wang_2dcrystals_01

Figure 1: (a) Schematic of the graphene FET device structure. (b) ambipolar IDS-VGS characteristics of the fabricated GFET. (c) SEM image of the device. (d) SEM image of the T-shape gate of a self-aligned graphene transistor.