e+14 -4.400000000000000e-02 6.750000000000000e-02 -9.293760835698061e+13 -4.400000000000000e-02 6.900000000000001e-02 -4.320808863682337e+13 -4.400000000000000e-02 7.050000000000001e-02 -1.939733037249774e+13 -4.400000000000000e-02 7.200000000000001e-02 -8.377320772870229e+12 -4.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -4.200000000000000e-02 0.000000000000000e+00 1.989431807171152e+20 -4.200000000000000e-02 1.500000000000000e-03 1.970951763628351e+20 -4.200000000000000e-02 3.000000000000000e-03 1.922882087093316e+20 -4.200000000000000e-02 4.500000000000001e-03 1.847033926628456e+20 -4.200000000000000e-02 6.000000000000000e-03 1.746376832119270e+20 -4.200000000000000e-02 7.500000000000000e-03 1.624847746677084e+20 -4.200000000000000e-02 9.000000000000001e-03 1.487101082818680e+20 -4.200000000000000e-02 1.050000000000000e-02 1.338221541478265e+20 -4.200000000000000e-02 1.200000000000000e-02 1.183423358133491e+20 -4.200000000000000e-02 1.350000000000000e-02 1.027759329291821e+20 -4.200000000000000e-02 1.500000000000000e-02 8.758605713741046e+19 -4.200000000000000e-02 1.650000000000000e-02 7.317239473953815e+19 -4.200000000000000e-02 1.800000000000000e-02 5.985589931440779e+19 -4.200000000000000e-02 1.950000000000000e-02 4.787005136864495e+19 -4.200000000000000e-02 2.100000000000000e-02 3.735872955364316e+19 -4.200000000000000e-02 2.250000000000000e-02 2.838020342741137e+19 -4.200000000000000e-02 2.400000000000000e-02 2.091630096561227e+19 -4.200000000000000e-02 2.550000000000000e-02 1.488545966044199e+19 -4.200000000000000e-02 2.700000000000000e-02 1.015816526594317e+19 -4.200000000000000e-02 2.850000000000000e-02 6.573232798031931e+18 -4.200000000000000e-02 3.000000000000000e-02 3.953490237100842e+18 -4.200000000000000e-02 3.150000000000000e-02 2.119667953417670e+18 -4.200000000000000e-02 3.300000000000000e-02 9.016397436504415e+17 -4.200000000000000e-02 3.450000000000000e-02 1.465549417090339e+17 -4.200000000000000e-02 3.600000000000000e-02 -2.762092664992479e+17 -4.200000000000000e-02 3.750000000000000e-02 -4.730104689158108e+17 -4.200000000000000e-02 3.900000000000000e-02 -5.263087812756535e+17 -4.200000000000000e-02 4.050000000000000e-02 -4.967939001255357e+17 -4.200000000000000e-02 4.200000000000000e-02 -4.265969631959489e+17 -4.200000000000000e-02 4.350000000000000e-02 -3.429732067402881e+17 -4.200000000000000e-02 4.500000000000000e-02 -2.619623229535023e+17 -4.200000000000000e-02 4.650000000000000e-02 -1.916827851343041e+17 -4.200000000000000e-02 4.800000000000000e-02 -1.350654563015210e+17 -4.200000000000000e-02 4.950000000000000e-02 -9.195938243961150e+16 -4.200000000000000e-02 5.100000000000000e-02 -6.063707594382187e+16 -4.200000000000000e-02 5.250000000000000e-02 -3.878497024167046e+16 -4.200000000000000e-02 5.400000000000000e-02 -2.409093063399427e+16 -4.200000000000000e-02 5.550000000000000e-02 -1.454246582394635e+16 -4.200000000000000e-02 5.700000000000000e-02 -8.535509238497410e+15 -4.200000000000000e-02 5.850000000000000e-02 -4.872416917815305e+15 -4.200000000000000e-02 6.000000000000000e-02 -2.705296602650832e+15 -4.200000000000000e-02 6.150000000000000e-02 -1.460799474785822e+15 -4.200000000000000e-02 6.300000000000000e-02 -7.668931211870464e+14 -4.200000000000000e-02 6.450000000000000e-02 -3.912112311618227e+14 -4.200000000000000e-02 6.600000000000000e-02 -1.937583341575321e+14 -4.200000000000000e-02 6.750000000000000e-02 -9.305922517311216e+13 -4.200000000000000e-02 6.900000000000001e-02 -4.326709592500695e+13 -4.200000000000000e-02 7.050000000000001e-02 -1.942531030328053e+13 -4.200000000000000e-02 7.200000000000001e-02 -8.390287087890936e+12 -4.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -4.000000000000001e-02 0.000000000000000e+00 1.989421145628713e+20 -4.000000000000001e-02 1.500000000000000e-03 1.970937228155259e+20 -4.000000000000001e-02 3.000000000000000e-03 1.922862719874640e+20 -4.000000000000001e-02 4.500000000000001e-03 1.847008707254924e+20 -4.000000000000001e-02 6.000000000000000e-03 1.746344737643572e+20 -4.000000000000001e-02 7.500000000000000e-03 1.624807829921964e+20 -4.000000000000001e-02 9.000000000000001e-03 1.487052564121875e+20 -4.000000000000001e-02 1.050000000000000e-02 1.338163905724376e+20 -4.000000000000001e-02 1.200000000000000e-02 1.183356446168754e+20 -4.000000000000001e-02 1.350000000000000e-02 1.027683411330084e+20 -4.000000000000001e-02 1.500000000000000e-02 8.757763903412412e+19 -4.000000000000001e-02 1.650000000000000e-02 7.316327225966690e+19 -4.000000000000001e-02 1.800000000000000e-02 5.984623790400483e+19 -4.000000000000001e-02 1.950000000000000e-02 4.786005143539942e+19 -4.000000000000001e-02 2.100000000000000e-02 3.734861416381628e+19 -4.000000000000001e-02 2.250000000000000e-02 2.837020349416584e+19 -4.000000000000001e-02 2.400000000000000e-02 2.090663955520931e+19 -4.000000000000001e-02 2.550000000000000e-02 1.487633718057074e+19 -4.000000000000001e-02 2.700000000000000e-02 1.014974716265683e+19 -4.000000000000001e-02 2.850000000000000e-02 6.565641001858186e+18 -4.000000000000001e-02 3.000000000000000e-02 3.946799040627195e+18 -4.000000000000001e-02 3.150000000000000e-02 2.113904378028856e+18 -4.000000000000001e-02 3.300000000000000e-02 8.967878739698781e+17 -4.000000000000001e-02 3.450000000000000e-02 1.425632661969972e+17 -4.000000000000001e-02 3.600000000000000e-02 -2.794187140690205e+17 -4.000000000000001e-02 3.750000000000000e-02 -4.755324062690330e+17 -4.000000000000001e-02 3.900000000000000e-02 -5.282455031432884e+17 -4.000000000000001e-02 4.050000000000000e-02 -4.982474474347308e+17 -4.000000000000001e-02 4.200000000000000e-02 -4.276631174398431e+17 -4.000000000000001e-02 4.350000000000000e-02 -3.437374645083992e+17 -4.000000000000001e-02 4.500000000000000e-02 -2.624977356142840e+17 -4.000000000000001e-02 4.650000000000000e-02 -1.920493631067496e+17 -4.000000000000001e-02 4.800000000000000e-02 -1.353107424625703e+17 -4.000000000000001e-02 4.950000000000000e-02 -9.211978403397130e+16 -4.000000000000001e-02 5.100000000000000e-02 -6.073958760437985e+16 -4.000000000000001e-02 5.250000000000000e-02 -3.884899778071269e+16 -4.000000000000001e-02 5.400000000000000e-02 -2.413001376099571e+16 -4.000000000000001e-02 5.550000000000000e-02 -1.456578111017354e+16 -4.000000000000001e-02 5.700000000000000e-02 -8.549102421134604e+15 -4.000000000000001e-02 5.850000000000000e-02 -4.880162079815409e+15 -4.000000000000001e-02 6.000000000000000e-02 -2.709609496936378e+15 -4.000000000000001e-02 6.150000000000000e-02 -1.463146598998204e+15 -4.000000000000001e-02 6.300000000000000e-02 -7.681414594638420e+14 -4.000000000000001e-02 6.450000000000000e-02 -3.918601008011537e+14 -4.000000000000001e-02 6.600000000000000e-02 -1.940879526539601e+14 -4.000000000000001e-02 6.750000000000000e-02 -9.322286712357545e+13 -4.000000000000001e-02 6.900000000000001e-02 -4.334649339681272e+13 -4.000000000000001e-02 7.050000000000001e-02 -1.946295880118375e+13 -4.000000000000001e-02 7.200000000000001e-02 -8.407733960353173e+12 -4.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -3.800000000000001e-02 0.000000000000000e+00 1.989406937781634e+20 -3.800000000000001e-02 1.500000000000000e-03 1.970917857808042e+20 -3.800000000000001e-02 3.000000000000000e-03 1.922836910618345e+20 -3.800000000000001e-02 4.500000000000001e-03 1.846975099265777e+20 -3.800000000000001e-02 6.000000000000000e-03 1.746301967715543e+20 -3.800000000000001e-02 7.500000000000000e-03 1.624754635822152e+20 -3.800000000000001e-02 9.000000000000001e-03 1.486987906852194e+20 -3.800000000000001e-02 1.050000000000000e-02 1.338087098828731e+20 -3.800000000000001e-02 1.200000000000000e-02 1.183267277554722e+20 -3.800000000000001e-02 1.350000000000000e-02 1.027582241091623e+20 -3.800000000000001e-02 1.500000000000000e-02 8.756642085205788e+19 -3.800000000000001e-02 1.650000000000000e-02 7.315111540715390e+19 -3.800000000000001e-02 1.800000000000000e-02 5.983336285873269e+19 -3.800000000000001e-02 1.950000000000000e-02 4.784672526583570e+19 -3.800000000000001e-02 2.100000000000000e-02 3.733513413382744e+19 -3.800000000000001e-02 2.250000000000000e-02 2.835687732460213e+19 -3.800000000000001e-02 2.400000000000000e-02 2.089376450993717e+19 -3.800000000000001e-02 2.550000000000000e-02 1.486418032805773e+19 -3.800000000000001e-02 2.700000000000000e-02 1.013852898059059e+19 -3.800000000000001e-02 2.850000000000000e-02 6.555523978012075e+18 -3.800000000000001e-02 3.000000000000000e-02 3.937882179223959e+18 -3.800000000000001e-02 3.150000000000000e-02 2.106223688464357e+18 -3.800000000000001e-02 3.300000000000000e-02 8.903221470018336e+17 -3.800000000000001e-02 3.450000000000000e-02 1.372438562158820e+17 -3.800000000000001e-02 3.600000000000000e-02 -2.836957068719258e+17 -3.800000000000001e-02 3.750000000000000e-02 -4.788932051836803e+17 -3.800000000000001e-02 3.900000000000000e-02 -5.308264287727078e+17 -3.800000000000001e-02 4.050000000000000e-02 -5.001844821564257e+17 -3.800000000000001e-02 4.200000000000000e-02 -4.290839021477375e+17 -3.800000000000001e-02 4.350000000000000e-02 -3.447559341679633e+17 -3.800000000000001e-02 4.500000000000000e-02 -2.632112403676613e+17 -3.800000000000001e-02 4.650000000000000e-02 -1.925378743896941e+17 -3.800000000000001e-02 4.800000000000000e-02 -1.356376171419825e+17 -3.800000000000001e-02 4.950000000000000e-02 -9.233353934535653e+16 -3.800000000000001e-02 5.100000000000000e-02 -6.087619729339601e+16 -3.800000000000001e-02 5.250000000000000e-02 -3.893432253449602e+16 -3.800000000000001e-02 5.400000000000000e-02 -2.418209694642442e+16 -3.800000000000001e-02 5.550000000000000e-02 -1.459685166335240e+16 -3.800000000000001e-02 5.700000000000000e-02 -8.567217047731223e+15 -3.800000000000001e-02 5.850000000000000e-02 -4.890483482926577e+15 -3.800000000000001e-02 6.000000000000000e-02 -2.715356971359298e+15 -3.800000000000001e-02 6.150000000000000e-02 -1.466274437402055e+15 -3.800000000000001e-02 6.300000000000000e-02 -7.698050273238475e+14 -3.800000000000001e-02 6.450000000000000e-02 -3.927248012572633e+14 -3.800000000000001e-02 6.600000000000000e-02 -1.945272107836782e+14 -3.800000000000001e-02 6.750000000000000e-02 -9.344094061727472e+13 -3.800000000000001e-02 6.900000000000001e-02 -4.345230052034401e+13 -3.800000000000001e-02 7.050000000000001e-02 -1.951313016278779e+13 -3.800000000000001e-02 7.200000000000001e-02 -8.430984113637179e+12 -3.800000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -3.600000000000000e-02 0.000000000000000e+00 1.958381060798761e+20 -3.600000000000000e-02 1.500000000000000e-03 1.940112140205665e+20 -3.600000000000000e-02 3.000000000000000e-03 1.892693693052508e+20 -3.600000000000000e-02 4.500000000000001e-03 1.817907571102690e+20 -3.600000000000000e-02 6.000000000000000e-03 1.718677236249814e+20 -3.600000000000000e-02 7.500000000000000e-03 1.598880069383853e+20 -3.600000000000000e-02 9.000000000000001e-03 1.463101582750769e+20 -3.600000000000000e-02 1.050000000000000e-02 1.316352794172394e+20 -3.600000000000000e-02 1.200000000000000e-02 1.163774026624757e+20 -3.600000000000000e-02 1.350000000000000e-02 1.010348095414202e+20 -3.600000000000000e-02 1.500000000000000e-02 8.606435167516353e+19 -3.600000000000000e-02 1.650000000000000e-02 7.186044579939289e+19 -3.600000000000000e-02 1.800000000000000e-02 5.873991634599145e+19 -3.600000000000000e-02 1.950000000000000e-02 4.693330436711146e+19 -3.600000000000000e-02 2.100000000000000e-02 3.658269879996856e+19 -3.600000000000000e-02 2.250000000000000e-02 2.774561851118980e+19 -3.600000000000000e-02 2.400000000000000e-02 2.040402051318057e+19 -3.600000000000000e-02 2.550000000000000e-02 1.447716589005718e+19 -3.600000000000000e-02 2.700000000000000e-02 9.836868002863948e+18 -3.600000000000000e-02 2.850000000000000e-02 6.323594032003104e+18 -3.600000000000000e-02 3.000000000000000e-02 3.761991759497413e+18 -3.600000000000000e-02 3.150000000000000e-02 1.974651014089971e+18 -3.600000000000000e-02 3.300000000000000e-02 7.932476399756314e+17 -3.600000000000000e-02 3.450000000000000e-02 6.660802833781465e+16 -3.600000000000000e-02 3.600000000000000e-02 -3.343803027763710e+17 -3.600000000000000e-02 3.750000000000000e-02 -5.147519904273275e+17 -3.600000000000000e-02 3.900000000000000e-02 -5.558361671690104e+17 -3.600000000000000e-02 4.050000000000000e-02 -5.173766841968634e+17 -3.600000000000000e-02 4.200000000000000e-02 -4.407296929506065e+17 -3.600000000000000e-02 4.350000000000000e-02 -3.525277404729331e+17 -3.600000000000000e-02 4.500000000000000e-02 -2.683196726049307e+17 -3.600000000000000e-02 4.650000000000000e-02 -1.958443310129411e+17 -3.600000000000000e-02 4.800000000000000e-02 -1.377445315723872e+17 -3.600000000000000e-02 4.950000000000000e-02 -9.365497016089387e+16 -3.600000000000000e-02 5.100000000000000e-02 -6.169177954381297e+16 -3.600000000000000e-02 5.250000000000000e-02 -3.942958933873210e+16 -3.600000000000000e-02 5.400000000000000e-02 -2.447796153772654e+16 -3.600000000000000e-02 5.550000000000000e-02 -1.477070247514070e+16 -3.600000000000000e-02 5.700000000000000e-02 -8.667690816199799e+15 -3.600000000000000e-02 5.850000000000000e-02 -4.947591707883359e+15 -3.600000000000000e-02 6.000000000000000e-02 -2.747280314497794e+15 -3.600000000000000e-02 6.150000000000000e-02 -1.483825024335633e+15 -3.600000000000000e-02 6.300000000000000e-02 -7.792952025245114e+14 -3.600000000000000e-02 6.450000000000000e-02 -3.977725436196496e+14 -3.600000000000000e-02 6.600000000000000e-02 -1.971685000039686e+14 -3.600000000000000e-02 6.750000000000000e-02 -9.480081613249694e+13 -3.600000000000000e-02 6.900000000000001e-02 -4.414131261309257e+13 -3.600000000000000e-02 7.050000000000001e-02 -1.985675821926582e+13 -3.600000000000000e-02 7.200000000000001e-02 -8.599709825651975e+12 -3.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -3.400000000000000e-02 0.000000000000000e+00 1.726993792496927e+20 -3.400000000000000e-02 1.500000000000000e-03 1.710409546330492e+20 -3.400000000000000e-02 3.000000000000000e-03 1.667986710346478e+20 -3.400000000000000e-02 4.500000000000001e-03 1.601290298604086e+20 -3.400000000000000e-02 6.000000000000000e-03 1.512899954498958e+20 -3.400000000000000e-02 7.500000000000000e-03 1.406246490511158e+20 -3.400000000000000e-02 9.000000000000001e-03 1.285396583767275e+20 -3.400000000000000e-02 1.050000000000000e-02 1.154803990150382e+20 -3.400000000000000e-02 1.200000000000000e-02 1.019047478485169e+20 -3.400000000000000e-02 1.350000000000000e-02 8.825755714961849e+19 -3.400000000000000e-02 1.500000000000000e-02 7.494763432186913e+19 -3.400000000000000e-02 1.650000000000000e-02 6.232873191058366e+19 -3.400000000000000e-02 1.800000000000000e-02 5.068563588035280e+19 -3.400000000000000e-02 1.950000000000000e-02 4.022596729795009e+19 -3.400000000000000e-02 2.100000000000000e-02 3.107782132754312e+19 -3.400000000000000e-02 2.250000000000000e-02 2.329289396233297e+19 -3.400000000000000e-02 2.400000000000000e-02 1.685432655009150e+19 -3.400000000000000e-02 2.550000000000000e-02 1.168816513045004e+19 -3.400000000000000e-02 2.700000000000000e-02 7.677116089246907e+18 -3.400000000000000e-02 2.850000000000000e-02 4.675202822535769e+18 -3.400000000000000e-02 3.000000000000000e-02 2.521996543347087e+18 -3.400000000000000e-02 3.150000000000000e-02 1.055296062086532e+18 -3.400000000000000e-02 3.300000000000000e-02 1.214354675712281e+17 -3.400000000000000e-02 3.450000000000000e-02 -4.172404537381523e+17 -3.400000000000000e-02 3.600000000000000e-02 -6.778278849010461e+17 -3.400000000000000e-02 3.750000000000000e-02 -7.550172450636564e+17 -3.400000000000000e-02 3.900000000000000e-02 -7.214848272470981e+17 -3.400000000000000e-02 4.050000000000000e-02 -6.299241280510703e+17 -3.400000000000000e-02 4.200000000000000e-02 -5.160853627373839e+17 -3.400000000000000e-02 4.350000000000000e-02 -4.022451593906061e+17 -3.400000000000000e-02 4.500000000000000e-02 -3.006411883982574e+17 -3.400000000000000e-02 4.650000000000000e-02 -2.165477728749881e+17 -3.400000000000000e-02 4.800000000000000e-02 -1.508103898797980e+17 -3.400000000000000e-02 4.950000000000000e-02 -1.017786949844395e+17 -3.400000000000000e-02 5.100000000000000e-02 -6.666769297302212e+16 -3.400000000000000e-02 5.250000000000000e-02 -4.243200751934748e+16 -3.400000000000000e-02 5.400000000000000e-02 -2.626253037580935e+16 -3.400000000000000e-02 5.550000000000000e-02 -1.581553192142089e+16 -3.400000000000000e-02 5.700000000000000e-02 -9.270246799458944e+15 -3.400000000000000e-02 5.850000000000000e-02 -5.289873114334828e+15 -3.400000000000000e-02 6.000000000000000e-02 -2.938794708319736e+15 -3.400000000000000e-02 6.150000000000000e-02 -1.589374092591848e+15 -3.400000000000000e-02 6.300000000000000e-02 -8.365944852369806e+14 -3.400000000000000e-02 6.450000000000000e-02 -4.284131037158241e+14 -3.400000000000000e-02 6.600000000000000e-02 -2.133087958797110e+14 -3.400000000000000e-02 6.750000000000000e-02 -1.031763247637738e+14 -3.400000000000000e-02 6.900000000000001e-02 -4.842300913542045e+13 -3.400000000000000e-02 7.050000000000001e-02 -2.201324801978717e+13 -3.400000000000000e-02 7.200000000000001e-02 -9.669820322929199e+12 -3.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -3.200000000000000e-02 0.000000000000000e+00 1.342599655230234e+20 -3.200000000000000e-02 1.500000000000000e-03 1.328817423555858e+20 -3.200000000000000e-02 3.000000000000000e-03 1.294697861801759e+20 -3.200000000000000e-02 4.500000000000001e-03 1.241445804867175e+20 -3.200000000000000e-02 6.000000000000000e-03 1.171069713414357e+20 -3.200000000000000e-02 7.500000000000000e-03 1.086258452923842e+20 -3.200000000000000e-02 9.000000000000001e-03 9.902166195924669e+19 -3.200000000000000e-02 1.050000000000000e-02 8.864719681133681e+19 -3.200000000000000e-02 1.200000000000000e-02 7.786700583440361e+19 -3.200000000000000e-02 1.350000000000000e-02 6.703714316853097e+19 -3.200000000000000e-02 1.500000000000000e-02 5.648656058304769e+19 -3.200000000000000e-02 1.650000000000000e-02 4.650141510171733e+19 -3.200000000000000e-02 1.800000000000000e-02 3.731323053980244e+19 -3.200000000000000e-02 1.950000000000000e-02 2.909152154529509e+19 -3.200000000000000e-02 2.100000000000000e-02 2.194111634061327e+19 -3.200000000000000e-02 2.250000000000000e-02 1.590403077171095e+19 -3.200000000000000e-02 2.400000000000000e-02 1.096538034106400e+19 -3.200000000000000e-02 2.550000000000000e-02 7.062502038169486e+18 -3.200000000000000e-02 2.700000000000000e-02 4.096228305862271e+18 -3.200000000000000e-02 2.850000000000000e-02 1.943140167647320e+18 -3.200000000000000e-02 3.000000000000000e-02 4.676412941466499e+17 -3.200000000000000e-02 3.150000000000000e-02 -4.671629714480762e+17 -3.200000000000000e-02 3.300000000000000e-02 -9.905506030424362e+17 -3.200000000000000e-02 3.450000000000000e-02 -1.217688699866603e+18 -3.200000000000000e-02 3.600000000000000e-02 -1.245688473361006e+18 -3.200000000000000e-02 3.750000000000000e-02 -1.152041382721101e+18 -3.200000000000000e-02 3.900000000000000e-02 -9.950423853116484e+17 -3.200000000000000e-02 4.050000000000000e-02 -8.156724541153292e+17 -3.200000000000000e-02 4.200000000000000e-02 -6.403739572144260e+17 -3.200000000000000e-02 4.350000000000000e-02 -4.841957228605541e+17 -3.200000000000000e-02 4.500000000000000e-02 -3.538850744187377e+17 -3.200000000000000e-02 4.650000000000000e-02 -2.506330397996606e+17 -3.200000000000000e-02 4.800000000000000e-02 -1.723097011756985e+17 -3.200000000000000e-02 4.950000000000000e-02 -1.151392757159180e+17 -3.200000000000000e-02 5.100000000000000e-02 -7.484766859874830e+16 -3.200000000000000e-02 5.250000000000000e-02 -4.736589239419738e+16 -3.200000000000000e-02 5.400000000000000e-02 -2.919425268608602e+16 -3.200000000000000e-02 5.550000000000000e-02 -1.753163156528608e+16 -3.200000000000000e-02 5.700000000000000e-02 -1.025980193144227e+16 -3.200000000000000e-02 5.850000000000000e-02 -5.851969168421649e+15 -3.200000000000000e-02 6.000000000000000e-02 -3.253317970495488e+15 -3.200000000000000e-02 6.150000000000000e-02 -1.762742046364302e+15 -3.200000000000000e-02 6.300000000000000e-02 -9.307323214366696e+14 -3.200000000000000e-02 6.450000000000000e-02 -4.787686885896277e+14 -3.200000000000000e-02 6.600000000000000e-02 -2.398445048027427e+14 -3.200000000000000e-02 6.750000000000000e-02 -1.169524591872856e+14 -3.200000000000000e-02 6.900000000000001e-02 -5.546918723444174e+13 -3.200000000000000e-02 7.050000000000001e-02 -2.556405228323774e+13 -3.200000000000000e-02 7.200000000000001e-02 -1.143287099991862e+13 -3.200000000000000e-02 7.350000000000000e-02 -4.952313197235734e+12 -3.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -3.000000000000000e-02 0.000000000000000e+00 9.193893977537623e+19 -3.000000000000000e-02 1.500000000000000e-03 9.086943440554013e+19 -3.000000000000000e-02 3.000000000000000e-03 8.837193599308005e+19 -3.000000000000000e-02 4.500000000000001e-03 8.452727597276753e+19 -3.000000000000000e-02 6.000000000000000e-03 7.947341358811813e+19 -3.000000000000000e-02 7.500000000000000e-03 7.339754310321480e+19 -3.000000000000000e-02 9.000000000000001e-03 6.652520001645658e+19 -3.000000000000000e-02 1.050000000000000e-02 5.910719264215435e+19 -3.000000000000000e-02 1.200000000000000e-02 5.140531111149910e+19 -3.000000000000000e-02 1.350000000000000e-02 4.367781913689892e+19 -3.000000000000000e-02 1.500000000000000e-02 3.616572128001666e+19 -3.000000000000000e-02 1.650000000000000e-02 2.908072548081019e+19 -3.000000000000000e-02 1.800000000000000e-02 2.259568976166265e+19 -3.000000000000000e-02 1.950000000000000e-02 1.683815416661504e+19 -3.000000000000000e-02 2.100000000000000e-02 1.188731741186186e+19 -3.000000000000000e-02 2.250000000000000e-02 7.774533143775795e+18 -3.000000000000000e-02 2.400000000000000e-02 4.487094800879145e+18 -3.000000000000000e-02 2.550000000000000e-02 1.974783365064548e+18 -3.000000000000000e-02 2.700000000000000e-02 1.584075936105094e+17 -3.000000000000000e-02 2.850000000000000e-02 -1.060591239195777e+18 -3.000000000000000e-02 3.000000000000000e-02 -1.790442322253633e+18 -3.000000000000000e-02 3.150000000000000e-02 -2.140151422875073e+18 -3.000000000000000e-02 3.300000000000000e-02 -2.212121425768509e+18 -3.000000000000000e-02 3.450000000000000e-02 -2.096740154170911e+18 -3.000000000000000e-02 3.600000000000000e-02 -1.869100618986776e+18 -3.000000000000000e-02 3.750000000000000e-02 -1.587748906824069e+18 -3.000000000000000e-02 3.900000000000000e-02 -1.295141939281723e+18 -3.000000000000000e-02 4.050000000000000e-02 -1.019365395236765e+18 -3.000000000000000e-02 4.200000000000000e-02 -7.766172546537050e+17 -3.000000000000000e-02 4.350000000000000e-02 -5.739943380066424e+17 -3.000000000000000e-02 4.500000000000000e-02 -4.122061001964026e+17 -3.000000000000000e-02 4.650000000000000e-02 -2.879551925477066e+17 -3.000000000000000e-02 4.800000000000000e-02 -1.958427924082032e+17 -3.000000000000000e-02 4.950000000000000e-02 -1.297592635061398e+17 -3.000000000000000e-02 5.100000000000000e-02 -8.379629750694573e+16 -3.000000000000000e-02 5.250000000000000e-02 -5.276217146836358e+16 -3.000000000000000e-02 5.400000000000000e-02 -3.240014834595936e+16 -3.000000000000000e-02 5.550000000000000e-02 -1.940797457899783e+16 -3.000000000000000e-02 5.700000000000000e-02 -1.134167476171395e+16 -3.000000000000000e-02 5.850000000000000e-02 -6.466490987238027e+15 -3.000000000000000e-02 6.000000000000000e-02 -3.597188040060895e+15 -3.000000000000000e-02 6.150000000000000e-02 -1.952303140326216e+15 -3.000000000000000e-02 6.300000000000000e-02 -1.033677600381894e+15 -3.000000000000000e-02 6.450000000000000e-02 -5.338460816849367e+14 -3.000000000000000e-02 6.600000000000000e-02 -2.688753543920622e+14 -3.000000000000000e-02 6.750000000000000e-02 -1.320281525738987e+14 -3.000000000000000e-02 6.900000000000001e-02 -6.318247239724449e+13 -3.000000000000000e-02 7.050000000000001e-02 -2.945235895254494e+13 -3.000000000000000e-02 7.200000000000001e-02 -1.336419786187471e+13 -3.000000000000000e-02 7.350000000000000e-02 -5.897549606023740e+12 -3.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -2.800000000000000e-02 0.000000000000000e+00 5.534705202268496e+19 -2.800000000000000e-02 1.500000000000000e-03 5.454694169460486e+19 -2.800000000000000e-02 3.000000000000000e-03 5.284327114738221e+19 -2.800000000000000e-02 4.500000000000001e-03 5.028262046390616e+19 -2.800000000000000e-02 6.000000000000000e-03 4.694856694941878e+19 -2.800000000000000e-02 7.500000000000000e-03 4.295761133154121e+19 -2.800000000000000e-02 9.000000000000001e-03 3.845309555876263e+19 -2.800000000000000e-02 1.050000000000000e-02 3.359748305719909e+19 -2.800000000000000e-02 1.200000000000000e-02 2.856347124255147e+19 -2.800000000000000e-02 1.350000000000000e-02 2.352448791076519e+19 -2.800000000000000e-02 1.500000000000000e-02 1.864518688147912e+19 -2.800000000000000e-02 1.650000000000000e-02 1.407259602377684e+19 -2.800000000000000e-02 1.800000000000000e-02 9.928568188940055e+18 -2.800000000000000e-02 1.950000000000000e-02 6.304125977496618e+18 -2.800000000000000e-02 2.100000000000000e-02 3.256162523948290e+18 -2.800000000000000e-02 2.250000000000000e-02 8.067619391286429e+17 -2.800000000000000e-02 2.400000000000000e-02 -1.054849859092831e+18 -2.800000000000000e-02 2.550000000000000e-02 -2.367988929818816e+18 -2.800000000000000e-02 2.700000000000000e-02 -3.194352843216528e+18 -2.800000000000000e-02 2.850000000000000e-02 -3.610729649142036e+18 -2.800000000000000e-02 3.000000000000000e-02 -3.701384181533150e+18 -2.800000000000000e-02 3.150000000000000e-02 -3.550908944209832e+18 -2.800000000000000e-02 3.300000000000000e-02 -3.238197362469479e+18 -2.800000000000000e-02 3.450000000000000e-02 -2.831986097093342e+18 -2.800000000000000e-02 3.600000000000000e-02 -2.388161855300778e+18 -2.800000000000000e-02 3.750000000000000e-02 -1.948782387482348e+18 -2.800000000000000e-02 3.900000000000000e-02 -1.542560785437272e+18 -2.800000000000000e-02 4.050000000000000e-02 -1.186432668762420e+18 -2.800000000000000e-02 4.200000000000000e-02 -8.877759483633558e+17 -2.800000000000000e-02 4.350000000000000e-02 -6.468749446751380e+17 -2.800000000000000e-02 4.500000000000000e-02 -4.592954295132971e+17 -2.800000000000000e-02 4.650000000000000e-02 -3.179400697305523e+17 -2.800000000000000e-02 4.800000000000000e-02 -2.146610547965453e+17 -2.800000000000000e-02 4.950000000000000e-02 -1.414000550930842e+17 -2.800000000000000e-02 5.100000000000000e-02 -9.089433935677376e+16 -2.800000000000000e-02 5.250000000000000e-02 -5.702868298006871e+16 -2.800000000000000e-02 5.400000000000000e-02 -3.492832746873703e+16 -2.800000000000000e-02 5.550000000000000e-02 -2.088491014726528e+16 -2.800000000000000e-02 5.700000000000000e-02 -1.219231807760366e+16 -2.800000000000000e-02 5.850000000000000e-02 -6.949520562406188e+15 -2.800000000000000e-02 6.000000000000000e-02 -3.867610351966497e+15 -2.800000000000000e-02 6.150000000000000e-02 -2.101565500702896e+15 -2.800000000000000e-02 6.300000000000000e-02 -1.114902238468741e+15 -2.800000000000000e-02 6.450000000000000e-02 -5.774213821708770e+14 -2.800000000000000e-02 6.600000000000000e-02 -2.919210023264782e+14 -2.800000000000000e-02 6.750000000000000e-02 -1.440427822943261e+14 -2.800000000000000e-02 6.900000000000001e-02 -6.935664800530206e+13 -2.800000000000000e-02 7.050000000000001e-02 -3.257964118886531e+13 -2.800000000000000e-02 7.200000000000001e-02 -1.492535400576321e+13 -2.800000000000000e-02 7.350000000000000e-02 -6.665598163865572e+12 -2.