Hi Xiaojin,
I just burned in a melt of Scandium for a user the other day and it ran very nicely. Literature on the material indicated it was non-toxic in pure form and it appeared to not contaminate more than anything else.
Good luck,
Mark Heiden
NanoFab Cleanroom Manager
Center for Nanoscale Science and Engineering
University of California, Riverside
951-827-2551
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of xiaojin.wang at louisville.edu
Sent: Wednesday, June 14, 2017 1:44 PM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] inquiry about evaporating scandium
Hi colleagues,
We want to evaporate a thick layer of scandium. Does anyone have experience with it? Are there any contamination, safety issues related with this process? Thank you.
Best wishes
Xiaojin Wang, Ph.D.
Senior Process Engineer
Micro/Nano Technology Center
University of Louisville
Shumaker Research Building, Room 232
2210 South Brook Street
Louisville, KY 40292
502-852-7671
http://louisville.edu/micronano/
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170615/e54a5d99/attachment.html>
More information about the labnetwork
mailing list