[labnetwork] Looking for XeF2
Michael Khbeis
khbeis at uw.edu
Wed Dec 10 00:06:33 EST 2014
Steve,
Call Pelchem in South Africa, I found them to be very responsive and economical when in short order.
Best,
Dr. Michael Khbeis
Associate Director, Washington Nanofabrication Facility (WNF)
National Nanotechnology Infrastructure Network (NNIN)
University of Washington
Fluke Hall, Box 352143
(O) 206.543.5101
(F) 206.221.1681
(C) 443.254.5192
khbeis at uw.edu
www.wnf.washington.edu/
> On Dec 9, 2014, at 2:55 PM, Paolini, Steven <spaolini at cns.fas.harvard.edu> wrote:
>
> Dear colleagues,
> Just recently, my custom made Xenon Difluoride etcher has become popular with many of my users and I found myself in the horrible and embarrassing predicament of running out of etchant. Since this is somewhat of a specialty item, lead times are astronomical. Is there anybody out there that can lend me a sample cylinder? I will replace it with an identical new one. The cylinder is aluminum and is 2” diameter by 10.5” long measured from the bottom to the centerline of the male VCR fitting on the valve. Similar or not so similar cylinders can be fitted, it’s just a matter of finding one.
> Thank you in advance.
> Steve Paolini
> Equipment Dood
> Harvard University Center for Nanoscale systems
>
> Steve Paolini
> Principal Equipment Engineer
> Harvard University Center for Nanoscale Systems
> 617- 496- 9816
> spaolini at cns.fas.harvard.edu
> www.cns.fas.harvard.edu
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list