Given recent advances in the field of global optimization, we aim to make advances towards deterministic global optimization of some…
Photolithography’s accuracy and scalability have made it the method for sub-micron-scale definition of single-crystal semiconductor devices for over half a…
Electron-beam lithography (EBL) readily enables the fabrication of sub-10-nm features [1] . However, the resolution limits of this technique at…