[labnetwork] Free Vacuum Training with Kurt Lesker
Olona, Leonard E.
len.olona at ou.edu
Tue Mar 31 10:37:35 EDT 2015
KJL just finished a presentation here at OU. It was excellent. We had a very nice turn out from across the board. Physics, Mechanical, Electrical Engineering.
-Len
Leonard E. Olona
Facility Manager RIL
Cleanroom Manager
University of Oklahoma
web: http://arrc.ou.edu/
web: http://cleanroom.ou.edu/ voice: +1- 405- 325-4374
From: Mike Young <myoung6 at nd.edu<mailto:myoung6 at nd.edu>>
Date: Monday, March 30, 2015 11:30 AM
To: "labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>" <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: Re: [labnetwork] Free Vacuum Training with Kurt Lesker
KJL gave a similar presentation here (at Notre Dame) a few weeks ago. I did not personally attend, but staff who did attend reported that it was time well spent.
--Mike
On Mar 30, 2015, at 9:32 AM, Ferraguto, Thomas <Thomas_Ferraguto at uml.edu<mailto:Thomas_Ferraguto at uml.edu>> wrote:
Colleagues
You are invited to a free Training Session conducted by Kurt J. Lesker Company at the UMass Lowell Saab Emerging Technology and Innovation Center.
Kurt J. Lesker is a leading component and equipment manufacture for thins films and semi-conductor processing equipment.
The Course will cover: Vacuum Basics, Physical Vapor Deposition and Atomic Layer Deposition Basics
Lunch will be served to registered attendees. Attendance is limited.
**E-Mail Thomas_ferraguto at uml.edu<mailto:Thomas_ferraguto at uml.edu><mailto:Thomas_ferraguto at uml.edu> if you would like to attend**
The Event will be held in the Saab ETIC Atrium, April 9th 2015, 10:00 AM - 3:00 PM
Thomas S. Ferraguto
Saab ETIC Nanofabrication Laboratory Director
University of Massachusetts Lowell
1 University Avenue
Lowell MA 01854-5120
978-934-1809 land
617-755-0910 mobile
978-934-1014 fax
--
Michael P. Young (574) 631-3268 (office)
Nanofabrication Specialist (574) 631-4393 (fax)
Department of Electrical Engineering (765) 637-6302 (cell)
University of Notre Dame mike.young at nd.edu<mailto:mike.young at nd.edu>
B-38 Stinson-Remick Hall
Notre Dame, IN 46556-5637
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20150331/476b91fc/attachment.html>
More information about the labnetwork
mailing list