[labnetwork] Gold Deposition over Chrome
Charles Ellis
elliscd at auburn.edu
Fri May 31 11:56:22 EDT 2019
Try using ultrasonic agitation in alcohol or acetone
Get Outlook for iOS<https://aka.ms/o0ukef>
________________________________
From: labnetwork-bounces at mtl.mit.edu on behalf of Felix Lu <fplu at uchicago.edu>
Sent: Friday, May 31, 2019 10:44 AM
To: Jim Carroll; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Gold Deposition over Chrome
Jim – How are you patterning the chrome? I would suspect that you have a thin layer of chrome in the “blanked” areas.
___________________________________________________
Felix P. Lu, Ph.D.
Director of Corporate Engagement
Institute for Molecular Engineering
The University of Chicago
Eckhardt Research Center
5640 S. Ellis Ave., Room ACC104
Chicago, IL 60637
773.834.5063 office
fplu at uchicago.edu<mailto:fplu at uchicago.edu> | ime.uchicago.edu<http://ime.uchicago.edu/>
From: <labnetwork-bounces at mtl.mit.edu> on behalf of Jim Carroll <jim at photomaskportal.com>
Date: Thursday, May 30, 2019 at 6:45 PM
To: "labnetwork at mtl.mit.edu" <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Gold Deposition over Chrome
Dear LabNetwork colleagues,
We are trying to add a thin film of gold over patterned chrome on a standard photomask using e-beam evaporation. We want the gold to preferentially adhere to the chrome while lifting off the glass.
After a few tests, it appears that the gold sticks equally well to both the glass and chrome. Ultrasonic agitation and swabbing do not selectively remove the gold from the glass while leaving it on the chrome. Eventually, after enough pressure is applied with a swab, the gold releases from both the glass and chrome.
Does anyone have a suggested approach?
Thanks,
Jim Carroll
PhotomaskPORTAL
We help you make masks
(415) 448-6275
· [Image removed by sender.]
<http://www.photomaskportal.com>
-------------- next part --------------