[labnetwork] Ta/Ti wire vendor
J Romans
hromans at eng.ucsd.edu
Sat Apr 3 14:36:03 EDT 2021
Have you tried California Fine Wire?
https://calfinewire. <https://calfinewire.com/>com/
<https://calfinewire.com/>
J. Hal Romans
Equipment Engineer
Nano3 Cleanroom Facility
University of California San Diego
ph: (858) 534-6674
On Sat, Apr 3, 2021 at 5:10 AM Miller, Dale A. <dale at slac.stanford.edu>
wrote:
> Labnetwork,
>
>
>
> I am coating some ceramic “beam kicker pipes” with TiN for our new
> accelerator, and I’ve run out of my circa 1960’s supply of 0.010” Ta (80%)
> /Ti (20%) wire. I’ve contact all of my deposition material vendors and no
> luck. Anyone got any contacts?
>
> Thanks,
>
>
>
> Dale Miller
>
> Master Science and Engineering Technician
>
> APFD –Coating Lab
>
> SLAC National Accelerator Laboratory
>
> 926-5202
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!Mih3wA!Siv5zD38Kh3rlfFib2IzJBgTYV2hv0cuUxUmEV3VDUKtN327aVowdcwAaZTC1uM$
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210403/cbedce86/attachment.html>
More information about the labnetwork
mailing list