[labnetwork] hotplate parameters for Shipley 1813
Walsh,Kevin M.
kevin.walsh at louisville.edu
Tue Aug 28 18:21:09 EDT 2012
Processing Experts!
What hotplate processing parameters do you recommend for Shipley 1813. We have Brewer Science hotplates capable of hard contact (vacuum), proximity contact (nitrogen cushion), or soft contact (gravity).
Dehydration Bake - temp, time, soft/hard/proximity contact?
Soft Bake - temp, time, soft/hard/proximity contact?
Hard Bake - temp, time, soft/hard/proximity contact?
If soft contact, do you use alum foil to keep your hotplate surfaces clean?
Thanks in advance,
Kevin
Dr. Kevin M. Walsh
Samuel T. Fife Professor of Electrical and Computer Engineering
Founding Director of the UofL Micro/Nanotechnology Center
University of Louisville
BRB Building, Room 234
2210 S. Brook St
Louisville, KY 40292
(502) 852-0826 office
(502) 852-8128 fax
walsh at louisville.edu<mailto:walsh at louisville.edu> or walsh at ieee.org<mailto:walsh at ieee.org>
www.louisville.edu /micronano<http://www.louisville.edu/micronano>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20120828/88436f11/attachment.html>
More information about the labnetwork
mailing list