Hi Ahad,
We have used a similar one to identify issues with our fumehoods and laminar flow benches, which worked well.
I don’t know how much they cost but you can probably also try a $6 ultrasonic pond fogger with DI water, which produces a dense mist.
Best regards,
Peter
On 27 Dec 2018, at 14:58, Morrison, Richard H., Jr <rmorrison at draper.com<mailto:rmorrison at draper.com>> wrote:
I have one here at Draper and it is very effective. I used it when we had issues around a Class 10 cleanroom certification. It is very good at identifying air flow around and in exhaust hoods, it give you an excellent visual of the air flow, I like it better than smoke sticks and it is much cleaner.
Rick
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Ahad Syed
Sent: Sunday, December 23, 2018 6:00 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: [labnetwork] DI Water Foggers
Dear Colleagues,
Does anyone have experience using DI Water foggers (please see the pic below) for testing of wet bench exhaust in the cleanroom?
I have found one from Applied Physics, USA (http://www.appliedphysicsusa.com/DI_water_fogger_120410.html?)
Please share your experience and the effectiveness of the foggers.
Thank you and Happy Holidays.
Ahad
<image001.png>
--
Nanofabrication Core Lab
4700 King Abdullah University of Science and Technology
0247 Building 3, Thuwal 23955-6900, Kingdom of Saudi Arabia
Tel:+966 12 808 2348
Visit The Core Labs<https://corelabs.kaust.edu.sa/visitor-information>
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181227/f57bb87d/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 142592 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181227/f57bb87d/attachment.png>
More information about the labnetwork
mailing list