MIT researchers are using graphene layers to create a new kind of filtration material that can be far more efficient and possibly less expensive than existing desalination systems. The details of this new technology are explained in a recent paper in the journal NanoLetters here. (The paper is also available in the password protected part of our website for our members).

Graphic: David Cohen-Tanugi