I need to electroplate Nickel into a photoresist mask. The features should be 25 microns wide and 25 microns tall. Does anyone have a suggestion about external vendors that would be good for this? Also any other guidance about this process is highly appreciated.
Thank you for the help,
Milan Begliarbekov