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -2.600000000000001e-02 0.000000000000000e+00 2.914185367742163e+19 -2.600000000000001e-02 1.500000000000000e-03 2.853797993711005e+19 -2.600000000000001e-02 3.000000000000000e-03 2.740704744638411e+19 -2.600000000000001e-02 4.500000000000001e-03 2.577115132120753e+19 -2.600000000000001e-02 6.000000000000000e-03 2.367491221993154e+19 -2.600000000000001e-02 7.500000000000000e-03 2.118412315014070e+19 -2.600000000000001e-02 9.000000000000001e-03 1.838310299418075e+19 -2.600000000000001e-02 1.050000000000000e-02 1.537080408521239e+19 -2.600000000000001e-02 1.200000000000000e-02 1.225580045391693e+19 -2.600000000000001e-02 1.350000000000000e-02 9.150384573554479e+18 -2.600000000000001e-02 1.500000000000000e-02 6.164117351587587e+18 -2.600000000000001e-02 1.650000000000000e-02 3.397291446323331e+18 -2.600000000000001e-02 1.800000000000000e-02 9.348556066708936e+17 -2.600000000000001e-02 1.950000000000000e-02 -1.158621146539403e+18 -2.600000000000001e-02 2.100000000000000e-02 -2.842414966552431e+18 -2.600000000000001e-02 2.250000000000000e-02 -4.101148074805183e+18 -2.600000000000001e-02 2.400000000000000e-02 -4.944144427740471e+18 -2.600000000000001e-02 2.550000000000000e-02 -5.402719541626129e+18 -2.600000000000001e-02 2.700000000000000e-02 -5.525745879650286e+18 -2.600000000000001e-02 2.850000000000000e-02 -5.374050740735109e+18 -2.600000000000001e-02 3.000000000000000e-02 -5.014332151337360e+18 -2.600000000000001e-02 3.150000000000000e-02 -4.513297284645262e+18 -2.600000000000001e-02 3.300000000000000e-02 -3.932638011641697e+18 -2.600000000000001e-02 3.450000000000000e-02 -3.325282180819807e+18 -2.600000000000001e-02 3.600000000000000e-02 -2.733135718536769e+18 -2.600000000000001e-02 3.750000000000000e-02 -2.186303982577649e+18 -2.600000000000001e-02 3.900000000000000e-02 -1.703590645170674e+18 -2.600000000000001e-02 4.050000000000000e-02 -1.293945640809708e+18 -2.600000000000001e-02 4.200000000000000e-02 -9.584806748814760e+17 -2.600000000000001e-02 4.350000000000000e-02 -6.926857792578845e+17 -2.600000000000001e-02 4.500000000000000e-02 -4.885460553526322e+17 -2.600000000000001e-02 4.650000000000000e-02 -3.363511031203452e+17 -2.600000000000001e-02 4.800000000000000e-02 -2.260881684637283e+17 -2.600000000000001e-02 4.950000000000000e-02 -1.483961486041606e+17 -2.600000000000001e-02 5.100000000000000e-02 -9.512084021468994e+16 -2.600000000000001e-02 5.250000000000000e-02 -5.954898183433835e+16 -2.600000000000001e-02 5.400000000000000e-02 -3.641219482606543e+16 -2.600000000000001e-02 5.550000000000000e-02 -2.174772213383878e+16 -2.600000000000001e-02 5.700000000000000e-02 -1.268787663635168e+16 -2.600000000000001e-02 5.850000000000000e-02 -7.230697569140109e+15 -2.600000000000001e-02 6.000000000000000e-02 -4.025220590007995e+15 -2.600000000000001e-02 6.150000000000000e-02 -2.188839972952641e+15 -2.600000000000001e-02 6.300000000000000e-02 -1.162636764882976e+15 -2.600000000000001e-02 6.450000000000000e-02 -6.032044479823062e+14 -2.600000000000001e-02 6.600000000000000e-02 -3.056703440162091e+14 -2.600000000000001e-02 6.750000000000000e-02 -1.512795541930365e+14 -2.600000000000001e-02 6.900000000000001e-02 -7.311486710479986e+13 -2.600000000000001e-02 7.050000000000001e-02 -3.450471529512656e+13 -2.600000000000001e-02 7.200000000000001e-02 -1.589764560151039e+13 -2.600000000000001e-02 7.350000000000000e-02 -7.149650121722969e+12 -2.600000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -2.400000000000001e-02 0.000000000000000e+00 1.322862412585930e+19 -2.400000000000001e-02 1.500000000000000e-03 1.274824777256670e+19 -2.400000000000001e-02 3.000000000000000e-03 1.197066216976835e+19 -2.400000000000001e-02 4.500000000000001e-03 1.090315148748512e+19 -2.400000000000001e-02 6.000000000000000e-03 9.566665193457306e+18 -2.400000000000001e-02 7.500000000000000e-03 7.996098177053554e+18 -2.400000000000001e-02 9.000000000000001e-03 6.239717446036837e+18 -2.400000000000001e-02 1.050000000000000e-02 4.357589773798611e+18 -2.400000000000001e-02 1.200000000000000e-02 2.418931385932679e+18 -2.400000000000001e-02 1.350000000000000e-02 4.984123728822871e+17 -2.400000000000001e-02 1.500000000000000e-02 -1.328404253887360e+18 -2.400000000000001e-02 1.650000000000000e-02 -2.990148771299340e+18 -2.400000000000001e-02 1.800000000000000e-02 -4.424775831115029e+18 -2.400000000000001e-02 1.950000000000000e-02 -5.584175308497932e+18 -2.400000000000001e-02 2.100000000000000e-02 -6.437697690069335e+18 -2.400000000000001e-02 2.250000000000000e-02 -6.974126609950446e+18 -2.400000000000001e-02 2.400000000000000e-02 -7.201818810934232e+18 -2.400000000000001e-02 2.550000000000000e-02 -7.146979625760078e+18 -2.400000000000001e-02 2.700000000000000e-02 -6.850304650441136e+18 -2.400000000000001e-02 2.850000000000000e-02 -6.362445067038545e+18 -2.400000000000001e-02 3.000000000000000e-02 -5.738901618191494e+18 -2.400000000000001e-02 3.150000000000000e-02 -5.034994644633937e+18 -2.400000000000001e-02 3.300000000000000e-02 -4.301492204744822e+18 -2.400000000000001e-02 3.450000000000000e-02 -3.581325128864513e+18 -2.400000000000001e-02 3.600000000000000e-02 -2.907613375856433e+18 -2.400000000000001e-02 3.750000000000000e-02 -2.303015297774890e+18 -2.400000000000001e-02 3.900000000000000e-02 -1.780229593630664e+18 -2.400000000000001e-02 4.050000000000000e-02 -1.343356074301765e+18 -2.400000000000001e-02 4.200000000000000e-02 -9.897670484900717e+17 -2.400000000000001e-02 4.350000000000000e-02 -7.121517395087365e+17 -2.400000000000001e-02 4.500000000000000e-02 -5.004556252077232e+17 -2.400000000000001e-02 4.650000000000000e-02 -3.435232219244355e+17 -2.400000000000001e-02 4.800000000000000e-02 -2.303450444957540e+17 -2.400000000000001e-02 4.950000000000000e-02 -1.508902977076603e+17 -2.400000000000001e-02 5.100000000000000e-02 -9.656615602621195e+16 -2.400000000000001e-02 5.250000000000000e-02 -6.037907480347927e+16 -2.400000000000001e-02 5.400000000000000e-02 -3.688574202765028e+16 -2.400000000000001e-02 5.550000000000000e-02 -2.201660815582021e+16 -2.400000000000001e-02 5.700000000000000e-02 -1.284009917570268e+16 -2.400000000000001e-02 5.850000000000000e-02 -7.316711993004244e+15 -2.400000000000001e-02 6.000000000000000e-02 -4.073747789975011e+15 -2.400000000000001e-02 6.150000000000000e-02 -2.216161320710901e+15 -2.400000000000001e-02 6.300000000000000e-02 -1.177968106759702e+15 -2.400000000000001e-02 6.450000000000000e-02 -6.117637312146299e+14 -2.400000000000001e-02 6.600000000000000e-02 -3.104144833923311e+14 -2.400000000000001e-02 6.750000000000000e-02 -1.538844619100445e+14 -2.400000000000001e-02 6.900000000000001e-02 -7.452884983702806e+13 -2.400000000000001e-02 7.050000000000001e-02 -3.526210200684492e+13 -2.400000000000001e-02 7.200000000000001e-02 -1.629735750666656e+13 -2.400000000000001e-02 7.350000000000000e-02 -7.357237502186653e+12 -2.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -2.200000000000001e-02 0.000000000000000e+00 4.936077265675553e+18 -2.200000000000001e-02 1.500000000000000e-03 4.525649509850940e+18 -2.200000000000001e-02 3.000000000000000e-03 3.939361000771191e+18 -2.200000000000001e-02 4.500000000000001e-03 3.176852224954116e+18 -2.200000000000001e-02 6.000000000000000e-03 2.246718520543935e+18 -2.200000000000001e-02 7.500000000000000e-03 1.167617086952452e+18 -2.200000000000001e-02 9.000000000000001e-03 -3.124299754961453e+16 -2.200000000000001e-02 1.050000000000000e-02 -1.310469391763214e+18 -2.200000000000001e-02 1.200000000000000e-02 -2.621896058229221e+18 -2.200000000000001e-02 1.350000000000000e-02 -3.911100865840639e+18 -2.200000000000001e-02 1.500000000000000e-02 -5.120937841081623e+18 -2.200000000000001e-02 1.650000000000000e-02 -6.195810062572501e+18 -2.200000000000001e-02 1.800000000000000e-02 -7.086244170723265e+18 -2.200000000000001e-02 1.950000000000000e-02 -7.753216717657689e+18 -2.200000000000001e-02 2.100000000000000e-02 -8.171657853029051e+18 -2.200000000000001e-02 2.250000000000000e-02 -8.332634624435956e+18 -2.200000000000001e-02 2.400000000000000e-02 -8.243887916024720e+18 -2.200000000000001e-02 2.550000000000000e-02 -7.928634968024945e+18 -2.200000000000001e-02 2.700000000000000e-02 -7.422808392852585e+18 -2.200000000000001e-02 2.850000000000000e-02 -6.771131754972357e+18 -2.200000000000001e-02 3.000000000000000e-02 -6.022586800528418e+18 -2.200000000000001e-02 3.150000000000000e-02 -5.225881102431894e+18 -2.200000000000001e-02 3.300000000000000e-02 -4.425472942429039e+18 -2.200000000000001e-02 3.450000000000000e-02 -3.658570975025584e+18 -2.200000000000001e-02 3.600000000000000e-02 -2.953334437892521e+18 -2.200000000000001e-02 3.750000000000000e-02 -2.328297133360604e+18 -2.200000000000001e-02 3.900000000000000e-02 -1.792863512099884e+18 -2.200000000000001e-02 4.050000000000000e-02 -1.348604930264083e+18 -2.200000000000001e-02 4.200000000000000e-02 -9.910299958427988e+17 -2.200000000000001e-02 4.350000000000000e-02 -7.115111291163574e+17 -2.200000000000001e-02 4.500000000000000e-02 -4.991049236389391e+17 -2.200000000000001e-02 4.650000000000000e-02 -3.420858161097948e+17 -2.200000000000001e-02 4.800000000000000e-02 -2.291002021936006e+17 -2.200000000000001e-02 4.950000000000000e-02 -1.499250735523683e+17 -2.200000000000001e-02 5.100000000000000e-02 -9.587166813760691e+16 -2.200000000000001e-02 5.250000000000000e-02 -5.990738712200502e+16 -2.200000000000001e-02 5.400000000000000e-02 -3.658051194405098e+16 -2.200000000000001e-02 5.550000000000000e-02 -2.182741521238855e+16 -2.200000000000001e-02 5.700000000000000e-02 -1.272742534692974e+16 -2.200000000000001e-02 5.850000000000000e-02 -7.252136831055472e+15 -2.200000000000001e-02 6.000000000000000e-02 -4.038118030971709e+15 -2.200000000000001e-02 6.150000000000000e-02 -2.197247497145245e+15 -2.200000000000001e-02 6.300000000000000e-02 -1.168326401261602e+15 -2.200000000000001e-02 6.450000000000000e-02 -6.070602480914924e+14 -2.200000000000001e-02 6.600000000000000e-02 -3.082319638197642e+14 -2.200000000000001e-02 6.750000000000000e-02 -1.529312569275509e+14 -2.200000000000001e-02 6.900000000000001e-02 -7.414472857450944e+13 -2.200000000000001e-02 7.050000000000001e-02 -3.512533121020334e+13 -2.200000000000001e-02 7.200000000000001e-02 -1.625941452316093e+13 -2.200000000000001e-02 7.350000000000000e-02 -7.353918731442747e+12 -2.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -2.000000000000000e-02 0.000000000000000e+00 1.207375061613780e+18 -2.000000000000000e-02 1.500000000000000e-03 8.352829904211695e+17 -2.000000000000000e-02 3.000000000000000e-03 3.438281887074204e+17 -2.000000000000000e-02 4.500000000000001e-03 -2.706941657663538e+17 -2.000000000000000e-02 6.000000000000000e-03 -1.005266883037249e+18 -2.000000000000000e-02 7.500000000000000e-03 -1.848701796150976e+18 -2.000000000000000e-02 9.000000000000001e-03 -2.780692587048290e+18 -2.000000000000000e-02 1.050000000000000e-02 -3.771648641943134e+18 -2.000000000000000e-02 1.200000000000000e-02 -4.783534197520865e+18 -2.000000000000000e-02 1.350000000000000e-02 -5.771822364430568e+18 -2.000000000000000e-02 1.500000000000000e-02 -6.688510330321378e+18 -2.000000000000000e-02 1.650000000000000e-02 -7.485955832333266e+18 -2.000000000000000e-02 1.800000000000000e-02 -8.121122203432826e+18 -2.000000000000000e-02 1.950000000000000e-02 -8.559699206695996e+18 -2.000000000000000e-02 2.100000000000000e-02 -8.779531806156063e+18 -2.000000000000000e-02 2.250000000000000e-02 -8.772855142446311e+18 -2.000000000000000e-02 2.400000000000000e-02 -8.546995537529940e+18 -2.000000000000000e-02 2.550000000000000e-02 -8.123426490199068e+18 -2.000000000000000e-02 2.700000000000000e-02 -7.535321182555880e+18 -2.000000000000000e-02 2.850000000000000e-02 -6.823968929657406e+18 -2.000000000000000e-02 3.000000000000000e-02 -6.034578407394790e+18 -2.000000000000000e-02 3.150000000000000e-02 -5.212048114020049e+18 -2.000000000000000e-02 3.300000000000000e-02 -4.397239443549349e+18 -2.000000000000000e-02 3.450000000000000e-02 -3.624157163379741e+18 -2.000000000000000e-02 3.600000000000000e-02 -2.918259459448756e+18 -2.000000000000000e-02 3.750000000000000e-02 -2.295925435268496e+18 -2.000000000000000e-02 3.900000000000000e-02 -1.764939361756833e+18 -2.000000000000000e-02 4.050000000000000e-02 -1.325734450307207e+18 -2.000000000000000e-02 4.200000000000000e-02 -9.730858455167872e+17 -2.000000000000000e-02 4.350000000000000e-02 -6.979495414984801e+17 -2.000000000000000e-02 4.500000000000000e-02 -4.891965886763196e+17 -2.000000000000000e-02 4.650000000000000e-02 -3.350702867636375e+17 -2.000000000000000e-02 4.800000000000000e-02 -2.242780431358930e+17 -2.000000000000000e-02 4.950000000000000e-02 -1.467033741597250e+17 -2.000000000000000e-02 5.100000000000000e-02 -9.377762575037661e+16 -2.000000000000000e-02 5.250000000000000e-02 -5.858233892205775e+16 -2.000000000000000e-02 5.400000000000000e-02 -3.576386719644496e+16 -2.000000000000000e-02 5.550000000000000e-02 -2.133702958372741e+16 -2.000000000000000e-02 5.700000000000000e-02 -1.244045117412421e+16 -2.000000000000000e-02 5.850000000000000e-02 -7.088454173795158e+15 -2.000000000000000e-02 6.000000000000000e-02 -3.947119960518128e+15 -2.000000000000000e-02 6.150000000000000e-02 -2.147940573194273e+15 -2.000000000000000e-02 6.300000000000000e-02 -1.142290871201876e+15 -2.000000000000000e-02 6.450000000000000e-02 -5.936665705674556e+14 -2.000000000000000e-02 6.600000000000000e-02 -3.015215729057487e+14 -2.000000000000000e-02 6.750000000000000e-02 -1.496587166660793e+14 -2.000000000000000e-02 6.900000000000001e-02 -7.259233524039362e+13 -2.000000000000000e-02 7.050000000000001e-02 -3.440972324580082e+13 -2.000000000000000e-02 7.200000000000001e-02 -1.593928632705993e+13 -2.000000000000000e-02 7.350000000000000e-02 -7.215199315060976e+12 -2.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -1.800000000000000e-02 0.000000000000000e+00 -2.365715564310274e+17 -1.800000000000000e-02 1.500000000000000e-03 -5.857588803726921e+17 -1.800000000000000e-02 3.000000000000000e-03 -1.030165374279596e+18 -1.800000000000000e-02 4.500000000000001e-03 -1.574684053148194e+18 -1.800000000000000e-02 6.000000000000000e-03 -2.218485008284348e+18 -1.800000000000000e-02 7.500000000000000e-03 -2.953468967188130e+18 -1.800000000000000e-02 9.000000000000001e-03 -3.763167624574861e+18 -1.800000000000000e-02 1.050000000000000e-02 -4.622378013405886e+18 -1.800000000000000e-02 1.200000000000000e-02 -5.497766090931403e+18 -1.800000000000000e-02 1.350000000000000e-02 -6.349562821085976e+18 -1.800000000000000e-02 1.500000000000000e-02 -7.134315340564293e+18 -1.800000000000000e-02 1.650000000000000e-02 -7.808471630126708e+18 -1.800000000000000e-02 1.800000000000000e-02 -8.332405248926820e+18 -1.800000000000000e-02 1.950000000000000e-02 -8.674365739629171e+18 -1.800000000000000e-02 2.100000000000000e-02 -8.813802104679658e+18 -1.800000000000000e-02 2.250000000000000e-02 -8.743567340102588e+18 -1.800000000000000e-02 2.400000000000000e-02 -8.470666077623576e+18 -1.800000000000000e-02 2.550000000000000e-02 -8.015428052071390e+18 -1.800000000000000e-02 2.700000000000000e-02 -7.409234573128051e+18 -1.800000000000000e-02 2.850000000000000e-02 -6.691144799509481e+18 -1.800000000000000e-02 3.000000000000000e-02 -5.903920680441351e+18 -1.800000000000000e-02 3.150000000000000e-02 -5.090007255997321e+18 -1.800000000000000e-02 3.300000000000000e-02 -4.287983550138314e+18 -1.800000000000000e-02 3.450000000000000e-02 -3.529874932843573e+18 -1.800000000000000e-02 3.600000000000000e-02 -2.839542768254548e+18 -1.800000000000000e-02 3.750000000000000e-02 -2.232180381763348e+18 -1.800000000000000e-02 3.900000000000000e-02 -1.714781962623040e+18 -1.800000000000000e-02 4.050000000000000e-02 -1.287338524509586e+18 -1.800000000000000e-02 4.200000000000000e-02 -9.444635699093916e+17 -1.800000000000000e-02 4.350000000000000e-02 -6.771574980765615e+17 -1.800000000000000e-02 4.500000000000000e-02 -4.744702158372650e+17 -1.800000000000000e-02 4.650000000000000e-02 -3.248966188569087e+17 -1.800000000000000e-02 4.800000000000000e-02 -2.174203275531352e+17 -1.800000000000000e-02 4.950000000000000e-02 -1.421920134835867e+17 -1.800000000000000e-02 5.100000000000000e-02 -9.088065771836405e+16 -1.800000000000000e-02 5.250000000000000e-02 -5.676619327000657e+16 -1.800000000000000e-02 5.400000000000000e-02 -3.465219781172213e+16 -1.800000000000000e-02 5.550000000000000e-02 -2.067259413306323e+16 -1.800000000000000e-02 5.700000000000000e-02 -1.205265358084332e+16 -1.800000000000000e-02 5.850000000000000e-02 -6.867427066407405e+15 -1.800000000000000e-02 6.000000000000000e-02 -3.824099411068063e+15 -1.800000000000000e-02 6.150000000000000e-02 -2.081076035081338e+15 -1.800000000000000e-02 6.300000000000000e-02 -1.106802587989374e+15 -1.800000000000000e-02 6.450000000000000e-02 -5.752749610926719e+14 -1.800000000000000e-02 6.600000000000000e-02 -2.922155697285392e+14 -1.800000000000000e-02 6.750000000000000e-02 -1.450618174114340e+14 -1.800000000000000e-02 6.900000000000001e-02 -7.037588261645841e+13 -1.800000000000000e-02 7.050000000000001e-02 -3.336678926178532e+13 -1.800000000000000e-02 7.200000000000001e-02 -1.546049326072604e+13 -1.800000000000000e-02 7.350000000000000e-02 -7.000818219428047e+12 -1.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -1.600000000000000e-02 0.000000000000000e+00 -7.079438509647896e+17 -1.600000000000000e-02 1.500000000000000e-03 -1.040595189491889e+18 -1.600000000000000e-02 3.000000000000000e-03 -1.458038614166008e+18 -1.600000000000000e-02 4.500000000000001e-03 -1.965434431249883e+18 -1.600000000000000e-02 6.000000000000000e-03 -2.562697262673092e+18 -1.600000000000000e-02 7.500000000000000e-03 -3.242957067450232e+18 -1.600000000000000e-02 9.000000000000001e-03 -3.991437274767256e+18 -1.600000000000000e-02 1.050000000000000e-02 -4.785032579529854e+18 -1.600000000000000e-02 1.200000000000000e-02 -5.592819147847467e+18 -1.600000000000000e-02 1.350000000000000e-02 -6.377621877810833e+18 -1.600000000000000e-02 1.500000000000000e-02 -7.098607647848304e+18 -1.600000000000000e-02 1.650000000000000e-02 -7.714694722791504e+18 -1.600000000000000e-02 1.800000000000000e-02 -8.188401339977895e+18 -1.600000000000000e-02 1.950000000000000e-02 -8.489638367804979e+18 -1.600000000000000e-02 2.100000000000000e-02 -8.598912663518717e+18 -1.600000000000000e-02 2.250000000000000e-02 -8.509464958291016e+18 -1.600000000000000e-02 2.400000000000000e-02 -8.228013730617380e+18 -1.600000000000000e-02 2.550000000000000e-02 -7.773988730419677e+18 -1.600000000000000e-02 2.700000000000000e-02 -7.177373326726943e+18 -1.600000000000000e-02 2.850000000000000e-02 -6.475486753150162e+18 -1.600000000000000e-02 3.000000000000000e-02 -5.709184386008850e+18 -1.600000000000000e-02 3.150000000000000e-02 -4.919010600684399e+18 -1.600000000000000e-02 3.300000000000000e-02 -4.141799554909806e+18 -1.600000000000000e-02 3.450000000000000e-02 -3.408100141549346e+18 -1.600000000000000e-02 3.600000000000000e-02 -2.740633290031797e+18 -1.600000000000000e-02 3.750000000000000e-02 -2.153810283316089e+18 -1.600000000000000e-02 3.900000000000000e-02 -1.654184550736463e+18 -1.600000000000000e-02 4.050000000000000e-02 -1.241601122916574e+18 -1.600000000000000e-02 4.200000000000000e-02 -9.107583084853590e+17 -1.600000000000000e-02 4.350000000000000e-02 -6.529021791881420e+17 -1.600000000000000e-02 4.500000000000000e-02 -4.574228336191276e+17 -1.600000000000000e-02 4.650000000000000e-02 -3.131936560038632e+17 -1.600000000000000e-02 4.800000000000000e-02 -2.095723510786771e+17 -1.600000000000000e-02 4.950000000000000e-02 -1.370507253979670e+17 -1.600000000000000e-02 5.100000000000000e-02 -8.759016420320406e+16 -1.600000000000000e-02 5.250000000000000e-02 -5.470868105744658e+16 -1.600000000000000e-02 5.400000000000000e-02 -3.339521504789989e+16 -1.600000000000000e-02 5.550000000000000e-02 -1.992230025274896e+16 -1.600000000000000e-02 5.700000000000000e-02 -1.161507586339696e+16 -1.600000000000000e-02 5.850000000000000e-02 -6.618079921288706e+15 -1.600000000000000e-02 6.000000000000000e-02 -3.685270463855425e+15 -1.600000000000000e-02 6.150000000000000e-02 -2.005552817980324e+15 -1.600000000000000e-02 6.300000000000000e-02 -1.066660362387986e+15 -1.600000000000000e-02 6.450000000000000e-02 -5.544283372325223e+14 -1.600000000000000e-02 6.600000000000000e-02 -2.816383161010808e+14 -1.600000000000000e-02 6.750000000000000e-02 -1.398185874713709e+14 -1.600000000000000e-02 6.900000000000001e-02 -6.783669250029758e+13 -1.600000000000000e-02 7.050000000000001e-02 -3.216552618130479e+13 -1.600000000000000e-02 7.200000000000001e-02 -1.490535976516063e+13 -1.600000000000000e-02 7.350000000000000e-02 -6.750244886133698e+12 -1.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -1.400000000000000e-02 0.000000000000000e+00 -8.241538731789586e+17 -1.400000000000000e-02 1.500000000000000e-03 -1.142682913033287e+18 -1.400000000000000e-02 3.000000000000000e-03 -1.540610619971717e+18 -1.400000000000000e-02 4.500000000000001e-03 -2.023029469908121e+18 -1.400000000000000e-02 6.000000000000000e-03 -2.590071459169521e+18 -1.400000000000000e-02 7.500000000000000e-03 -3.235414526611826e+18 -1.400000000000000e-02 9.000000000000001e-03 -3.945185802452335e+18 -1.400000000000000e-02 1.050000000000000e-02 -4.697534932464232e+18 -1.400000000000000e-02 1.200000000000000e-02 -5.463102983734320e+18 -1.400000000000000e-02 1.350000000000000e-02 -6.206508468574790e+18 -1.400000000000000e-02 1.500000000000000e-02 -6.888822123934835e+18 -1.400000000000000e-02 1.650000000000000e-02 -7.470829905069733e+18 -1.400000000000000e-02 1.800000000000000e-02 -7.916722563060836e+18 -1.400000000000000e-02 1.950000000000000e-02 -8.197736179668392e+18 -1.400000000000000e-02 2.100000000000000e-02 -8.295230825842719e+18 -1.400000000000000e-02 2.250000000000000e-02 -8.202749126793068e+18 -1.400000000000000e-02 2.400000000000000e-02 -7.926738143898982e+18 -1.400000000000000e-02 2.550000000000000e-02 -7.485821777992083e+18 -1.400000000000000e-02 2.700000000000000e-02 -6.908737206345798e+18 -1.400000000000000e-02 2.850000000000000e-02 -6.231252584099068e+18 -1.400000000000000e-02 3.000000000000000e-02 -5.492524723516768e+18 -1.400000000000000e-02 3.150000000000000e-02 -4.731409881179668e+18 -1.400000000000000e-02 3.300000000000000e-02 -3.983203340587858e+18 -1.400000000000000e-02 3.450000000000000e-02 -3.277169234717000e+18 -1.400000000000000e-02 3.600000000000000e-02 -2.635060732405999e+18 -1.400000000000000e-02 3.750000000000000e-02 -2.070658344203916e+18 -1.400000000000000e-02 3.900000000000000e-02 -1.590204079292936e+18 -1.400000000000000e-02 4.050000000000000e-02 -1.193505171994741e+18 -1.400000000000000e-02 4.200000000000000e-02 -8.754333986418188e+17 -1.400000000000000e-02 4.350000000000000e-02 -6.275517571272087e+17 -1.400000000000000e-02 4.500000000000000e-02 -4.396467176241859e+17 -1.400000000000000e-02 4.650000000000000e-02 -3.010136137214081e+17 -1.400000000000000e-02 4.800000000000000e-02 -2.014172181318716e+17 -1.400000000000000e-02 4.950000000000000e-02 -1.317150226540097e+17 -1.400000000000000e-02 5.100000000000000e-02 -8.417873119141280e+16 -1.400000000000000e-02 5.250000000000000e-02 -5.257724837859417e+16 -1.400000000000000e-02 5.400000000000000e-02 -3.209384836333410e+16 -1.400000000000000e-02 5.550000000000000e-02 -1.914583186642269e+16 -1.400000000000000e-02 5.700000000000000e-02 -1.116233910705027e+16 -1.400000000000000e-02 5.850000000000000e-02 -6.360111429699760e+15 -1.400000000000000e-02 6.000000000000000e-02 -3.541626693411958e+15 -1.400000000000000e-02 6.150000000000000e-02 -1.927389012707135e+15 -1.400000000000000e-02 6.300000000000000e-02 -1.025095903134199e+15 -1.400000000000000e-02 6.450000000000000e-02 -5.328293157472596e+14 -1.400000000000000e-02 6.600000000000000e-02 -2.706700350376744e+14 -1.400000000000000e-02 6.750000000000000e-02 -1.343756714578967e+14 -1.400000000000000e-02 6.900000000000001e-02 -6.519727517474893e+13 -1.400000000000000e-02 7.050000000000001e-02 -3.091480298244505e+13 -1.400000000000000e-02 7.200000000000001e-02 -1.432622100668534e+13 -1.400000000000000e-02 7.350000000000000e-02 -6.488208427771121e+12 -1.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 -1.200000000000001e-02 0.000000000000000e+00 -8.293332565113194e+17 -1.200000000000001e-02 1.500000000000000e-03 -1.134930780957068e+18 -1.200000000000001e-02 3.000000000000000e-03 -1.516229750525101e+18 -1.200000000000001e-02 4.500000000000001e-03 -1.978155852183071e+18 -1.200000000000001e-02 6.000000000000000e-03 -2.520892188716312e+18 -1.200000000000001e-02 7.500000000000000e-03 -3.138441070470564e+18 -1.200000000000001e-02 9.000000000000001e-03 -3.817565842846541e+18 -1.200000000000001e-02 1.050000000000000e-02 -4.537375616398904e+18 -1.200000000000001e-02 1.200000000000000e-02 -5.269769948054355e+18 -1.200000000000001e-02 1.350000000000000e-02 -5.980860652590078e+18 -1.200000000000001e-02 1.500000000000000e-02 -6.633343899338216e+18 -1.200000000000001e-02 1.650000000000000e-02 -7.189630294898576e+18 -1.200000000000001e-02 1.800000000000000e-02 -7.615385829263282e+18 -1.200000000000001e-02 1.950000000000000e-02 -7.883026961817153e+18 -1.200000000000001e-02 2.100000000000000e-02 -7.974677277513679e+18 -1.200000000000001e-02 2.250000000000000e-02 -7.884145501511898e+18 -1.200000000000001e-02 2.400000000000000e-02 -7.617620607419679e+18 -1.200000000000001e-02 2.550000000000000e-02 -7.192975433904669e+18 -1.200000000000001e-02 2.700000000000000e-02 -6.637787554865949e+18 -1.200000000000001e-02 2.850000000000000e-02 -5.986381811049746e+18 -1.200000000000001e-02 3.000000000000000e-02 -5.276334825563865e+18 -1.200000000000001e-02 3.150000000000000e-02 -4.544934139130806e+18 -1.200000000000001e-02 3.300000000000000e-02 -3.826048702219177e+18 -1.200000000000001e-02 3.450000000000000e-02 -3.147757805177031e+18 -1.200000000000001e-02 3.600000000000000e-02 -2.530930652458536e+18 -1.200000000000001e-02 3.750000000000000e-02 -1.988783290532392e+18 -1.200000000000001e-02 3.900000000000000e-02 -1.527295547045770e+18 -1.200000000000001e-02 4.050000000000000e-02 -1.146270759738252e+18 -1.200000000000001e-02 4.200000000000000e-02 -8.407752652401930e+17 -1.200000000000001e-02 4.350000000000000e-02 -6.027001307814374e+17 -1.200000000000001e-02 4.500000000000000e-02 -4.222321909799549e+17 -1.200000000000001e-02 4.650000000000000e-02 -2.890880447456242e+17 -1.200000000000001e-02 4.800000000000000e-02 -1.934361724236052e+17 -1.200000000000001e-02 4.950000000000000e-02 -1.264951985200591e+17 -1.200000000000001e-02 5.100000000000000e-02 -8.084240113719291e+16 -1.200000000000001e-02 5.250000000000000e-02 -5.049323492734806e+16 -1.200000000000001e-02 5.400000000000000e-02 -3.082166005572288e+16 -1.200000000000001e-02 5.550000000000000e-02 -1.838686575492668e+16 -1.200000000000001e-02 5.700000000000000e-02 -1.071983840107994e+16 -1.200000000000001e-02 5.850000000000000e-02 -6.107980323086356e+15 -1.200000000000001e-02 6.000000000000000e-02 -3.401229040222035e+15 -1.200000000000001e-02 6.150000000000000e-02 -1.850985363629642e+15 -1.200000000000001e-02 6.300000000000000e-02 -9.844619700260137e+14 -1.200000000000001e-02 6.450000000000000e-02 -5.117098181243922e+14 -1.200000000000001e-02 6.600000000000000e-02 -2.599425608146879e+14 -1.200000000000001e-02 6.750000000000000e-02 -1.290505503762825e+14 -1.200000000000001e-02 6.900000000000001e-02 -6.261395509665655e+13 -1.200000000000001e-02 7.050000000000001e-02 -2.969006861704456e+13 -1.200000000000001e-02 7.200000000000001e-02 -1.375878315840488e+13 -1.200000000000001e-02 7.350000000000000e-02 -6.231284478725463e+12 -1.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -1.000000000000001e-02 0.000000000000000e+00 -8.062498167485686e+17 -1.000000000000001e-02 1.500000000000000e-03 -1.100042961273176e+18 -1.000000000000001e-02 3.000000000000000e-03 -1.466503642515067e+18 -1.000000000000001e-02 4.500000000000001e-03 -1.910376538007188e+18 -1.000000000000001e-02 6.000000000000000e-03 -2.431850759240482e+18 -1.000000000000001e-02 7.500000000000000e-03 -3.025175977377610e+18 -1.000000000000001e-02 9.000000000000001e-03 -3.677643747285813e+18 -1.000000000000001e-02 1.050000000000000e-02 -4.369186907751309e+18 -1.000000000000001e-02 1.200000000000000e-02 -5.072805883962434e+18 -1.000000000000001e-02 1.350000000000000e-02 -5.755934678692391e+18 -1.000000000000001e-02 1.500000000000000e-02 -6.382720828926362e+18 -1.000000000000001e-02 1.650000000000000e-02 -6.917034479987851e+18 -1.000000000000001e-02 1.800000000000000e-02 -7.325872822746300e+18 -1.000000000000001e-02 1.950000000000000e-02 -7.582720718193961e+18 -1.000000000000001e-02 2.100000000000000e-02 -7.670393837511430e+18 -1.000000000000001e-02 2.250000000000000e-02 -7.582940971719055e+18 -1.000000000000001e-02 2.400000000000000e-02 -7.326312876656825e+18 -1.000000000000001e-02 2.550000000000000e-02 -6.917693176913390e+18 -1.000000000000001e-02 2.700000000000000e-02 -6.383595836580439e+18 -1.000000000000001e-02 2.850000000000000e-02 -5.757021859253849e+18 -1.000000000000001e-02 3.000000000000000e-02 -5.074098584990459e+18 -1.000000000000001e-02 3.150000000000000e-02 -4.370675269124651e+18 -1.000000000000001e-02 3.300000000000000e-02 -3.679314121335551e+18 -1.000000000000001e-02 3.450000000000000e-02 -3.027010551216258e+18 -1.000000000000001e-02 3.600000000000000e-02 -2.433827449952617e+18 -1.000000000000001e-02 3.750000000000000e-02 -1.912469204695871e+18 -1.000000000000001e-02 3.900000000000000e-02 -1.468682627045617e+18 -1.000000000000001e-02 4.050000000000000e-02 -1.102275935491959e+18 -1.000000000000001e-02 4.200000000000000e-02 -8.085028818552740e+17 -1.000000000000001e-02 4.350000000000000e-02 -5.795644105145659e+17 -1.000000000000001e-02 4.500000000000000e-02 -4.060231029157104e+17 -1.000000000000001e-02 4.650000000000000e-02 -2.779896915383605e+17 -1.000000000000001e-02 4.800000000000000e-02 -1.860096829833821e+17 -1.000000000000001e-02 4.950000000000000e-02 -1.216385778379597e+17 -1.000000000000001e-02 5.100000000000000e-02 -7.773847906601075e+16 -1.000000000000001e-02 5.250000000000000e-02 -4.855452084843528e+16 -1.000000000000001e-02 5.400000000000000e-02 -2.963822808614001e+16 -1.000000000000001e-02 5.550000000000000e-02 -1.768087406461686e+16 -1.000000000000001e-02 5.700000000000000e-02 -1.030823139066797e+16 -1.000000000000001e-02 5.850000000000000e-02 -5.873453301806211e+15 -1.000000000000001e-02 6.000000000000000e-02 -3.270633007955181e+15 -1.000000000000001e-02 6.150000000000000e-02 -1.779914103232651e+15 -1.000000000000001e-02 6.300000000000000e-02 -9.466625695791412e+14 -1.000000000000001e-02 6.450000000000000e-02 -4.920625338328256e+14 -1.000000000000001e-02 6.600000000000000e-02 -2.499621900242186e+14 -1.000000000000001e-02 6.750000000000000e-02 -1.240958535022039e+14 -1.000000000000001e-02 6.900000000000001e-02 -6.021007154373089e+13 -1.000000000000001e-02 7.050000000000001e-02 -2.855025130923464e+13 -1.000000000000001e-02 7.200000000000001e-02 -1.323060310097650e+13 -1.000000000000001e-02 7.350000000000000e-02 -5.992088989100577e+12 -1.