[labnetwork] updated survey
Mark Heiden
mheiden at engr.ucr.edu
Thu May 18 13:04:06 EDT 2017
Greetings Network,
At UC Riverside we have been fortunate to have a facility that was designed to be class 100 in one bay and 1,000 in the other and after 11 years of operation the particle counting still comes out well under the designed spec. when measured anywhere around the working height. The floor is another story of course as that is where the particles that shed from the users end up. A well designed room is essential though. Since we are strictly a research lab working almost exclusively with small fragments, should there be contamination on a sample it won’t cause thousands of dollars of damage as it could in a production environment. Yield is a non-issue here.
Obviously when doing Nanoscale research any particle in the micron region that lands on a sample could completely obscure the area of interest rendering that sample worthless. However that particle would have to land on exactly the “wrong spot” in order to cause failure of the experiment so it becomes a matter of random fortune.
So far, that has not been an issue so the protocols we are using are adequate for the work product we have. The largest wafers we use are 4 inch and even in that scale the contamination is extremely minimal.
We do use full length smocks, hair nets, shoe covers, gloves and face masks and try to enforce taking them off whenever leaving the clean area. As for smocks, we started out using Tyvek disposable smocks and due to their excellent chemical resistance have never changed. We do re-use them but if they get torn or damaged they get tossed. This may be unusual but the results speak for themselves and the peace of mind having the students all in plastic bags is worth it to me.
Cheers,
Mark Heiden
UC Riverside
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Harold Gilles
Sent: Thursday, May 18, 2017 5:56 AM
To: Bill Flounders <bill at eecs.berkeley.edu>; Paolini, Steven <spaolini at cns.fas.harvard.edu>; Ferraguto, Thomas <Thomas_Ferraguto at uml.edu>
Cc: Fab Network (labnetwork at mtl.mit.edu) <labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] updated survey
Good Morning Folks,
I started work at Intel as a process engineer in 1976. In those days we did not have bunny suits, we wore smocks and hair cover and gloves when needed. I retired from Intel in 2010.
We made lots of changes in this area based on need over the years. Changes were justified by data. Defects are expensive and don’t help you make devices. There are different levels of protocol that can be applied and your lab will need to decide based on what they are making. You should also consider what you may be doing in the future. Getting folks on board with the proper level of discipline is difficult, maintaining the culture is difficult and trying to change to the next level can be an endless task. In a university setting it is even more difficult to make the changes and those that need to benefit from the change will likely be gone before they can benefit. I would always error on the side of better control in this topic.
Hal Gilles
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Bill Flounders
Sent: Wednesday, May 17, 2017 7:30 PM
To: Paolini, Steven; Ferraguto, Thomas
Cc: Fab Network (labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>)
Subject: Re: [labnetwork] updated survey
Steve,
Have I seen a study - no.
Am I an advocate of modest gowning - yes.
Am I an advocate of no gowning - no
Modest gowning = frock coat, booties and bouffant cap. (and gloves)
This is easy to don and remove for staff that are primarily in the chases.
We switched to full bunny suit instead of frock coat for researchers and
process staff who are mainly in the bays.
I like the additional layer of chemical protection provided to the legs.
Full bunny suit emphasizes you are in a clean room and provides some
level of training on protocol and attention to your environment.
Disposable suits with a single zipper are quick to don and remove.
I don't see either of our protocols as significant impact on productivity.
I have been to many labs that have complex and expensive protocol
that I consider of questionable value.
Good Luck with the national debate.
Bill Flounders
UC Berkeley
Paolini, Steven wrote:
Not to start a national debate but has anybody ever seen a comprehensive study of the benefits of full gowning versus the expense and trouble? As a former Field service engineer and long time fab rat, I have visited many sites and no two follow the same protocol. The interesting part of this is that every site believes that theirs is the best. How can something that’s fairly scientific be so subjective? I do notice that all of these sites are of the “wrap em’ up” method, but my perennial question is “at what expense?” Is the ten minutes lost to dash out of the clean room to retrieve an item worth whatever benefit full gowning provides? Has anyone ever estimated if the loss of working time because of the added activity is worth the effort? I am a firm believer in that higher air changes per hour is the best contributor to a clean room’s performance. I do doubt however, that the obstacle of full gowning in a clean room class 100 or dirtier offers little, if any, contribution to the overall room performance.
After donning bunny suits for more than 35 years, I have yet to find a comprehensive study on this subject. I have seen many a paper written that emphasizes high particle counts on personnel that aren’t fully gowned but that’s half of the equation, If loss of productivity and general work habit change is factored in, does it become a “non value add” activity? Wouldn’t it be nice if you could just wear booties, a hairnet, and lab coat without any detrimental effects to your space?
I think the microelectronic and nanofabrication community has been influenced by the larger fabs in that whatever they do must be the right thing. It’s been many years since we have been gowning up to enter a clean space but maybe it’s time to determine if the trouble and expense equate to the benefit. Other industries that are under constant expense pressure have altered their methods to lower costs. The food packaging business for example has moved from providing a clean general space to mini environments in which critical process steps are done in a high HEPA flow area directed at the product.
Is there anyone in this network that questions this practice and has access to a good scientific study that might help settle this (my) dispute? Is there anyone here that can support my claim of full gowning to be high cost/low benefit ?
Thanks for listening.
Steve Paolini
Principal Equipment Engineer
Harvard University Center for Nanoscale Systems
11 Oxford St.
Cambridge, MA 02138
617- 496- 9816
spaolini at cns.fas.harvard.edu<mailto:spaolini at cns.fas.harvard.edu>
www.cns.fas.harvard.edu<http://www.cns.fas.harvard.edu>
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Ferraguto, Thomas
Sent: Wednesday, May 17, 2017 12:45 PM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: [labnetwork] updated survey
Here’s the updated flash survey for ERP Systems and Interlocks.
On a side note, I did a video audit of our “Honor System” run lab and we did not book 31% of the Activity.
Institution
System
FTE's
Interlocks
Total
52% Home Grown
0.60
83.3%
UC Davis
Badger
0.25
Yes
University of Houston
Home Grown
0.0025
No
Stanford
Badger
0
Yes
University of Utah
Coral
1
Yes
University of Freiburg
Home Grown/w Coral
1
Yes
MIT
Coral
1
Yes
Delft University
Phoenix
2
Yes
University of Delaware
FOM
0.1
Yes
UNC
Home Grown
0.1
No
UC San Diego
FOM
0.25
Yes
University of Louisville
FOM
0.1
Yes
UMass Lowell
FOM
0.2
No
Purdue
Ilab
2
Yes
EPFL-Lausanne-Switzerland:
Home Grown
1
Yes
Cal-Tech
Home Grown/Labrunr
0.3
Yes
University of Texas
Home Grown
0.2
Yes
Harvard
Home Grown
0.1
Yes
Berkeley
Home Grown
0.75
Yes
UCSB
Home Grown/SignupMonkey
0.125
No
Washington Nanofabrication Facility (WNF)
Home Grown/w Coral
1
Yes
Georgia Tech
Home Grown SUMS
2
Yes
Columbia University
Badger
0
Yes
University of Alberta
Home Grown LMACS
0.5
Yes
University of Florida
Home Grown
0.5
Yes
Best Regards
Tom
Thomas S. Ferraguto
Saab ETIC Nanofabrication Laboratory Director
Saab ETIC Building Director
1 University Avenue
Lowell MA 01854
Mobile 617-755-0910
Land 978-934-1809
Fax 978-934-1014
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170518/71c1a112/attachment.html>
More information about the labnetwork
mailing list