Figure 1

Figure 1: Carpet of vertically-aligned CNTs grown on a conductive substrate at 475 °C. The catalyst/underlayer system is Fe/Ta. The HRTEM image on the inset shows the crystalline nature of the CNTs (scale bar 5 nm).