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 -8.000000000000007e-03 0.000000000000000e+00 -7.796458372618282e+17 -8.000000000000007e-03 1.500000000000000e-03 -1.063080069064229e+18 -8.000000000000007e-03 3.000000000000000e-03 -1.416597273008448e+18 -8.000000000000007e-03 4.500000000000001e-03 -1.844776718901418e+18 -8.000000000000007e-03 6.000000000000000e-03 -2.347803515517003e+18 -8.000000000000007e-03 7.500000000000000e-03 -2.920133282054803e+18 -8.000000000000007e-03 9.000000000000001e-03 -3.549509109183656e+18 -8.000000000000007e-03 1.050000000000000e-02 -4.216574804840705e+18 -8.000000000000007e-03 1.200000000000000e-02 -4.895285920745754e+18 -8.000000000000007e-03 1.350000000000000e-02 -5.554227396519947e+18 -8.000000000000007e-03 1.500000000000000e-02 -6.158813022418338e+18 -8.000000000000007e-03 1.650000000000000e-02 -6.674188395067929e+18 -8.000000000000007e-03 1.800000000000000e-02 -7.068515371518550e+18 -8.000000000000007e-03 1.950000000000000e-02 -7.316214311702624e+18 -8.000000000000007e-03 2.100000000000000e-02 -7.400707112480937e+18 -8.000000000000007e-03 2.250000000000000e-02 -7.316252586026588e+18 -8.000000000000007e-03 2.400000000000000e-02 -7.068591841422612e+18 -8.000000000000007e-03 2.550000000000000e-02 -6.674302859431265e+18 -8.000000000000007e-03 2.700000000000000e-02 -6.158965075950330e+18 -8.000000000000007e-03 2.850000000000000e-02 -5.554416320175082e+18 -8.000000000000007e-03 3.000000000000000e-02 -4.895510558503153e+18 -8.000000000000007e-03 3.150000000000000e-02 -4.216833443268196e+18 -8.000000000000007e-03 3.300000000000000e-02 -3.549799376671971e+18 -8.000000000000007e-03 3.450000000000000e-02 -2.920452083188212e+18 -8.000000000000007e-03 3.600000000000000e-02 -2.348147012860173e+18 -8.000000000000007e-03 3.750000000000000e-02 -1.845140369847565e+18 -8.000000000000007e-03 3.900000000000000e-02 -1.416975923746503e+18 -8.000000000000007e-03 4.050000000000000e-02 -1.063468101803399e+18 -8.000000000000007e-03 4.200000000000000e-02 -7.800373612738523e+17 -8.000000000000007e-03 4.350000000000000e-02 -5.591589528576735e+17 -8.000000000000007e-03 4.500000000000000e-02 -3.917275398307875e+17 -8.000000000000007e-03 4.650000000000000e-02 -2.682019137411241e+17 -8.000000000000007e-03 4.800000000000000e-02 -1.794603812887205e+17 -8.000000000000007e-03 4.950000000000000e-02 -1.173557159157171e+17 -8.000000000000007e-03 5.100000000000000e-02 -7.500131124270181e+16 -8.000000000000007e-03 5.250000000000000e-02 -4.684491053240150e+16 -8.000000000000007e-03 5.400000000000000e-02 -2.859465891430279e+16 -8.000000000000007e-03 5.550000000000000e-02 -1.705832468947108e+16 -8.000000000000007e-03 5.700000000000000e-02 -9.945274672582528e+15 -8.000000000000007e-03 5.850000000000000e-02 -5.666646713402861e+15 -8.000000000000007e-03 6.000000000000000e-02 -3.155472811003026e+15 -8.000000000000007e-03 6.150000000000000e-02 -1.717242772223689e+15 -8.000000000000007e-03 6.300000000000000e-02 -9.133303748924832e+14 -8.000000000000007e-03 6.450000000000000e-02 -4.747369713785160e+14 -8.000000000000007e-03 6.600000000000000e-02 -2.411610451208019e+14 -8.000000000000007e-03 6.750000000000000e-02 -1.197264783332491e+14 -8.000000000000007e-03 6.900000000000001e-02 -5.809011109562173e+13 -8.000000000000007e-03 7.050000000000001e-02 -2.754502386455253e+13 -8.000000000000007e-03 7.200000000000001e-02 -1.276477150149658e+13 -8.000000000000007e-03 7.350000000000000e-02 -5.781118639192665e+12 -8.000000000000007e-03 1.200000000000000e-01 0.000000000000000e+00 -6.000000000000005e-03 0.000000000000000e+00 -7.565173220934929e+17 -6.000000000000005e-03 1.500000000000000e-03 -1.031424418853124e+18 -6.000000000000005e-03 3.000000000000000e-03 -1.374302025330810e+18 -6.000000000000005e-03 4.500000000000001e-03 -1.789591982051936e+18 -6.000000000000005e-03 6.000000000000000e-03 -2.277474306911029e+18 -6.000000000000005e-03 7.500000000000000e-03 -2.832571995474740e+18 -6.000000000000005e-03 9.000000000000001e-03 -3.442997506452853e+18 -6.000000000000005e-03 1.050000000000000e-02 -4.089977592923896e+18 -6.000000000000005e-03 1.200000000000000e-02 -4.748251919162305e+18 -6.000000000000005e-03 1.350000000000000e-02 -5.387351030475012e+18 -6.000000000000005e-03 1.500000000000000e-02 -5.973729626236625e+18 -6.000000000000005e-03 1.650000000000000e-02 -6.473582176302137e+18 -6.000000000000005e-03 1.800000000000000e-02 -6.856028571863976e+18 -6.000000000000005e-03 1.950000000000000e-02 -7.096258844745521e+18 -6.000000000000005e-03 2.100000000000000e-02 -7.178193702377045e+18 -6.000000000000005e-03 2.250000000000000e-02 -7.096264714308682e+18 -6.000000000000005e-03 2.400000000000000e-02 -6.856040298914520e+18 -6.000000000000005e-03 2.550000000000000e-02 -6.473599729997158e+18 -6.000000000000005e-03 2.700000000000000e-02 -5.973752944422739e+18 -6.000000000000005e-03 2.850000000000000e-02 -5.387380002882912e+18 -6.000000000000005e-03 3.000000000000000e-02 -4.748286368510285e+18 -6.000000000000005e-03 3.150000000000000e-02 -4.090017256448376e+18 -6.000000000000005e-03 3.300000000000000e-02 -3.443042020455432e+18 -6.000000000000005e-03 3.450000000000000e-02 -2.832620885257599e+18 -6.000000000000005e-03 3.600000000000000e-02 -2.277526983983850e+18 -6.000000000000005e-03 3.750000000000000e-02 -1.789647749782758e+18 -6.000000000000005e-03 3.900000000000000e-02 -1.374360093356369e+18 -6.000000000000005e-03 4.050000000000000e-02 -1.031483925656494e+18 -6.000000000000005e-03 4.200000000000000e-02 -7.565773643013956e+17 -6.000000000000005e-03 4.350000000000000e-02 -5.423419201222025e+17 -6.000000000000005e-03 4.500000000000000e-02 -3.799460700483580e+17 -6.000000000000005e-03 4.650000000000000e-02 -2.601355406522535e+17 -6.000000000000005e-03 4.800000000000000e-02 -1.740629652261027e+17 -6.000000000000005e-03 4.950000000000000e-02 -1.138261420471271e+17 -6.000000000000005e-03 5.100000000000000e-02 -7.274557944944832e+16 -6.000000000000005e-03 5.250000000000000e-02 -4.543600631524986e+16 -6.000000000000005e-03 5.400000000000000e-02 -2.773464730715848e+16 -6.000000000000005e-03 5.550000000000000e-02 -1.654527905006096e+16 -6.000000000000005e-03 5.700000000000000e-02 -9.646160811394468e+15 -6.000000000000005e-03 5.850000000000000e-02 -5.496216757644654e+15 -6.000000000000005e-03 6.000000000000000e-02 -3.060568885118201e+15 -6.000000000000005e-03 6.150000000000000e-02 -1.665595037449166e+15 -6.000000000000005e-03 6.300000000000000e-02 -8.858610979424261e+14 -6.000000000000005e-03 6.450000000000000e-02 -4.604588187498821e+14 -6.000000000000005e-03 6.600000000000000e-02 -2.339079120547487e+14 -6.000000000000005e-03 6.750000000000000e-02 -1.161256029657286e+14 -6.000000000000005e-03 6.900000000000001e-02 -5.634300476394413e+13 -6.000000000000005e-03 7.050000000000001e-02 -2.671658709510326e+13 -6.000000000000005e-03 7.200000000000001e-02 -1.238086262929413e+13 -6.000000000000005e-03 7.350000000000000e-02 -5.607248240339111e+12 -6.000000000000005e-03 1.200000000000000e-01 0.000000000000000e+00 -4.000000000000004e-03 0.000000000000000e+00 -7.390868594206536e+17 -4.000000000000004e-03 1.500000000000000e-03 -1.007641196091990e+18 -4.000000000000004e-03 3.000000000000000e-03 -1.342594694670214e+18 -4.000000000000004e-03 4.500000000000001e-03 -1.748286603756136e+18 -4.000000000000004e-03 6.000000000000000e-03 -2.224892856822159e+18 -4.000000000000004e-03 7.500000000000000e-03 -2.767160795917116e+18 -4.000000000000004e-03 9.000000000000001e-03 -3.363477683710082e+18 -4.000000000000004e-03 1.050000000000000e-02 -3.995504196480894e+18 -4.000000000000004e-03 1.200000000000000e-02 -4.638563822466501e+18 -4.000000000000004e-03 1.350000000000000e-02 -5.262891294211610e+18 -4.000000000000004e-03 1.500000000000000e-02 -5.835716561363955e+18 -4.000000000000004e-03 1.650000000000000e-02 -6.324015341113397e+18 -4.000000000000004e-03 1.800000000000000e-02 -6.697621154179312e+18 -4.000000000000004e-03 1.950000000000000e-02 -6.932297376706426e+18 -4.000000000000004e-03 2.100000000000000e-02 -7.012336297589424e+18 -4.000000000000004e-03 2.250000000000000e-02 -6.932298171141018e+18 -4.000000000000004e-03 2.400000000000000e-02 -6.697622741414060e+18 -4.000000000000004e-03 2.550000000000000e-02 -6.324017716973772e+18 -4.000000000000004e-03 2.700000000000000e-02 -5.835719717437611e+18 -4.000000000000004e-03 2.850000000000000e-02 -5.262895215573797e+18 -4.000000000000004e-03 3.000000000000000e-02 -4.638568485122468e+18 -4.000000000000004e-03 3.150000000000000e-02 -3.995509564866072e+18 -4.000000000000004e-03 3.300000000000000e-02 -3.363483708598559e+18 -4.000000000000004e-03 3.450000000000000e-02 -2.767167413059416e+18 -4.000000000000004e-03 3.600000000000000e-02 -2.224899986567197e+18 -4.000000000000004e-03 3.750000000000000e-02 -1.748294151816059e+18 -4.000000000000004e-03 3.900000000000000e-02 -1.342602554070804e+18 -4.000000000000004e-03 4.050000000000000e-02 -1.007649250228512e+18 -4.000000000000004e-03 4.200000000000000e-02 -7.390949860231959e+17 -4.000000000000004e-03 4.350000000000000e-02 -5.298099119246249e+17 -4.000000000000004e-03 4.500000000000000e-02 -3.711665712326959e+17 -4.000000000000004e-03 4.650000000000000e-02 -2.541245274109814e+17 -4.000000000000004e-03 4.800000000000000e-02 -1.700408495441456e+17 -4.000000000000004e-03 4.950000000000000e-02 -1.111959325093780e+17 -4.000000000000004e-03 5.100000000000000e-02 -7.106462841923586e+16 -4.000000000000004e-03 5.250000000000000e-02 -4.438610446536875e+16 -4.000000000000004e-03 5.400000000000000e-02 -2.709377534971486e+16 -4.000000000000004e-03 5.550000000000000e-02 -1.616296279217313e+16 -4.000000000000004e-03 5.700000000000000e-02 -9.423264338488952e+15 -4.000000000000004e-03 5.850000000000000e-02 -5.369214173338498e+15 -4.000000000000004e-03 6.000000000000000e-02 -2.989847484565887e+15 -4.000000000000004e-03 6.150000000000000e-02 -1.627107681228957e+15 -4.000000000000004e-03 6.300000000000000e-02 -8.653912678630897e+14 -4.000000000000004e-03 6.450000000000000e-02 -4.498188751552435e+14 -4.000000000000004e-03 6.600000000000000e-02 -2.285029413842634e+14 -4.000000000000004e-03 6.750000000000000e-02 -1.134422593933214e+14 -4.000000000000004e-03 6.900000000000001e-02 -5.504107323149214e+13 -4.000000000000004e-03 7.050000000000001e-02 -2.609924068722680e+13 -4.000000000000004e-03 7.200000000000001e-02 -1.209477530453137e+13 -4.000000000000004e-03 7.350000000000000e-02 -5.477680402440231e+12 -4.000000000000004e-03 1.200000000000000e-01 0.000000000000000e+00 -2.000000000000002e-03 0.000000000000000e+00 -7.283090381006491e+17 -2.000000000000002e-03 1.500000000000000e-03 -9.929445360989157e+17 -2.000000000000002e-03 3.000000000000000e-03 -1.323010188043536e+18 -2.000000000000002e-03 4.500000000000001e-03 -1.722781930141353e+18 -2.000000000000002e-03 6.000000000000000e-03 -2.192433139092777e+18 -2.000000000000002e-03 7.500000000000000e-03 -2.726787818169970e+18 -2.000000000000002e-03 9.000000000000001e-03 -3.314402700751265e+18 -2.000000000000002e-03 1.050000000000000e-02 -3.937206090408730e+18 -2.000000000000002e-03 1.200000000000000e-02 -4.570881576052108e+18 -2.000000000000002e-03 1.350000000000000e-02 -5.186098245995719e+18 -2.000000000000002e-03 1.500000000000000e-02 -5.750564250283002e+18 -2.000000000000002e-03 1.650000000000000e-02 -6.231737214050859e+18 -2.000000000000002e-03 1.800000000000000e-02 -6.599890861816324e+18 -2.000000000000002e-03 1.950000000000000e-02 -6.831142241355321e+18 -2.000000000000002e-03 2.100000000000000e-02 -6.910012855230497e+18 -2.000000000000002e-03 2.250000000000000e-02 -6.831142337157982e+18 -2.000000000000002e-03 2.400000000000000e-02 -6.599891053224546e+18 -2.000000000000002e-03 2.550000000000000e-02 -6.231737500561226e+18 -2.000000000000002e-03 2.700000000000000e-02 -5.750564630881052e+18 -2.000000000000002e-03 2.850000000000000e-02 -5.186098718881638e+18 -2.000000000000002e-03 3.000000000000000e-02 -4.570882138332319e+18 -2.000000000000002e-03 3.150000000000000e-02 -3.937206737794418e+18 -2.000000000000002e-03 3.300000000000000e-02 -3.314403427306168e+18 -2.000000000000002e-03 3.450000000000000e-02 -2.726788616146099e+18 -2.000000000000002e-03 3.600000000000000e-02 -2.192433998884827e+18 -2.000000000000002e-03 3.750000000000000e-02 -1.722782840378940e+18 -2.000000000000002e-03 3.900000000000000e-02 -1.323011135826397e+18 -2.000000000000002e-03 4.050000000000000e-02 -9.929455073654217e+17 -2.000000000000002e-03 4.200000000000000e-02 -7.283100181059960e+17 -2.000000000000002e-03 4.350000000000000e-02 -5.220788570820353e+17 -2.000000000000002e-03 4.500000000000000e-02 -3.657504597965220e+17 -2.000000000000002e-03 4.650000000000000e-02 -2.504163084411736e+17 -2.000000000000002e-03 4.800000000000000e-02 -1.675595905672409e+17 -2.000000000000002e-03 4.950000000000000e-02 -1.095733463586774e+17 -2.000000000000002e-03 5.100000000000000e-02 -7.002764364298136e+16 -2.000000000000002e-03 5.250000000000000e-02 -4.373841632689816e+16 -2.000000000000002e-03 5.400000000000000e-02 -2.669841924034458e+16 -2.000000000000002e-03 5.550000000000000e-02 -1.592711060228361e+16 -2.000000000000002e-03 5.700000000000000e-02 -9.285758759146480e+15 -2.000000000000002e-03 5.850000000000000e-02 -5.290865855600780e+15 -2.000000000000002e-03 6.000000000000000e-02 -2.946219215763670e+15 -2.000000000000002e-03 6.150000000000000e-02 -1.603364700877545e+15 -2.000000000000002e-03 6.300000000000000e-02 -8.527633591327697e+14 -2.000000000000002e-03 6.450000000000000e-02 -4.432550563538083e+14 -2.000000000000002e-03 6.600000000000000e-02 -2.251685952577803e+14 -2.000000000000002e-03 6.750000000000000e-02 -1.117868945623322e+14 -2.000000000000002e-03 6.900000000000001e-02 -5.423790649416511e+13 -2.000000000000002e-03 7.050000000000001e-02 -2.571839709821219e+13 -2.000000000000002e-03 7.200000000000001e-02 -1.191828675730764e+13 -2.000000000000002e-03 7.350000000000000e-02 -5.397749383476070e+12 -2.000000000000002e-03 1.200000000000000e-01 0.000000000000000e+00 0.000000000000000e+00 0.000000000000000e+00 -7.246650090268723e+17 0.000000000000000e+00 1.500000000000000e-03 -9.879761404838597e+17 0.000000000000000e+00 3.000000000000000e-03 -1.316389971458999e+18 0.000000000000000e+00 4.500000000000001e-03 -1.714161040080982e+18 0.000000000000000e+00 6.000000000000000e-03 -2.181461856540056e+18 0.000000000000000e+00 7.500000000000000e-03 -2.713142328730486e+18 0.000000000000000e+00 9.000000000000001e-03 -3.297816459270212e+18 0.000000000000000e+00 1.050000000000000e-02 -3.917502992889978e+18 0.000000000000000e+00 1.200000000000000e-02 -4.548007211171584e+18 0.000000000000000e+00 1.350000000000000e-02 -5.160144989937638e+18 0.000000000000000e+00 1.500000000000000e-02 -5.721786084492332e+18 0.000000000000000e+00 1.650000000000000e-02 -6.200550978731613e+18 0.000000000000000e+00 1.800000000000000e-02 -6.566862162553176e+18 0.000000000000000e+00 1.950000000000000e-02 -6.796956206061924e+18 0.000000000000000e+00 2.100000000000000e-02 -6.875432073993469e+18 0.000000000000000e+00 2.250000000000000e-02 -6.796956226060913e+18 0.000000000000000e+00 2.400000000000000e-02 -6.566862202510008e+18 0.000000000000000e+00 2.550000000000000e-02 -6.200551038541201e+18 0.000000000000000e+00 2.700000000000000e-02 -5.721786163942906e+18 0.000000000000000e+00 2.850000000000000e-02 -5.160145088653480e+18 0.000000000000000e+00 3.000000000000000e-02 -4.548007328548657e+18 0.000000000000000e+00 3.150000000000000e-02 -3.917503128032982e+18 0.000000000000000e+00 3.300000000000000e-02 -3.297816610939941e+18 0.000000000000000e+00 3.450000000000000e-02 -2.713142495309532e+18 0.000000000000000e+00 3.600000000000000e-02 -2.181462036023294e+18 0.000000000000000e+00 3.750000000000000e-02 -1.714161230094825e+18 0.000000000000000e+00 3.900000000000000e-02 -1.316390169310490e+18 0.000000000000000e+00 4.050000000000000e-02 -9.879763432376050e+17 0.000000000000000e+00 4.200000000000000e-02 -7.246652136048676e+17 0.000000000000000e+00 4.350000000000000e-02 -5.194661297742071e+17 0.000000000000000e+00 4.500000000000000e-02 -3.639200729785981e+17 0.000000000000000e+00 4.650000000000000e-02 -2.491631077544458e+17 0.000000000000000e+00 4.800000000000000e-02 -1.667210437415144e+17 0.000000000000000e+00 4.950000000000000e-02 -1.090249898974549e+17 0.000000000000000e+00 5.100000000000000e-02 -6.967719243452322e+16 0.000000000000000e+00 5.250000000000000e-02 -4.351952875183248e+16 0.000000000000000e+00 5.400000000000000e-02 -2.656480781115440e+16 0.000000000000000e+00 5.550000000000000e-02 -1.584740385976395e+16 0.000000000000000e+00 5.700000000000000e-02 -9.239288460514990e+15 0.000000000000000e+00 5.850000000000000e-02 -5.264387877545319e+15 0.000000000000000e+00 6.000000000000000e-02 -2.931474950891171e+15 0.000000000000000e+00 6.150000000000000e-02 -1.595340710815957e+15 0.000000000000000e+00 6.300000000000000e-02 -8.484957307806091e+14 0.000000000000000e+00 6.450000000000000e-02 -4.410367999042846e+14 0.000000000000000e+00 6.600000000000000e-02 -2.240417458897189e+14 0.000000000000000e+00 6.750000000000000e-02 -1.112274604697413e+14 0.000000000000000e+00 6.900000000000001e-02 -5.396647455835280e+13 0.000000000000000e+00 7.050000000000001e-02 -2.558969017471727e+13 0.000000000000000e+00 7.200000000000001e-02 -1.185864206190902e+13 0.000000000000000e+00 7.350000000000000e-02 -5.370736515853893e+12 0.000000000000000e+00 1.200000000000000e-01 0.000000000000000e+00 2.000000000000002e-03 0.000000000000000e+00 -7.283090381006491e+17 2.000000000000002e-03 1.500000000000000e-03 -9.929445360989157e+17 2.000000000000002e-03 3.000000000000000e-03 -1.323010188043536e+18 2.000000000000002e-03 4.500000000000001e-03 -1.722781930141353e+18 2.000000000000002e-03 6.000000000000000e-03 -2.192433139092778e+18 2.000000000000002e-03 7.500000000000000e-03 -2.726787818169970e+18 2.000000000000002e-03 9.000000000000001e-03 -3.314402700751265e+18 2.000000000000002e-03 1.050000000000000e-02 -3.937206090408730e+18 2.000000000000002e-03 1.200000000000000e-02 -4.570881576052108e+18 2.000000000000002e-03 1.350000000000000e-02 -5.186098245995719e+18 2.000000000000002e-03 1.500000000000000e-02 -5.750564250283002e+18 2.000000000000002e-03 1.650000000000000e-02 -6.231737214050859e+18 2.000000000000002e-03 1.800000000000000e-02 -6.599890861816324e+18 2.000000000000002e-03 1.950000000000000e-02 -6.831142241355321e+18 2.000000000000002e-03 2.100000000000000e-02 -6.910012855230497e+18 2.000000000000002e-03 2.250000000000000e-02 -6.831142337157982e+18 2.000000000000002e-03 2.400000000000000e-02 -6.599891053224546e+18 2.000000000000002e-03 2.550000000000000e-02 -6.231737500561226e+18 2.000000000000002e-03 2.700000000000000e-02 -5.750564630881052e+18 2.000000000000002e-03 2.850000000000000e-02 -5.186098718881638e+18 2.000000000000002e-03 3.000000000000000e-02 -4.570882138332319e+18 2.000000000000002e-03 3.150000000000000e-02 -3.937206737794418e+18 2.000000000000002e-03 3.300000000000000e-02 -3.314403427306168e+18 2.000000000000002e-03 3.450000000000000e-02 -2.726788616146099e+18 2.000000000000002e-03 3.600000000000000e-02 -2.192433998884827e+18 2.000000000000002e-03 3.750000000000000e-02 -1.722782840378940e+18 2.000000000000002e-03 3.900000000000000e-02 -1.323011135826397e+18 2.000000000000002e-03 4.050000000000000e-02 -9.929455073654217e+17 2.000000000000002e-03 4.200000000000000e-02 -7.283100181059960e+17 2.000000000000002e-03 4.350000000000000e-02 -5.220788570820353e+17 2.000000000000002e-03 4.500000000000000e-02 -3.657504597965220e+17 2.000000000000002e-03 4.650000000000000e-02 -2.504163084411736e+17 2.000000000000002e-03 4.800000000000000e-02 -1.675595905672409e+17 2.000000000000002e-03 4.950000000000000e-02 -1.095733463586774e+17 2.000000000000002e-03 5.100000000000000e-02 -7.002764364298136e+16 2.000000000000002e-03 5.250000000000000e-02 -4.373841632689816e+16 2.000000000000002e-03 5.400000000000000e-02 -2.669841924034458e+16 2.000000000000002e-03 5.550000000000000e-02 -1.592711060228361e+16 2.000000000000002e-03 5.700000000000000e-02 -9.285758759146480e+15 2.000000000000002e-03 5.850000000000000e-02 -5.290865855600780e+15 2.000000000000002e-03 6.000000000000000e-02 -2.946219215763670e+15 2.000000000000002e-03 6.150000000000000e-02 -1.603364700877545e+15 2.000000000000002e-03 6.300000000000000e-02 -8.527633591327697e+14 2.000000000000002e-03 6.450000000000000e-02 -4.432550563538083e+14 2.000000000000002e-03 6.600000000000000e-02 -2.251685952577803e+14 2.000000000000002e-03 6.750000000000000e-02 -1.117868945623322e+14 2.000000000000002e-03 6.900000000000001e-02 -5.423790649416511e+13 2.000000000000002e-03 7.050000000000001e-02 -2.571839709821219e+13 2.000000000000002e-03 7.200000000000001e-02 -1.191828675730764e+13 2.000000000000002e-03 7.350000000000000e-02 -5.397749383476070e+12 2.000000000000002e-03 1.200000000000000e-01 0.000000000000000e+00 4.000000000000004e-03 0.000000000000000e+00 -7.390868594206536e+17 4.000000000000004e-03 1.500000000000000e-03 -1.007641196091990e+18 4.000000000000004e-03 3.000000000000000e-03 -1.342594694670214e+18 4.000000000000004e-03 4.500000000000001e-03 -1.748286603756136e+18 4.000000000000004e-03 6.000000000000000e-03 -2.224892856822159e+18 4.000000000000004e-03 7.500000000000000e-03 -2.767160795917116e+18 4.000000000000004e-03 9.000000000000001e-03 -3.363477683710082e+18 4.000000000000004e-03 1.050000000000000e-02 -3.995504196480894e+18 4.000000000000004e-03 1.200000000000000e-02 -4.638563822466501e+18 4.000000000000004e-03 1.350000000000000e-02 -5.262891294211610e+18 4.000000000000004e-03 1.500000000000000e-02 -5.835716561363954e+18 4.000000000000004e-03 1.650000000000000e-02 -6.324015341113397e+18 4.000000000000004e-03 1.800000000000000e-02 -6.697621154179312e+18 4.000000000000004e-03 1.950000000000000e-02 -6.932297376706426e+18 4.000000000000004e-03 2.100000000000000e-02 -7.012336297589424e+18 4.000000000000004e-03 2.250000000000000e-02 -6.932298171141018e+18 4.000000000000004e-03 2.400000000000000e-02 -6.697622741414060e+18 4.000000000000004e-03 2.550000000000000e-02 -6.324017716973772e+18 4.000000000000004e-03 2.700000000000000e-02 -5.835719717437611e+18 4.000000000000004e-03 2.850000000000000e-02 -5.262895215573797e+18 4.000000000000004e-03 3.000000000000000e-02 -4.638568485122468e+18 4.000000000000004e-03 3.150000000000000e-02 -3.995509564866072e+18 4.000000000000004e-03 3.300000000000000e-02 -3.363483708598559e+18 4.000000000000004e-03 3.450000000000000e-02 -2.767167413059416e+18 4.000000000000004e-03 3.600000000000000e-02 -2.224899986567197e+18 4.000000000000004e-03 3.750000000000000e-02 -1.748294151816059e+18 4.000000000000004e-03 3.900000000000000e-02 -1.342602554070804e+18 4.000000000000004e-03 4.050000000000000e-02 -1.007649250228512e+18 4.000000000000004e-03 4.200000000000000e-02 -7.390949860231958e+17 4.000000000000004e-03 4.350000000000000e-02 -5.298099119246249e+17 4.000000000000004e-03 4.500000000000000e-02 -3.711665712326959e+17 4.000000000000004e-03 4.650000000000000e-02 -2.541245274109814e+17 4.000000000000004e-03 4.800000000000000e-02 -1.700408495441456e+17 4.000000000000004e-03 4.950000000000000e-02 -1.111959325093780e+17 4.000000000000004e-03 5.100000000000000e-02 -7.106462841923587e+16 4.000000000000004e-03 5.250000000000000e-02 -4.438610446536875e+16 4.000000000000004e-03 5.400000000000000e-02 -2.709377534971486e+16 4.000000000000004e-03 5.550000000000000e-02 -1.616296279217313e+16 4.000000000000004e-03 5.700000000000000e-02 -9.423264338488952e+15 4.000000000000004e-03 5.850000000000000e-02 -5.369214173338498e+15 4.000000000000004e-03 6.000000000000000e-02 -2.989847484565887e+15 4.000000000000004e-03 6.150000000000000e-02 -1.627107681228957e+15 4.000000000000004e-03 6.300000000000000e-02 -8.653912678630897e+14 4.000000000000004e-03 6.450000000000000e-02 -4.498188751552436e+14 4.000000000000004e-03 6.600000000000000e-02 -2.285029413842634e+14 4.000000000000004e-03 6.750000000000000e-02 -1.134422593933214e+14 4.000000000000004e-03 6.900000000000001e-02 -5.504107323149214e+13 4.000000000000004e-03 7.050000000000001e-02 -2.609924068722680e+13 4.000000000000004e-03 7.200000000000001e-02 -1.209477530453137e+13 4.000000000000004e-03 7.350000000000000e-02 -5.477680402440232e+12 4.000000000000004e-03 1.200000000000000e-01 0.000000000000000e+00 5.999999999999991e-03 0.000000000000000e+00 -7.565173220934927e+17 5.999999999999991e-03 1.500000000000000e-03 -1.031424418853124e+18 5.999999999999991e-03 3.000000000000000e-03 -1.374302025330810e+18 5.999999999999991e-03 4.500000000000001e-03 -1.789591982051935e+18 5.999999999999991e-03 6.000000000000000e-03 -2.277474306911029e+18 5.999999999999991e-03 7.500000000000000e-03 -2.832571995474740e+18 5.999999999999991e-03 9.000000000000001e-03 -3.442997506452853e+18 5.999999999999991e-03 1.050000000000000e-02 -4.089977592923895e+18 5.999999999999991e-03 1.200000000000000e-02 -4.748251919162302e+18 5.999999999999991e-03 1.350000000000000e-02 -5.387351030475010e+18 5.999999999999991e-03 1.500000000000000e-02 -5.973729626236623e+18 5.999999999999991e-03 1.650000000000000e-02 -6.473582176302136e+18 5.999999999999991e-03 1.800000000000000e-02 -6.856028571863975e+18 5.999999999999991e-03 1.950000000000000e-02 -7.096258844745521e+18 5.999999999999991e-03 2.100000000000000e-02 -7.178193702377044e+18 5.999999999999991e-03 2.250000000000000e-02 -7.096264714308680e+18 5.999999999999991e-03 2.400000000000000e-02 -6.856040298914518e+18 5.999999999999991e-03 2.550000000000000e-02 -6.473599729997158e+18 5.999999999999991e-03 2.700000000000000e-02 -5.973752944422738e+18 5.999999999999991e-03 2.850000000000000e-02 -5.387380002882911e+18 5.999999999999991e-03 3.000000000000000e-02 -4.748286368510284e+18 5.999999999999991e-03 3.150000000000000e-02 -4.090017256448375e+18 5.999999999999991e-03 3.300000000000000e-02 -3.443042020455431e+18 5.999999999999991e-03 3.450000000000000e-02 -2.832620885257598e+18 5.999999999999991e-03 3.600000000000000e-02 -2.277526983983850e+18 5.999999999999991e-03 3.750000000000000e-02 -1.789647749782757e+18 5.999999999999991e-03 3.900000000000000e-02 -1.374360093356369e+18 5.999999999999991e-03 4.050000000000000e-02 -1.031483925656494e+18 5.999999999999991e-03 4.200000000000000e-02 -7.565773643013955e+17 5.999999999999991e-03 4.350000000000000e-02 -5.423419201222024e+17 5.999999999999991e-03 4.500000000000000e-02 -3.799460700483579e+17 5.999999999999991e-03 4.650000000000000e-02 -2.601355406522535e+17 5.999999999999991e-03 4.800000000000000e-02 -1.740629652261026e+17 5.999999999999991e-03 4.950000000000000e-02 -1.138261420471271e+17 5.999999999999991e-03 5.100000000000000e-02 -7.274557944944832e+16 5.999999999999991e-03 5.250000000000000e-02 -4.543600631524984e+16 5.999999999999991e-03 5.400000000000000e-02 -2.773464730715848e+16 5.999999999999991e-03 5.550000000000000e-02 -1.654527905006096e+16 5.999999999999991e-03 5.700000000000000e-02 -9.646160811394468e+15 5.999999999999991e-03 5.850000000000000e-02 -5.496216757644654e+15 5.999999999999991e-03 6.000000000000000e-02 -3.060568885118200e+15 5.999999999999991e-03 6.150000000000000e-02 -1.665595037449166e+15 5.999999999999991e-03 6.300000000000000e-02 -8.858610979424259e+14 5.999999999999991e-03 6.450000000000000e-02 -4.604588187498821e+14 5.999999999999991e-03 6.600000000000000e-02 -2.339079120547487e+14 5.999999999999991e-03 6.750000000000000e-02 -1.161256029657286e+14 5.999999999999991e-03 6.900000000000001e-02 -5.634300476394412e+13 5.999999999999991e-03 7.050000000000001e-02 -2.671658709510325e+13 5.999999999999991e-03 7.200000000000001e-02 -1.238086262929412e+13 5.999999999999991e-03 7.350000000000000e-02 -5.607248240339111e+12 5.999999999999991e-03 1.200000000000000e-01 0.000000000000000e+00 7.999999999999993e-03 0.000000000000000e+00 -7.796458372618280e+17 7.999999999999993e-03 1.500000000000000e-03 -1.063080069064228e+18 7.999999999999993e-03 3.000000000000000e-03 -1.416597273008447e+18 7.999999999999993e-03 4.500000000000001e-03 -1.844776718901417e+18 7.999999999999993e-03 6.000000000000000e-03 -2.347803515517002e+18 7.999999999999993e-03 7.500000000000000e-03 -2.920133282054802e+18 7.999999999999993e-03 9.000000000000001e-03 -3.549509109183655e+18 7.999999999999993e-03 1.050000000000000e-02 -4.216574804840703e+18 7.999999999999993e-03 1.200000000000000e-02 -4.895285920745753e+18 7.999999999999993e-03 1.350000000000000e-02 -5.554227396519946e+18 7.999999999999993e-03 1.500000000000000e-02 -6.158813022418337e+18 7.999999999999993e-03 1.650000000000000e-02 -6.674188395067927e+18 7.999999999999993e-03 1.800000000000000e-02 -7.068515371518548e+18 7.999999999999993e-03 1.950000000000000e-02 -7.316214311702621e+18 7.999999999999993e-03 2.100000000000000e-02 -7.400707112480935e+18 7.999999999999993e-03 2.250000000000000e-02 -7.316252586026586e+18 7.999999999999993e-03 2.400000000000000e-02 -7.068591841422610e+18 7.999999999999993e-03 2.550000000000000e-02 -6.674302859431264e+18 7.999999999999993e-03 2.700000000000000e-02 -6.158965075950327e+18 7.999999999999993e-03 2.850000000000000e-02 -5.554416320175081e+18 7.999999999999993e-03 3.000000000000000e-02 -4.895510558503151e+18 7.999999999999993e-03 3.150000000000000e-02 -4.216833443268195e+18 7.999999999999993e-03 3.300000000000000e-02 -3.549799376671970e+18 7.999999999999993e-03 3.450000000000000e-02 -2.920452083188212e+18 7.999999999999993e-03 3.600000000000000e-02 -2.348147012860172e+18 7.999999999999993e-03 3.750000000000000e-02 -1.845140369847565e+18 7.999999999999993e-03 3.900000000000000e-02 -1.416975923746503e+18 7.999999999999993e-03 4.050000000000000e-02 -1.063468101803399e+18 7.999999999999993e-03 4.200000000000000e-02 -7.800373612738520e+17 7.999999999999993e-03 4.350000000000000e-02 -5.591589528576733e+17 7.999999999999993e-03 4.500000000000000e-02 -3.917275398307874e+17 7.999999999999993e-03 4.650000000000000e-02 -2.682019137411240e+17 7.999999999999993e-03 4.800000000000000e-02 -1.794603812887205e+17 7.999999999999993e-03 4.950000000000000e-02 -1.173557159157170e+17 7.999999999999993e-03 5.100000000000000e-02 -7.500131124270179e+16 7.999999999999993e-03 5.250000000000000e-02 -4.684491053240149e+16 7.999999999999993e-03 5.400000000000000e-02 -2.859465891430278e+16 7.999999999999993e-03 5.550000000000000e-02 -1.705832468947107e+16 7.999999999999993e-03 5.700000000000000e-02 -9.945274672582526e+15 7.999999999999993e-03 5.850000000000000e-02 -5.666646713402860e+15 7.999999999999993e-03 6.000000000000000e-02 -3.155472811003025e+15 7.999999999999993e-03 6.150000000000000e-02 -1.717242772223689e+15 7.999999999999993e-03 6.300000000000000e-02 -9.133303748924830e+14 7.999999999999993e-03 6.450000000000000e-02 -4.747369713785159e+14 7.999999999999993e-03 6.600000000000000e-02 -2.411610451208018e+14 7.999999999999993e-03 6.750000000000000e-02 -1.197264783332491e+14 7.999999999999993e-03 6.900000000000001e-02 -5.809011109562172e+13 7.999999999999993e-03 7.050000000000001e-02 -2.754502386455252e+13 7.999999999999993e-03 7.200000000000001e-02 -1.276477150149657e+13 7.999999999999993e-03 7.350000000000000e-02 -5.781118639192663e+12 7.999999999999993e-03 1.200000000000000e-01 0.000000000000000e+00 9.999999999999995e-03 0.000000000000000e+00 -8.062498167485682e+17 9.999999999999995e-03 1.500000000000000e-03 -1.100042961273176e+18 9.999999999999995e-03 3.000000000000000e-03 -1.466503642515066e+18 9.999999999999995e-03 4.500000000000001e-03 -1.910376538007188e+18 9.999999999999995e-03 6.000000000000000e-03 -2.431850759240481e+18 9.999999999999995e-03 7.500000000000000e-03 -3.025175977377608e+18 9.999999999999995e-03 9.000000000000001e-03 -3.677643747285812e+18 9.999999999999995e-03 1.050000000000000e-02 -4.369186907751307e+18 9.999999999999995e-03 1.200000000000000e-02 -5.072805883962431e+18 9.999999999999995e-03 1.350000000000000e-02 -5.755934678692389e+18 9.999999999999995e-03 1.500000000000000e-02 -6.382720828926360e+18 9.999999999999995e-03 1.650000000000000e-02 -6.917034479987847e+18 9.999999999999995e-03 1.800000000000000e-02 -7.325872822746296e+18 9.999999999999995e-03 1.950000000000000e-02 -7.582720718193958e+18 9.999999999999995e-03 2.100000000000000e-02 -7.670393837511427e+18 9.999999999999995e-03 2.250000000000000e-02 -7.582940971719052e+18 9.999999999999995e-03 2.400000000000000e-02 -7.326312876656822e+18 9.999999999999995e-03 2.550000000000000e-02 -6.917693176913386e+18 9.999999999999995e-03 2.700000000000000e-02 -6.383595836580436e+18 9.999999999999995e-03 2.850000000000000e-02 -5.757021859253847e+18 9.999999999999995e-03 3.000000000000000e-02 -5.074098584990457e+18 9.999999999999995e-03 3.150000000000000e-02 -4.370675269124649e+18 9.999999999999995e-03 3.300000000000000e-02 -3.679314121335549e+18 9.999999999999995e-03 3.450000000000000e-02 -3.027010551216256e+18 9.999999999999995e-03 3.600000000000000e-02 -2.433827449952616e+18 9.999999999999995e-03 