gabor_01

Figure 1: Experimental schematic image of the dual-gated graphene photodetector device incorporating boron nitride (BN) top gate dielectric and monolayer graphene (MLG). The current I is measured at fixed bias voltage  VSD while the top- and bottom-gate voltages, VTG and  VBG, respectively, are varied.