Figure 1

Figure 1: Comparison of inverse dose versus measured feature half-width, which is the radial distance to the threshold for exposure, for 20 keV Ne+ and 30 keV He+, in thin (< 20 nm) HSQ on Si. We see from this plot that the neon beam is somewhat broader and also requires lower doses to achieve exposure.

Figure 1: Comparison of inverse dose versus measured feature half-width, which is the radial distance to the threshold for exposure, for 20 keV Ne+ and 30 keV He+, in thin (< 20 nm) HSQ on Si. We see from this plot that the neon beam is somewhat broader and also requires lower doses to achieve exposure.