3.750000000000000e-02 -1.912469204695870e+18 9.999999999999995e-03 3.900000000000000e-02 -1.468682627045616e+18 9.999999999999995e-03 4.050000000000000e-02 -1.102275935491959e+18 9.999999999999995e-03 4.200000000000000e-02 -8.085028818552737e+17 9.999999999999995e-03 4.350000000000000e-02 -5.795644105145656e+17 9.999999999999995e-03 4.500000000000000e-02 -4.060231029157102e+17 9.999999999999995e-03 4.650000000000000e-02 -2.779896915383604e+17 9.999999999999995e-03 4.800000000000000e-02 -1.860096829833820e+17 9.999999999999995e-03 4.950000000000000e-02 -1.216385778379597e+17 9.999999999999995e-03 5.100000000000000e-02 -7.773847906601072e+16 9.999999999999995e-03 5.250000000000000e-02 -4.855452084843526e+16 9.999999999999995e-03 5.400000000000000e-02 -2.963822808614000e+16 9.999999999999995e-03 5.550000000000000e-02 -1.768087406461685e+16 9.999999999999995e-03 5.700000000000000e-02 -1.030823139066796e+16 9.999999999999995e-03 5.850000000000000e-02 -5.873453301806208e+15 9.999999999999995e-03 6.000000000000000e-02 -3.270633007955179e+15 9.999999999999995e-03 6.150000000000000e-02 -1.779914103232650e+15 9.999999999999995e-03 6.300000000000000e-02 -9.466625695791409e+14 9.999999999999995e-03 6.450000000000000e-02 -4.920625338328252e+14 9.999999999999995e-03 6.600000000000000e-02 -2.499621900242185e+14 9.999999999999995e-03 6.750000000000000e-02 -1.240958535022039e+14 9.999999999999995e-03 6.900000000000001e-02 -6.021007154373087e+13 9.999999999999995e-03 7.050000000000001e-02 -2.855025130923462e+13 9.999999999999995e-03 7.200000000000001e-02 -1.323060310097650e+13 9.999999999999995e-03 7.350000000000000e-02 -5.992088989100574e+12 9.999999999999995e-03 1.200000000000000e-01 0.000000000000000e+00 1.200000000000000e-02 0.000000000000000e+00 -8.293332565113192e+17 1.200000000000000e-02 1.500000000000000e-03 -1.134930780957068e+18 1.200000000000000e-02 3.000000000000000e-03 -1.516229750525101e+18 1.200000000000000e-02 4.500000000000001e-03 -1.978155852183071e+18 1.200000000000000e-02 6.000000000000000e-03 -2.520892188716312e+18 1.200000000000000e-02 7.500000000000000e-03 -3.138441070470564e+18 1.200000000000000e-02 9.000000000000001e-03 -3.817565842846540e+18 1.200000000000000e-02 1.050000000000000e-02 -4.537375616398902e+18 1.200000000000000e-02 1.200000000000000e-02 -5.269769948054354e+18 1.200000000000000e-02 1.350000000000000e-02 -5.980860652590076e+18 1.200000000000000e-02 1.500000000000000e-02 -6.633343899338214e+18 1.200000000000000e-02 1.650000000000000e-02 -7.189630294898575e+18 1.200000000000000e-02 1.800000000000000e-02 -7.615385829263279e+18 1.200000000000000e-02 1.950000000000000e-02 -7.883026961817150e+18 1.200000000000000e-02 2.100000000000000e-02 -7.974677277513677e+18 1.200000000000000e-02 2.250000000000000e-02 -7.884145501511896e+18 1.200000000000000e-02 2.400000000000000e-02 -7.617620607419677e+18 1.200000000000000e-02 2.550000000000000e-02 -7.192975433904668e+18 1.200000000000000e-02 2.700000000000000e-02 -6.637787554865947e+18 1.200000000000000e-02 2.850000000000000e-02 -5.986381811049744e+18 1.200000000000000e-02 3.000000000000000e-02 -5.276334825563864e+18 1.200000000000000e-02 3.150000000000000e-02 -4.544934139130805e+18 1.200000000000000e-02 3.300000000000000e-02 -3.826048702219175e+18 1.200000000000000e-02 3.450000000000000e-02 -3.147757805177031e+18 1.200000000000000e-02 3.600000000000000e-02 -2.530930652458536e+18 1.200000000000000e-02 3.750000000000000e-02 -1.988783290532391e+18 1.200000000000000e-02 3.900000000000000e-02 -1.527295547045769e+18 1.200000000000000e-02 4.050000000000000e-02 -1.146270759738252e+18 1.200000000000000e-02 4.200000000000000e-02 -8.407752652401926e+17 1.200000000000000e-02 4.350000000000000e-02 -6.027001307814373e+17 1.200000000000000e-02 4.500000000000000e-02 -4.222321909799549e+17 1.200000000000000e-02 4.650000000000000e-02 -2.890880447456241e+17 1.200000000000000e-02 4.800000000000000e-02 -1.934361724236052e+17 1.200000000000000e-02 4.950000000000000e-02 -1.264951985200590e+17 1.200000000000000e-02 5.100000000000000e-02 -8.084240113719288e+16 1.200000000000000e-02 5.250000000000000e-02 -5.049323492734806e+16 1.200000000000000e-02 5.400000000000000e-02 -3.082166005572287e+16 1.200000000000000e-02 5.550000000000000e-02 -1.838686575492668e+16 1.200000000000000e-02 5.700000000000000e-02 -1.071983840107994e+16 1.200000000000000e-02 5.850000000000000e-02 -6.107980323086354e+15 1.200000000000000e-02 6.000000000000000e-02 -3.401229040222034e+15 1.200000000000000e-02 6.150000000000000e-02 -1.850985363629642e+15 1.200000000000000e-02 6.300000000000000e-02 -9.844619700260135e+14 1.200000000000000e-02 6.450000000000000e-02 -5.117098181243921e+14 1.200000000000000e-02 6.600000000000000e-02 -2.599425608146879e+14 1.200000000000000e-02 6.750000000000000e-02 -1.290505503762825e+14 1.200000000000000e-02 6.900000000000001e-02 -6.261395509665653e+13 1.200000000000000e-02 7.050000000000001e-02 -2.969006861704455e+13 1.200000000000000e-02 7.200000000000001e-02 -1.375878315840487e+13 1.200000000000000e-02 7.350000000000000e-02 -6.231284478725462e+12 1.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 1.400000000000000e-02 0.000000000000000e+00 -8.241538731789585e+17 1.400000000000000e-02 1.500000000000000e-03 -1.142682913033287e+18 1.400000000000000e-02 3.000000000000000e-03 -1.540610619971717e+18 1.400000000000000e-02 4.500000000000001e-03 -2.023029469908121e+18 1.400000000000000e-02 6.000000000000000e-03 -2.590071459169521e+18 1.400000000000000e-02 7.500000000000000e-03 -3.235414526611827e+18 1.400000000000000e-02 9.000000000000001e-03 -3.945185802452336e+18 1.400000000000000e-02 1.050000000000000e-02 -4.697534932464232e+18 1.400000000000000e-02 1.200000000000000e-02 -5.463102983734320e+18 1.400000000000000e-02 1.350000000000000e-02 -6.206508468574790e+18 1.400000000000000e-02 1.500000000000000e-02 -6.888822123934835e+18 1.400000000000000e-02 1.650000000000000e-02 -7.470829905069733e+18 1.400000000000000e-02 1.800000000000000e-02 -7.916722563060836e+18 1.400000000000000e-02 1.950000000000000e-02 -8.197736179668392e+18 1.400000000000000e-02 2.100000000000000e-02 -8.295230825842719e+18 1.400000000000000e-02 2.250000000000000e-02 -8.202749126793068e+18 1.400000000000000e-02 2.400000000000000e-02 -7.926738143898983e+18 1.400000000000000e-02 2.550000000000000e-02 -7.485821777992083e+18 1.400000000000000e-02 2.700000000000000e-02 -6.908737206345798e+18 1.400000000000000e-02 2.850000000000000e-02 -6.231252584099068e+18 1.400000000000000e-02 3.000000000000000e-02 -5.492524723516768e+18 1.400000000000000e-02 3.150000000000000e-02 -4.731409881179668e+18 1.400000000000000e-02 3.300000000000000e-02 -3.983203340587858e+18 1.400000000000000e-02 3.450000000000000e-02 -3.277169234717000e+18 1.400000000000000e-02 3.600000000000000e-02 -2.635060732405999e+18 1.400000000000000e-02 3.750000000000000e-02 -2.070658344203917e+18 1.400000000000000e-02 3.900000000000000e-02 -1.590204079292936e+18 1.400000000000000e-02 4.050000000000000e-02 -1.193505171994741e+18 1.400000000000000e-02 4.200000000000000e-02 -8.754333986418186e+17 1.400000000000000e-02 4.350000000000000e-02 -6.275517571272087e+17 1.400000000000000e-02 4.500000000000000e-02 -4.396467176241859e+17 1.400000000000000e-02 4.650000000000000e-02 -3.010136137214081e+17 1.400000000000000e-02 4.800000000000000e-02 -2.014172181318716e+17 1.400000000000000e-02 4.950000000000000e-02 -1.317150226540097e+17 1.400000000000000e-02 5.100000000000000e-02 -8.417873119141278e+16 1.400000000000000e-02 5.250000000000000e-02 -5.257724837859416e+16 1.400000000000000e-02 5.400000000000000e-02 -3.209384836333410e+16 1.400000000000000e-02 5.550000000000000e-02 -1.914583186642269e+16 1.400000000000000e-02 5.700000000000000e-02 -1.116233910705027e+16 1.400000000000000e-02 5.850000000000000e-02 -6.360111429699760e+15 1.400000000000000e-02 6.000000000000000e-02 -3.541626693411959e+15 1.400000000000000e-02 6.150000000000000e-02 -1.927389012707135e+15 1.400000000000000e-02 6.300000000000000e-02 -1.025095903134199e+15 1.400000000000000e-02 6.450000000000000e-02 -5.328293157472596e+14 1.400000000000000e-02 6.600000000000000e-02 -2.706700350376744e+14 1.400000000000000e-02 6.750000000000000e-02 -1.343756714578967e+14 1.400000000000000e-02 6.900000000000001e-02 -6.519727517474893e+13 1.400000000000000e-02 7.050000000000001e-02 -3.091480298244504e+13 1.400000000000000e-02 7.200000000000001e-02 -1.432622100668534e+13 1.400000000000000e-02 7.350000000000000e-02 -6.488208427771121e+12 1.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 1.600000000000000e-02 0.000000000000000e+00 -7.079438509647896e+17 1.600000000000000e-02 1.500000000000000e-03 -1.040595189491889e+18 1.600000000000000e-02 3.000000000000000e-03 -1.458038614166008e+18 1.600000000000000e-02 4.500000000000001e-03 -1.965434431249883e+18 1.600000000000000e-02 6.000000000000000e-03 -2.562697262673091e+18 1.600000000000000e-02 7.500000000000000e-03 -3.242957067450232e+18 1.600000000000000e-02 9.000000000000001e-03 -3.991437274767257e+18 1.600000000000000e-02 1.050000000000000e-02 -4.785032579529854e+18 1.600000000000000e-02 1.200000000000000e-02 -5.592819147847467e+18 1.600000000000000e-02 1.350000000000000e-02 -6.377621877810833e+18 1.600000000000000e-02 1.500000000000000e-02 -7.098607647848303e+18 1.600000000000000e-02 1.650000000000000e-02 -7.714694722791504e+18 1.600000000000000e-02 1.800000000000000e-02 -8.188401339977895e+18 1.600000000000000e-02 1.950000000000000e-02 -8.489638367804979e+18 1.600000000000000e-02 2.100000000000000e-02 -8.598912663518717e+18 1.600000000000000e-02 2.250000000000000e-02 -8.509464958291016e+18 1.600000000000000e-02 2.400000000000000e-02 -8.228013730617380e+18 1.600000000000000e-02 2.550000000000000e-02 -7.773988730419677e+18 1.600000000000000e-02 2.700000000000000e-02 -7.177373326726943e+18 1.600000000000000e-02 2.850000000000000e-02 -6.475486753150162e+18 1.600000000000000e-02 3.000000000000000e-02 -5.709184386008850e+18 1.600000000000000e-02 3.150000000000000e-02 -4.919010600684399e+18 1.600000000000000e-02 3.300000000000000e-02 -4.141799554909806e+18 1.600000000000000e-02 3.450000000000000e-02 -3.408100141549346e+18 1.600000000000000e-02 3.600000000000000e-02 -2.740633290031797e+18 1.600000000000000e-02 3.750000000000000e-02 -2.153810283316089e+18 1.600000000000000e-02 3.900000000000000e-02 -1.654184550736463e+18 1.600000000000000e-02 4.050000000000000e-02 -1.241601122916574e+18 1.600000000000000e-02 4.200000000000000e-02 -9.107583084853590e+17 1.600000000000000e-02 4.350000000000000e-02 -6.529021791881418e+17 1.600000000000000e-02 4.500000000000000e-02 -4.574228336191276e+17 1.600000000000000e-02 4.650000000000000e-02 -3.131936560038632e+17 1.600000000000000e-02 4.800000000000000e-02 -2.095723510786771e+17 1.600000000000000e-02 4.950000000000000e-02 -1.370507253979670e+17 1.600000000000000e-02 5.100000000000000e-02 -8.759016420320406e+16 1.600000000000000e-02 5.250000000000000e-02 -5.470868105744657e+16 1.600000000000000e-02 5.400000000000000e-02 -3.339521504789989e+16 1.600000000000000e-02 5.550000000000000e-02 -1.992230025274896e+16 1.600000000000000e-02 5.700000000000000e-02 -1.161507586339696e+16 1.600000000000000e-02 5.850000000000000e-02 -6.618079921288706e+15 1.600000000000000e-02 6.000000000000000e-02 -3.685270463855425e+15 1.600000000000000e-02 6.150000000000000e-02 -2.005552817980324e+15 1.600000000000000e-02 6.300000000000000e-02 -1.066660362387986e+15 1.600000000000000e-02 6.450000000000000e-02 -5.544283372325223e+14 1.600000000000000e-02 6.600000000000000e-02 -2.816383161010808e+14 1.600000000000000e-02 6.750000000000000e-02 -1.398185874713710e+14 1.600000000000000e-02 6.900000000000001e-02 -6.783669250029758e+13 1.600000000000000e-02 7.050000000000001e-02 -3.216552618130479e+13 1.600000000000000e-02 7.200000000000001e-02 -1.490535976516063e+13 1.600000000000000e-02 7.350000000000000e-02 -6.750244886133698e+12 1.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 1.800000000000000e-02 0.000000000000000e+00 -2.365715564310275e+17 1.800000000000000e-02 1.500000000000000e-03 -5.857588803726921e+17 1.800000000000000e-02 3.000000000000000e-03 -1.030165374279596e+18 1.800000000000000e-02 4.500000000000001e-03 -1.574684053148194e+18 1.800000000000000e-02 6.000000000000000e-03 -2.218485008284348e+18 1.800000000000000e-02 7.500000000000000e-03 -2.953468967188130e+18 1.800000000000000e-02 9.000000000000001e-03 -3.763167624574862e+18 1.800000000000000e-02 1.050000000000000e-02 -4.622378013405886e+18 1.800000000000000e-02 1.200000000000000e-02 -5.497766090931403e+18 1.800000000000000e-02 1.350000000000000e-02 -6.349562821085976e+18 1.800000000000000e-02 1.500000000000000e-02 -7.134315340564292e+18 1.800000000000000e-02 1.650000000000000e-02 -7.808471630126708e+18 1.800000000000000e-02 1.800000000000000e-02 -8.332405248926820e+18 1.800000000000000e-02 1.950000000000000e-02 -8.674365739629171e+18 1.800000000000000e-02 2.100000000000000e-02 -8.813802104679658e+18 1.800000000000000e-02 2.250000000000000e-02 -8.743567340102588e+18 1.800000000000000e-02 2.400000000000000e-02 -8.470666077623576e+18 1.800000000000000e-02 2.550000000000000e-02 -8.015428052071390e+18 1.800000000000000e-02 2.700000000000000e-02 -7.409234573128051e+18 1.800000000000000e-02 2.850000000000000e-02 -6.691144799509481e+18 1.800000000000000e-02 3.000000000000000e-02 -5.903920680441351e+18 1.800000000000000e-02 3.150000000000000e-02 -5.090007255997320e+18 1.800000000000000e-02 3.300000000000000e-02 -4.287983550138315e+18 1.800000000000000e-02 3.450000000000000e-02 -3.529874932843573e+18 1.800000000000000e-02 3.600000000000000e-02 -2.839542768254549e+18 1.800000000000000e-02 3.750000000000000e-02 -2.232180381763348e+18 1.800000000000000e-02 3.900000000000000e-02 -1.714781962623041e+18 1.800000000000000e-02 4.050000000000000e-02 -1.287338524509586e+18 1.800000000000000e-02 4.200000000000000e-02 -9.444635699093916e+17 1.800000000000000e-02 4.350000000000000e-02 -6.771574980765615e+17 1.800000000000000e-02 4.500000000000000e-02 -4.744702158372650e+17 1.800000000000000e-02 4.650000000000000e-02 -3.248966188569087e+17 1.800000000000000e-02 4.800000000000000e-02 -2.174203275531352e+17 1.800000000000000e-02 4.950000000000000e-02 -1.421920134835867e+17 1.800000000000000e-02 5.100000000000000e-02 -9.088065771836405e+16 1.800000000000000e-02 5.250000000000000e-02 -5.676619327000658e+16 1.800000000000000e-02 5.400000000000000e-02 -3.465219781172213e+16 1.800000000000000e-02 5.550000000000000e-02 -2.067259413306323e+16 1.800000000000000e-02 5.700000000000000e-02 -1.205265358084332e+16 1.800000000000000e-02 5.850000000000000e-02 -6.867427066407405e+15 1.800000000000000e-02 6.000000000000000e-02 -3.824099411068062e+15 1.800000000000000e-02 6.150000000000000e-02 -2.081076035081338e+15 1.800000000000000e-02 6.300000000000000e-02 -1.106802587989374e+15 1.800000000000000e-02 6.450000000000000e-02 -5.752749610926719e+14 1.800000000000000e-02 6.600000000000000e-02 -2.922155697285392e+14 1.800000000000000e-02 6.750000000000000e-02 -1.450618174114340e+14 1.800000000000000e-02 6.900000000000001e-02 -7.037588261645839e+13 1.800000000000000e-02 7.050000000000001e-02 -3.336678926178532e+13 1.800000000000000e-02 7.200000000000001e-02 -1.546049326072604e+13 1.800000000000000e-02 7.350000000000000e-02 -7.000818219428047e+12 1.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 1.999999999999999e-02 0.000000000000000e+00 1.207375061613765e+18 1.999999999999999e-02 1.500000000000000e-03 8.352829904211543e+17 1.999999999999999e-02 3.000000000000000e-03 3.438281887074058e+17 1.999999999999999e-02 4.500000000000001e-03 -2.706941657663677e+17 1.999999999999999e-02 6.000000000000000e-03 -1.005266883037262e+18 1.999999999999999e-02 7.500000000000000e-03 -1.848701796150988e+18 1.999999999999999e-02 9.000000000000001e-03 -2.780692587048301e+18 1.999999999999999e-02 1.050000000000000e-02 -3.771648641943144e+18 1.999999999999999e-02 1.200000000000000e-02 -4.783534197520873e+18 1.999999999999999e-02 1.350000000000000e-02 -5.771822364430575e+18 1.999999999999999e-02 1.500000000000000e-02 -6.688510330321384e+18 1.999999999999999e-02 1.650000000000000e-02 -7.485955832333271e+18 1.999999999999999e-02 1.800000000000000e-02 -8.121122203432828e+18 1.999999999999999e-02 1.950000000000000e-02 -8.559699206695998e+18 1.999999999999999e-02 2.100000000000000e-02 -8.779531806156064e+18 1.999999999999999e-02 2.250000000000000e-02 -8.772855142446312e+18 1.999999999999999e-02 2.400000000000000e-02 -8.546995537529940e+18 1.999999999999999e-02 2.550000000000000e-02 -8.123426490199068e+18 1.999999999999999e-02 2.700000000000000e-02 -7.535321182555880e+18 1.999999999999999e-02 2.850000000000000e-02 -6.823968929657405e+18 1.999999999999999e-02 3.000000000000000e-02 -6.034578407394789e+18 1.999999999999999e-02 3.150000000000000e-02 -5.212048114020048e+18 1.999999999999999e-02 3.300000000000000e-02 -4.397239443549348e+18 1.999999999999999e-02 3.450000000000000e-02 -3.624157163379740e+18 1.999999999999999e-02 3.600000000000000e-02 -2.918259459448755e+18 1.999999999999999e-02 3.750000000000000e-02 -2.295925435268496e+18 1.999999999999999e-02 3.900000000000000e-02 -1.764939361756833e+18 1.999999999999999e-02 4.050000000000000e-02 -1.325734450307207e+18 1.999999999999999e-02 4.200000000000000e-02 -9.730858455167869e+17 1.999999999999999e-02 4.350000000000000e-02 -6.979495414984800e+17 1.999999999999999e-02 4.500000000000000e-02 -4.891965886763195e+17 1.999999999999999e-02 4.650000000000000e-02 -3.350702867636374e+17 1.999999999999999e-02 4.800000000000000e-02 -2.242780431358930e+17 1.999999999999999e-02 4.950000000000000e-02 -1.467033741597250e+17 1.999999999999999e-02 5.100000000000000e-02 -9.377762575037658e+16 1.999999999999999e-02 5.250000000000000e-02 -5.858233892205774e+16 1.999999999999999e-02 5.400000000000000e-02 -3.576386719644495e+16 1.999999999999999e-02 5.550000000000000e-02 -2.133702958372740e+16 1.999999999999999e-02 5.700000000000000e-02 -1.244045117412421e+16 1.999999999999999e-02 5.850000000000000e-02 -7.088454173795156e+15 1.999999999999999e-02 6.000000000000000e-02 -3.947119960518127e+15 1.999999999999999e-02 6.150000000000000e-02 -2.147940573194272e+15 1.999999999999999e-02 6.300000000000000e-02 -1.142290871201876e+15 1.999999999999999e-02 6.450000000000000e-02 -5.936665705674555e+14 1.999999999999999e-02 6.600000000000000e-02 -3.015215729057487e+14 1.999999999999999e-02 6.750000000000000e-02 -1.496587166660793e+14 1.999999999999999e-02 6.900000000000001e-02 -7.259233524039361e+13 1.999999999999999e-02 7.050000000000001e-02 -3.440972324580082e+13 1.999999999999999e-02 7.200000000000001e-02 -1.593928632705993e+13 1.999999999999999e-02 7.350000000000000e-02 -7.215199315060974e+12 1.999999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 2.199999999999999e-02 0.000000000000000e+00 4.936077265675517e+18 2.199999999999999e-02 1.500000000000000e-03 4.525649509850903e+18 2.199999999999999e-02 3.000000000000000e-03 3.939361000771156e+18 2.199999999999999e-02 4.500000000000001e-03 3.176852224954082e+18 2.199999999999999e-02 6.000000000000000e-03 2.246718520543902e+18 2.199999999999999e-02 7.500000000000000e-03 1.167617086952422e+18 2.199999999999999e-02 9.000000000000001e-03 -3.124299754964275e+16 2.199999999999999e-02 1.050000000000000e-02 -1.310469391763238e+18 2.199999999999999e-02 1.200000000000000e-02 -2.621896058229244e+18 2.199999999999999e-02 1.350000000000000e-02 -3.911100865840659e+18 2.199999999999999e-02 1.500000000000000e-02 -5.120937841081639e+18 2.199999999999999e-02 1.650000000000000e-02 -6.195810062572515e+18 2.199999999999999e-02 1.800000000000000e-02 -7.086244170723277e+18 2.199999999999999e-02 1.950000000000000e-02 -7.753216717657698e+18 2.199999999999999e-02 2.100000000000000e-02 -8.171657853029059e+18 2.199999999999999e-02 2.250000000000000e-02 -8.332634624435961e+18 2.199999999999999e-02 2.400000000000000e-02 -8.243887916024726e+18 2.199999999999999e-02 2.550000000000000e-02 -7.928634968024948e+18 2.199999999999999e-02 2.700000000000000e-02 -7.422808392852588e+18 2.199999999999999e-02 2.850000000000000e-02 -6.771131754972359e+18 2.199999999999999e-02 3.000000000000000e-02 -6.022586800528419e+18 2.199999999999999e-02 3.150000000000000e-02 -5.225881102431892e+18 2.199999999999999e-02 3.300000000000000e-02 -4.425472942429039e+18 2.199999999999999e-02 3.450000000000000e-02 -3.658570975025584e+18 2.199999999999999e-02 3.600000000000000e-02 -2.953334437892521e+18 2.199999999999999e-02 3.750000000000000e-02 -2.328297133360604e+18 2.199999999999999e-02 3.900000000000000e-02 -1.792863512099884e+18 2.199999999999999e-02 4.050000000000000e-02 -1.348604930264083e+18 2.199999999999999e-02 4.200000000000000e-02 -9.910299958427988e+17 2.199999999999999e-02 4.350000000000000e-02 -7.115111291163574e+17 2.199999999999999e-02 4.500000000000000e-02 -4.991049236389391e+17 2.199999999999999e-02 4.650000000000000e-02 -3.420858161097949e+17 2.199999999999999e-02 4.800000000000000e-02 -2.291002021936006e+17 2.199999999999999e-02 4.950000000000000e-02 -1.499250735523683e+17 2.199999999999999e-02 5.100000000000000e-02 -9.587166813760691e+16 2.199999999999999e-02 5.250000000000000e-02 -5.990738712200502e+16 2.199999999999999e-02 5.400000000000000e-02 -3.658051194405098e+16 2.199999999999999e-02 5.550000000000000e-02 -2.182741521238855e+16 2.199999999999999e-02 5.700000000000000e-02 -1.272742534692974e+16 2.199999999999999e-02 5.850000000000000e-02 -7.252136831055471e+15 2.199999999999999e-02 6.000000000000000e-02 -4.038118030971709e+15 2.199999999999999e-02 6.150000000000000e-02 -2.197247497145245e+15 2.199999999999999e-02 6.300000000000000e-02 -1.168326401261602e+15 2.199999999999999e-02 6.450000000000000e-02 -6.070602480914924e+14 2.199999999999999e-02 6.600000000000000e-02 -3.082319638197642e+14 2.199999999999999e-02 6.750000000000000e-02 -1.529312569275509e+14 2.199999999999999e-02 6.900000000000001e-02 -7.414472857450942e+13 2.199999999999999e-02 7.050000000000001e-02 -3.512533121020334e+13 2.199999999999999e-02 7.200000000000001e-02 -1.625941452316093e+13 2.199999999999999e-02 7.350000000000000e-02 -7.353918731442747e+12 2.199999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 2.399999999999999e-02 0.000000000000000e+00 1.322862412585921e+19 2.399999999999999e-02 1.500000000000000e-03 1.274824777256662e+19 2.399999999999999e-02 3.000000000000000e-03 1.197066216976827e+19 2.399999999999999e-02 4.500000000000001e-03 1.090315148748504e+19 2.399999999999999e-02 6.000000000000000e-03 9.566665193457232e+18 2.399999999999999e-02 7.500000000000000e-03 7.996098177053486e+18 2.399999999999999e-02 9.000000000000001e-03 6.239717446036777e+18 2.399999999999999e-02 1.050000000000000e-02 4.357589773798554e+18 2.399999999999999e-02 1.200000000000000e-02 2.418931385932629e+18 2.399999999999999e-02 1.350000000000000e-02 4.984123728822426e+17 2.399999999999999e-02 1.500000000000000e-02 -1.328404253887397e+18 2.399999999999999e-02 1.650000000000000e-02 -2.990148771299373e+18 2.399999999999999e-02 1.800000000000000e-02 -4.424775831115056e+18 2.399999999999999e-02 1.950000000000000e-02 -5.584175308497955e+18 2.399999999999999e-02 2.100000000000000e-02 -6.437697690069352e+18 2.399999999999999e-02 2.250000000000000e-02 -6.974126609950460e+18 2.399999999999999e-02 2.400000000000000e-02 -7.201818810934243e+18 2.399999999999999e-02 2.550000000000000e-02 -7.146979625760087e+18 2.399999999999999e-02 2.700000000000000e-02 -6.850304650441142e+18 2.399999999999999e-02 2.850000000000000e-02 -6.362445067038549e+18 2.399999999999999e-02 3.000000000000000e-02 -5.738901618191496e+18 2.399999999999999e-02 3.150000000000000e-02 -5.034994644633940e+18 2.399999999999999e-02 3.300000000000000e-02 -4.301492204744823e+18 2.399999999999999e-02 3.450000000000000e-02 -3.581325128864514e+18 2.399999999999999e-02 3.600000000000000e-02 -2.907613375856433e+18 2.399999999999999e-02 3.750000000000000e-02 -2.303015297774891e+18 2.399999999999999e-02 3.900000000000000e-02 -1.780229593630664e+18 2.399999999999999e-02 4.050000000000000e-02 -1.343356074301765e+18 2.399999999999999e-02 4.200000000000000e-02 -9.897670484900717e+17 2.399999999999999e-02 4.350000000000000e-02 -7.121517395087365e+17 2.399999999999999e-02 4.500000000000000e-02 -5.004556252077232e+17 2.399999999999999e-02 4.650000000000000e-02 -3.435232219244356e+17 2.399999999999999e-02 4.800000000000000e-02 -2.303450444957540e+17 2.399999999999999e-02 4.950000000000000e-02 -1.508902977076603e+17 2.399999999999999e-02 5.100000000000000e-02 -9.656615602621194e+16 2.399999999999999e-02 5.250000000000000e-02 -6.037907480347927e+16 2.399999999999999e-02 5.400000000000000e-02 -3.688574202765028e+16 2.399999999999999e-02 5.550000000000000e-02 -2.201660815582021e+16 2.399999999999999e-02 5.700000000000000e-02 -1.284009917570268e+16 2.399999999999999e-02 5.850000000000000e-02 -7.316711993004245e+15 2.399999999999999e-02 6.000000000000000e-02 -4.073747789975011e+15 2.399999999999999e-02 6.150000000000000e-02 -2.216161320710901e+15 2.399999999999999e-02 6.300000000000000e-02 -1.177968106759702e+15 2.399999999999999e-02 6.450000000000000e-02 -6.117637312146299e+14 2.399999999999999e-02 6.600000000000000e-02 -3.104144833923310e+14 2.399999999999999e-02 6.750000000000000e-02 -1.538844619100445e+14 2.399999999999999e-02 6.900000000000001e-02 -7.452884983702806e+13 2.399999999999999e-02 7.050000000000001e-02 -3.526210200684492e+13 2.399999999999999e-02 7.200000000000001e-02 -1.629735750666656e+13 2.399999999999999e-02 7.350000000000000e-02 -7.357237502186653e+12 2.399999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 2.600000000000000e-02 0.000000000000000e+00 2.914185367742149e+19 2.600000000000000e-02 1.500000000000000e-03 2.853797993710991e+19 2.600000000000000e-02 3.000000000000000e-03 2.740704744638398e+19 2.600000000000000e-02 4.500000000000001e-03 2.577115132120740e+19 2.600000000000000e-02 6.000000000000000e-03 2.367491221993142e+19 2.600000000000000e-02 7.500000000000000e-03 2.118412315014058e+19 2.600000000000000e-02 9.000000000000001e-03 1.838310299418065e+19 2.600000000000000e-02 1.050000000000000e-02 1.537080408521229e+19 2.600000000000000e-02 1.200000000000000e-02 1.225580045391685e+19 2.600000000000000e-02 1.350000000000000e-02 9.150384573554403e+18 2.600000000000000e-02 1.500000000000000e-02 6.164117351587521e+18 2.600000000000000e-02 1.650000000000000e-02 3.397291446323273e+18 2.600000000000000e-02 1.800000000000000e-02 9.348556066708439e+17 2.600000000000000e-02 1.950000000000000e-02 -1.158621146539443e+18 2.600000000000000e-02 2.100000000000000e-02 -2.842414966552463e+18 2.600000000000000e-02 2.250000000000000e-02 -4.101148074805210e+18 2.600000000000000e-02 2.400000000000000e-02 -4.944144427740492e+18 2.600000000000000e-02 2.550000000000000e-02 -5.402719541626146e+18 2.600000000000000e-02 2.700000000000000e-02 -5.525745879650299e+18 2.600000000000000e-02 2.850000000000000e-02 -5.374050740735119e+18 2.600000000000000e-02 3.000000000000000e-02 -5.014332151337368e+18 2.600000000000000e-02 3.150000000000000e-02 -4.513297284645268e+18 2.600000000000000e-02 3.300000000000000e-02 -3.932638011641701e+18 2.600000000000000e-02 3.450000000000000e-02 -3.325282180819810e+18 2.600000000000000e-02 3.600000000000000e-02 -2.733135718536771e+18 2.600000000000000e-02 3.750000000000000e-02 -2.186303982577651e+18 2.600000000000000e-02 3.900000000000000e-02 -1.703590645170675e+18 2.600000000000000e-02 4.050000000000000e-02 -1.293945640809708e+18 2.600000000000000e-02 4.200000000000000e-02 -9.584806748814764e+17 2.600000000000000e-02 4.350000000000000e-02 -6.926857792578848e+17 2.600000000000000e-02 4.500000000000000e-02 -4.885460553526324e+17 2.600000000000000e-02 4.650000000000000e-02 -3.363511031203453e+17 2.600000000000000e-02 4.800000000000000e-02 -2.260881684637284e+17 2.600000000000000e-02 4.950000000000000e-02 -1.483961486041607e+17 2.600000000000000e-02 5.100000000000000e-02 -9.512084021468998e+16 2.600000000000000e-02 5.250000000000000e-02 -5.954898183433837e+16 2.600000000000000e-02 5.400000000000000e-02 -3.641219482606545e+16 2.600000000000000e-02 5.550000000000000e-02 -2.174772213383878e+16 2.600000000000000e-02 5.700000000000000e-02 -1.268787663635168e+16 2.600000000000000e-02 5.850000000000000e-02 -7.230697569140112e+15 2.600000000000000e-02 6.000000000000000e-02 -4.025220590007996e+15 2.600000000000000e-02 6.150000000000000e-02 -2.188839972952642e+15 2.600000000000000e-02 6.300000000000000e-02 -1.162636764882977e+15 2.600000000000000e-02 6.450000000000000e-02 -6.032044479823064e+14 2.600000000000000e-02 6.600000000000000e-02 -3.056703440162092e+14 2.600000000000000e-02 6.750000000000000e-02 -1.512795541930365e+14 2.600000000000000e-02 6.900000000000001e-02 -7.311486710479989e+13 2.600000000000000e-02 7.050000000000001e-02 -3.450471529512657e+13 2.600000000000000e-02 7.200000000000001e-02 -1.589764560151040e+13 2.600000000000000e-02 7.350000000000000e-02 -7.149650121722973e+12 2.