What is the lapse of time between 24mw/cm2 and 20mw/cm2, what brand ???
Regards
Sent from Yahoo Mail for iPhone
Mario Portillo, hbtusainc at yahoo.com
On Monday, July 8, 2019, 6:00 PM, Morrison, Richard H., Jr <rmorrison at draper.com> wrote:
#yiv8440840048 #yiv8440840048 -- _filtered #yiv8440840048 {panose-1:2 4 5 3 5 4 6 3 2 4;} _filtered #yiv8440840048 {font-family:Calibri;panose-1:2 15 5 2 2 2 4 3 2 4;}#yiv8440840048 #yiv8440840048 p.yiv8440840048MsoNormal, #yiv8440840048 li.yiv8440840048MsoNormal, #yiv8440840048 div.yiv8440840048MsoNormal {margin:0in;margin-bottom:.0001pt;font-size:12.0pt;font-family:New serif;}#yiv8440840048 a:link, #yiv8440840048 span.yiv8440840048MsoHyperlink {color:#0563C1;text-decoration:underline;}#yiv8440840048 a:visited, #yiv8440840048 span.yiv8440840048MsoHyperlinkFollowed {color:#954F72;text-decoration:underline;}#yiv8440840048 p.yiv8440840048gmail-msolistparagraph, #yiv8440840048 li.yiv8440840048gmail-msolistparagraph, #yiv8440840048 div.yiv8440840048gmail-msolistparagraph {margin-right:0in;margin-left:0in;font-size:12.0pt;font-family:New serif;}#yiv8440840048 span.yiv8440840048EmailStyle18 {font-family:sans-serif;color:#1F497D;}#yiv8440840048 .yiv8440840048MsoChpDefault {font-family:sans-serif;} _filtered #yiv8440840048 {margin:1.0in 1.0in 1.0in 1.0in;}#yiv8440840048 div.yiv8440840048WordSection1 {}#yiv8440840048
HI,
We leave the lamp on all the time, 350w lamp we run at 24 mw/cm2 and change the lamp when it drops below 20 mw/cm2,
Rick
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu]On Behalf Of Youry Borisenkov
Sent: Friday, July 05, 2019 11:59 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] MA6 lamp life
HI Everyone,
I have 3 quick questions about your policy for changing the UV-lamp on the MA6 (Karl Suss) mask aligners.
1. do you turn off the UV - power supply during nights and weekends? or just leave it on?
2. do you change the UV lamp on a regular basis (after 1 month or so)? or you monitor it's power and have a lower limit before you decide to change it? or you just wait for it to fail and then change it?
3. how often do you change the lamp?
Thanks and Happy July 4th
Youry
P.S.
You can use this template to reply):
|
1- Off/On
|
2- Change every ___ / wait for the power to decrease by ___ % / wait for it to fail
|
3- Every ___ month
|
|
|
|
|
Youry Borisenkov, Ph.D.
Process Engineer at CNI Shared Labs
CEPSR/MC 8903
530 west 120th st. NY
NY 10027
Work 212-851-5688
Cell 646-592-1514
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email._______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190708/92a330d1/attachment.html>
More information about the labnetwork
mailing list