[labnetwork] Type R or Type S Thermocouples
Keith Barnes
kbarnes at semitorrinc.com
Thu Oct 25 20:37:59 EDT 2018
Try Vulcan out of Maine. Great product good prices
Sent from my iPhone
On Oct 25, 2018, at 4:40 PM, Rehn, Larry A <lrehn at tamu.edu<mailto:lrehn at tamu.edu>> wrote:
I need a Type R or Type S thermocouple for doing calibration profiles in a Minibrute diffusion furnace. From my days in the semiconductor industry, I recall purchasing the Pt-Pt/Rh wire from Johnson-Matthey, and other components from other vendors to make my own. Any suggestions for a pre-made product, or suppliers to assemble the components myself?
Regards,
Larry A Rehn
Technical Lab Manager
AggieFab Nanofabrication Facility
Texas A&M University
979 845-3199
lrehn at tamu.edu<mailto:lrehn at tamu.edu>
<image001.jpg>
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181026/27a7e852/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.jpg
Type: image/jpeg
Size: 13188 bytes
Desc: image001.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181026/27a7e852/attachment.jpg>
More information about the labnetwork
mailing list