Figure 2

Figure 2: Scanning-electron micrographs of templated QDs (6-nm-diameter CdSe). The solution concentration was 2 µM and the PMMA thickness was 12 nm. (a) An overview of the pattern. (b) Histogram of the number of QDs in each cluster versus the number of clusters. We analyzed 54 clusters of QDs, and the QDs were counted by using high-resolution SEM micrographs. On the inset of every histogram bar is presented one illustrative SEM image used.

Figure 2: Scanning-electron micrographs of templated QDs (6-nm-diameter CdSe). The solution concentration was 2 µM and the PMMA thickness was 12 nm. (a) An overview of the pattern. (b) Histogram of the number of QDs in each cluster versus the number of clusters. We analyzed 54 clusters of QDs, and the QDs were counted by using high-resolution SEM micrographs. On the inset of every histogram bar is presented one illustrative SEM image used.