Sub-5 keV Scanning-Electron-Beam Lithography

Scanning-electron-beam lithography (SEBL) commonly uses voltages between 10-100 keV. Higher voltages result in distributed proximity effects, lower sensitivity, and a higher probability of substrate damage. Proximity effects raise concern because these effects limit resolution at voltages 10-50 keV and complex and computationally-intensive programs are used to correct such effects. Proximity effects can be reduced by using either very high voltages (100 keV) or very low voltages around 1 keV [1]. Our research efforts have investigated the feasibility of SEBL at energies of 2 keV and below.

Nested Ls patterned in 15-nm-thick hydrogen silsesquioxane (HSQ) on silicon were used to investigate the resolution limit for dense patterns at low-voltages. Ls at 20-nm pitch were sucessfully patterned at energies of 2 keV and 1.5 keV, as shown in Figure 1. At 1 keV energy, the finest pitch possible was 25 nm. Nested Ls were also patterned in 11-nm-thick poly methyl methacrylate (PMMA) on silicon, with the minimum resolvable pitch at an energy of 2 keV being 70 nm. Monte-Carlo simulations of point-spread and line-spread functions were performed for a 2 keV, 9-nm diameter electron-beam incident on 15-nm-thick HSQ on silicon. The simulated distributed-energy-profile of dense Ls is in agreement with experimental results. To demonstrate pattern-transfer capability of patterns fabricated with low-voltage SEBL, dense line patterns in HSQ were reactive-ion-etched (RIE) into XHRiC anti-reflective  layer with HSQ as the etch mask.


References
  1. L.D. Jackel, R.E. Howard, P.M. Mankeiwich, H.G. Craighead, and R.W. Epworth, “Beam energy effects in electron beam lithography: The range and intensity of backscattered exposure,” Applied Physics Letters, vol. 45, 1984, p. 698. []

Microsystems Technology Laboratories | Massachusetts Institute of Technology | 60 Vassar Street, 39-321 | Cambridge, MA 02139 | http://www-mtl.mit.edu
Copyright © Massachusetts Institute of Technology.