Teflon lined stainless steel was designed and implemented for our acid exhaust system. Our cleanroom has been in place since 2006 and was designed by Abbie Gregg. She would be a great source for this type of information.
Cheers!
Julia Aebersold, Ph.D.
MNTC Cleanroom Manager
Shumaker Research Building, Room 233
2210 South Brook Street
University of Louisville
Louisville, KY 40292
502-852-1572
http://louisville.edu/micronano/
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Iulian Codreanu
Sent: Thursday, December 19, 2013 1:52 PM
To: Fab Network
Subject: [labnetwork] Corrosive exhaust material of construction
Dear Lab Network,
I, once again, seek your wisdom. Could you please share with me the type of material used for your corrosive exhaust system, how long you had it in operation, if you had any problems with it, and what you would do differently of you were in a position to do so?
Thank you very much for your help.
Iulian
--
iulian Codreanu, Ph.D.
Director of Operations, UD NanoFab
University of Delaware
149 Evans Hall
Newark, DE 19716
302-831-2784
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list