chang_postarrays_02

Figure 2: SEM images of PDMS cylinders templated by post arrays. The height of the posts was 19 nm and the diameter was 10 nm. Arrows indicate the direction of the PDMS cylinders. Each figure is annotated Lx, Lx/Ly. Scale bar = 100 nm.