Figure 2

Figure 2: Three capacitance-voltage sweeps for a single device. The increase in the capacitance of the device with voltage indirectly demonstrates deflection of the gold membrane, which bows under the electrostatic force to decrease the gap spacing over the air cavities in the PDMS spacer layer, thus increasing the capacitance.