I'm wondering if anyone has worked with Cryogenic ICP etch systems for Si processing. Oxford Instruments is the only vendor I could find that manufactures these systems. There also seems to be only a couple of university micro/nanofab facilities with such a system: Georgia Tech and U. Michigan (I'm sure I missed a few others...) So, my questions are: does anyone know of other vendors that manufacture cryo ICP etch systems, and is there a particular reason these systems seen to be unpopular?