Adehsion issue occurs in this most so slowly ramping temp works well, Coat
PR on PDMS, put sample at hotplate @50deg C and ramp up to 80deg C for 2min.
Next shrink/expand issue: during deposition/ evaporation chamber temp
should not exceed more than 90deg C.
Thanks,
Hitesh
On 26-Jan-2018 6:35 AM, "Mohamed Ghoneim" <mghoneim at mit.edu> wrote:
**This might work for having electrodes on PDMS without running into
thermal expansion/shrinking issues.....but it depends on what you are
trying to do ultimately.
[image: Inline image 1]
**You can also try transfer printing the electrodes or using the
traditional process with PR (additive or lift-off) but with slower heating
up and cooling down rates (sometimes, moving to 70% of required temperature
then 100% does the trick and same when cooling down to room temperature).
Best of luck and wish you all a great day!
Mohamed T. Ghoneim
<https://scholar.google.com/citations?hl=en&user=-5mNcfYAAAAJ&view_op=list_works&sortby=pubdate>
,
Postdoctoral Researcher
MIT Media Lab, Building E-15, Fourth Floor, Room 443g.
Website <https://sites.google.com/view/mtghoneim>
On Thu, Jan 25, 2018 at 9:59 AM, Carsen Kline <carsen at stanford.edu> wrote:
> Hello Esta,
>
>
>
> Have you considered using a shadow mask and an evaporator? Substrate shape
> and topography could present a challenge, and some fixturing would be
> required, but no resist would be required and with a great enough throw
> distance (on the order of 60cm+), your temperatures should stay cool enough
> to get the job done.
>
>
>
> Best,
>
>
> Carsen
>
>
>
>
>
> *From:* labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl
> .mit.edu] *On Behalf Of *Abelev, Esta
> *Sent:* Wednesday, January 24, 2018 11:57 AM
> *To:* labnetwork at mtl.mit.edu
> *Subject:* [labnetwork] Device on PDMS
>
>
>
> Dear All,
>
>
>
> We have a group here that is interesting to make some gold electrodes on
> PDMS substrates.
>
> We found it is very challenging to bake the resist on PDMS dew to it temp.
> sensitivity (shrinks).
>
> Can anyone advise us on how to do it, any tricks?
>
>
>
> Thank you, Esta
>
>
>
> -----------------------
>
> *Esta Abelev, PhD*
>
> Technical Director, Petersen Institute of NanoScience and Engineering
>
> University of Pittsburgh | 3700 O’Hara Street | 636| Pittsburgh, PA 15261
>
> 412-383-4096 <(412)%20383-4096> | eabelev at pitt.edu | nano.pitt.edu
> <https://na01.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.nano.pitt.edu%2F&data=01%7C01%7Ceabelev%40pitt.edu%7C9f5bd58ba84940765cf308d4024fbe18%7C9ef9f489e0a04eeb87cc3a526112fd0d%7C1&sdata=3KfbG5VbshqdoIAPxvX%2F2s1UeU7ultmBoZmm%2FaZ2Itc%3D&reserved=0>
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
>
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180126/c8d5ea34/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image.png
Type: image/png
Size: 17942 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180126/c8d5ea34/attachment.png>
More information about the labnetwork
mailing list