Sorry to hear about the troubles. As some other suggested, I would start with particle counts. We recently had a brush fire producing a haze of smoke (as opposed to a thick cloud) not far from our air intakes. There was a significant burning smell within the lab, but we saw no change in particle counts. Unless you have carbon filters installed, the burning smell will penetrate as Danny has suggested. Similarly, we get odors from lawnmower exhaust when grass is being cut near the air intakes. Again, we do not see any increase in particle count.
If the smell is persisting in the lab and will not go away, I suspect that your prefilters in the make-up air unit may be contaminated with large smoke particles and ash and may therefore need to be replaced. Our make-up air unit has two banks of prefilters in series and a hepa filter at the output. We have gauges monitoring the pressure drop across the filters at each stage. During our smoke event, we did not see any increase in the pressure drop across the final hepa. Most of the large particles were captured by the first bank of Merv8 prefilters. With this in mind, I would at least replace the first bank of pre-filters in your system (I would assume these are on a regular replacement schedule anyway). If you have additional concerns, you can check the pressure drop across other filters in the system.
Best Regards,
Matt
--
Matthew T. Moneck, Ph.D.
Executive Manager, Carnegie Mellon Nanofabrication Facility
Electrical and Computer Engineering | Carnegie Mellon University
5000 Forbes Ave., Pittsburgh, PA 15213-3890
T: 412.268.5430
F: 412.268.3497
www.ece.cmu.edu<http://www.ece.cmu.edu>
nanofab.ece.cmu.edu
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Leslie George
Sent: Wednesday, June 06, 2018 3:55 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Cleanroom recovery after smoke in intake
Dear colleagues,
A fire broke out on Monday at one of the retail locations on our campus. The smoke from the fire got into the air intake for our cleanroom, and we can smell smoke throughout the Facility. I'd like to draw on the collective wisdom of the group to help answer the following:
1. Recommend recovery method for the air handling system? (both upstream of the AHU) and downstream including the HEPA's.
2. Recommended cleaning scheme for the interior of the facility?
I appreciate everyone's assistance.
Kind regards,
Leslie George, BSc, MSc
Micro & Nano Fabrication Instructor,
Research Laboratories
Khalifa University - Masdar City Campus
Opposite Presidential Flight Airport
Masdar City, SAF 1A (Undercroft)
Khalifa City A,
United Arab Emirates
P O Box 127788, Abu Dhabi, UAE
T +971 2 810 9227
Fax +971 2 810 9901
M +971 50 84 9720
leslie.george at ku.ac.ae<mailto:leslie.george at ku.ac.ae>
[cid:image001.png at 01D3DFD3.27E5A010]
ku.ac.ae
[cid:image002.jpg at 01D3E08C.D51AC120]<https://www.facebook.com/khalifauniversity>[cid:image003.jpg at 01D3E08C.D51AC120]<https://www.linkedin.com/school/khalifa-university-/>[cid:image004.jpg at 01D3E08C.D51AC120]<https://twitter.com/KhalifaUni>[cid:image005.jpg at 01D3E08C.D51AC120]<https://www.instagram.com/khalifa_university/>[cid:image006.jpg at 01D3E08C.D51AC120]<https://www.youtube.com/user/KhalifaUniversity>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 9620 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.jpg
Type: image/jpeg
Size: 973 bytes
Desc: image002.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image003.jpg
Type: image/jpeg
Size: 995 bytes
Desc: image003.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment-0001.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image004.jpg
Type: image/jpeg
Size: 989 bytes
Desc: image004.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment-0002.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image005.jpg
Type: image/jpeg
Size: 997 bytes
Desc: image005.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment-0003.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image006.jpg
Type: image/jpeg
Size: 982 bytes
Desc: image006.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180607/457a9fdb/attachment-0004.jpg>
More information about the labnetwork
mailing list