Hi Michael,
That sounds like an easy way to get a thicker HSQ solution. We will definitely give it a try. Thank you!
Best regards,
Mengdi
________________________________
From: labnetwork-bounces at mtl.mit.edu <labnetwork-bounces at mtl.mit.edu> on behalf of Michael Rooks <michael.rooks at yale.edu>
Sent: Saturday, March 9, 2019 7:50 AM
To: labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Has anyone using thicker than 200nm HSQ for EBL patterning?
Multiple-spins seldom produce good results. It's easier to use a thicker solution of HSQ. Of course you can buy thicker HSQ, such as Fox-16, but if you are in a hurry you can thicken the 6% HSQ (well, any resist really) by bubbling nitrogen through it. Just put a tube in the bottle and blow in some dry nitrogen. The solvent will evaporate, and the bubbles will keep the solution agitated, so a skin does not form on the surface. No need to be precise about the solution. Just keep bubbling until you get the thickness you want.
------------------------------------
Michael Rooks
Yale Institute for Nanoscience and Quantum Engineering
nano.yale.edu
On 3/8/2019 10:02 PM, Zhao, Mengdi wrote:
Hello everyone,
I am trying to spin 350nm HSQ by double coating XR1541 6% at 2000rpm and bake at 80C between coating. However, HSQ thickness measured by reflectance spectrum actually get thinner after the second spin and bake. I wonder if the HSQ still get dissolved again during the 2nd dispense even with 80C bake for 4min after the first coating. Any suggestion on getting over 200nm HSQ spin coated on Si?
Best regards,
Mengdi
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190310/ca87ea92/attachment.html>
More information about the labnetwork
mailing list