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 2.800000000000000e-02 0.000000000000000e+00 5.534705202268496e+19 2.800000000000000e-02 1.500000000000000e-03 5.454694169460486e+19 2.800000000000000e-02 3.000000000000000e-03 5.284327114738221e+19 2.800000000000000e-02 4.500000000000001e-03 5.028262046390616e+19 2.800000000000000e-02 6.000000000000000e-03 4.694856694941878e+19 2.800000000000000e-02 7.500000000000000e-03 4.295761133154121e+19 2.800000000000000e-02 9.000000000000001e-03 3.845309555876263e+19 2.800000000000000e-02 1.050000000000000e-02 3.359748305719909e+19 2.800000000000000e-02 1.200000000000000e-02 2.856347124255147e+19 2.800000000000000e-02 1.350000000000000e-02 2.352448791076519e+19 2.800000000000000e-02 1.500000000000000e-02 1.864518688147911e+19 2.800000000000000e-02 1.650000000000000e-02 1.407259602377684e+19 2.800000000000000e-02 1.800000000000000e-02 9.928568188940057e+18 2.800000000000000e-02 1.950000000000000e-02 6.304125977496619e+18 2.800000000000000e-02 2.100000000000000e-02 3.256162523948290e+18 2.800000000000000e-02 2.250000000000000e-02 8.067619391286436e+17 2.800000000000000e-02 2.400000000000000e-02 -1.054849859092831e+18 2.800000000000000e-02 2.550000000000000e-02 -2.367988929818815e+18 2.800000000000000e-02 2.700000000000000e-02 -3.194352843216528e+18 2.800000000000000e-02 2.850000000000000e-02 -3.610729649142036e+18 2.800000000000000e-02 3.000000000000000e-02 -3.701384181533150e+18 2.800000000000000e-02 3.150000000000000e-02 -3.550908944209832e+18 2.800000000000000e-02 3.300000000000000e-02 -3.238197362469479e+18 2.800000000000000e-02 3.450000000000000e-02 -2.831986097093342e+18 2.800000000000000e-02 3.600000000000000e-02 -2.388161855300778e+18 2.800000000000000e-02 3.750000000000000e-02 -1.948782387482348e+18 2.800000000000000e-02 3.900000000000000e-02 -1.542560785437272e+18 2.800000000000000e-02 4.050000000000000e-02 -1.186432668762420e+18 2.800000000000000e-02 4.200000000000000e-02 -8.877759483633559e+17 2.800000000000000e-02 4.350000000000000e-02 -6.468749446751380e+17 2.800000000000000e-02 4.500000000000000e-02 -4.592954295132971e+17 2.800000000000000e-02 4.650000000000000e-02 -3.179400697305524e+17 2.800000000000000e-02 4.800000000000000e-02 -2.146610547965454e+17 2.800000000000000e-02 4.950000000000000e-02 -1.414000550930842e+17 2.800000000000000e-02 5.100000000000000e-02 -9.089433935677376e+16 2.800000000000000e-02 5.250000000000000e-02 -5.702868298006871e+16 2.800000000000000e-02 5.400000000000000e-02 -3.492832746873703e+16 2.800000000000000e-02 5.550000000000000e-02 -2.088491014726528e+16 2.800000000000000e-02 5.700000000000000e-02 -1.219231807760366e+16 2.800000000000000e-02 5.850000000000000e-02 -6.949520562406188e+15 2.800000000000000e-02 6.000000000000000e-02 -3.867610351966498e+15 2.800000000000000e-02 6.150000000000000e-02 -2.101565500702896e+15 2.800000000000000e-02 6.300000000000000e-02 -1.114902238468741e+15 2.800000000000000e-02 6.450000000000000e-02 -5.774213821708770e+14 2.800000000000000e-02 6.600000000000000e-02 -2.919210023264782e+14 2.800000000000000e-02 6.750000000000000e-02 -1.440427822943261e+14 2.800000000000000e-02 6.900000000000001e-02 -6.935664800530206e+13 2.800000000000000e-02 7.050000000000001e-02 -3.257964118886531e+13 2.800000000000000e-02 7.200000000000001e-02 -1.492535400576321e+13 2.800000000000000e-02 7.350000000000000e-02 -6.665598163865572e+12 2.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 3.000000000000000e-02 0.000000000000000e+00 9.193893977537623e+19 3.000000000000000e-02 1.500000000000000e-03 9.086943440554013e+19 3.000000000000000e-02 3.000000000000000e-03 8.837193599308005e+19 3.000000000000000e-02 4.500000000000001e-03 8.452727597276753e+19 3.000000000000000e-02 6.000000000000000e-03 7.947341358811813e+19 3.000000000000000e-02 7.500000000000000e-03 7.339754310321480e+19 3.000000000000000e-02 9.000000000000001e-03 6.652520001645658e+19 3.000000000000000e-02 1.050000000000000e-02 5.910719264215435e+19 3.000000000000000e-02 1.200000000000000e-02 5.140531111149910e+19 3.000000000000000e-02 1.350000000000000e-02 4.367781913689892e+19 3.000000000000000e-02 1.500000000000000e-02 3.616572128001666e+19 3.000000000000000e-02 1.650000000000000e-02 2.908072548081019e+19 3.000000000000000e-02 1.800000000000000e-02 2.259568976166265e+19 3.000000000000000e-02 1.950000000000000e-02 1.683815416661504e+19 3.000000000000000e-02 2.100000000000000e-02 1.188731741186186e+19 3.000000000000000e-02 2.250000000000000e-02 7.774533143775795e+18 3.000000000000000e-02 2.400000000000000e-02 4.487094800879145e+18 3.000000000000000e-02 2.550000000000000e-02 1.974783365064548e+18 3.000000000000000e-02 2.700000000000000e-02 1.584075936105093e+17 3.000000000000000e-02 2.850000000000000e-02 -1.060591239195777e+18 3.000000000000000e-02 3.000000000000000e-02 -1.790442322253634e+18 3.000000000000000e-02 3.150000000000000e-02 -2.140151422875073e+18 3.000000000000000e-02 3.300000000000000e-02 -2.212121425768509e+18 3.000000000000000e-02 3.450000000000000e-02 -2.096740154170911e+18 3.000000000000000e-02 3.600000000000000e-02 -1.869100618986776e+18 3.000000000000000e-02 3.750000000000000e-02 -1.587748906824069e+18 3.000000000000000e-02 3.900000000000000e-02 -1.295141939281723e+18 3.000000000000000e-02 4.050000000000000e-02 -1.019365395236765e+18 3.000000000000000e-02 4.200000000000000e-02 -7.766172546537050e+17 3.000000000000000e-02 4.350000000000000e-02 -5.739943380066423e+17 3.000000000000000e-02 4.500000000000000e-02 -4.122061001964026e+17 3.000000000000000e-02 4.650000000000000e-02 -2.879551925477066e+17 3.000000000000000e-02 4.800000000000000e-02 -1.958427924082032e+17 3.000000000000000e-02 4.950000000000000e-02 -1.297592635061398e+17 3.000000000000000e-02 5.100000000000000e-02 -8.379629750694573e+16 3.000000000000000e-02 5.250000000000000e-02 -5.276217146836358e+16 3.000000000000000e-02 5.400000000000000e-02 -3.240014834595936e+16 3.000000000000000e-02 5.550000000000000e-02 -1.940797457899783e+16 3.000000000000000e-02 5.700000000000000e-02 -1.134167476171395e+16 3.000000000000000e-02 5.850000000000000e-02 -6.466490987238028e+15 3.000000000000000e-02 6.000000000000000e-02 -3.597188040060895e+15 3.000000000000000e-02 6.150000000000000e-02 -1.952303140326215e+15 3.000000000000000e-02 6.300000000000000e-02 -1.033677600381894e+15 3.000000000000000e-02 6.450000000000000e-02 -5.338460816849367e+14 3.000000000000000e-02 6.600000000000000e-02 -2.688753543920622e+14 3.000000000000000e-02 6.750000000000000e-02 -1.320281525738987e+14 3.000000000000000e-02 6.900000000000001e-02 -6.318247239724448e+13 3.000000000000000e-02 7.050000000000001e-02 -2.945235895254495e+13 3.000000000000000e-02 7.200000000000001e-02 -1.336419786187471e+13 3.000000000000000e-02 7.350000000000000e-02 -5.897549606023740e+12 3.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 3.200000000000000e-02 0.000000000000000e+00 1.342599655230234e+20 3.200000000000000e-02 1.500000000000000e-03 1.328817423555858e+20 3.200000000000000e-02 3.000000000000000e-03 1.294697861801759e+20 3.200000000000000e-02 4.500000000000001e-03 1.241445804867175e+20 3.200000000000000e-02 6.000000000000000e-03 1.171069713414357e+20 3.200000000000000e-02 7.500000000000000e-03 1.086258452923842e+20 3.200000000000000e-02 9.000000000000001e-03 9.902166195924669e+19 3.200000000000000e-02 1.050000000000000e-02 8.864719681133681e+19 3.200000000000000e-02 1.200000000000000e-02 7.786700583440361e+19 3.200000000000000e-02 1.350000000000000e-02 6.703714316853097e+19 3.200000000000000e-02 1.500000000000000e-02 5.648656058304769e+19 3.200000000000000e-02 1.650000000000000e-02 4.650141510171733e+19 3.200000000000000e-02 1.800000000000000e-02 3.731323053980244e+19 3.200000000000000e-02 1.950000000000000e-02 2.909152154529509e+19 3.200000000000000e-02 2.100000000000000e-02 2.194111634061327e+19 3.200000000000000e-02 2.250000000000000e-02 1.590403077171095e+19 3.200000000000000e-02 2.400000000000000e-02 1.096538034106400e+19 3.200000000000000e-02 2.550000000000000e-02 7.062502038169485e+18 3.200000000000000e-02 2.700000000000000e-02 4.096228305862271e+18 3.200000000000000e-02 2.850000000000000e-02 1.943140167647319e+18 3.200000000000000e-02 3.000000000000000e-02 4.676412941466501e+17 3.200000000000000e-02 3.150000000000000e-02 -4.671629714480763e+17 3.200000000000000e-02 3.300000000000000e-02 -9.905506030424361e+17 3.200000000000000e-02 3.450000000000000e-02 -1.217688699866603e+18 3.200000000000000e-02 3.600000000000000e-02 -1.245688473361006e+18 3.200000000000000e-02 3.750000000000000e-02 -1.152041382721101e+18 3.200000000000000e-02 3.900000000000000e-02 -9.950423853116484e+17 3.200000000000000e-02 4.050000000000000e-02 -8.156724541153292e+17 3.200000000000000e-02 4.200000000000000e-02 -6.403739572144261e+17 3.200000000000000e-02 4.350000000000000e-02 -4.841957228605541e+17 3.200000000000000e-02 4.500000000000000e-02 -3.538850744187377e+17 3.200000000000000e-02 4.650000000000000e-02 -2.506330397996606e+17 3.200000000000000e-02 4.800000000000000e-02 -1.723097011756985e+17 3.200000000000000e-02 4.950000000000000e-02 -1.151392757159180e+17 3.200000000000000e-02 5.100000000000000e-02 -7.484766859874830e+16 3.200000000000000e-02 5.250000000000000e-02 -4.736589239419738e+16 3.200000000000000e-02 5.400000000000000e-02 -2.919425268608602e+16 3.200000000000000e-02 5.550000000000000e-02 -1.753163156528609e+16 3.200000000000000e-02 5.700000000000000e-02 -1.025980193144227e+16 3.200000000000000e-02 5.850000000000000e-02 -5.851969168421649e+15 3.200000000000000e-02 6.000000000000000e-02 -3.253317970495488e+15 3.200000000000000e-02 6.150000000000000e-02 -1.762742046364302e+15 3.200000000000000e-02 6.300000000000000e-02 -9.307323214366695e+14 3.200000000000000e-02 6.450000000000000e-02 -4.787686885896277e+14 3.200000000000000e-02 6.600000000000000e-02 -2.398445048027427e+14 3.200000000000000e-02 6.750000000000000e-02 -1.169524591872855e+14 3.200000000000000e-02 6.900000000000001e-02 -5.546918723444175e+13 3.200000000000000e-02 7.050000000000001e-02 -2.556405228323774e+13 3.200000000000000e-02 7.200000000000001e-02 -1.143287099991862e+13 3.200000000000000e-02 7.350000000000000e-02 -4.952313197235734e+12 3.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 3.400000000000000e-02 0.000000000000000e+00 1.726993792496927e+20 3.400000000000000e-02 1.500000000000000e-03 1.710409546330492e+20 3.400000000000000e-02 3.000000000000000e-03 1.667986710346478e+20 3.400000000000000e-02 4.500000000000001e-03 1.601290298604086e+20 3.400000000000000e-02 6.000000000000000e-03 1.512899954498958e+20 3.400000000000000e-02 7.500000000000000e-03 1.406246490511158e+20 3.400000000000000e-02 9.000000000000001e-03 1.285396583767275e+20 3.400000000000000e-02 1.050000000000000e-02 1.154803990150382e+20 3.400000000000000e-02 1.200000000000000e-02 1.019047478485169e+20 3.400000000000000e-02 1.350000000000000e-02 8.825755714961849e+19 3.400000000000000e-02 1.500000000000000e-02 7.494763432186913e+19 3.400000000000000e-02 1.650000000000000e-02 6.232873191058366e+19 3.400000000000000e-02 1.800000000000000e-02 5.068563588035280e+19 3.400000000000000e-02 1.950000000000000e-02 4.022596729795009e+19 3.400000000000000e-02 2.100000000000000e-02 3.107782132754312e+19 3.400000000000000e-02 2.250000000000000e-02 2.329289396233297e+19 3.400000000000000e-02 2.400000000000000e-02 1.685432655009150e+19 3.400000000000000e-02 2.550000000000000e-02 1.168816513045004e+19 3.400000000000000e-02 2.700000000000000e-02 7.677116089246908e+18 3.400000000000000e-02 2.850000000000000e-02 4.675202822535769e+18 3.400000000000000e-02 3.000000000000000e-02 2.521996543347087e+18 3.400000000000000e-02 3.150000000000000e-02 1.055296062086532e+18 3.400000000000000e-02 3.300000000000000e-02 1.214354675712276e+17 3.400000000000000e-02 3.450000000000000e-02 -4.172404537381524e+17 3.400000000000000e-02 3.600000000000000e-02 -6.778278849010463e+17 3.400000000000000e-02 3.750000000000000e-02 -7.550172450636564e+17 3.400000000000000e-02 3.900000000000000e-02 -7.214848272470981e+17 3.400000000000000e-02 4.050000000000000e-02 -6.299241280510703e+17 3.400000000000000e-02 4.200000000000000e-02 -5.160853627373839e+17 3.400000000000000e-02 4.350000000000000e-02 -4.022451593906061e+17 3.400000000000000e-02 4.500000000000000e-02 -3.006411883982574e+17 3.400000000000000e-02 4.650000000000000e-02 -2.165477728749881e+17 3.400000000000000e-02 4.800000000000000e-02 -1.508103898797980e+17 3.400000000000000e-02 4.950000000000000e-02 -1.017786949844395e+17 3.400000000000000e-02 5.100000000000000e-02 -6.666769297302213e+16 3.400000000000000e-02 5.250000000000000e-02 -4.243200751934748e+16 3.400000000000000e-02 5.400000000000000e-02 -2.626253037580935e+16 3.400000000000000e-02 5.550000000000000e-02 -1.581553192142088e+16 3.400000000000000e-02 5.700000000000000e-02 -9.270246799458944e+15 3.400000000000000e-02 5.850000000000000e-02 -5.289873114334828e+15 3.400000000000000e-02 6.000000000000000e-02 -2.938794708319736e+15 3.400000000000000e-02 6.150000000000000e-02 -1.589374092591848e+15 3.400000000000000e-02 6.300000000000000e-02 -8.365944852369805e+14 3.400000000000000e-02 6.450000000000000e-02 -4.284131037158241e+14 3.400000000000000e-02 6.600000000000000e-02 -2.133087958797110e+14 3.400000000000000e-02 6.750000000000000e-02 -1.031763247637737e+14 3.400000000000000e-02 6.900000000000001e-02 -4.842300913542044e+13 3.400000000000000e-02 7.050000000000001e-02 -2.201324801978717e+13 3.400000000000000e-02 7.200000000000001e-02 -9.669820322929199e+12 3.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 3.600000000000000e-02 0.000000000000000e+00 1.958381060798761e+20 3.600000000000000e-02 1.500000000000000e-03 1.940112140205665e+20 3.600000000000000e-02 3.000000000000000e-03 1.892693693052508e+20 3.600000000000000e-02 4.500000000000001e-03 1.817907571102690e+20 3.600000000000000e-02 6.000000000000000e-03 1.718677236249814e+20 3.600000000000000e-02 7.500000000000000e-03 1.598880069383853e+20 3.600000000000000e-02 9.000000000000001e-03 1.463101582750769e+20 3.600000000000000e-02 1.050000000000000e-02 1.316352794172394e+20 3.600000000000000e-02 1.200000000000000e-02 1.163774026624757e+20 3.600000000000000e-02 1.350000000000000e-02 1.010348095414202e+20 3.600000000000000e-02 1.500000000000000e-02 8.606435167516353e+19 3.600000000000000e-02 1.650000000000000e-02 7.186044579939289e+19 3.600000000000000e-02 1.800000000000000e-02 5.873991634599145e+19 3.600000000000000e-02 1.950000000000000e-02 4.693330436711146e+19 3.600000000000000e-02 2.100000000000000e-02 3.658269879996856e+19 3.600000000000000e-02 2.250000000000000e-02 2.774561851118980e+19 3.600000000000000e-02 2.400000000000000e-02 2.040402051318057e+19 3.600000000000000e-02 2.550000000000000e-02 1.447716589005718e+19 3.600000000000000e-02 2.700000000000000e-02 9.836868002863948e+18 3.600000000000000e-02 2.850000000000000e-02 6.323594032003104e+18 3.600000000000000e-02 3.000000000000000e-02 3.761991759497414e+18 3.600000000000000e-02 3.150000000000000e-02 1.974651014089972e+18 3.600000000000000e-02 3.300000000000000e-02 7.932476399756319e+17 3.600000000000000e-02 3.450000000000000e-02 6.660802833781453e+16 3.600000000000000e-02 3.600000000000000e-02 -3.343803027763712e+17 3.600000000000000e-02 3.750000000000000e-02 -5.147519904273275e+17 3.600000000000000e-02 3.900000000000000e-02 -5.558361671690104e+17 3.600000000000000e-02 4.050000000000000e-02 -5.173766841968634e+17 3.600000000000000e-02 4.200000000000000e-02 -4.407296929506065e+17 3.600000000000000e-02 4.350000000000000e-02 -3.525277404729331e+17 3.600000000000000e-02 4.500000000000000e-02 -2.683196726049307e+17 3.600000000000000e-02 4.650000000000000e-02 -1.958443310129411e+17 3.600000000000000e-02 4.800000000000000e-02 -1.377445315723872e+17 3.600000000000000e-02 4.950000000000000e-02 -9.365497016089387e+16 3.600000000000000e-02 5.100000000000000e-02 -6.169177954381297e+16 3.600000000000000e-02 5.250000000000000e-02 -3.942958933873210e+16 3.600000000000000e-02 5.400000000000000e-02 -2.447796153772654e+16 3.600000000000000e-02 5.550000000000000e-02 -1.477070247514070e+16 3.600000000000000e-02 5.700000000000000e-02 -8.667690816199799e+15 3.600000000000000e-02 5.850000000000000e-02 -4.947591707883358e+15 3.600000000000000e-02 6.000000000000000e-02 -2.747280314497795e+15 3.600000000000000e-02 6.150000000000000e-02 -1.483825024335633e+15 3.600000000000000e-02 6.300000000000000e-02 -7.792952025245112e+14 3.600000000000000e-02 6.450000000000000e-02 -3.977725436196495e+14 3.600000000000000e-02 6.600000000000000e-02 -1.971685000039686e+14 3.600000000000000e-02 6.750000000000000e-02 -9.480081613249694e+13 3.600000000000000e-02 6.900000000000001e-02 -4.414131261309258e+13 3.600000000000000e-02 7.050000000000001e-02 -1.985675821926582e+13 3.600000000000000e-02 7.200000000000001e-02 -8.599709825651975e+12 3.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 3.800000000000001e-02 0.000000000000000e+00 1.989406937781634e+20 3.800000000000001e-02 1.500000000000000e-03 1.970917857808042e+20 3.800000000000001e-02 3.000000000000000e-03 1.922836910618345e+20 3.800000000000001e-02 4.500000000000001e-03 1.846975099265777e+20 3.800000000000001e-02 6.000000000000000e-03 1.746301967715543e+20 3.800000000000001e-02 7.500000000000000e-03 1.624754635822152e+20 3.800000000000001e-02 9.000000000000001e-03 1.486987906852194e+20 3.800000000000001e-02 1.050000000000000e-02 1.338087098828732e+20 3.800000000000001e-02 1.200000000000000e-02 1.183267277554722e+20 3.800000000000001e-02 1.350000000000000e-02 1.027582241091623e+20 3.800000000000001e-02 1.500000000000000e-02 8.756642085205788e+19 3.800000000000001e-02 1.650000000000000e-02 7.315111540715389e+19 3.800000000000001e-02 1.800000000000000e-02 5.983336285873269e+19 3.800000000000001e-02 1.950000000000000e-02 4.784672526583570e+19 3.800000000000001e-02 2.100000000000000e-02 3.733513413382744e+19 3.800000000000001e-02 2.250000000000000e-02 2.835687732460212e+19 3.800000000000001e-02 2.400000000000000e-02 2.089376450993717e+19 3.800000000000001e-02 2.550000000000000e-02 1.486418032805773e+19 3.800000000000001e-02 2.700000000000000e-02 1.013852898059059e+19 3.800000000000001e-02 2.850000000000000e-02 6.555523978012075e+18 3.800000000000001e-02 3.000000000000000e-02 3.937882179223959e+18 3.800000000000001e-02 3.150000000000000e-02 2.106223688464356e+18 3.800000000000001e-02 3.300000000000000e-02 8.903221470018335e+17 3.800000000000001e-02 3.450000000000000e-02 1.372438562158822e+17 3.800000000000001e-02 3.600000000000000e-02 -2.836957068719258e+17 3.800000000000001e-02 3.750000000000000e-02 -4.788932051836803e+17 3.800000000000001e-02 3.900000000000000e-02 -5.308264287727078e+17 3.800000000000001e-02 4.050000000000000e-02 -5.001844821564257e+17 3.800000000000001e-02 4.200000000000000e-02 -4.290839021477375e+17 3.800000000000001e-02 4.350000000000000e-02 -3.447559341679633e+17 3.800000000000001e-02 4.500000000000000e-02 -2.632112403676613e+17 3.800000000000001e-02 4.650000000000000e-02 -1.925378743896941e+17 3.800000000000001e-02 4.800000000000000e-02 -1.356376171419825e+17 3.800000000000001e-02 4.950000000000000e-02 -9.233353934535653e+16 3.800000000000001e-02 5.100000000000000e-02 -6.087619729339601e+16 3.800000000000001e-02 5.250000000000000e-02 -3.893432253449602e+16 3.800000000000001e-02 5.400000000000000e-02 -2.418209694642442e+16 3.800000000000001e-02 5.550000000000000e-02 -1.459685166335240e+16 3.800000000000001e-02 5.700000000000000e-02 -8.567217047731223e+15 3.800000000000001e-02 5.850000000000000e-02 -4.890483482926576e+15 3.800000000000001e-02 6.000000000000000e-02 -2.715356971359299e+15 3.800000000000001e-02 6.150000000000000e-02 -1.466274437402055e+15 3.800000000000001e-02 6.300000000000000e-02 -7.698050273238475e+14 3.800000000000001e-02 6.450000000000000e-02 -3.927248012572633e+14 3.800000000000001e-02 6.600000000000000e-02 -1.945272107836782e+14 3.800000000000001e-02 6.750000000000000e-02 -9.344094061727472e+13 3.800000000000001e-02 6.900000000000001e-02 -4.345230052034402e+13 3.800000000000001e-02 7.050000000000001e-02 -1.951313016278779e+13 3.800000000000001e-02 7.200000000000001e-02 -8.430984113637178e+12 3.800000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 4.000000000000001e-02 0.000000000000000e+00 1.989421145628713e+20 4.000000000000001e-02 1.500000000000000e-03 1.970937228155259e+20 4.000000000000001e-02 3.000000000000000e-03 1.922862719874640e+20 4.000000000000001e-02 4.500000000000001e-03 1.847008707254924e+20 4.000000000000001e-02 6.000000000000000e-03 1.746344737643572e+20 4.000000000000001e-02 7.500000000000000e-03 1.624807829921964e+20 4.000000000000001e-02 9.000000000000001e-03 1.487052564121875e+20 4.000000000000001e-02 1.050000000000000e-02 1.338163905724376e+20 4.000000000000001e-02 1.200000000000000e-02 1.183356446168754e+20 4.000000000000001e-02 1.350000000000000e-02 1.027683411330084e+20 4.000000000000001e-02 1.500000000000000e-02 8.757763903412412e+19 4.000000000000001e-02 1.650000000000000e-02 7.316327225966690e+19 4.000000000000001e-02 1.800000000000000e-02 5.984623790400483e+19 4.000000000000001e-02 1.950000000000000e-02 4.786005143539942e+19 4.000000000000001e-02 2.100000000000000e-02 3.734861416381628e+19 4.000000000000001e-02 2.250000000000000e-02 2.837020349416584e+19 4.000000000000001e-02 2.400000000000000e-02 2.090663955520931e+19 4.000000000000001e-02 2.550000000000000e-02 1.487633718057074e+19 4.000000000000001e-02 2.700000000000000e-02 1.014974716265683e+19 4.000000000000001e-02 2.850000000000000e-02 6.565641001858186e+18 4.000000000000001e-02 3.000000000000000e-02 3.946799040627195e+18 4.000000000000001e-02 3.150000000000000e-02 2.113904378028855e+18 4.000000000000001e-02 3.300000000000000e-02 8.967878739698780e+17 4.000000000000001e-02 3.450000000000000e-02 1.425632661969971e+17 4.000000000000001e-02 3.600000000000000e-02 -2.794187140690207e+17 4.000000000000001e-02 3.750000000000000e-02 -4.755324062690330e+17 4.000000000000001e-02 3.900000000000000e-02 -5.282455031432886e+17 4.000000000000001e-02 4.050000000000000e-02 -4.982474474347308e+17 4.000000000000001e-02 4.200000000000000e-02 -4.276631174398431e+17 4.000000000000001e-02 4.350000000000000e-02 -3.437374645083992e+17 4.000000000000001e-02 4.500000000000000e-02 -2.624977356142840e+17 4.000000000000001e-02 4.650000000000000e-02 -1.920493631067496e+17 4.000000000000001e-02 4.800000000000000e-02 -1.353107424625703e+17 4.000000000000001e-02 4.950000000000000e-02 -9.211978403397130e+16 4.000000000000001e-02 5.100000000000000e-02 -6.073958760437985e+16 4.000000000000001e-02 5.250000000000000e-02 -3.884899778071269e+16 4.000000000000001e-02 5.400000000000000e-02 -2.413001376099571e+16 4.000000000000001e-02 5.550000000000000e-02 -1.456578111017354e+16 4.000000000000001e-02 5.700000000000000e-02 -8.549102421134604e+15 4.000000000000001e-02 5.850000000000000e-02 -4.880162079815408e+15 4.000000000000001e-02 6.000000000000000e-02 -2.709609496936379e+15 4.000000000000001e-02 6.150000000000000e-02 -1.463146598998204e+15 4.000000000000001e-02 6.300000000000000e-02 -7.681414594638420e+14 4.000000000000001e-02 6.450000000000000e-02 -3.918601008011537e+14 4.000000000000001e-02 6.600000000000000e-02 -1.940879526539601e+14 4.000000000000001e-02 6.750000000000000e-02 -9.322286712357545e+13 4.000000000000001e-02 6.900000000000001e-02 -4.334649339681272e+13 4.000000000000001e-02 7.050000000000001e-02 -1.946295880118375e+13 4.000000000000001e-02 7.200000000000001e-02 -8.407733960353174e+12 4.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 4.200000000000001e-02 0.000000000000000e+00 1.989431807171152e+20 4.200000000000001e-02 1.500000000000000e-03 1.970951763628351e+20 4.200000000000001e-02 3.000000000000000e-03 1.922882087093316e+20 4.200000000000001e-02 4.500000000000001e-03 1.847033926628456e+20 4.200000000000001e-02 6.000000000000000e-03 1.746376832119270e+20 4.200000000000001e-02 7.500000000000000e-03 1.624847746677084e+20 4.200000000000001e-02 9.000000000000001e-03 1.487101082818680e+20 4.200000000000001e-02 1.050000000000000e-02 1.338221541478265e+20 4.200000000000001e-02 1.200000000000000e-02 1.183423358133491e+20 4.200000000000001e-02 1.350000000000000e-02 1.027759329291821e+20 4.200000000000001e-02 1.500000000000000e-02 8.758605713741046e+19 4.200000000000001e-02 1.650000000000000e-02 7.317239473953815e+19 4.200000000000001e-02 1.800000000000000e-02 5.985589931440779e+19 4.200000000000001e-02 1.950000000000000e-02 4.787005136864495e+19 4.200000000000001e-02 2.100000000000000e-02 3.735872955364316e+19 4.200000000000001e-02 2.250000000000000e-02 2.838020342741137e+19 4.200000000000001e-02 2.400000000000000e-02 2.091630096561227e+19 4.200000000000001e-02 2.550000000000000e-02 1.488545966044199e+19 4.200000000000001e-02 2.700000000000000e-02 1.015816526594317e+19 4.200000000000001e-02 2.850000000000000e-02 6.573232798031930e+18 4.200000000000001e-02 3.000000000000000e-02 3.953490237100842e+18 4.200000000000001e-02 3.150000000000000e-02 2.119667953417670e+18 4.200000000000001e-02 3.300000000000000e-02 9.016397436504412e+17 4.200000000000001e-02 3.450000000000000e-02 1.465549417090340e+17 4.200000000000001e-02 3.600000000000000e-02 -2.762092664992481e+17 4.200000000000001e-02 3.750000000000000e-02 -4.730104689158108e+17 4.200000000000001e-02 3.900000000000000e-02 -5.263087812756536e+17 4.200000000000001e-02 4.050000000000000e-02 -4.967939001255357e+17 4.200000000000001e-02 4.200000000000000e-02 -4.265969631959489e+17 4.200000000000001e-02 4.350000000000000e-02 -3.429732067402881e+17 4.200000000000001e-02 4.500000000000000e-02 -2.619623229535023e+17 4.200000000000001e-02 4.650000000000000e-02 -1.916827851343041e+17 4.200000000000001e-02 4.800000000000000e-02 -1.350654563015210e+17 4.200000000000001e-02 4.950000000000000e-02 -9.195938243961150e+16 4.200000000000001e-02 5.100000000000000e-02 -6.063707594382187e+16 4.200000000000001e-02 5.250000000000000e-02 -3.878497024167045e+16 4.200000000000001e-02 5.400000000000000e-02 -2.409093063399426e+16 4.200000000000001e-02 5.550000000000000e-02 -1.454246582394635e+16 4.200000000000001e-02 5.700000000000000e-02 -8.535509238497410e+15 4.200000000000001e-02 5.850000000000000e-02 -4.872416917815304e+15 4.200000000000001e-02 6.000000000000000e-02 -2.705296602650833e+15 4.200000000000001e-02 6.150000000000000e-02 -1.460799474785822e+15 4.200000000000001e-02 6.300000000000000e-02 -7.668931211870464e+14 4.200000000000001e-02 6.450000000000000e-02 -3.912112311618227e+14 4.200000000000001e-02 6.600000000000000e-02 -1.937583341575321e+14 4.200000000000001e-02 6.750000000000000e-02 -9.305922517311216e+13 4.200000000000001e-02 6.900000000000001e-02 -4.326709592500695e+13 4.200000000000001e-02 7.050000000000001e-02 -1.942531030328053e+13 4.200000000000001e-02 7.200000000000001e-02 -8.390287087890936e+12 4.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 4.400000000000001e-02 0.000000000000000e+00 1.989439730706913e+20 4.400000000000001e-02 1.500000000000000e-03 1.970962566224833e+20 4.400000000000001e-02 3.000000000000000e-03 1.922896480587564e+20 4.400000000000001e-02 4.500000000000001e-03 1.847052669376908e+20 4.400000000000001e-02 6.000000000000000e-03 1.746400684364606e+20 4.400000000000001e-02 7.500000000000000e-03 1.624877412350552e+20 4.400000000000001e-02 9.000000000000001e-03 1.487137141356309e+20 4.400000000000001e-02 1.050000000000000e-02 1.338264375707894e+20 4.400000000000001e-02 1.200000000000000e-02 1.183473086336371e+20 4.400000000000001e-02 1.350000000000000e-02 1.027815750648127e+20 4.400000000000001e-02 1.500000000000000e-02 8.759231337498678e+19 4.400000000000001e-02 1.650000000000000e-02 7.317917446169389e+19 4.400000000000001e-02 1.800000000000000e-02 5.986307956353842e+19 4.400000000000001e-02 1.950000000000000e-02 4.787748320406005e+19 4.400000000000001e-02 2.100000000000000e-02 3.736624719506208e+19 4.400000000000001e-02 2.250000000000000e-02 2.838763526282646e+19 4.400000000000001e-02 2.400000000000000e-02 2.092348121474290e+19 4.400000000000001e-02 2.550000000000000e-02 1.489223938259773e+19 4.400000000000001e-02 2.700000000000000e-02 1.016442150351949e+19 4.400000000000001e-02 2.850000000000000e-02 6.578874933662535e+18 4.400000000000001e-02 3.000000000000000e-02 3.958463057388865e+18 4.400000000000001e-02 3.150000000000000e-02 2.123951376380652e+18 4.400000000000001e-02 3.300000000000000e-02 9.052455974132736e+17 4.400000000000001e-02 3.450000000000000e-02 1.495215090557911e+17 4.400000000000001e-02 3.600000000000000e-02 -2.738240419656136e+17 4.400000000000001e-02 3.750000000000000e-02 -4.711361940705544e+17 4.400000000000001e-02 3.900000000000000e-02 -5.248694318508439e+17 4.400000000000001e-02 4.050000000000000e-02 -4.957136404773198e+17 4.400000000000001e-02 4.200000000000000e-02 -4.258046096198615e+17 4.400000000000001e-02 4.350000000000000e-02 -3.424052191539859e+17 4.400000000000001e-02 4.500000000000000e-02 -2.615644104198491e+17 4.400000000000001e-02 4.650000000000000e-02 -1.914103485998669e+17 4.400000000000001e-02 4.800000000000000e-02 -1.348831624467760e+17 4.400000000000001e-02 4.950000000000000e-02 -9.184017381888051e+16 4.400000000000001e-02 5.100000000000000e-02 -6.056089045631015e+16 4.400000000000001e-02 5.250000000000000e-02 -3.873738571080286e+16 4.400000000000001e-02 5.400000000000000e-02 -2.406188450336014e+16 4.400000000000001e-02 5.550000000000000e-02 -1.452513817128687e+16 4.400000000000001e-02 5.700000000000000e-02 -8.525406941447359e+15 4.400000000000001e-02 5.850000000000000e-02 -4.866660802465856e+15 4.400000000000001e-02 6.000000000000000e-02 -2.702091309204776e+15 4.400000000000001e-02 6.150000000000000e-02 -1.459055119056946e+15 4.400000000000001e-02 6.300000000000000e-02 -7.659653705323445e+14 4.400000000000001e-02 6.450000000000000e-02 -3.907289987061692e+14 4.400000000000001e-02 6.600000000000000e-02 -1.935133654807341e+14 4.400000000000001e-02 6.750000000000000e-02 -9.293760835698062e+13 4.400000000000001e-02 6.900000000000001e-02 -4.320808863682337e+13 4.400000000000001e-02 7.050000000000001e-02 -1.939733037249774e+13 4.400000000000001e-02 7.200000000000001e-02 -8.377320772870229e+12 4.