[labnetwork] Aluminimum source crucible suggestions
Clifford F Knollenberg
cknollen at stanford.edu
Tue May 31 13:11:33 EDT 2016
Hi All,
We've been having crucible cracking issues with out Al e-beam evaporation source. In short it cracks its crucible after just a few uses. This wasn't so bad when it happened ever 4-5 months, but not its happening about every week or two. I've tried a variety of crucibles, had the most luck with carbon crucible. Is there anything else out there we should be trying?
Cheers,
Cliff
Clifford Knollenberg
Science & Engineering Associate
Stanford Nano Shared Facilities (SNSF)
Email: cknollen at stanford.edu
Tel: 650-723-1675