Hello Frank,
Typical positive resist (example is AZ1500 series) is photosensitive in
the violet-blue light spectrum and white LEDs have a very strong blue
emission. Your best bet is to use the standard amber filters or use a
single wavelength LED like green or yellow.
Best Regards,
Brent
--
Brent P. Gila, PhD.
Director, Nanoscale Research Facility
1041 Center Drive
University of Florida
Gainesville, Florida 32611
Tel:352-273-2245
Fax:352-846-2877
email:bgila at ufl.edu
On 7/7/2017 12:57 PM, Frank Gavin wrote:
>
> Hello everyone
>
> We are suppliers of wet process equipment and one of our vendors of
> HEPA and ULPA fan/filter units tells us that we do not need to add
> yellow lens covers over LED light because such lights do not emit
> ultraviolet light. I am always suspicious of simple convenient
> solutions so I want to put this statement out to this learned
> community and learn if this statement is true. Perhaps some members
> have experience using LED lights in photosensitive areas of their fab
> and would care to comment?
>
> Best Regards,
>
> FRANK GAVIN, Sales Eng.
>
> Description: WaFab_Logo200px <http://www.wafabintl.com/>
>
> 6161 Industrial Way, Livermore CA 94551
> *(925) 455-5252 ext 2420* Fax: (925) 455-5351
> http://www.wafabintl.com <http://www.wafabintl.com/>
>
> direct dial: 925-800-5551
>
> cell (408) 314-6199
>
> **
>
> *Please visit us at:*
>
> Description: Description: Description: \\WAFAB-DC\Folder
> Redirection\fgavin\Desktop\semi17-hdpi-logo.png
> <http://www.semi.org/en/semicon-west-2017>
>
> **
>
> *July 11^th –13^th *
>
> *Moscone Center, San Francisco **Booth: 7817 (West Hall)*
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170707/6767441c/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: not available
Type: image/png
Size: 12639 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170707/6767441c/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: not available
Type: image/png
Size: 8427 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170707/6767441c/attachment-0001.png>
More information about the labnetwork
mailing list