Hi Nava,
You could contact Felix Mayorca from Hybond at this address: FMayorca at hybond.com<mailto:FMayorca at hybond.com>. He is very keen and prompt to help.
Regards,
Marwane
On Dec 5, 2018, at 3:36 PM, Nava Ariel-Sternberg <na2661 at columbia.edu<mailto:na2661 at columbia.edu>> wrote:
Dear all,
We’ve been having some problems with our Al wire supply. The vendor we used to purchase from, SPM became Coining and Coining became Ametek and started manufacturing abroad. That by itself is not a problem but apparently the wire’s coiling direction is different now it’s against the spooling direction on our westbond bonders.
Is anyone familiar with this issue? Does anyone have a vendor to recommend for Al wires?
Thanks,
Nava
Nava Ariel-Sternberg, Ph.D.
Director of CNI Shared Labs
CEPSR/MC 8903
530 west 120th st. NY
NY 10027
Office: 212-8549927
Cell: 201-5627600
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181206/be872490/attachment.html>
More information about the labnetwork
mailing list