Thank you Mark for the anneal recipe, we will try it.
Rick
From: Mark Cooper [mailto:markc at exper-tech.com]
Sent: Friday, May 31, 2019 11:53 AM
To: Morrison, Richard H., Jr <rmorrison at draper.com>; labnetwork at mtl.mit.edu
Subject: RE: furnace boat question
Hello Richard,
We often build different boat designs for different processes, so that its obvious what boat goes with what process. Shell and rail boats can achieve the same process results, but appear completely different.
It is more difficult to do this with automated boat loading mass transfer tools, but for hand loaded its relatively easy.
We also do this from time to time with silicon carbide paddles, 2 inch square handle for oxide, and1.75 or 1.25 square for anneal.
Scribe is fine, but the boats (any quartz) should be annealed at 1175 for 8 hours to relieve the stress. The anneal is part of the process when we manufacture boats with the various suppliers.
I am glad to review boats and quartz offline.
[Image removed by sender. Expertech]
Mark Cooper
General Manager
10 Victor Square Ste 100
Scotts Valley Ca 95066
831 440 4422 direct
831 439 9300 office
831 332 9396 mobile
markc at exper-tech.com
From: labnetwork-bounces at mtl.mit.edu <labnetwork-bounces at mtl.mit.edu> On Behalf Of Morrison, Richard H., Jr
Sent: Friday, May 31, 2019 6:57 AM
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] furnace boat question
HI Everyone,
We are having an issue controlling the quartz boats for our furnace operations. We use 4" and 6" boats with 2 different slot widths. DO you think we could lightly scribe a tube number and size on the rail of the boat? I am concerned that it would crack.
Rick
Richard H. Morrison
Principal Member of the Technical Staff
Draper
555 Technology Square
Cambridge, MA
02139-3573
Work 617-258-3420
Cell 508-930-3461
www.draper.com<http://www.draper.com>
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190531/3eb8945a/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.jpg
Type: image/jpeg
Size: 549 bytes
Desc: image001.jpg
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20190531/3eb8945a/attachment.jpg>
More information about the labnetwork
mailing list