[labnetwork] Looking for XeF2
Bob Bicchieri
bic at mtl.mit.edu
Wed Dec 10 14:44:20 EST 2014
Hi,
~$100/gm through Sigma-Aldrich and $50/gm from Alfa Aesar.
I buy it from Pelchem (South Africa) ~1,000/200gms and ~$1,000 for Hazardous shipping (and it has a higher purity)
Regards,
Bob
-----------------------------------------------------------------
Robert J. Bicchieri
Research Specialist
Massachusetts Institute of Technology
Microsystems Technology Laboratories
60 Vassar St. Bldg. 39-215
Cambridge, MA 02139
Phone 617.253.6418
Fax 617.258.8500
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of mark crain
Sent: Wednesday, December 10, 2014 9:48 AM
To: Morrison, Richard H., Jr.
Cc: Fab Network (labnetwork at mtl.mit.edu)
Subject: Re: [labnetwork] Looking for XeF2
I see that xenon difluoride can be purchased from Alfa Aesar. Has anyone consulted with the chemical supplier, their chemistry departments, or environmental health and safety to develop a protocol for reloading the canister with the crystals?
Best Regards,
Mark
Mark Crain
University of Louisville
On Wed, Dec 10, 2014 at 9:11 AM, Morrison, Richard H., Jr. <rmorrison at draper.com> wrote:
The material is only available from Pellchem in South Africa, we got the past bottle through Middlesex Gas (Draper supplier of gases).
Rick
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Paolini, Steven
Sent: Tuesday, December 09, 2014 5:55 PM
To: Fab Network (labnetwork at mtl.mit.edu)
Subject: [labnetwork] Looking for XeF2
Dear colleagues,
Just recently, my custom made Xenon Difluoride etcher has become popular with many of my users and I found myself in the horrible and embarrassing predicament of running out of etchant. Since this is somewhat of a specialty item, lead times are astronomical. Is there anybody out there that can lend me a sample cylinder? I will replace it with an identical new one. The cylinder is aluminum and is 2” diameter by 10.5” long measured from the bottom to the centerline of the male VCR fitting on the valve. Similar or not so similar cylinders can be fitted, it’s just a matter of finding one.
Thank you in advance.
Steve Paolini
Equipment Dood
Harvard University Center for Nanoscale systems
Steve Paolini
Principal Equipment Engineer
Harvard University Center for Nanoscale Systems
617- 496- 9816 <tel:617-%20496-%209816>
spaolini at cns.fas.harvard.edu
www.cns.fas.harvard.edu
_____
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper Laboratory. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
_____
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20141210/6f808cab/attachment.html>
More information about the labnetwork
mailing list