[labnetwork] Liquid nitrogen and argon shortage
Manish Keswani
manish.keswani01 at gmail.com
Fri Dec 3 20:24:00 EST 2021
Hello everyone,
We just learned that there is a severe shortage of liquid nitrogen and argon in the US. Our entire lab will be impacted by this and we will need to evaluate consumption of these gases for different tools in our Nano fabrication center and make priority for tools usage based on that. Nitrogen is used as a purge gas for pumps and equipment and we will be looking into tools that consume significant amount of nitrogen and how to minimize their use or use them more efficiently.
If you have any thoughts or ideas that will help with this issue, please share them.
Thanks,
Manish