HI,
The answer for MTL is the same as EPFL's, except that our HEPAs have
been unchanged since 1985 :)
Vicky
On Sep 25, 2012, at 4:22 AM, Flückiger Philippe wrote:
> Dear Denis,
>
> Let me mention that EPFL is running with the original HEPA filters
> since 14 years (1998) and still reach the class 100 specifications.
> EPFL has no plan to change the HEPA filters. Only some pre-filters
> might be occasionally changed for example after construction work in
> the area.
>
> Anyway, back to your question facilities would pay for this.
>
> With my very best regards,
> Philippe
>
> Dr Philippe Flückiger
> Director of Operations
> http://cmi.epfl.ch/
> Phone +41 21 693 6695
>
> De : labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu
> ] De la part de Dennis Grimard
> Envoyé : vendredi 21 septembre 2012 00:17
> À : labnetwork at mtl.mit.edu
> Objet : [labnetwork] HEPA Filters
>
> All:
>
> Do any of you have to pay for the replacement of your HEPA filters
> in your cleanrooms?
>
> Thanks ...
>
> --
> Dennis S Grimard, Ph.D
> Managing Director, Lurie Nanofabrication Facility
>
> University of Michigan
> 1246D EECS Building
> 1301 Beal Avenue
> Ann Arbor, MI 48109-2122
> (734) 368-7172 (Cell)
> (734) 647-1781 (Fax)
> http://www.lnf.umich.edu
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20120926/51f7131b/attachment.html>
More information about the labnetwork
mailing list