[labnetwork] Has anyone using thicker than 200nm HSQ for EBL patterning?
Mason Risley
mrisley at andrew.cmu.edu
Mon Apr 1 10:08:55 EDT 2019
Hi Mark,
Thanks for mentioning about the dry HSQ, I didn't realize that was available. Do you know if dry HSQ has a better shelf life than the standard XR1541 in MIBK? That's a challenge my lab is always fighting that our HSQ ends up gelling or solidifying before we use the entire bottled, I'm wondering if by prepping smaller quantities from dry HSQ as needed would be a better way to manage shelf life.
Mason Risley
Process Development Engineer
Clair and John Bertucci Nanotechnology Laboratory
5000 Forbes Street, Pittsburgh PA 15213
nanofab-staff at lists.andrew.cmu.edu<mailto:nanofab-staff at lists.andrew.cmu.edu> | http://www.nanofab.ece.cmu.edu/
ph: 412.268.5419 | cell : 505.795.4805
From: labnetwork-bounces at mtl.mit.edu <labnetwork-bounces at mtl.mit.edu> On Behalf Of Mark K Mondol
Sent: Saturday, March 9, 2019 5:06 PM
To: Michael Rooks <michael.rooks at yale.edu>; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Has anyone using thicker than 200nm HSQ for EBL patterning?
As usual I agree with Mike, but have to chime in anyway. Applied Quantum Materials in Canada offers dry HSQ, which you mix with MIBK to make a solution. I just got some and haven't used it yet, but others have. As it is dry you can make whatever dilution you want to achieve thicker films.
________________________________
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [labnetwork-bounces at mtl.mit.edu] on behalf of Michael Rooks [michael.rooks at yale.edu]
Sent: Saturday, March 09, 2019 8:50 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Has anyone using thicker than 200nm HSQ for EBL patterning?
Multiple-spins seldom produce good results. It's easier to use a thicker solution of HSQ. Of course you can buy thicker HSQ, such as Fox-16, but if you are in a hurry you can thicken the 6% HSQ (well, any resist really) by bubbling nitrogen through it. Just put a tube in the bottle and blow in some dry nitrogen. The solvent will evaporate, and the bubbles will keep the solution agitated, so a skin does not form on the surface. No need to be precise about the solution. Just keep bubbling until you get the thickness you want.
------------------------------------
Michael Rooks
Yale Institute for Nanoscience and Quantum Engineering
nano.yale.edu
On 3/8/2019 10:02 PM, Zhao, Mengdi wrote:
Hello everyone,
I am trying to spin 350nm HSQ by double coating XR1541 6% at 2000rpm and bake at 80C between coating. However, HSQ thickness measured by reflectance spectrum actually get thinner after the second spin and bake. I wonder if the HSQ still get dissolved again during the 2nd dispense even with 80C bake for 4min after the first coating. Any suggestion on getting over 200nm HSQ spin coated on Si?
Best regards,
Mengdi
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190401/fcd49170/attachment.html>
More information about the labnetwork
mailing list