[labnetwork] Sputtering targets storage
prabhakararao yp
prabhakararaoyp at gmail.com
Fri Dec 15 12:27:32 EST 2017
hi,
you can store targets at slightly at elevated temperature from room temp
in nitrogen ambient oven with out plastic case
Thanks& regards,
prabhakararao
Dr. Y.P. Prabhakara Rao .M.Tech.Ph.D
National Nanofabrication centre
Centre For Nanoscience and Engineering,
Indian Institute Of Science,Bangalore-560012
Mobile: +91 9448365748
Tel: +91 80 22933181 extn 321
Email: prabhakarayp at iisc.ac.in <prabhakararaoyp at gmail.com>
prabhakararaoyp at gmail.com
On Thu, Dec 14, 2017 at 11:20 PM, Guo, Jing <jguo5 at central.uh.edu> wrote:
> Hi All,
>
> We have a lot sputtering targets for our UHV sputtering system. Right now
> each target is covered by Aluminum foil stored in a plastic box.
> We are wondering whether the Aluminum foil is necessary for all the
> targets. After several times the foil will become wrinkled and it is kind
> annoying to cover a target with wrinkled foil.
> Do you have any good idea to store those targets? Please advise.
> And for those used ones, any good way to dispose them or recycle them?
>
> Thanks.
>
> Best Regards,
>
> Jing
>
> Research Lab Supervisor
> Nanofabrication Facility
> University of Houston
> Postal Address:
> UNIVERSITY OF HOUSTON
> NANOFABRICATION FACILITY
> 3517 CULLEN BLVD, RM 1011
> HOUSTON TX 77204-5062
> Phone: 832-842-8822
> Email: jguo5 at central.uh.edu
> Web: www.uh.edu/nanofab
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20171215/66a03e1e/attachment.html>
More information about the labnetwork
mailing list