[labnetwork] joining long PVDF pipe runs
Iulian Codreanu
codreanu at seas.upenn.edu
Thu Jul 5 08:33:52 EDT 2012
Good Morning.
We are trying to determine how to best join long runs of PVDF pipe on
our ultrapure water system (we are trying to achieve Type E-1.1 per ASTM
D5127). We are aware of the following methods:
- fully welded system
- systems using flanges
- systems using unions
- systems using GF sanitary couplings with clamps
Knowing how other University Fabs do it would be very helpful in making
a decision (affecting water quality, cost, and schedule) and thus your
input will be much appreciated.
Iulian
--