We have had really good service from Vacnet.inc in Albuquerque,NM. Each time they have rebuilt a CTI Cryopump it has lasted at least 5 years and the service is quick and very reasonable.
Charles Ellis
Director, Microlab
Auburn University
> On Sep 9, 2014, at 10:12 AM, "Peter Modh" <peter.modh at chalmers.se> wrote:
>
> Hi labnetwork,
>
> We are looking for recommendations of where to service/repair CTI cryo pumps. Our local serviceman in Sweden has discontinued this service and we have not been fully satisfied with the price and delivery time at the alternative service points in Europe, which we have used lately. Therefore, we would like to ship our CTI cryo pumps directly to USA or Canada for service/repair.
>
> Thanks in advance,
>
> Peter Modh
>
>
> -----------------------------------------------------------------------------
> Peter Modh
> Ph.D., Head of Nanofabrication Laboratory
> Department of Microtechnology and Nanoscience - MC2
> Chalmers University of Technology
> SE-412 96 Göteborg, Sweden
> Phone: +46-(0)31-772 16 05
> Fax: +46-(0)31-772 83 90
> E-mail: peter.modh at chalmers.se
>
>
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
More information about the labnetwork
mailing list