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 4.599999999999999e-02 0.000000000000000e+00 1.989445563050528e+20 4.599999999999999e-02 1.500000000000000e-03 1.970970517782890e+20 4.599999999999999e-02 3.000000000000000e-03 1.922907075327944e+20 4.599999999999999e-02 4.500000000000001e-03 1.847066465509413e+20 4.599999999999999e-02 6.000000000000000e-03 1.746418241487460e+20 4.599999999999999e-02 7.500000000000000e-03 1.624899248612349e+20 4.599999999999999e-02 9.000000000000001e-03 1.487163683267401e+20 4.599999999999999e-02 1.050000000000000e-02 1.338295905059591e+20 4.599999999999999e-02 1.200000000000000e-02 1.183509690192945e+20 4.599999999999999e-02 1.350000000000000e-02 1.027857281190442e+20 4.599999999999999e-02 1.500000000000000e-02 8.759691845640287e+19 4.599999999999999e-02 1.650000000000000e-02 7.318416486880756e+19 4.599999999999999e-02 1.800000000000000e-02 5.986836478991145e+19 4.599999999999999e-02 1.950000000000000e-02 4.788295361766566e+19 4.599999999999999e-02 2.100000000000000e-02 3.737178076861466e+19 4.599999999999999e-02 2.250000000000000e-02 2.839310567643208e+19 4.599999999999999e-02 2.400000000000000e-02 2.092876644111593e+19 4.599999999999999e-02 2.550000000000000e-02 1.489722978971139e+19 4.599999999999999e-02 2.700000000000000e-02 1.016902658493558e+19 4.599999999999999e-02 2.850000000000000e-02 6.583027987894027e+18 4.599999999999999e-02 3.000000000000000e-02 3.962123443046311e+18 4.599999999999999e-02 3.150000000000000e-02 2.127104311550304e+18 4.599999999999999e-02 3.300000000000000e-02 9.078997885225124e+17 4.599999999999999e-02 3.450000000000000e-02 1.517051352355005e+17 4.599999999999999e-02 3.600000000000000e-02 -2.720683296802268e+17 4.599999999999999e-02 3.750000000000000e-02 -4.697565808200591e+17 4.599999999999999e-02 3.900000000000000e-02 -5.238099578128791e+17 4.599999999999999e-02 4.050000000000000e-02 -4.949184846716355e+17 4.599999999999999e-02 4.200000000000000e-02 -4.252213752583621e+17 4.599999999999999e-02 4.350000000000000e-02 -3.419871357538044e+17 4.599999999999999e-02 4.500000000000000e-02 -2.612715155942288e+17 4.599999999999999e-02 4.650000000000000e-02 -1.912098139484097e+17 4.599999999999999e-02 4.800000000000000e-02 -1.347489798757799e+17 4.599999999999999e-02 4.950000000000000e-02 -9.175242692671581e+16 4.599999999999999e-02 5.100000000000000e-02 -6.050481196369599e+16 4.599999999999999e-02 5.250000000000000e-02 -3.870235976491788e+16 4.599999999999999e-02 5.400000000000000e-02 -2.404050427366765e+16 4.599999999999999e-02 5.550000000000000e-02 -1.451238366024518e+16 4.599999999999999e-02 5.700000000000000e-02 -8.517970858683957e+15 4.599999999999999e-02 5.850000000000000e-02 -4.862423850223992e+15 4.599999999999999e-02 6.000000000000000e-02 -2.699731961897151e+15 4.599999999999999e-02 6.150000000000000e-02 -1.457771136463238e+15 4.599999999999999e-02 6.300000000000000e-02 -7.652824733043197e+14 4.599999999999999e-02 6.450000000000000e-02 -3.903740378063192e+14 4.599999999999999e-02 6.600000000000000e-02 -1.933330493262907e+14 4.599999999999999e-02 6.750000000000000e-02 -9.284808884417131e+13 4.599999999999999e-02 6.900000000000001e-02 -4.316465464588022e+13 4.599999999999999e-02 7.050000000000001e-02 -1.937673494949797e+13 4.599999999999999e-02 7.200000000000001e-02 -8.367776548308961e+12 4.599999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 4.799999999999999e-02 0.000000000000000e+00 1.989449815202412e+20 4.799999999999999e-02 1.500000000000000e-03 1.970976314977775e+20 4.799999999999999e-02 3.000000000000000e-03 1.922914799571960e+20 4.799999999999999e-02 4.500000000000001e-03 1.847076523773243e+20 4.799999999999999e-02 6.000000000000000e-03 1.746431041754034e+20 4.799999999999999e-02 7.500000000000000e-03 1.624915168645164e+20 4.799999999999999e-02 9.000000000000001e-03 1.487183034019810e+20 4.799999999999999e-02 1.050000000000000e-02 1.338318891975498e+20 4.799999999999999e-02 1.200000000000000e-02 1.183536376747781e+20 4.799999999999999e-02 1.350000000000000e-02 1.027887559614590e+20 4.799999999999999e-02 1.500000000000000e-02 8.760027585557420e+19 4.799999999999999e-02 1.650000000000000e-02 7.318780319508111e+19 4.799999999999999e-02 1.800000000000000e-02 5.987221805829953e+19 4.799999999999999e-02 1.950000000000000e-02 4.788694189940206e+19 4.799999999999999e-02 2.100000000000000e-02 3.737581509799592e+19 4.799999999999999e-02 2.250000000000000e-02 2.839709395816848e+19 4.799999999999999e-02 2.400000000000000e-02 2.093261970950402e+19 4.799999999999999e-02 2.550000000000000e-02 1.490086811598495e+19 4.799999999999999e-02 2.700000000000000e-02 1.017238398410691e+19 4.799999999999999e-02 2.850000000000000e-02 6.586055830308845e+18 4.799999999999999e-02 3.000000000000000e-02 3.964792098529826e+18 4.799999999999999e-02 3.150000000000000e-02 2.129403003141051e+18 4.799999999999999e-02 3.300000000000000e-02 9.098348637634396e+17 4.799999999999999e-02 3.450000000000000e-02 1.532971385170601e+17 4.799999999999999e-02 3.600000000000000e-02 -2.707883030228337e+17 4.799999999999999e-02 3.750000000000000e-02 -4.687507544371005e+17 4.799999999999999e-02 3.900000000000000e-02 -5.230375334112850e+17 4.799999999999999e-02 4.050000000000000e-02 -4.943387651831244e+17 4.799999999999999e-02 4.200000000000000e-02 -4.247961600699507e+17 4.799999999999999e-02 4.350000000000000e-02 -3.416823261892190e+17 4.799999999999999e-02 4.500000000000000e-02 -2.610579765151171e+17 4.799999999999999e-02 4.650000000000000e-02 -1.910636113491952e+17 4.799999999999999e-02 4.800000000000000e-02 -1.346511521911061e+17 4.799999999999999e-02 4.950000000000000e-02 -9.168845382473944e+16 4.799999999999999e-02 5.100000000000000e-02 -6.046392715241454e+16 4.799999999999999e-02 5.250000000000000e-02 -3.867682360799379e+16 4.799999999999999e-02 5.400000000000000e-02 -2.402491671745165e+16 4.799999999999999e-02 5.550000000000000e-02 -1.450308480514730e+16 4.799999999999999e-02 5.700000000000000e-02 -8.512549478288684e+15 4.799999999999999e-02 5.850000000000000e-02 -4.859334840788432e+15 4.799999999999999e-02 6.000000000000000e-02 -2.698011846663610e+15 4.799999999999999e-02 6.150000000000000e-02 -1.456835030951386e+15 4.799999999999999e-02 6.300000000000000e-02 -7.647845975057580e+14 4.799999999999999e-02 6.450000000000000e-02 -3.901152485856012e+14 4.799999999999999e-02 6.600000000000000e-02 -1.932015873057949e+14 4.799999999999999e-02 6.750000000000000e-02 -9.278282338826119e+13 4.799999999999999e-02 6.900000000000001e-02 -4.313298848582259e+13 4.799999999999999e-02 7.050000000000001e-02 -1.936171956760459e+13 4.799999999999999e-02 7.200000000000001e-02 -8.360818197579029e+12 4.799999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 4.999999999999999e-02 0.000000000000000e+00 1.989452885859048e+20 4.999999999999999e-02 1.500000000000000e-03 1.970980501374553e+20 4.999999999999999e-02 3.000000000000000e-03 1.922920377571475e+20 4.999999999999999e-02 4.500000000000001e-03 1.847083787266039e+20 4.999999999999999e-02 6.000000000000000e-03 1.746440285361641e+20 4.999999999999999e-02 7.500000000000000e-03 1.624926665166395e+20 4.999999999999999e-02 9.000000000000001e-03 1.487197008007081e+20 4.999999999999999e-02 1.050000000000000e-02 1.338335491788441e+20 4.999999999999999e-02 1.200000000000000e-02 1.183555648224655e+20 4.999999999999999e-02 1.350000000000000e-02 1.027909424930454e+20 4.999999999999999e-02 1.500000000000000e-02 8.760270037387151e+19 4.999999999999999e-02 1.650000000000000e-02 7.319043058258305e+19 4.999999999999999e-02 1.800000000000000e-02 5.987500066448799e+19 4.999999999999999e-02 1.950000000000000e-02 4.788982200437354e+19 4.999999999999999e-02 2.100000000000000e-02 3.737872845589678e+19 4.999999999999999e-02 2.250000000000000e-02 2.839997406313996e+19 4.999999999999999e-02 2.400000000000000e-02 2.093540231569248e+19 4.999999999999999e-02 2.550000000000000e-02 1.490349550348689e+19 4.999999999999999e-02 2.700000000000000e-02 1.017480850240421e+19 4.999999999999999e-02 2.850000000000000e-02 6.588242361895177e+18 4.999999999999999e-02 3.000000000000000e-02 3.966719246217297e+18 4.999999999999999e-02 3.150000000000000e-02 2.131062984435258e+18 4.999999999999999e-02 3.300000000000000e-02 9.112322624905032e+17 4.999999999999999e-02 3.450000000000000e-02 1.544467906401823e+17 4.999999999999999e-02 3.600000000000000e-02 -2.698639422621676e+17 4.999999999999999e-02 3.750000000000000e-02 -4.680244051575135e+17 4.999999999999999e-02 3.900000000000000e-02 -5.224797334597834e+17 4.999999999999999e-02 4.050000000000000e-02 -4.939201255053661e+17 4.999999999999999e-02 4.200000000000000e-02 -4.244890944063283e+17 4.999999999999999e-02 4.350000000000000e-02 -3.414622104601042e+17 4.999999999999999e-02 4.500000000000000e-02 -2.609037710191147e+17 4.999999999999999e-02 4.650000000000000e-02 -1.909580323403201e+17 4.999999999999999e-02 4.800000000000000e-02 -1.345805067303284e+17 4.999999999999999e-02 4.950000000000000e-02 -9.164225617341437e+16 4.999999999999999e-02 5.100000000000000e-02 -6.043440252100353e+16 4.999999999999999e-02 5.250000000000000e-02 -3.865838288154290e+16 4.999999999999999e-02 5.400000000000000e-02 -2.401366029147214e+16 4.999999999999999e-02 5.550000000000000e-02 -1.449636971314359e+16 4.999999999999999e-02 5.700000000000000e-02 -8.508634472865093e+15 4.999999999999999e-02 5.850000000000000e-02 -4.857104137939342e+15 4.999999999999999e-02 6.000000000000000e-02 -2.696769679544257e+15 4.999999999999999e-02 6.150000000000000e-02 -1.456159030027499e+15 4.999999999999999e-02 6.300000000000000e-02 -7.644250605779779e+14 4.999999999999999e-02 6.450000000000000e-02 -3.899283660706681e+14 4.999999999999999e-02 6.600000000000000e-02 -1.931066530850407e+14 4.999999999999999e-02 6.750000000000000e-02 -9.273569247413384e+13 4.999999999999999e-02 6.900000000000001e-02 -4.311012102784490e+13 4.999999999999999e-02 7.050000000000001e-02 -1.935087633262312e+13 4.999999999999999e-02 7.200000000000001e-02 -8.355793281623920e+12 4.999999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 5.199999999999999e-02 0.000000000000000e+00 1.989455082325985e+20 5.199999999999999e-02 1.500000000000000e-03 1.970983495939949e+20 5.199999999999999e-02 3.000000000000000e-03 1.922924367562203e+20 5.199999999999999e-02 4.500000000000001e-03 1.847088982904517e+20 5.199999999999999e-02 6.000000000000000e-03 1.746446897393167e+20 5.199999999999999e-02 7.500000000000000e-03 1.624934888726293e+20 5.199999999999999e-02 9.000000000000001e-03 1.487207003719612e+20 5.199999999999999e-02 1.050000000000000e-02 1.338347365776517e+20 5.199999999999999e-02 1.200000000000000e-02 1.183569433276778e+20 5.199999999999999e-02 1.350000000000000e-02 1.027925065377774e+20 5.199999999999999e-02 1.500000000000000e-02 8.760443465253200e+19 5.199999999999999e-02 1.650000000000000e-02 7.319230997531956e+19 5.199999999999999e-02 1.800000000000000e-02 5.987699108647763e+19 5.199999999999999e-02 1.950000000000000e-02 4.789188216807601e+19 5.199999999999999e-02 2.100000000000000e-02 3.738081240570384e+19 5.199999999999999e-02 2.250000000000000e-02 2.840203422684243e+19 5.199999999999999e-02 2.400000000000000e-02 2.093739273768211e+19 5.199999999999999e-02 2.550000000000000e-02 1.490537489622340e+19 5.199999999999999e-02 2.700000000000000e-02 1.017654278106470e+19 5.199999999999999e-02 2.850000000000000e-02 6.589806406627241e+18 5.199999999999999e-02 3.000000000000000e-02 3.968097751429543e+18 5.199999999999999e-02 3.150000000000000e-02 2.132250383242922e+18 5.199999999999999e-02 3.300000000000000e-02 9.122318337435873e+17 5.199999999999999e-02 3.450000000000000e-02 1.552691466299679e+17 5.199999999999999e-02 3.600000000000000e-02 -2.692027391095199e+17 5.199999999999999e-02 3.750000000000000e-02 -4.675048413096924e+17 5.199999999999999e-02 3.900000000000000e-02 -5.220807343869389e+17 5.199999999999999e-02 4.050000000000000e-02 -4.936206689657379e+17 5.199999999999999e-02 4.200000000000000e-02 -4.242694477126383e+17 5.199999999999999e-02 4.350000000000000e-02 -3.413047597977316e+17 5.199999999999999e-02 4.500000000000000e-02 -2.607934665098245e+17 5.199999999999999e-02 4.650000000000000e-02 -1.908825107728844e+17 5.199999999999999e-02 4.800000000000000e-02 -1.345299734284249e+17 5.199999999999999e-02 4.950000000000000e-02 -9.160921059856861e+16 5.199999999999999e-02 5.100000000000000e-02 -6.041328329980718e+16 5.199999999999999e-02 5.250000000000000e-02 -3.864519207229905e+16 5.199999999999999e-02 5.400000000000000e-02 -2.400560847375993e+16 5.199999999999999e-02 5.550000000000000e-02 -1.449156635043921e+16 5.199999999999999e-02 5.700000000000000e-02 -8.505834036023911e+15 5.199999999999999e-02 5.850000000000000e-02 -4.855508497125492e+15 5.199999999999999e-02 6.000000000000000e-02 -2.695881146786938e+15 5.199999999999999e-02 6.150000000000000e-02 -1.455675480788839e+15 5.199999999999999e-02 6.300000000000000e-02 -7.641678807405622e+14 5.199999999999999e-02 6.450000000000000e-02 -3.897946874104451e+14 5.199999999999999e-02 6.600000000000000e-02 -1.930387458255292e+14 5.199999999999999e-02 6.750000000000000e-02 -9.270197932842900e+13 5.199999999999999e-02 6.900000000000001e-02 -4.309376373970452e+13 5.199999999999999e-02 7.050000000000001e-02 -1.934312007396337e+13 5.199999999999999e-02 7.200000000000001e-02 -8.352198916293100e+12 5.199999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 5.399999999999999e-02 0.000000000000000e+00 1.989456638657451e+20 5.399999999999999e-02 1.500000000000000e-03 1.970985617773096e+20 5.399999999999999e-02 3.000000000000000e-03 1.922927194715217e+20 5.399999999999999e-02 4.500000000000001e-03 1.847092664332867e+20 5.399999999999999e-02 6.000000000000000e-03 1.746451582422815e+20 5.399999999999999e-02 7.500000000000000e-03 1.624940715622578e+20 5.399999999999999e-02 9.000000000000001e-03 1.487214086294668e+20 5.399999999999999e-02 1.050000000000000e-02 1.338355779224934e+20 5.399999999999999e-02 1.200000000000000e-02 1.183579200831217e+20 5.399999999999999e-02 1.350000000000000e-02 1.027936147593446e+20 5.399999999999999e-02 1.500000000000000e-02 8.760566349527261e+19 5.399999999999999e-02 1.650000000000000e-02 7.319364164027839e+19 5.399999999999999e-02 1.800000000000000e-02 5.987840142246829e+19 5.399999999999999e-02 1.950000000000000e-02 4.789334192034532e+19 5.399999999999999e-02 2.100000000000000e-02 3.738228901188632e+19 5.399999999999999e-02 2.250000000000000e-02 2.840349397911174e+19 5.399999999999999e-02 2.400000000000000e-02 2.093880307367277e+19 5.399999999999999e-02 2.550000000000000e-02 1.490670656118223e+19 5.399999999999999e-02 2.700000000000000e-02 1.017777162380533e+19 5.399999999999999e-02 2.850000000000000e-02 6.590914628194385e+18 5.399999999999999e-02 3.000000000000000e-02 3.969074506873497e+18 5.399999999999999e-02 3.150000000000000e-02 2.133091728084586e+18 5.399999999999999e-02 3.300000000000000e-02 9.129400912491786e+17 5.399999999999999e-02 3.450000000000000e-02 1.558518362583828e+17 5.399999999999999e-02 3.600000000000000e-02 -2.687342361447352e+17 5.399999999999999e-02 3.750000000000000e-02 -4.671366984747341e+17 5.399999999999999e-02 3.900000000000000e-02 -5.217980190855593e+17 5.399999999999999e-02 4.050000000000000e-02 -4.934084856510058e+17 5.399999999999999e-02 4.200000000000000e-02 -4.241138145660225e+17 5.399999999999999e-02 4.350000000000000e-02 -3.411931963518627e+17 5.399999999999999e-02 4.500000000000000e-02 -2.607153090034293e+17 5.399999999999999e-02 4.650000000000000e-02 -1.908289991129548e+17 5.399999999999999e-02 4.800000000000000e-02 -1.344941674863823e+17 5.399999999999999e-02 4.950000000000000e-02 -9.158579578312762e+16 5.399999999999999e-02 5.100000000000000e-02 -6.039831903700110e+16 5.399999999999999e-02 5.250000000000000e-02 -3.863584557536554e+16 5.399999999999999e-02 5.400000000000000e-02 -2.399990326734195e+16 5.399999999999999e-02 5.550000000000000e-02 -1.448816287352152e+16 5.399999999999999e-02 5.700000000000000e-02 -8.503849754857780e+15 5.399999999999999e-02 5.850000000000000e-02 -4.854377887797594e+15 5.399999999999999e-02 6.000000000000000e-02 -2.695251566862152e+15 5.399999999999999e-02 6.150000000000000e-02 -1.455332856512133e+15 5.399999999999999e-02 6.300000000000000e-02 -7.639856530608700e+14 5.399999999999999e-02 6.450000000000000e-02 -3.896999678853005e+14 5.399999999999999e-02 6.600000000000000e-02 -1.929906293695139e+14 5.399999999999999e-02 6.750000000000000e-02 -9.267809149811289e+13 5.399999999999999e-02 6.900000000000001e-02 -4.308217359837061e+13 5.399999999999999e-02 7.050000000000001e-02 -1.933762428925154e+13 5.399999999999999e-02 7.200000000000001e-02 -8.349652088124986e+12 5.399999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 5.599999999999999e-02 0.000000000000000e+00 1.989457731042385e+20 5.599999999999999e-02 1.500000000000000e-03 1.970987107082163e+20 5.599999999999999e-02 3.000000000000000e-03 1.922929179086430e+20 5.599999999999999e-02 4.500000000000001e-03 1.847095248317675e+20 5.599999999999999e-02 6.000000000000000e-03 1.746454870832717e+20 5.599999999999999e-02 7.500000000000000e-03 1.624944805505648e+20 5.599999999999999e-02 9.000000000000001e-03 1.487219057535342e+20 5.599999999999999e-02 1.050000000000000e-02 1.338361684602095e+20 5.599999999999999e-02 1.200000000000000e-02 1.183586056651810e+20 5.599999999999999e-02 1.350000000000000e-02 1.027943926171276e+20 5.599999999999999e-02 1.500000000000000e-02 8.760652601673780e+19 5.599999999999999e-02 1.650000000000000e-02 7.319457633238622e+19 5.599999999999999e-02 1.800000000000000e-02 5.987939133356501e+19 5.599999999999999e-02 1.950000000000000e-02 4.789436651659714e+19 5.599999999999999e-02 2.100000000000000e-02 3.738332543785516e+19 5.599999999999999e-02 2.250000000000000e-02 2.840451857536356e+19 5.599999999999999e-02 2.400000000000000e-02 2.093979298476950e+19 5.599999999999999e-02 2.550000000000000e-02 1.490764125329006e+19 5.599999999999999e-02 2.700000000000000e-02 1.017863414527051e+19 5.599999999999999e-02 2.850000000000000e-02 6.591692485977357e+18 5.599999999999999e-02 3.000000000000000e-02 3.969760088932775e+18 5.599999999999999e-02 3.150000000000000e-02 2.133682265800738e+18 5.599999999999999e-02 3.300000000000000e-02 9.134372153166080e+17 5.599999999999999e-02 3.450000000000000e-02 1.562608245653760e+17 5.599999999999999e-02 3.600000000000000e-02 -2.684053951545329e+17 5.599999999999999e-02 3.750000000000000e-02 -4.668782999938639e+17 5.599999999999999e-02 3.900000000000000e-02 -5.215995819642624e+17 5.599999999999999e-02 4.050000000000000e-02 -4.932595547443404e+17 5.599999999999999e-02 4.200000000000000e-02 -4.240045760725907e+17 5.599999999999999e-02 4.350000000000000e-02 -3.411148902646711e+17 5.599999999999999e-02 4.500000000000000e-02 -2.606604504566823e+17 5.599999999999999e-02 4.650000000000000e-02 -1.907914394205701e+17 5.599999999999999e-02 4.800000000000000e-02 -1.344690353904908e+17 5.599999999999999e-02 4.950000000000000e-02 -9.156936098618123e+16 5.599999999999999e-02 5.100000000000000e-02 -6.038781566056878e+16 5.599999999999999e-02 5.250000000000000e-02 -3.862928529392110e+16 5.599999999999999e-02 5.400000000000000e-02 -2.399589879806681e+16 5.599999999999999e-02 5.550000000000000e-02 -1.448577398208674e+16 5.599999999999999e-02 5.700000000000000e-02 -8.502456993162429e+15 5.599999999999999e-02 5.850000000000000e-02 -4.853584316104640e+15 5.599999999999999e-02 6.000000000000000e-02 -2.694809666380320e+15 5.599999999999999e-02 6.150000000000000e-02 -1.455092369439717e+15 5.599999999999999e-02 6.300000000000000e-02 -7.638577479351047e+14 5.599999999999999e-02 6.450000000000000e-02 -3.896334845014561e+14 5.599999999999999e-02 6.600000000000000e-02 -1.929568565564680e+14 5.599999999999999e-02 6.750000000000000e-02 -9.266132469327837e+13 5.599999999999999e-02 6.900000000000001e-02 -4.307403850886359e+13 5.599999999999999e-02 7.050000000000001e-02 -1.933376681251732e+13 5.599999999999999e-02 7.200000000000001e-02 -8.347864476178791e+12 5.599999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 5.800000000000000e-02 0.000000000000000e+00 1.989458490593149e+20 5.800000000000000e-02 1.500000000000000e-03 1.970988142619915e+20 5.800000000000000e-02 3.000000000000000e-03 1.922930558847925e+20 5.800000000000000e-02 4.500000000000001e-03 1.847097044999022e+20 5.800000000000000e-02 6.000000000000000e-03 1.746457157310839e+20 5.800000000000000e-02 7.500000000000000e-03 1.624947649259449e+20 5.800000000000000e-02 9.000000000000001e-03 1.487222514109606e+20 5.800000000000000e-02 1.050000000000000e-02 1.338365790694730e+20 5.800000000000000e-02 1.200000000000000e-02 1.183590823601265e+20 5.800000000000000e-02 1.350000000000000e-02 1.027949334726947e+20 5.800000000000000e-02 1.500000000000000e-02 8.760712574016591e+19 5.800000000000000e-02 1.650000000000000e-02 7.319522623708745e+19 5.800000000000000e-02 1.800000000000000e-02 5.988007963281369e+19 5.800000000000000e-02 1.950000000000000e-02 4.789507893292691e+19 5.800000000000000e-02 2.100000000000000e-02 3.738404607955523e+19 5.800000000000000e-02 2.250000000000000e-02 2.840523099169332e+19 5.800000000000000e-02 2.400000000000000e-02 2.094048128401817e+19 5.800000000000000e-02 2.550000000000000e-02 1.490829115799129e+19 5.800000000000000e-02 2.700000000000000e-02 1.017923386869862e+19 5.800000000000000e-02 2.850000000000000e-02 6.592233341544457e+18 5.800000000000000e-02 3.000000000000000e-02 3.970236783878280e+18 5.800000000000000e-02 3.150000000000000e-02 2.134092875064225e+18 5.800000000000000e-02 3.300000000000000e-02 9.137828727430615e+17 5.800000000000000e-02 3.450000000000000e-02 1.565451999455012e+17 5.800000000000000e-02 3.600000000000000e-02 -2.681767473423811e+17 5.800000000000000e-02 3.750000000000000e-02 -4.666986318591892e+17 5.800000000000000e-02 3.900000000000000e-02 -5.214616058147369e+17 5.800000000000000e-02 4.050000000000000e-02 -4.931560009691561e+17 5.800000000000000e-02 4.200000000000000e-02 -4.239286209962161e+17 5.800000000000000e-02 4.350000000000000e-02 -3.410604429297951e+17 5.800000000000000e-02 4.500000000000000e-02 -2.606223065297838e+17 5.800000000000000e-02 4.650000000000000e-02 -1.907653236328651e+17 5.800000000000000e-02 4.800000000000000e-02 -1.344515606871794e+17 5.800000000000000e-02 4.950000000000000e-02 -9.155793363838426e+16 5.800000000000000e-02 5.100000000000000e-02 -6.038051251371965e+16 5.800000000000000e-02 5.250000000000000e-02 -3.862472383703446e+16 5.800000000000000e-02 5.400000000000000e-02 -2.399311443369049e+16 5.800000000000000e-02 5.550000000000000e-02 -1.448411295193447e+16 5.800000000000000e-02 5.700000000000000e-02 -8.501488586169449e+15 5.800000000000000e-02 5.850000000000000e-02 -4.853032534432690e+15 5.800000000000000e-02 6.000000000000000e-02 -2.694502406697464e+15 5.800000000000000e-02 6.150000000000000e-02 -1.454925155361798e+15 5.800000000000000e-02 6.300000000000000e-02 -7.637688136840821e+14 5.800000000000000e-02 6.450000000000000e-02 -3.895872576601760e+14 5.800000000000000e-02 6.600000000000000e-02 -1.929333738397654e+14 5.800000000000000e-02 6.750000000000000e-02 -9.264966649568012e+13 5.800000000000000e-02 6.900000000000001e-02 -4.306838206555861e+13 5.800000000000000e-02 7.050000000000001e-02 -1.933108465414295e+13 5.800000000000000e-02 7.200000000000001e-02 -8.346621524196977e+12 5.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 6.000000000000000e-02 0.000000000000000e+00 1.989459013778971e+20 6.000000000000000e-02 1.500000000000000e-03 1.970988855908211e+20 6.000000000000000e-02 3.000000000000000e-03 1.922931509240824e+20 6.000000000000000e-02 4.500000000000001e-03 1.847098282570298e+20 6.000000000000000e-02 6.000000000000000e-03 1.746458732258812e+20 6.000000000000000e-02 7.500000000000000e-03 1.624949608064233e+20 6.000000000000000e-02 9.000000000000001e-03 1.487224895030980e+20 6.000000000000000e-02 1.050000000000000e-02 1.338368619010562e+20 6.000000000000000e-02 1.200000000000000e-02 1.183594107121588e+20 6.000000000000000e-02 1.350000000000000e-02 1.027953060191761e+20 6.000000000000000e-02 1.500000000000000e-02 8.760753883539235e+19 6.000000000000000e-02 1.650000000000000e-02 7.319567389765421e+19 6.000000000000000e-02 1.800000000000000e-02 5.988055373991150e+19 6.000000000000000e-02 1.950000000000000e-02 4.789556965210056e+19 6.000000000000000e-02 2.100000000000000e-02 3.738454246444253e+19 6.000000000000000e-02 2.250000000000000e-02 2.840572171086698e+19 6.000000000000000e-02 2.400000000000000e-02 2.094095539111598e+19 6.000000000000000e-02 2.550000000000000e-02 1.490873881855804e+19 6.000000000000000e-02 2.700000000000000e-02 1.017964696392505e+19 6.000000000000000e-02 2.850000000000000e-02 6.592605888025865e+18 6.000000000000000e-02 3.000000000000000e-02 3.970565135910610e+18 6.000000000000000e-02 3.150000000000000e-02 2.134375706647462e+18 6.000000000000000e-02 3.300000000000000e-02 9.140209648804669e+17 6.000000000000000e-02 3.450000000000000e-02 1.567410804239677e+17 6.000000000000000e-02 3.600000000000000e-02 -2.680192525450998e+17 6.000000000000000e-02 3.750000000000000e-02 -4.665748747316567e+17 6.000000000000000e-02 3.900000000000000e-02 -5.213665665248586e+17 6.000000000000000e-02 4.050000000000000e-02 -4.930846721395604e+17 6.000000000000000e-02 4.200000000000000e-02 -4.238763024140108e+17 6.000000000000000e-02 4.350000000000000e-02 -3.410229390853974e+17 6.000000000000000e-02 4.500000000000000e-02 -2.605960326285474e+17 6.000000000000000e-02 4.650000000000000e-02 -1.907473348288099e+17 6.000000000000000e-02 4.800000000000000e-02 -1.344395239446029e+17 6.000000000000000e-02 4.950000000000000e-02 -9.155006237205629e+16 6.000000000000000e-02 5.100000000000000e-02 -6.037548203640306e+16 6.000000000000000e-02 5.250000000000000e-02 -3.862158186195537e+16 6.000000000000000e-02 5.400000000000000e-02 -2.399119653690907e+16 6.000000000000000e-02 5.550000000000000e-02 -1.448296881849777e+16 6.000000000000000e-02 5.700000000000000e-02 -8.500821538181498e+15 6.000000000000000e-02 5.850000000000000e-02 -4.852652461945884e+15 6.000000000000000e-02 6.000000000000000e-02 -2.694290763292663e+15 6.000000000000000e-02 6.150000000000000e-02 -1.454809976707532e+15 6.000000000000000e-02 6.300000000000000e-02 -7.637075549223892e+14 6.000000000000000e-02 6.450000000000000e-02 -3.895554161702976e+14 6.000000000000000e-02 6.600000000000000e-02 -1.929171987201704e+14 6.000000000000000e-02 6.750000000000000e-02 -9.264163621780375e+13 6.000000000000000e-02 6.900000000000001e-02 -4.306448585337416e+13 6.000000000000000e-02 7.050000000000001e-02 -1.932923715783204e+13 6.000000000000000e-02 7.200000000000001e-02 -8.345765366997990e+12 6.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 6.200000000000000e-02 0.000000000000000e+00 1.989459370791165e+20 6.200000000000000e-02 1.500000000000000e-03 1.970989342642768e+20 6.200000000000000e-02 3.000000000000000e-03 1.922932157771116e+20 6.200000000000000e-02 4.500000000000001e-03 1.847099127065728e+20 6.200000000000000e-02 6.000000000000000e-03 1.746459806973774e+20 6.200000000000000e-02 7.500000000000000e-03 1.624950944715887e+20 6.200000000000000e-02 9.000000000000001e-03 1.487226519727079e+20 6.200000000000000e-02 1.050000000000000e-02 1.338370549000249e+20 6.200000000000000e-02 1.200000000000000e-02 1.183596347734284e+20 6.200000000000000e-02 1.350000000000000e-02 1.027955602379089e+20 6.200000000000000e-02 1.500000000000000e-02 8.760782072382842e+19 6.200000000000000e-02 1.650000000000000e-02 7.319597937283033e+19 6.200000000000000e-02 1.800000000000000e-02 5.988087726170450e+19 6.200000000000000e-02 1.950000000000000e-02 4.789590450966261e+19 6.200000000000000e-02 2.100000000000000e-02 3.738488118818132e+19 6.200000000000000e-02 2.250000000000000e-02 2.840605656842903e+19 6.200000000000000e-02 2.400000000000000e-02 2.094127891290898e+19 6.200000000000000e-02 2.550000000000000e-02 1.490904429373417e+19 6.200000000000000e-02 2.700000000000000e-02 1.017992885236114e+19 6.200000000000000e-02 2.850000000000000e-02 6.592860106758721e+18 6.200000000000000e-02 3.000000000000000e-02 3.970789197180153e+18 6.200000000000000e-02 3.150000000000000e-02 2.134568705616154e+18 6.200000000000000e-02 3.300000000000000e-02 9.141834344902840e+17 6.200000000000000e-02 3.450000000000000e-02 1.568747455892869e+17 6.200000000000000e-02 3.600000000000000e-02 -2.679117810488064e+17 6.200000000000000e-02 3.750000000000000e-02 -4.664904251885445e+17 6.200000000000000e-02 3.900000000000000e-02 -5.213017134956396e+17 6.200000000000000e-02 4.050000000000000e-02 -4.930359986838156e+17 6.200000000000000e-02 4.200000000000000e-02 -4.238406011946015e+17 6.200000000000000e-02 4.350000000000000e-02 -3.409973471652593e+17 6.200000000000000e-02 4.500000000000000e-02 -2.605781038110366e+17 6.200000000000000e-02 4.650000000000000e-02 -1.907350596062520e+17 6.200000000000000e-02 4.800000000000000e-02 -1.344313102971838e+17 6.200000000000000e-02 4.950000000000000e-02 -9.154469116751752e+16 6.200000000000000e-02 5.100000000000000e-02 -6.037204933301464e+16 6.200000000000000e-02 5.250000000000000e-02 -3.861943783708029e+16 6.200000000000000e-02 5.400000000000000e-02 -2.398988780011018e+16 6.200000000000000e-02 5.550000000000000e-02 -1.448218808329557e+16 6.200000000000000e-02 5.700000000000000e-02 -8.500366357143125e+15 6.200000000000000e-02 5.850000000000000e-02 -4.852393107608076e+15 6.200000000000000e-02 6.000000000000000e-02 -2.694146341802003e+15 6.200000000000000e-02 6.150000000000000e-02 -1.454731380953712e+15 6.200000000000000e-02 6.300000000000000e-02 -7.636657530921455e+14 6.200000000000000e-02 6.450000000000000e-02 -3.895336881347019e+14 6.200000000000000e-02 6.600000000000000e-02 -1.929061611218775e+14 6.200000000000000e-02 6.750000000000000e-02 -9.263615650676614e+13 6.200000000000000e-02 6.900000000000001e-02 -4.306182715124198e+13 6.200000000000000e-02 7.050000000000001e-02 -1.932797646099406e+13 6.200000000000000e-02 7.200000000000001e-02 -8.345181141380217e+12 6.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 6.400000000000000e-02 0.000000000000000e+00 1.989459612141154e+20 6.400000000000000e-02 1.500000000000000e-03 1.970989671688616e+20 6.400000000000000e-02 3.000000000000000e-03 1.922932596195297e+20 6.400000000000000e-02 4.500000000000001e-03 1.847099697967692e+20 6.400000000000000e-02 6.000000000000000e-03 1.746460533510426e+20 6.400000000000000e-02 7.500000000000000e-03 1.624951848328891e+20 6.400000000000000e-02 9.000000000000001e-03 1.487227618065990e+20 6.400000000000000e-02 1.050000000000000e-02 1.338371853725960e+20 6.400000000000000e-02 1.200000000000000e-02 1.183597862449628e+20 6.400000000000000e-02 1.350000000000000e-02 1.027957320967117e+20 6.400000000000000e-02 1.500000000000000e-02 8.760801128810593e+19 6.400000000000000e-02 1.650000000000000e-02 7.319618588238794e+19 6.400000000000000e-02 1.800000000000000e-02 5.988109597126772e+19 6.400000000000000e-02 1.950000000000000e-02 4.789613088251515e+19 6.400000000000000e-02 2.100000000000000e-02 3.738511017467487e+19 6.400000000000000e-02 2.250000000000000e-02 2.840628294128157e+19 6.400000000000000e-02 2.400000000000000e-02 2.094149762247220e+19 6.400000000000000e-02 2.550000000000000e-02 1.490925080329178e+19 6.400000000000000e-02 2.700000000000000e-02 1.018011941663863e+19 6.400000000000000e-02 2.850000000000000e-02 6.593031965561527e+18 6.400000000000000e-02 3.000000000000000e-02 3.970940668714556e+18 6.400000000000000e-02 3.150000000000000e-02 2.134699178187274e+18 6.400000000000000e-02 3.300000000000000e-02 9.142932683814472e+17 6.400000000000000e-02 3.450000000000000e-02 1.569651068896952e+17 6.400000000000000e-02 3.600000000000000e-02 -2.678391273836672e+17 6.400000000000000e-02 3.750000000000000e-02 -4.664333349921851e+17 6.400000000000000e-02 3.900000000000000e-02 -5.212578710775969e+17 6.400000000000000e-02 4.050000000000000e-02 -4.930030940990948e+17 6.400000000000000e-02 4.200000000000000e-02 -4.238164661957462e+17 6.400000000000000e-02 4.350000000000000e-02 -3.409800463286644e+17 6.400000000000000e-02 4.500000000000000e-02 -2.605659834409972e+17 6.400000000000000e-02 4.650000000000000e-02 -1.907267612207266e+17 6.400000000000000e-02 4.800000000000000e-02 -1.344257576473209e+17 6.400000000000000e-02 4.950000000000000e-02 -9.154106008663176e+16 6.400000000000000e-02 5.100000000000000e-02 -6.036972873182171e+16 6.400000000000000e-02 5.250000000000000e-02 -3.861798841773938e+16 6.400000000000000e-02 5.400000000000000e-02 -2.398900305830959e+16 6.400000000000000e-02 5.550000000000000e-02 -1.448166028498718e+16 6.400000000000000e-02 5.700000000000000e-02 -8.500058642336128e+15 6.400000000000000e-02 5.850000000000000e-02 -4.852217776996134e+15 6.400000000000000e-02 6.000000000000000e-02 -2.694048708932049e+15 6.400000000000000e-02 6.150000000000000e-02 -1.454678248078705e+15 6.400000000000000e-02 6.300000000000000e-02 -7.636374939138380e+14 6.400000000000000e-02 6.450000000000000e-02 -3.895189993895300e+14 6.400000000000000e-02 6.600000000000000e-02 -1.928986994041387e+14 6.400000000000000e-02 6.750000000000000e-02 -9.263245207252528e+13 6.400000000000000e-02 6.900000000000001e-02 -4.306002979602613e+13 6.400000000000000e-02 7.050000000000001e-02 -1.932712419551840e+13 6.400000000000000e-02 7.200000000000001e-02 -8.344786188915020e+12 6.