Hi Cliff,
We had the same issue with Al in graphite crucibles.
Al deposition in intermetallic crucibles has been working perfectly for us.
Regards,
Yusha
Yusha Bey, Ph.D.
Senior Development Engineer
Center for Nano-Micromanufacturing (CNM2)
University of California Davis
________________________________
From: labnetwork-bounces at mtl.mit.edu <labnetwork-bounces at mtl.mit.edu> on behalf of Clifford F Knollenberg <cknollen at stanford.edu>
Sent: Tuesday, May 31, 2016 10:11:33 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Aluminimum source crucible suggestions
Hi All,
We've been having crucible cracking issues with out Al e-beam evaporation source. In short it cracks its crucible after just a few uses. This wasn't so bad when it happened ever 4-5 months, but not its happening about every week or two. I've tried a variety of crucibles, had the most luck with carbon crucible. Is there anything else out there we should be trying?
Cheers,
Cliff
Clifford Knollenberg
Science & Engineering Associate
Stanford Nano Shared Facilities (SNSF)
Email: cknollen at stanford.edu
Tel: 650-723-1675
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20160531/683fc09d/attachment.html>
More information about the labnetwork
mailing list