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 6.600000000000000e-02 0.000000000000000e+00 1.989459773784305e+20 6.600000000000000e-02 1.500000000000000e-03 1.970989892065703e+20 6.600000000000000e-02 3.000000000000000e-03 1.922932889828068e+20 6.600000000000000e-02 4.500000000000001e-03 1.847100080326907e+20 6.600000000000000e-02 6.000000000000000e-03 1.746461020105326e+20 6.600000000000000e-02 7.500000000000000e-03 1.624952453519942e+20 6.600000000000000e-02 9.000000000000001e-03 1.487228353673908e+20 6.600000000000000e-02 1.050000000000000e-02 1.338372727560579e+20 6.600000000000000e-02 1.200000000000000e-02 1.183598876923929e+20 6.600000000000000e-02 1.350000000000000e-02 1.027958471984301e+20 6.600000000000000e-02 1.500000000000000e-02 8.760813891773810e+19 6.600000000000000e-02 1.650000000000000e-02 7.319632419130515e+19 6.600000000000000e-02 1.800000000000000e-02 5.988124245108795e+19 6.600000000000000e-02 1.950000000000000e-02 4.789628249479152e+19 6.600000000000000e-02 2.100000000000000e-02 3.738526353742643e+19 6.600000000000000e-02 2.250000000000000e-02 2.840643455355793e+19 6.600000000000000e-02 2.400000000000000e-02 2.094164410229243e+19 6.600000000000000e-02 2.550000000000000e-02 1.490938911220899e+19 6.600000000000000e-02 2.700000000000000e-02 1.018024704627080e+19 6.600000000000000e-02 2.850000000000000e-02 6.593147067279842e+18 6.600000000000000e-02 3.000000000000000e-02 3.971042116144659e+18 6.600000000000000e-02 3.150000000000000e-02 2.134786561649068e+18 6.600000000000000e-02 3.300000000000000e-02 9.143668291731886e+17 6.600000000000000e-02 3.450000000000000e-02 1.570256259947766e+17 6.600000000000000e-02 3.600000000000000e-02 -2.677904678936504e+17 6.600000000000000e-02 3.750000000000000e-02 -4.663950990706460e+17 6.600000000000000e-02 3.900000000000000e-02 -5.212285078004803e+17 6.600000000000000e-02 4.050000000000000e-02 -4.929810563903482e+17 6.600000000000000e-02 4.200000000000000e-02 -4.238003018806548e+17 6.600000000000000e-02 4.350000000000000e-02 -3.409684591653196e+17 6.600000000000000e-02 4.500000000000000e-02 -2.605578658735792e+17 6.600000000000000e-02 4.650000000000000e-02 -1.907212034115389e+17 6.600000000000000e-02 4.800000000000000e-02 -1.344220387831721e+17 6.600000000000000e-02 4.950000000000000e-02 -9.153862818531238e+16 6.600000000000000e-02 5.100000000000000e-02 -6.036817451882553e+16 6.600000000000000e-02 5.250000000000000e-02 -3.861701767516481e+16 6.600000000000000e-02 5.400000000000000e-02 -2.398841050616882e+16 6.600000000000000e-02 5.550000000000000e-02 -1.448130679426557e+16 6.600000000000000e-02 5.700000000000000e-02 -8.499852551624113e+15 6.600000000000000e-02 5.850000000000000e-02 -4.852100350048092e+15 6.600000000000000e-02 6.000000000000000e-02 -2.693983319723511e+15 6.600000000000000e-02 6.150000000000000e-02 -1.454642662556680e+15 6.600000000000000e-02 6.300000000000000e-02 -7.636185674467135e+14 6.600000000000000e-02 6.450000000000000e-02 -3.895091616635504e+14 6.600000000000000e-02 6.600000000000000e-02 -1.928937019497209e+14 6.600000000000000e-02 6.750000000000000e-02 -9.262997104310144e+13 6.600000000000000e-02 6.900000000000001e-02 -4.305882602484662e+13 6.600000000000000e-02 7.050000000000001e-02 -1.932655339426116e+13 6.600000000000000e-02 7.200000000000001e-02 -8.344521671144301e+12 6.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 6.800000000000000e-02 0.000000000000000e+00 1.989459881040215e+20 6.800000000000000e-02 1.500000000000000e-03 1.970990038293644e+20 6.800000000000000e-02 3.000000000000000e-03 1.922933084663729e+20 6.800000000000000e-02 4.500000000000001e-03 1.847100334035683e+20 6.800000000000000e-02 6.000000000000000e-03 1.746461342978140e+20 6.800000000000000e-02 7.500000000000000e-03 1.624952855085469e+20 6.800000000000000e-02 9.000000000000001e-03 1.487228841775609e+20 6.800000000000000e-02 1.050000000000000e-02 1.338373307380553e+20 6.800000000000000e-02 1.200000000000000e-02 1.183599550063275e+20 6.800000000000000e-02 1.350000000000000e-02 1.027959235724646e+20 6.800000000000000e-02 1.500000000000000e-02 8.760822360448377e+19 6.800000000000000e-02 1.650000000000000e-02 7.319641596413169e+19 6.800000000000000e-02 1.800000000000000e-02 5.988133964559575e+19 6.800000000000000e-02 1.950000000000000e-02 4.789638309486431e+19 6.800000000000000e-02 2.100000000000000e-02 3.738536529900103e+19 6.800000000000000e-02 2.250000000000000e-02 2.840653515363073e+19 6.800000000000000e-02 2.400000000000000e-02 2.094174129680024e+19 6.800000000000000e-02 2.550000000000000e-02 1.490948088503553e+19 6.800000000000000e-02 2.700000000000000e-02 1.018033173301647e+19 6.800000000000000e-02 2.850000000000000e-02 6.593223441314448e+18 6.800000000000000e-02 3.000000000000000e-02 3.971109430079245e+18 6.800000000000000e-02 3.150000000000000e-02 2.134844543646493e+18 6.800000000000000e-02 3.300000000000000e-02 9.144156393433252e+17 6.800000000000000e-02 3.450000000000000e-02 1.570657825475492e+17 6.800000000000000e-02 3.600000000000000e-02 -2.677581806122025e+17 6.800000000000000e-02 3.750000000000000e-02 -4.663697281931515e+17 6.800000000000000e-02 3.900000000000000e-02 -5.212090242343314e+17 6.800000000000000e-02 4.050000000000000e-02 -4.929664335962225e+17 6.800000000000000e-02 4.200000000000000e-02 -4.237895762896018e+17 6.800000000000000e-02 4.350000000000000e-02 -3.409607706752847e+17 6.800000000000000e-02 4.500000000000000e-02 -2.605524795823582e+17 6.800000000000000e-02 4.650000000000000e-02 -1.907175156098498e+17 6.800000000000000e-02 4.800000000000000e-02 -1.344195711861340e+17 6.800000000000000e-02 4.950000000000000e-02 -9.153701453333360e+16 6.800000000000000e-02 5.100000000000000e-02 -6.036714324388983e+16 6.800000000000000e-02 5.250000000000000e-02 -3.861637355335614e+16 6.800000000000000e-02 5.400000000000000e-02 -2.398801732700203e+16 6.800000000000000e-02 5.550000000000000e-02 -1.448107224075065e+16 6.800000000000000e-02 5.700000000000000e-02 -8.499715803194971e+15 6.800000000000000e-02 5.850000000000000e-02 -4.852022433141857e+15 6.800000000000000e-02 6.000000000000000e-02 -2.693939931685967e+15 6.800000000000000e-02 6.150000000000000e-02 -1.454619050312395e+15 6.800000000000000e-02 6.300000000000000e-02 -7.636060090707285e+14 6.800000000000000e-02 6.450000000000000e-02 -3.895026339866800e+14 6.800000000000000e-02 6.600000000000000e-02 -1.928903859631116e+14 6.800000000000000e-02 6.750000000000000e-02 -9.262832479289905e+13 6.800000000000000e-02 6.900000000000001e-02 -4.305802728037027e+13 6.800000000000000e-02 7.050000000000001e-02 -1.932617464756988e+13 6.800000000000000e-02 7.200000000000001e-02 -8.344346154308668e+12 6.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 7.000000000000001e-02 0.000000000000000e+00 1.989459951549560e+20 7.000000000000001e-02 1.500000000000000e-03 1.970990134422951e+20 7.000000000000001e-02 3.000000000000000e-03 1.922933212747438e+20 7.000000000000001e-02 4.500000000000001e-03 1.847100500822197e+20 7.000000000000001e-02 6.000000000000000e-03 1.746461555232649e+20 7.000000000000001e-02 7.500000000000000e-03 1.624953119072061e+20 7.000000000000001e-02 9.000000000000001e-03 1.487229162650524e+20 7.000000000000001e-02 1.050000000000000e-02 1.338373688550470e+20 7.000000000000001e-02 1.200000000000000e-02 1.183599992580746e+20 7.000000000000001e-02 1.350000000000000e-02 1.027959737802632e+20 7.000000000000001e-02 1.500000000000000e-02 8.760827927700500e+19 7.000000000000001e-02 1.650000000000000e-02 7.319647629499685e+19 7.000000000000001e-02 1.800000000000000e-02 5.988140354063927e+19 7.000000000000001e-02 1.950000000000000e-02 4.789644922870433e+19 7.000000000000001e-02 2.100000000000000e-02 3.738543219640485e+19 7.000000000000001e-02 2.250000000000000e-02 2.840660128747074e+19 7.000000000000001e-02 2.400000000000000e-02 2.094180519184375e+19 7.000000000000001e-02 2.550000000000000e-02 1.490954121590070e+19 7.000000000000001e-02 2.700000000000000e-02 1.018038740553770e+19 7.000000000000001e-02 2.850000000000000e-02 6.593273649112962e+18 7.000000000000001e-02 3.000000000000000e-02 3.971153681826352e+18 7.000000000000001e-02 3.150000000000000e-02 2.134882660638206e+18 7.000000000000001e-02 3.300000000000000e-02 9.144477268348447e+17 7.000000000000001e-02 3.450000000000000e-02 1.570921812067405e+17 7.000000000000001e-02 3.600000000000000e-02 -2.677369551613025e+17 7.000000000000001e-02 3.750000000000000e-02 -4.663530495416704e+17 7.000000000000001e-02 3.900000000000000e-02 -5.211962158634158e+17 7.000000000000001e-02 4.050000000000000e-02 -4.929568206655323e+17 7.000000000000001e-02 4.200000000000000e-02 -4.237825253551144e+17 7.000000000000001e-02 4.350000000000000e-02 -3.409557163114482e+17 7.000000000000001e-02 4.500000000000000e-02 -2.605489386691962e+17 7.000000000000001e-02 4.650000000000000e-02 -1.907150912727682e+17 7.000000000000001e-02 4.800000000000000e-02 -1.344179490037320e+17 7.000000000000001e-02 4.950000000000000e-02 -9.153595372891435e+16 7.000000000000001e-02 5.100000000000000e-02 -6.036646529038833e+16 7.000000000000001e-02 5.250000000000000e-02 -3.861595011182714e+16 7.000000000000001e-02 5.400000000000000e-02 -2.398775885354978e+16 7.000000000000001e-02 5.550000000000000e-02 -1.448091804678042e+16 7.000000000000001e-02 5.700000000000000e-02 -8.499625905658287e+15 7.000000000000001e-02 5.850000000000000e-02 -4.851971211069470e+15 7.000000000000001e-02 6.000000000000000e-02 -2.693911408669497e+15 7.000000000000001e-02 6.150000000000000e-02 -1.454603527775060e+15 7.000000000000001e-02 6.300000000000000e-02 -7.635977532752296e+14 7.000000000000001e-02 6.450000000000000e-02 -3.894983427339424e+14 7.000000000000001e-02 6.600000000000000e-02 -1.928882060548689e+14 7.000000000000001e-02 6.750000000000000e-02 -9.262724255861755e+13 7.000000000000001e-02 6.900000000000001e-02 -4.305750219089530e+13 7.000000000000001e-02 7.050000000000001e-02 -1.932592566193409e+13 7.000000000000001e-02 7.200000000000001e-02 -8.344230770671219e+12 7.000000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 7.200000000000001e-02 0.000000000000000e+00 1.989459997473676e+20 7.200000000000001e-02 1.500000000000000e-03 1.970990197033850e+20 7.200000000000001e-02 3.000000000000000e-03 1.922933296170865e+20 7.200000000000001e-02 4.500000000000001e-03 1.847100609453519e+20 7.200000000000001e-02 6.000000000000000e-03 1.746461693478166e+20 7.200000000000001e-02 7.500000000000000e-03 1.624953291011695e+20 7.200000000000001e-02 9.000000000000001e-03 1.487229371642637e+20 7.200000000000001e-02 1.050000000000000e-02 1.338373936813897e+20 7.200000000000001e-02 1.200000000000000e-02 1.183600280801036e+20 7.200000000000001e-02 1.350000000000000e-02 1.027960064815850e+20 7.200000000000001e-02 1.500000000000000e-02 8.760831553760772e+19 7.200000000000001e-02 1.650000000000000e-02 7.319651558967016e+19 7.200000000000001e-02 1.800000000000000e-02 5.988144515673168e+19 7.200000000000001e-02 1.950000000000000e-02 4.789649230296871e+19 7.200000000000001e-02 2.100000000000000e-02 3.738547576799329e+19 7.200000000000001e-02 2.250000000000000e-02 2.840664436173513e+19 7.200000000000001e-02 2.400000000000000e-02 2.094184680793616e+19 7.200000000000001e-02 2.550000000000000e-02 1.490958051057399e+19 7.200000000000001e-02 2.700000000000000e-02 1.018042366614042e+19 7.200000000000001e-02 2.850000000000000e-02 6.593306350434817e+18 7.200000000000001e-02 3.000000000000000e-02 3.971182503855353e+18 7.200000000000001e-02 3.150000000000000e-02 2.134907486980946e+18 7.200000000000001e-02 3.300000000000000e-02 9.144686260460964e+17 7.200000000000001e-02 3.450000000000000e-02 1.571093751701545e+17 7.200000000000001e-02 3.600000000000000e-02 -2.677231306097009e+17 7.200000000000001e-02 3.750000000000000e-02 -4.663421864095214e+17 7.200000000000001e-02 3.900000000000000e-02 -5.211878735207493e+17 7.200000000000001e-02 4.050000000000000e-02 -4.929505595756268e+17 7.200000000000001e-02 4.200000000000000e-02 -4.237779329434797e+17 7.200000000000001e-02 4.350000000000000e-02 -3.409524243053560e+17 7.200000000000001e-02 4.500000000000000e-02 -2.605466324031500e+17 7.200000000000001e-02 4.650000000000000e-02 -1.907135122545771e+17 7.200000000000001e-02 4.800000000000000e-02 -1.344168924445838e+17 7.200000000000001e-02 4.950000000000000e-02 -9.153526280623373e+16 7.200000000000001e-02 5.100000000000000e-02 -6.036602372600370e+16 7.200000000000001e-02 5.250000000000000e-02 -3.861567431607158e+16 7.200000000000001e-02 5.400000000000000e-02 -2.398759050473141e+16 7.200000000000001e-02 5.550000000000000e-02 -1.448081761722968e+16 7.200000000000001e-02 5.700000000000000e-02 -8.499567353633145e+15 7.200000000000001e-02 5.850000000000000e-02 -4.851937849131190e+15 7.200000000000001e-02 6.000000000000000e-02 -2.693892831070609e+15 7.200000000000001e-02 6.150000000000000e-02 -1.454593417642683e+15 7.200000000000001e-02 6.300000000000000e-02 -7.635923761140365e+14 7.200000000000001e-02 6.450000000000000e-02 -3.894955477570447e+14 7.200000000000001e-02 6.600000000000000e-02 -1.928867862379647e+14 7.200000000000001e-02 6.750000000000000e-02 -9.262653767824820e+13 7.200000000000001e-02 6.900000000000001e-02 -4.305716018984305e+13 7.200000000000001e-02 7.050000000000001e-02 -1.932576349271628e+13 7.200000000000001e-02 7.200000000000001e-02 -8.344155619049826e+12 7.200000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 7.400000000000001e-02 0.000000000000000e+00 1.989460027109047e+20 7.400000000000001e-02 1.500000000000000e-03 1.970990237437398e+20 7.400000000000001e-02 3.000000000000000e-03 1.922933350004981e+20 7.400000000000001e-02 4.500000000000001e-03 1.847100679554585e+20 7.400000000000001e-02 6.000000000000000e-03 1.746461782689619e+20 7.400000000000001e-02 7.500000000000000e-03 1.624953401966358e+20 7.400000000000001e-02 9.000000000000001e-03 1.487229506507699e+20 7.400000000000001e-02 1.050000000000000e-02 1.338374097021199e+20 7.400000000000001e-02 1.200000000000000e-02 1.183600466792970e+20 7.400000000000001e-02 1.350000000000000e-02 1.027960275841316e+20 7.400000000000001e-02 1.500000000000000e-02 8.760833893700000e+19 7.400000000000001e-02 1.650000000000000e-02 7.319654094698378e+19 7.400000000000001e-02 1.800000000000000e-02 5.988147201208430e+19 7.400000000000001e-02 1.950000000000000e-02 4.789652009929680e+19 7.400000000000001e-02 2.100000000000000e-02 3.738550388525043e+19 7.400000000000001e-02 2.250000000000000e-02 2.840667215806322e+19 7.400000000000001e-02 2.400000000000000e-02 2.094187366328877e+19 7.400000000000001e-02 2.550000000000000e-02 1.490960586788762e+19 7.400000000000001e-02 2.700000000000000e-02 1.018044706553271e+19 7.400000000000001e-02 2.850000000000000e-02 6.593327452981413e+18 7.400000000000001e-02 3.000000000000000e-02 3.971201103048762e+18 7.400000000000001e-02 3.150000000000000e-02 2.134923507711141e+18 7.400000000000001e-02 3.300000000000000e-02 9.144821125522749e+17 7.400000000000001e-02 3.450000000000000e-02 1.571204706364390e+17 7.400000000000001e-02 3.600000000000000e-02 -2.677142094643835e+17 7.400000000000001e-02 3.750000000000000e-02 -4.663351763029158e+17 7.400000000000001e-02 3.900000000000000e-02 -5.211824901091668e+17 7.400000000000001e-02 4.050000000000000e-02 -4.929465192208652e+17 7.400000000000001e-02 4.200000000000000e-02 -4.237749694063807e+17 7.400000000000001e-02 4.350000000000000e-02 -3.409502999352079e+17 7.400000000000001e-02 4.500000000000000e-02 -2.605451441426168e+17 7.400000000000001e-02 4.650000000000000e-02 -1.907124932956156e+17 7.400000000000001e-02 4.800000000000000e-02 -1.344162106345715e+17 7.400000000000001e-02 4.950000000000000e-02 -9.153481694572307e+16 7.400000000000001e-02 5.100000000000000e-02 -6.036573877932653e+16 7.400000000000001e-02 5.250000000000000e-02 -3.861549634183531e+16 7.400000000000001e-02 5.400000000000000e-02 -2.398748186726410e+16 7.400000000000001e-02 5.550000000000000e-02 -1.448075280886250e+16 7.400000000000001e-02 5.700000000000000e-02 -8.499529569324477e+15 7.400000000000001e-02 5.850000000000000e-02 -4.851916320281066e+15 7.400000000000001e-02 6.000000000000000e-02 -2.693880842728122e+15 7.400000000000001e-02 6.150000000000000e-02 -1.454586893455663e+15 7.400000000000001e-02 6.300000000000000e-02 -7.635889061688417e+14 7.400000000000001e-02 6.450000000000000e-02 -3.894937441256662e+14 7.400000000000001e-02 6.600000000000000e-02 -1.928858700134613e+14 7.400000000000001e-02 6.750000000000000e-02 -9.262608281067728e+13 7.400000000000001e-02 6.900000000000001e-02 -4.305693949255219e+13 7.400000000000001e-02 7.050000000000001e-02 -1.932565884301771e+13 7.400000000000001e-02 7.200000000000001e-02 -8.344107122826977e+12 7.400000000000001e-02 1.200000000000000e-01 0.000000000000000e+00 7.599999999999998e-02 0.000000000000000e+00 1.989460046056975e+20 7.599999999999998e-02 1.500000000000000e-03 1.970990263270160e+20 7.599999999999998e-02 3.000000000000000e-03 1.922933384424828e+20 7.599999999999998e-02 4.500000000000001e-03 1.847100724375010e+20 7.599999999999998e-02 6.000000000000000e-03 1.746461839728627e+20 7.599999999999998e-02 7.500000000000000e-03 1.624953472907293e+20 7.599999999999998e-02 9.000000000000001e-03 1.487229592736194e+20 7.599999999999998e-02 1.050000000000000e-02 1.338374199452729e+20 7.599999999999998e-02 1.200000000000000e-02 1.183600585710386e+20 7.599999999999998e-02 1.350000000000000e-02 1.027960410764388e+20 7.599999999999998e-02 1.500000000000000e-02 8.760835389783835e+19 7.599999999999998e-02 1.650000000000000e-02 7.319655715965569e+19 7.599999999999998e-02 1.800000000000000e-02 5.988148918255541e+19 7.599999999999998e-02 1.950000000000000e-02 4.789653787139816e+19 7.599999999999998e-02 2.100000000000000e-02 3.738552186254375e+19 7.599999999999998e-02 2.250000000000000e-02 2.840668993016458e+19 7.599999999999998e-02 2.400000000000000e-02 2.094189083375988e+19 7.599999999999998e-02 2.550000000000000e-02 1.490962208055953e+19 7.599999999999998e-02 2.700000000000000e-02 1.018046202637106e+19 7.599999999999998e-02 2.850000000000000e-02 6.593340945288584e+18 7.599999999999998e-02 3.000000000000000e-02 3.971212994790333e+18 7.599999999999998e-02 3.150000000000000e-02 2.134933750864115e+18 7.599999999999998e-02 3.300000000000000e-02 9.144907354018079e+17 7.599999999999998e-02 3.450000000000000e-02 1.571275647299717e+17 7.599999999999998e-02 3.600000000000000e-02 -2.677085055635579e+17 7.599999999999998e-02 3.750000000000000e-02 -4.663306942603717e+17 7.599999999999998e-02 3.900000000000000e-02 -5.211790481244577e+17 7.599999999999998e-02 4.050000000000000e-02 -4.929439359446107e+17 7.599999999999998e-02 4.200000000000000e-02 -4.237730746136041e+17 7.599999999999998e-02 4.350000000000000e-02 -3.409489416794895e+17 7.599999999999998e-02 4.500000000000000e-02 -2.605441925954575e+17 7.599999999999998e-02 4.650000000000000e-02 -1.907118418051787e+17 7.599999999999998e-02 4.800000000000000e-02 -1.344157747066100e+17 7.599999999999998e-02 4.950000000000000e-02 -9.153453187648090e+16 7.599999999999998e-02 5.100000000000000e-02 -6.036555659334823e+16 7.599999999999998e-02 5.250000000000000e-02 -3.861538255068438e+16 7.599999999999998e-02 5.400000000000000e-02 -2.398741240787101e+16 7.599999999999998e-02 5.550000000000000e-02 -1.448071137242290e+16 7.599999999999998e-02 5.700000000000000e-02 -8.499505411221258e+15 7.599999999999998e-02 5.850000000000000e-02 -4.851902555408774e+15 7.599999999999998e-02 6.000000000000000e-02 -2.693873177757519e+15 7.599999999999998e-02 6.150000000000000e-02 -1.454582722094878e+15 7.599999999999998e-02 6.300000000000000e-02 -7.635866875945940e+14 7.599999999999998e-02 6.450000000000000e-02 -3.894925909402687e+14 7.599999999999998e-02 6.600000000000000e-02 -1.928852842082182e+14 7.599999999999998e-02 6.750000000000000e-02 -9.262579198260295e+13 7.599999999999998e-02 6.900000000000001e-02 -4.305679838561862e+13 7.599999999999998e-02 7.050000000000001e-02 -1.932559193327900e+13 7.599999999999998e-02 7.200000000000001e-02 -8.344076115861424e+12 7.599999999999998e-02 1.200000000000000e-01 0.000000000000000e+00 7.799999999999999e-02 0.000000000000000e+00 1.989460058060281e+20 7.799999999999999e-02 1.500000000000000e-03 1.970990279634934e+20 7.799999999999999e-02 3.000000000000000e-03 1.922933406229426e+20 7.799999999999999e-02 4.500000000000001e-03 1.847100752768261e+20 7.799999999999999e-02 6.000000000000000e-03 1.746461875862217e+20 7.799999999999999e-02 7.500000000000000e-03 1.624953517847603e+20 7.799999999999999e-02 9.000000000000001e-03 1.487229647361006e+20 7.799999999999999e-02 1.050000000000000e-02 1.338374264341987e+20 7.799999999999999e-02 1.200000000000000e-02 1.183600661043273e+20 7.799999999999999e-02 1.350000000000000e-02 1.027960496236684e+20 7.799999999999999e-02 1.500000000000000e-02 8.760836337536642e+19 7.799999999999999e-02 1.650000000000000e-02 7.319656743020669e+19 7.799999999999999e-02 1.800000000000000e-02 5.988150005986175e+19 7.799999999999999e-02 1.950000000000000e-02 4.789654912983071e+19 7.799999999999999e-02 2.100000000000000e-02 3.738553325096319e+19 7.799999999999999e-02 2.250000000000000e-02 2.840670118859713e+19 7.799999999999999e-02 2.400000000000000e-02 2.094190171106623e+19 7.799999999999999e-02 2.550000000000000e-02 1.490963235111052e+19 7.799999999999999e-02 2.700000000000000e-02 1.018047150389913e+19 7.799999999999999e-02 2.850000000000000e-02 6.593349492518157e+18 7.799999999999999e-02 3.000000000000000e-02 3.971220528079042e+18 7.799999999999999e-02 3.150000000000000e-02 2.134940239789909e+18 7.799999999999999e-02 3.300000000000000e-02 9.144961978830275e+17 7.799999999999999e-02 3.450000000000000e-02 1.571320587609236e+17 7.799999999999999e-02 3.600000000000000e-02 -2.677048922045379e+17 7.799999999999999e-02 3.750000000000000e-02 -4.663278549352586e+17 7.799999999999999e-02 3.900000000000000e-02 -5.211768676646502e+17 7.799999999999999e-02 4.050000000000000e-02 -4.929422994672522e+17 7.799999999999999e-02 4.200000000000000e-02 -4.237718742830269e+17 7.799999999999999e-02 4.350000000000000e-02 -3.409480812392922e+17 7.799999999999999e-02 4.500000000000000e-02 -2.605435898007007e+17 7.799999999999999e-02 4.650000000000000e-02 -1.907114290930859e+17 7.799999999999999e-02 4.800000000000000e-02 -1.344154985509966e+17 7.799999999999999e-02 4.950000000000000e-02 -9.153435128822227e+16 7.799999999999999e-02 5.100000000000000e-02 -6.036544118051618e+16 7.799999999999999e-02 5.250000000000000e-02 -3.861531046523020e+16 7.799999999999999e-02 5.400000000000000e-02 -2.398736840610235e+16 7.799999999999999e-02 5.550000000000000e-02 -1.448068512288993e+16 7.799999999999999e-02 5.700000000000000e-02 -8.499490107326108e+15 7.799999999999999e-02 5.850000000000000e-02 -4.851893835512167e+15 7.799999999999999e-02 6.000000000000000e-02 -2.693868322082163e+15 7.799999999999999e-02 6.150000000000000e-02 -1.454580079583274e+15 7.799999999999999e-02 6.300000000000000e-02 -7.635852821519829e+14 7.799999999999999e-02 6.450000000000000e-02 -3.894918604098852e+14 7.799999999999999e-02 6.600000000000000e-02 -1.928849131069799e+14 7.799999999999999e-02 6.750000000000000e-02 -9.262560774618691e+13 7.799999999999999e-02 6.900000000000001e-02 -4.305670899591380e+13 7.799999999999999e-02 7.050000000000001e-02 -1.932554954668862e+13 7.799999999999999e-02 7.200000000000001e-02 -8.344056473286615e+12 7.799999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 7.999999999999999e-02 0.000000000000000e+00 1.989460065594417e+20 7.999999999999999e-02 1.500000000000000e-03 1.970990289906641e+20 7.999999999999999e-02 3.000000000000000e-03 1.922933419915558e+20 7.999999999999999e-02 4.500000000000001e-03 1.847100770589904e+20 7.999999999999999e-02 6.000000000000000e-03 1.746461898542253e+20 7.999999999999999e-02 7.500000000000000e-03 1.624953546055368e+20 7.999999999999999e-02 9.000000000000001e-03 1.487229681647461e+20 7.999999999999999e-02 1.050000000000000e-02 1.338374305071145e+20 7.999999999999999e-02 1.200000000000000e-02 1.183600708327602e+20 7.999999999999999e-02 1.350000000000000e-02 1.027960549885234e+20 7.999999999999999e-02 1.500000000000000e-02 8.760836932414358e+19 7.999999999999999e-02 1.650000000000000e-02 7.319657387674196e+19 7.999999999999999e-02 1.800000000000000e-02 5.988150688724025e+19 7.999999999999999e-02 1.950000000000000e-02 4.789655619643138e+19 7.999999999999999e-02 2.100000000000000e-02 3.738554039915296e+19 7.999999999999999e-02 2.250000000000000e-02 2.840670825519780e+19 7.999999999999999e-02 2.400000000000000e-02 2.094190853844473e+19 7.999999999999999e-02 2.550000000000000e-02 1.490963879764580e+19 7.999999999999999e-02 2.700000000000000e-02 1.018047745267628e+19 7.999999999999999e-02 2.850000000000000e-02 6.593354857373165e+18 7.999999999999999e-02 3.000000000000000e-02 3.971225256511956e+18 7.999999999999999e-02 3.150000000000000e-02 2.134944312705669e+18 7.999999999999999e-02 3.300000000000000e-02 9.144996265284700e+17 7.999999999999999e-02 3.450000000000000e-02 1.571348795374392e+17 7.999999999999999e-02 3.600000000000000e-02 -2.677026242009626e+17 7.999999999999999e-02 3.750000000000000e-02 -4.663260727709425e+17 7.999999999999999e-02 3.900000000000000e-02 -5.211754990515092e+17 7.999999999999999e-02 4.050000000000000e-02 -4.929412722965563e+17 7.999999999999999e-02 4.200000000000000e-02 -4.237711208693679e+17 7.999999999999999e-02 4.350000000000000e-02 -3.409475411652413e+17 7.999999999999999e-02 4.500000000000000e-02 -2.605432114434282e+17 7.999999999999999e-02 4.650000000000000e-02 -1.907111700453420e+17 7.999999999999999e-02 4.800000000000000e-02 -1.344153252159044e+17 7.999999999999999e-02 4.950000000000000e-02 -9.153423793806416e+16 7.999999999999999e-02 5.100000000000000e-02 -6.036536873913566e+16 7.999999999999999e-02 5.250000000000000e-02 -3.861526521922312e+16 7.999999999999999e-02 5.400000000000000e-02 -2.398734078743283e+16 7.999999999999999e-02 5.550000000000000e-02 -1.448066864679822e+16 7.999999999999999e-02 5.700000000000000e-02 -8.499480501502630e+15 7.999999999999999e-02 5.850000000000000e-02 -4.851888362278931e+15 7.999999999999999e-02 6.000000000000000e-02 -2.693865274311652e+15 7.999999999999999e-02 6.150000000000000e-02 -1.454578420953249e+15 7.999999999999999e-02 6.300000000000000e-02 -7.635843999952835e+14 7.999999999999999e-02 6.450000000000000e-02 -3.894914018765614e+14 7.999999999999999e-02 6.600000000000000e-02 -1.928846801771962e+14 7.999999999999999e-02 6.750000000000000e-02 -9.262549210618323e+13 7.999999999999999e-02 6.900000000000001e-02 -4.305665288851650e+13 7.999999999999999e-02 7.050000000000001e-02 -1.932552294182096e+13 7.999999999999999e-02 7.200000000000001e-02 -8.344044144196246e+12 7.999999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 8.199999999999999e-02 0.000000000000000e+00 1.989460070280015e+20 8.199999999999999e-02 1.500000000000000e-03 1.970990296294776e+20 8.199999999999999e-02 3.000000000000000e-03 1.922933428427176e+20 8.199999999999999e-02 4.500000000000001e-03 1.847100781673462e+20 8.199999999999999e-02 6.000000000000000e-03 1.746461912647321e+20 8.199999999999999e-02 7.500000000000000e-03 1.624953563598218e+20 8.199999999999999e-02 9.000000000000001e-03 1.487229702970742e+20 8.199999999999999e-02 1.050000000000000e-02 1.338374330401243e+20 8.199999999999999e-02 1.200000000000000e-02 1.183600737734464e+20 8.199999999999999e-02 1.350000000000000e-02 1.027960583250104e+20 8.199999999999999e-02 1.500000000000000e-02 8.760837302378095e+19 8.199999999999999e-02 1.650000000000000e-02 7.319657788594287e+19 8.199999999999999e-02 1.800000000000000e-02 5.988151113329352e+19 8.199999999999999e-02 1.950000000000000e-02 4.789656059126066e+19 8.199999999999999e-02 2.100000000000000e-02 3.738554484472377e+19 8.199999999999999e-02 2.250000000000000e-02 2.840671265002707e+19 8.199999999999999e-02 2.400000000000000e-02 2.094191278449800e+19 8.199999999999999e-02 2.550000000000000e-02 1.490964280684672e+19 8.199999999999999e-02 2.700000000000000e-02 1.018048115231365e+19 8.199999999999999e-02 2.850000000000000e-02 6.593358193860242e+18 8.199999999999999e-02 3.000000000000000e-02 3.971228197198198e+18 8.199999999999999e-02 3.150000000000000e-02 2.134946845715561e+18 8.199999999999999e-02 3.300000000000000e-02 9.145017588565934e+17 8.199999999999999e-02 3.450000000000000e-02 1.571366338223882e+17 8.199999999999999e-02 3.600000000000000e-02 -2.677012136941343e+17 8.199999999999999e-02 3.750000000000000e-02 -4.663249644151334e+17 8.199999999999999e-02 3.900000000000000e-02 -5.211746478896317e+17 8.199999999999999e-02 4.050000000000000e-02 -4.929406334830656e+17 8.199999999999999e-02 4.200000000000000e-02 -4.237706523096521e+17 8.199999999999999e-02 4.350000000000000e-02 -3.409472052847580e+17 8.199999999999999e-02 4.500000000000000e-02 -2.605429761371340e+17 8.199999999999999e-02 4.650000000000000e-02 -1.907110089395061e+17 8.199999999999999e-02 4.800000000000000e-02 -1.344152174161048e+17 8.199999999999999e-02 4.950000000000000e-02 -9.153416744383136e+16 8.199999999999999e-02 5.100000000000000e-02 -6.036532368671026e+16 8.199999999999999e-02 5.250000000000000e-02 -3.861523708002500e+16 8.199999999999999e-02 5.400000000000000e-02 -2.398732361095111e+16 8.199999999999999e-02 5.550000000000000e-02 -1.448065840005958e+16 8.199999999999999e-02 5.700000000000000e-02 -8.499474527491055e+15 8.199999999999999e-02 5.850000000000000e-02 -4.851884958389741e+15 8.199999999999999e-02 6.000000000000000e-02 -2.693863378855594e+15 8.199999999999999e-02 6.150000000000000e-02 -1.454577389425343e+15 8.199999999999999e-02 6.300000000000000e-02 -7.635838513682612e+14 8.199999999999999e-02 6.450000000000000e-02 -3.894911167075292e+14 8.199999999999999e-02 6.600000000000000e-02 -1.928845353145275e+14 8.199999999999999e-02 6.750000000000000e-02 -9.262542018785975e+13 8.199999999999999e-02 6.900000000000001e-02 -4.305661799445024e+13 8.199999999999999e-02 7.050000000000001e-02 -1.932550639583845e+13 8.199999999999999e-02 7.200000000000001e-02 -8.344036476542480e+12 8.199999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 8.399999999999999e-02 0.000000000000000e+00 1.989460073167371e+20 8.399999999999999e-02 1.500000000000000e-03 1.970990300231269e+20 8.399999999999999e-02 3.000000000000000e-03 1.922933433672201e+20 8.399999999999999e-02 4.500000000000001e-03 1.847100788503366e+20 8.399999999999999e-02 6.000000000000000e-03 1.746461921339138e+20 8.399999999999999e-02 7.500000000000000e-03 1.624953574408462e+20 8.399999999999999e-02 9.000000000000001e-03 1.487229716110562e+20 8.399999999999999e-02 1.050000000000000e-02 1.338374346010142e+20 8.399999999999999e-02 1.200000000000000e-02 1.183600755855544e+20 8.399999999999999e-02 1.350000000000000e-02 1.027960603810186e+20 8.399999999999999e-02 1.500000000000000e-02 8.760837530356933e+19 8.399999999999999e-02 1.650000000000000e-02 7.319658035649033e+19 8.399999999999999e-02 1.800000000000000e-02 5.988151374979399e+19 8.399999999999999e-02 1.950000000000000e-02 4.789656329943979e+19 8.399999999999999e-02 2.100000000000000e-02 3.738554758417082e+19 8.399999999999999e-02 2.250000000000000e-02 2.840671535820621e+19 8.399999999999999e-02 2.400000000000000e-02 2.094191540099847e+19 8.399999999999999e-02 2.550000000000000e-02 1.490964527739417e+19 8.399999999999999e-02 2.700000000000000e-02 1.018048343210203e+19 8.399999999999999e-02 2.850000000000000e-02 6.593360249868363e+18 8.399999999999999e-02 3.000000000000000e-02 3.971230009306160e+18 8.399999999999999e-02 3.150000000000000e-02 2.134948406605439e+18 8.399999999999999e-02 3.300000000000000e-02 9.145030728385853e+17 8.399999999999999e-02 3.450000000000000e-02 1.571377148468362e+17 8.399999999999999e-02 3.600000000000000e-02 -2.677003445124393e+17 8.399999999999999e-02 3.750000000000000e-02 -4.663242814247636e+17 8.399999999999999e-02 3.900000000000000e-02 -5.211741233871562e+17 8.399999999999999e-02 4.050000000000000e-02 -4.929402398337892e+17 8.399999999999999e-02 4.200000000000000e-02 -4.237703635740575e+17 8.399999999999999e-02 4.350000000000000e-02 -3.409469983086826e+17 8.399999999999999e-02 4.500000000000000e-02 -2.605428311368267e+17 8.399999999999999e-02 4.650000000000000e-02 -1.907109096629620e+17 8.399999999999999e-02 4.800000000000000e-02 -1.344151509877751e+17 8.399999999999999e-02 4.950000000000000e-02 -9.153412400391635e+16 8.399999999999999e-02 5.100000000000000e-02 -6.036529592453097e+16 8.399999999999999e-02 5.250000000000000e-02 -3.861521974010475e+16 8.399999999999999e-02 5.400000000000000e-02 -2.398731302646957e+16 8.399999999999999e-02 5.550000000000000e-02 -1.448065208582027e+16 8.399999999999999e-02 5.700000000000000e-02 -8.499470846189128e+15 8.399999999999999e-02 5.850000000000000e-02 -4.851882860847130e+15 8.399999999999999e-02 6.000000000000000e-02 -2.693862210838767e+15 8.399999999999999e-02 6.150000000000000e-02 -1.454576753777820e+15 8.399999999999999e-02 6.300000000000000e-02 -7.635835132936376e+14 8.399999999999999e-02 6.450000000000000e-02 -3.894909409808347e+14 8.399999999999999e-02 6.600000000000000e-02 -1.928844460473383e+14 8.399999999999999e-02 6.750000000000000e-02 -9.262537587039241e+13 8.399999999999999e-02 6.900000000000001e-02 -4.305659649204909e+13 8.399999999999999e-02 7.050000000000001e-02 -1.932549619988276e+13 8.399999999999999e-02 7.200000000000001e-02 -8.344031751585352e+12 8.399999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 8.599999999999999e-02 0.000000000000000e+00 1.989460074930339e+20 8.599999999999999e-02 1.500000000000000e-03 1.970990302634821e+20 8.599999999999999e-02 3.000000000000000e-03 1.922933436874720e+20 8.599999999999999e-02 4.500000000000001e-03 1.847100792673584e+20 8.599999999999999e-02 6.000000000000000e-03 1.746461926646207e+20 8.599999999999999e-02 7.500000000000000e-03 1.624953581009004e+20 8.599999999999999e-02 9.000000000000001e-03 1.487229724133502e+20 8.599999999999999e-02 1.050000000000000e-02 1.338374355540657e+20 8.599999999999999e-02 1.200000000000000e-02 1.183600766919952e+20 8.599999999999999e-02 1.350000000000000e-02 1.027960616363805e+20 8.599999999999999e-02 1.500000000000000e-02 8.760837669556745e+19 8.599999999999999e-02 1.650000000000000e-02 7.319658186496254e+19 8.599999999999999e-02 1.800000000000000e-02 5.988151534738252e+19 8.599999999999999e-02 1.950000000000000e-02 4.789656495300566e+19 8.599999999999999e-02 2.100000000000000e-02 3.738554925682833e+19 8.599999999999999e-02 2.250000000000000e-02 2.840671701177208e+19 8.599999999999999e-02 2.400000000000000e-02 2.094191699858699e+19 8.599999999999999e-02 2.550000000000000e-02 1.490964678586639e+19 8.599999999999999e-02 2.700000000000000e-02 1.018048482410016e+19 8.599999999999999e-02 2.850000000000000e-02 6.593361505230255e+18 8.599999999999999e-02 3.000000000000000e-02 3.971231115746964e+18 8.599999999999999e-02 3.150000000000000e-02 2.134949359656961e+18 8.599999999999999e-02 3.300000000000000e-02 9.145038751325573e+17 8.599999999999999e-02 3.450000000000000e-02 1.571383749010852e+17 8.599999999999999e-02 3.600000000000000e-02 -2.676998138055972e+17 8.599999999999999e-02 3.750000000000000e-02 -4.663238644030239e+17 8.599999999999999e-02 3.900000000000000e-02 -5.211738031352986e+17 8.599999999999999e-02 4.050000000000000e-02 -4.929399994785612e+17 8.599999999999999e-02 4.200000000000000e-02 -4.237701872772525e+17 8.599999999999999e-02 4.350000000000000e-02 -3.409468719327821e+17 8.599999999999999e-02 4.500000000000000e-02 -2.605427426022249e+17 8.599999999999999e-02 4.650000000000000e-02 -1.907108490464746e+17 8.599999999999999e-02 4.800000000000000e-02 -1.344151104278217e+17 8.599999999999999e-02 4.950000000000000e-02 -9.153409748027894e+16 8.599999999999999e-02 5.100000000000000e-02 -6.036527897343940e+16 8.599999999999999e-02 5.250000000000000e-02 -3.861520915265869e+16 8.599999999999999e-02 5.400000000000000e-02 -2.398730656377390e+16 8.599999999999999e-02 5.550000000000000e-02 -1.448064823045835e+16 8.599999999999999e-02 5.700000000000000e-02 -8.499468598451823e+15 8.599999999999999e-02 5.850000000000000e-02 -4.851881580125020e+15 8.599999999999999e-02 6.000000000000000e-02 -2.693861497668523e+15 8.599999999999999e-02 6.150000000000000e-02 -1.454576365662777e+15 8.599999999999999e-02 6.300000000000000e-02 -7.635833068713015e+14 8.599999999999999e-02 6.450000000000000e-02 -3.894908336852489e+14 8.599999999999999e-02 6.600000000000000e-02 -1.928843915423846e+14 8.599999999999999e-02 6.750000000000000e-02 -9.262534881093719e+13 8.599999999999999e-02 6.900000000000001e-02 -4.305658336306642e+13 8.599999999999999e-02 7.050000000000001e-02 -1.932548997441404e+13 8.599999999999999e-02 7.200000000000001e-02 -8.344028866610793e+12 8.599999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 8.799999999999999e-02 0.000000000000000e+00 1.989460075996939e+20 8.799999999999999e-02 1.500000000000000e-03 1.970990304088977e+20 8.799999999999999e-02 3.000000000000000e-03 1.922933438812252e+20 8.799999999999999e-02 4.500000000000001e-03 1.847100795196577e+20 8.799999999999999e-02 6.000000000000000e-03 1.746461929856998e+20 8.799999999999999e-02 7.500000000000000e-03 1.624953585002351e+20 8.799999999999999e-02 9.000000000000001e-03 1.487229728987403e+20 8.799999999999999e-02 1.050000000000000e-02 1.338374361306646e+20 8.799999999999999e-02 1.200000000000000e-02 1.183600773613950e+20 8.799999999999999e-02 1.350000000000000e-02 1.027960623958780e+20 8.799999999999999e-02 1.500000000000000e-02 8.760837753773028e+19 8.799999999999999e-02 1.650000000000000e-02 7.319658277759255e+19 8.799999999999999e-02 1.800000000000000e-02 5.988151631392813e+19 8.799999999999999e-02 1.950000000000000e-02 4.789656595341774e+19 8.799999999999999e-02 2.100000000000000e-02 3.738555026879090e+19 8.799999999999999e-02 2.250000000000000e-02 2.840671801218416e+19 8.799999999999999e-02 2.400000000000000e-02 2.094191796513261e+19 8.799999999999999e-02 2.550000000000000e-02 1.490964769849638e+19 8.799999999999999e-02 2.700000000000000e-02 1.018048566626299e+19 8.799999999999999e-02 2.850000000000000e-02 6.593362264727780e+18 8.799999999999999e-02 3.000000000000000e-02 3.971231785146805e+18 8.799999999999999e-02 3.150000000000000e-02 2.134949936255852e+18 8.799999999999999e-02 3.300000000000000e-02 9.145043605226977e+17 8.799999999999999e-02 3.450000000000000e-02 1.571387742357888e+17 8.799999999999999e-02 3.600000000000000e-02 -2.676994927264440e+17 8.799999999999999e-02 3.750000000000000e-02 -4.663236121036820e+17 8.799999999999999e-02 3.900000000000000e-02 -5.211736093820111e+17 8.799999999999999e-02 4.050000000000000e-02 -4.929398540629627e+17 8.799999999999999e-02 4.200000000000000e-02 -4.237700806171827e+17 8.799999999999999e-02 4.350000000000000e-02 -3.409467954750019e+17 8.799999999999999e-02 4.500000000000000e-02 -2.605426890385383e+17 8.799999999999999e-02 4.650000000000000e-02 -1.907108123733268e+17 8.799999999999999e-02 4.800000000000000e-02 -1.344150858889342e+17 8.799999999999999e-02 4.950000000000000e-02 -9.153408143340266e+16 8.799999999999999e-02 5.100000000000000e-02 -6.036526871798065e+16 8.799999999999999e-02 5.250000000000000e-02 -3.861520274722362e+16 8.799999999999999e-02 5.400000000000000e-02 -2.398730265382458e+16 8.799999999999999e-02 5.550000000000000e-02 -1.448064589795340e+16 8.799999999999999e-02 5.700000000000000e-02 -8.499467238564342e+15 8.799999999999999e-02 5.850000000000000e-02 -4.851880805284490e+15 8.799999999999999e-02 6.000000000000000e-02 -2.693861066198492e+15 8.799999999999999e-02 6.150000000000000e-02 -1.454576130852070e+15 8.799999999999999e-02 6.300000000000000e-02 -7.635831819851995e+14 8.799999999999999e-02 6.450000000000000e-02 -3.894907687711134e+14 8.799999999999999e-02 6.600000000000000e-02 -1.928843585667321e+14 8.799999999999999e-02 6.750000000000000e-02 -9.262533243988962e+13 8.799999999999999e-02 6.900000000000001e-02 -4.305657541999445e+13 8.799999999999999e-02 7.050000000000001e-02 -1.932548620798771e+13 8.799999999999999e-02 7.200000000000001e-02 -8.344027121192955e+12 8.799999999999999e-02 1.200000000000000e-01 0.000000000000000e+00 9.000000000000000e-02 0.000000000000000e+00 1.989460076636346e+20 9.000000000000000e-02 1.500000000000000e-03 1.970990304960715e+20 9.000000000000000e-02 3.000000000000000e-03 1.922933439973766e+20 9.000000000000000e-02 4.500000000000001e-03 1.847100796709063e+20 9.000000000000000e-02 6.000000000000000e-03 1.746461931781805e+20 9.000000000000000e-02 7.500000000000000e-03 1.624953587396285e+20 9.000000000000000e-02 9.000000000000001e-03 1.487229731897222e+20 9.000000000000000e-02 1.050000000000000e-02 1.338374364763244e+20 9.000000000000000e-02 1.200000000000000e-02 1.183600777626872e+20 9.000000000000000e-02 1.350000000000000e-02 1.027960628511820e+20 9.000000000000000e-02 1.500000000000000e-02 8.760837804259049e+19 9.000000000000000e-02 1.650000000000000e-02 7.319658332469643e+19 9.000000000000000e-02 1.800000000000000e-02 5.988151689335339e+19 9.000000000000000e-02 1.950000000000000e-02 4.789656655314528e+19 9.000000000000000e-02 2.100000000000000e-02 3.738555087544273e+19 9.000000000000000e-02 2.250000000000000e-02 2.840671861191170e+19 9.000000000000000e-02 2.400000000000000e-02 2.094191854455787e+19 9.000000000000000e-02 2.550000000000000e-02 1.490964824560027e+19 9.000000000000000e-02 2.700000000000000e-02 1.018048617112320e+19 9.000000000000000e-02 2.850000000000000e-02 6.593362720031743e+18 9.000000000000000e-02 3.000000000000000e-02 3.971232186438964e+18 9.000000000000000e-02 3.150000000000000e-02 2.134950281915648e+18 9.000000000000000e-02 3.300000000000000e-02 9.145046515046277e+17 9.000000000000000e-02 3.450000000000000e-02 1.571390136291604e+17 9.000000000000000e-02 3.600000000000000e-02 -2.676993002457498e+17 9.000000000000000e-02 3.750000000000000e-02 -4.663234608551439e+17 9.000000000000000e-02 3.900000000000000e-02 -5.211734932306916e+17 9.000000000000000e-02 4.050000000000000e-02 -4.929397668891455e+17 9.000000000000000e-02 4.200000000000000e-02 -4.237700166765496e+17 9.000000000000000e-02 4.350000000000000e-02 -3.409467496400528e+17 9.000000000000000e-02 4.500000000000000e-02 -2.605426569281522e+17 9.000000000000000e-02 4.650000000000000e-02 -1.907107903884895e+17 9.000000000000000e-02 4.800000000000000e-02 -1.344150711783494e+17 9.000000000000000e-02 4.950000000000000e-02 -9.153407181361309e+16 9.000000000000000e-02 5.100000000000000e-02 -6.036526257003300e+16 9.000000000000000e-02 5.250000000000000e-02 -3.861519890729013e+16 9.000000000000000e-02 5.400000000000000e-02 -2.398730030988618e+16 9.000000000000000e-02 5.550000000000000e-02 -1.448064449966214e+16 9.000000000000000e-02 5.700000000000000e-02 -8.499466423338302e+15 9.000000000000000e-02 5.850000000000000e-02 -4.851880340782694e+15 9.000000000000000e-02 6.000000000000000e-02 -2.693860807540617e+15 9.000000000000000e-02 6.150000000000000e-02 -1.454575990087627e+15 9.000000000000000e-02 6.300000000000000e-02 -7.635831071184152e+14 9.000000000000000e-02 6.450000000000000e-02 -3.894907298563544e+14 9.000000000000000e-02 6.600000000000000e-02 -1.928843387984711e+14 9.000000000000000e-02 6.750000000000000e-02 -9.262532262576566e+13 9.000000000000000e-02 6.900000000000001e-02 -4.305657065827762e+13 9.000000000000000e-02 7.050000000000001e-02 -1.932548395008854e+13 9.000000000000000e-02 7.200000000000001e-02 -8.344026074848979e+12 9.000000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 9.200000000000000e-02 0.000000000000000e+00 1.989460077016162e+20 9.200000000000000e-02 1.500000000000000e-03 1.970990305478540e+20 9.200000000000000e-02 3.000000000000000e-03 1.922933440663721e+20 9.200000000000000e-02 4.500000000000001e-03 1.847100797607500e+20 9.200000000000000e-02 6.000000000000000e-03 1.746461932925168e+20 9.200000000000000e-02 7.500000000000000e-03 1.624953588818316e+20 9.200000000000000e-02 9.000000000000001e-03 1.487229733625696e+20 9.200000000000000e-02 1.050000000000000e-02 1.338374366816513e+20 9.200000000000000e-02 1.200000000000000e-02 1.183600780010604e+20 9.200000000000000e-02 1.350000000000000e-02 1.027960631216390e+20 9.200000000000000e-02 1.500000000000000e-02 8.760837834248464e+19 9.200000000000000e-02 1.650000000000000e-02 7.319658364968391e+19 9.200000000000000e-02 1.800000000000000e-02 5.988151723754023e+19 9.200000000000000e-02 1.950000000000000e-02 4.789656690939196e+19 9.200000000000000e-02 2.100000000000000e-02 3.738555123580255e+19 9.200000000000000e-02 2.250000000000000e-02 2.840671896815838e+19 9.200000000000000e-02 2.400000000000000e-02 2.094191888874471e+19 9.200000000000000e-02 2.550000000000000e-02 1.490964857058776e+19 9.200000000000000e-02 2.700000000000000e-02 1.018048647101734e+19 9.200000000000000e-02 2.850000000000000e-02 6.593362990488770e+18 9.200000000000000e-02 3.000000000000000e-02 3.971232424812211e+18 9.200000000000000e-02 3.150000000000000e-02 2.134950487242481e+18 9.200000000000000e-02 3.300000000000000e-02 9.145048243520297e+17 9.200000000000000e-02 3.450000000000000e-02 1.571391558322258e+17 9.200000000000000e-02 3.600000000000000e-02 -2.676991859094810e+17 9.200000000000000e-02 3.750000000000000e-02 -4.663233710113620e+17 9.200000000000000e-02 3.900000000000000e-02 -5.211734242351567e+17 9.200000000000000e-02 4.050000000000000e-02 -4.929397151066589e+17 9.200000000000000e-02 4.200000000000000e-02 -4.237699786949047e+17 9.200000000000000e-02 4.350000000000000e-02 -3.409467224134415e+17 9.200000000000000e-02 4.500000000000000e-02 -2.605426378541263e+17 9.200000000000000e-02 4.650000000000000e-02 -1.907107773291836e+17 9.200000000000000e-02 4.800000000000000e-02 -1.344150624400529e+17 9.200000000000000e-02 4.950000000000000e-02 -9.153406609932133e+16 9.200000000000000e-02 5.100000000000000e-02 -6.036525891806471e+16 9.200000000000000e-02 5.250000000000000e-02 -3.861519662631506e+16 9.200000000000000e-02 5.400000000000000e-02 -2.398729891755344e+16 9.200000000000000e-02 5.550000000000000e-02 -1.448064366905725e+16 9.200000000000000e-02 5.700000000000000e-02 -8.499465939082445e+15 9.200000000000000e-02 5.850000000000000e-02 -4.851880064862024e+15 9.200000000000000e-02 6.000000000000000e-02 -2.693860653894162e+15 9.200000000000000e-02 6.150000000000000e-02 -1.454575906471547e+15 9.200000000000000e-02 6.300000000000000e-02 -7.635830626464812e+14 9.200000000000000e-02 6.450000000000000e-02 -3.894907067404343e+14 9.200000000000000e-02 6.600000000000000e-02 -1.928843270558431e+14 9.200000000000000e-02 6.750000000000000e-02 -9.262531679603653e+13 9.200000000000000e-02 6.900000000000001e-02 -4.305656782975014e+13 9.200000000000000e-02 7.050000000000001e-02 -1.932548260886433e+13 9.200000000000000e-02 7.200000000000001e-02 -8.344025453305785e+12 9.200000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 9.400000000000000e-02 0.000000000000000e+00 1.989460077239723e+20 9.400000000000000e-02 1.500000000000000e-03 1.970990305783333e+20 9.400000000000000e-02 3.000000000000000e-03 1.922933441069831e+20 9.400000000000000e-02 4.500000000000001e-03 1.847100798136324e+20 9.400000000000000e-02 6.000000000000000e-03 1.746461933598154e+20 9.400000000000000e-02 7.500000000000000e-03 1.624953589655328e+20 9.400000000000000e-02 9.000000000000001e-03 1.487229734643081e+20 9.400000000000000e-02 1.050000000000000e-02 1.338374368025073e+20 9.400000000000000e-02 1.200000000000000e-02 1.183600781413677e+20 9.400000000000000e-02 1.350000000000000e-02 1.027960632808308e+20 9.400000000000000e-02 1.500000000000000e-02 8.760837851900325e+19 9.400000000000000e-02 1.650000000000000e-02 7.319658384097255e+19 9.400000000000000e-02 1.800000000000000e-02 5.988151744012965e+19 9.400000000000000e-02 1.950000000000000e-02 4.789656711907986e+19 9.400000000000000e-02 2.100000000000000e-02 3.738555144791144e+19 9.400000000000000e-02 2.250000000000000e-02 2.840671917784628e+19 9.400000000000000e-02 2.400000000000000e-02 2.094191909133414e+19 9.400000000000000e-02 2.550000000000000e-02 1.490964876187640e+19 9.400000000000000e-02 2.700000000000000e-02 1.018048664753596e+19 9.400000000000000e-02 2.850000000000000e-02 6.593363149680608e+18 9.400000000000000e-02 3.000000000000000e-02 3.971232565119440e+18 9.400000000000000e-02 3.150000000000000e-02 2.134950608098486e+18 9.400000000000000e-02 3.300000000000000e-02 9.145049260905431e+17 9.400000000000000e-02 3.450000000000000e-02 1.571392395333883e+17 9.400000000000000e-02 3.600000000000000e-02 -2.676991186108012e+17 9.400000000000000e-02 3.750000000000000e-02 -4.663233181290355e+17 9.400000000000000e-02 3.900000000000000e-02 -5.211733836241723e+17 9.400000000000000e-02 4.050000000000000e-02 -4.929396846273279e+17 9.400000000000000e-02 4.200000000000000e-02 -4.237699563387916e+17 9.400000000000000e-02 4.350000000000000e-02 -3.409467063877742e+17 9.400000000000000e-02 4.500000000000000e-02 -2.605426266270960e+17 9.400000000000000e-02 4.650000000000000e-02 -1.907107696424359e+17 9.400000000000000e-02 4.800000000000000e-02 -1.344150572966647e+17 9.400000000000000e-02 4.950000000000000e-02 -9.153406273587160e+16 9.400000000000000e-02 5.100000000000000e-02 -6.036525676850493e+16 9.400000000000000e-02 5.250000000000000e-02 -3.861519528372611e+16 9.400000000000000e-02 5.400000000000000e-02 -2.398729809802210e+16 9.400000000000000e-02 5.550000000000000e-02 -1.448064318016066e+16 9.400000000000000e-02 5.700000000000000e-02 -8.499465654047956e+15 9.400000000000000e-02 5.850000000000000e-02 -4.851879902454268e+15 9.400000000000000e-02 6.000000000000000e-02 -2.693860563457386e+15 9.400000000000000e-02 6.150000000000000e-02 -1.454575857254865e+15 9.400000000000000e-02 6.300000000000000e-02 -7.635830364701640e+14 9.400000000000000e-02 6.450000000000000e-02 -3.894906931343326e+14 9.400000000000000e-02 6.600000000000000e-02 -1.928843201440961e+14 9.400000000000000e-02 6.750000000000000e-02 -9.262531336464000e+13 9.400000000000000e-02 6.900000000000001e-02 -4.305656616487015e+13 9.400000000000000e-02 7.050000000000001e-02 -1.932548181941563e+13 9.400000000000000e-02 7.200000000000001e-02 -8.344025087463545e+12 9.400000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 9.600000000000000e-02 0.000000000000000e+00 1.989460077370114e+20 9.600000000000000e-02 1.500000000000000e-03 1.970990305961103e+20 9.600000000000000e-02 3.000000000000000e-03 1.922933441306693e+20 9.600000000000000e-02 4.500000000000001e-03 1.847100798444758e+20 9.600000000000000e-02 6.000000000000000e-03 1.746461933990671e+20 9.600000000000000e-02 7.500000000000000e-03 1.624953590143511e+20 9.600000000000000e-02 9.000000000000001e-03 1.487229735236467e+20 9.600000000000000e-02 1.050000000000000e-02 1.338374368729961e+20 9.600000000000000e-02 1.200000000000000e-02 1.183600782232013e+20 9.600000000000000e-02 1.350000000000000e-02 1.027960633736789e+20 9.600000000000000e-02 1.500000000000000e-02 8.760837862195708e+19 9.600000000000000e-02 1.650000000000000e-02 7.319658395254094e+19 9.600000000000000e-02 1.800000000000000e-02 5.988151755828919e+19 9.600000000000000e-02 1.950000000000000e-02 4.789656724137954e+19 9.600000000000000e-02 2.100000000000000e-02 3.738555157162317e+19 9.600000000000000e-02 2.250000000000000e-02 2.840671930014595e+19 9.600000000000000e-02 2.400000000000000e-02 2.094191920949367e+19 9.600000000000000e-02 2.550000000000000e-02 1.490964887344478e+19 9.600000000000000e-02 2.700000000000000e-02 1.018048675048978e+19 9.600000000000000e-02 2.850000000000000e-02 6.593363242528652e+18 9.600000000000000e-02 3.000000000000000e-02 3.971232646953104e+18 9.600000000000000e-02 3.150000000000000e-02 2.134950678587299e+18 9.600000000000000e-02 3.300000000000000e-02 9.145049854291497e+17 9.600000000000000e-02 3.450000000000000e-02 1.571392883517778e+17 9.600000000000000e-02 3.600000000000000e-02 -2.676990793590984e+17 9.600000000000000e-02 3.750000000000000e-02 -4.663232872856166e+17 9.600000000000000e-02 3.900000000000000e-02 -5.211733599379679e+17 9.600000000000000e-02 4.050000000000000e-02 -4.929396668503722e+17 9.600000000000000e-02 4.200000000000000e-02 -4.237699432996723e+17 9.600000000000000e-02 4.350000000000000e-02 -3.409466970408639e+17 9.600000000000000e-02 4.500000000000000e-02 -2.605426200789726e+17 9.600000000000000e-02 4.650000000000000e-02 -1.907107651591692e+17 9.600000000000000e-02 4.800000000000000e-02 -1.344150542968028e+17 9.600000000000000e-02 4.950000000000000e-02 -9.153406077415216e+16 9.600000000000000e-02 5.100000000000000e-02 -6.036525551478223e+16 9.600000000000000e-02 5.250000000000000e-02 -3.861519450066613e+16 9.600000000000000e-02 5.400000000000000e-02 -2.398729762003352e+16 9.600000000000000e-02 5.550000000000000e-02 -1.448064289501356e+16 9.600000000000000e-02 5.700000000000000e-02 -8.499465487802659e+15 9.600000000000000e-02 5.850000000000000e-02 -4.851879807730552e+15 9.600000000000000e-02 6.000000000000000e-02 -2.693860510710475e+15 9.600000000000000e-02 6.150000000000000e-02 -1.454575828549420e+15 9.600000000000000e-02 6.300000000000000e-02 -7.635830212029250e+14 9.600000000000000e-02 6.450000000000000e-02 -3.894906851986247e+14 9.600000000000000e-02 6.600000000000000e-02 -1.928843161128455e+14 9.600000000000000e-02 6.750000000000000e-02 -9.262531136329083e+13 9.600000000000000e-02 6.900000000000001e-02 -4.305656519383513e+13 9.600000000000000e-02 7.050000000000001e-02 -1.932548135897264e+13 9.600000000000000e-02 7.200000000000001e-02 -8.344024874087430e+12 9.600000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 9.800000000000000e-02 0.000000000000000e+00 1.989460077445473e+20 9.800000000000000e-02 1.500000000000000e-03 1.970990306063843e+20 9.800000000000000e-02 3.000000000000000e-03 1.922933441443586e+20 9.800000000000000e-02 4.500000000000001e-03 1.847100798623015e+20 9.800000000000000e-02 6.000000000000000e-03 1.746461934217524e+20 9.800000000000000e-02 7.500000000000000e-03 1.624953590425654e+20 9.800000000000000e-02 9.000000000000001e-03 1.487229735579411e+20 9.800000000000000e-02 1.050000000000000e-02 1.338374369137346e+20 9.800000000000000e-02 1.200000000000000e-02 1.183600782704965e+20 9.800000000000000e-02 1.350000000000000e-02 1.027960634273397e+20 9.800000000000000e-02 1.500000000000000e-02 8.760837868145851e+19 9.800000000000000e-02 1.650000000000000e-02 7.319658401702109e+19 9.800000000000000e-02 1.800000000000000e-02 5.988151762657865e+19 9.800000000000000e-02 1.950000000000000e-02 4.789656731206177e+19 9.800000000000000e-02 2.100000000000000e-02 3.738555164312148e+19 9.800000000000000e-02 2.250000000000000e-02 2.840671937082819e+19 9.800000000000000e-02 2.400000000000000e-02 2.094191927778313e+19 9.800000000000000e-02 2.550000000000000e-02 1.490964893792494e+19 9.800000000000000e-02 2.700000000000000e-02 1.018048680999121e+19 9.800000000000000e-02 2.850000000000000e-02 6.593363296189521e+18 9.800000000000000e-02 3.000000000000000e-02 3.971232694248289e+18 9.800000000000000e-02 3.150000000000000e-02 2.134950719325809e+18 9.800000000000000e-02 3.300000000000000e-02 9.145050197234770e+17 9.800000000000000e-02 3.450000000000000e-02 1.571393165660201e+17 9.800000000000000e-02 3.600000000000000e-02 -2.676990566738550e+17 9.800000000000000e-02 3.750000000000000e-02 -4.663232694598815e+17 9.800000000000000e-02 3.900000000000000e-02 -5.211733462486940e+17 9.800000000000000e-02 4.050000000000000e-02 -4.929396565763067e+17 9.800000000000000e-02 4.200000000000000e-02 -4.237699357638058e+17 9.800000000000000e-02 4.350000000000000e-02 -3.409466916388833e+17 9.800000000000000e-02 4.500000000000000e-02 -2.605426162945311e+17 9.800000000000000e-02 4.650000000000000e-02 -1.907107625680969e+17 9.800000000000000e-02 4.800000000000000e-02 -1.344150525630538e+17 9.800000000000000e-02 4.950000000000000e-02 -9.153405964039030e+16 9.800000000000000e-02 5.100000000000000e-02 -6.036525479020210e+16 9.800000000000000e-02 5.250000000000000e-02 -3.861519404810217e+16 9.800000000000000e-02 5.400000000000000e-02 -2.398729734378342e+16 9.800000000000000e-02 5.550000000000000e-02 -1.448064273021481e+16 9.800000000000000e-02 5.700000000000000e-02 -8.499465391722368e+15 9.800000000000000e-02 5.850000000000000e-02 -4.851879752985652e+15 9.800000000000000e-02 6.000000000000000e-02 -2.693860480225772e+15 9.800000000000000e-02 6.150000000000000e-02 -1.454575811959311e+15 9.800000000000000e-02 6.300000000000000e-02 -7.635830123793324e+14 9.800000000000000e-02 6.450000000000000e-02 -3.894906806122386e+14 9.800000000000000e-02 6.600000000000000e-02 -1.928843137830128e+14 9.800000000000000e-02 6.750000000000000e-02 -9.262531020662527e+13 9.800000000000000e-02 6.900000000000001e-02 -4.305656463263233e+13 9.800000000000000e-02 7.050000000000001e-02 -1.932548109286287e+13 9.800000000000000e-02 7.200000000000001e-02 -8.344024750768217e+12 9.800000000000000e-02 1.200000000000000e-01 0.000000000000000e+00 1.000000000000000e-01 0.000000000000000e+00 1.989460077488630e+20 1.000000000000000e-01 1.500000000000000e-03 1.970990306122682e+20 1.000000000000000e-01 3.000000000000000e-03 1.922933441521983e+20 1.000000000000000e-01 4.500000000000001e-03 1.847100798725102e+20 1.000000000000000e-01 6.000000000000000e-03 1.746461934347441e+20 1.000000000000000e-01 7.500000000000000e-03 1.624953590587235e+20 1.000000000000000e-01 9.000000000000001e-03 1.487229735775812e+20 1.000000000000000e-01 1.050000000000000e-02 1.338374369370652e+20 1.000000000000000e-01 1.200000000000000e-02 1.183600782975821e+20 1.000000000000000e-01 1.350000000000000e-02 1.027960634580709e+20 1.000000000000000e-01 1.500000000000000e-02 8.760837871553451e+19 1.000000000000000e-01 1.650000000000000e-02 7.319658405394838e+19 1.000000000000000e-01 1.800000000000000e-02 5.988151766568749e+19 1.000000000000000e-01 1.950000000000000e-02 4.789656735254094e+19 1.000000000000000e-01 2.100000000000000e-02 3.738555168406800e+19 1.000000000000000e-01 2.250000000000000e-02 2.840671941130736e+19 1.000000000000000e-01 2.400000000000000e-02 2.094191931689198e+19 1.000000000000000e-01 2.550000000000000e-02 1.490964897485222e+19 1.000000000000000e-01 2.700000000000000e-02 1.018048684406722e+19 1.000000000000000e-01 2.850000000000000e-02 6.593363326920687e+18 1.000000000000000e-01 3.000000000000000e-02 3.971232721333878e+18 1.000000000000000e-01 3.150000000000000e-02 2.134950742656438e+18 1.000000000000000e-01 3.300000000000000e-02 9.145050393635727e+17 1.000000000000000e-01 3.450000000000000e-02 1.571393327240980e+17 1.000000000000000e-01 3.600000000000000e-02 -2.676990436821914e+17 1.000000000000000e-01 3.750000000000000e-02 -4.663232592512207e+17 1.000000000000000e-01 3.900000000000000e-02 -5.211733384089526e+17 1.000000000000000e-01 4.050000000000000e-02 -4.929396506924289e+17 1.000000000000000e-01 4.200000000000000e-02 -4.237699314480732e+17 1.000000000000000e-01 4.350000000000000e-02 -3.409466885452108e+17 1.000000000000000e-01 4.500000000000000e-02 -2.605426141272108e+17 1.000000000000000e-01 4.650000000000000e-02 -1.907107610842099e+17 1.000000000000000e-01 4.800000000000000e-02 -1.344150515701492e+17 1.000000000000000e-01 4.950000000000000e-02 -9.153405899109366e+16 1.000000000000000e-01 5.100000000000000e-02 -6.036525437524065e+16 1.000000000000000e-01 5.250000000000000e-02 -3.861519378892229e+16 1.000000000000000e-01 5.400000000000000e-02 -2.398729718557711e+16 1.000000000000000e-01 5.550000000000000e-02 -1.448064263583584e+16 1.000000000000000e-01 5.700000000000000e-02 -8.499465336697928e+15 1.000000000000000e-01 5.850000000000000e-02 -4.851879721633672e+15 1.000000000000000e-01 6.000000000000000e-02 -2.693860462767418e+15 1.000000000000000e-01 6.150000000000000e-02 -1.454575802458284e+15 1.000000000000000e-01 6.300000000000000e-02 -7.635830073261291e+14 1.000000000000000e-01 6.450000000000000e-02 -3.894906779856507e+14 1.000000000000000e-01 6.600000000000000e-02 -1.928843124487357e+14 1.000000000000000e-01 6.750000000000000e-02 -9.262530954421184e+13 1.000000000000000e-01 6.900000000000001e-02 -4.305656431123582e+13 1.000000000000000e-01 7.050000000000001e-02 -1.932548094046387e+13 1.000000000000000e-01 7.200000000000001e-02 -8.344024680144258e+12 1.000000000000000e-01 1.200000000000000e-01 0.000000000000000e+00