[labnetwork] lab benchmarking exercise
Gheorghe Iordache
gheorghe.iordache at kaust.edu.sa
Wed Feb 17 15:19:43 EST 2021
Dear Rob,
As I mentioned in my reply to Julia and labnetwork, I will definitely share the conclusions with our community, hopefully at the UGIM 2022.
I hope I'll get enough feedback to make the exercise meaningful.
Please Stay Safe.
Kind regards,
Gheorghe
From: Robert Pearson [mailto:repemc at rit.edu]
Sent: 15 February 2021 20:16
To: Aebersold,Julia W. <julia.aebersold at louisville.edu>; Gheorghe Iordache <gheorghe.iordache at kaust.edu.sa>; labnetwork at mtl.mit.edu
Subject: RE: [labnetwork] lab benchmarking exercise
Hello Gheorghe,
A agree with Julia, I would also like to see a summary of your final results.
I think that you should share them at the 2022 University Government Industry Micro/Nano Electronics Symposium that will be held at the University of Wisconsin, June 6-9 2022.
https://ugim2020.wisc.edu/<https://urldefense.com/v3/__https:/ugim2020.wisc.edu/__;!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64JT9qJY-g$>
Sincerely,
Rob
[rob_image_2012]
Robert E. Pearson, PhD
Electrical & Microelectronic Engineering
Rochester Institute of Technology
Rochester NY 14623
(585) 475-2923 voice
robert.pearson at rit.edu<mailto:robert.pearson at rit.edu>
http://people.rit.edu/~repemc/<https://urldefense.com/v3/__http:/people.rit.edu/*repemc/__;fg!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64KIIHM-ag$>
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of Aebersold,Julia W.
Sent: Monday, February 15, 2021 10:16 AM
To: Gheorghe Iordache <gheorghe.iordache at kaust.edu.sa<mailto:gheorghe.iordache at kaust.edu.sa>>; labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] lab benchmarking exercise
Can you give moer information on how the data will be used and if it will be shared with this group thereafter?
Cheers!
Julia Aebersold, Ph.D.
Manager, Micro/Nano Technology Center
University of Louisville
2210 South Brook Street
Shumaker Research Building, Room 233
Louisville, KY 40292
(502) 852-1572
http://louisville.edu/micronano/<https://urldefense.com/v3/__http:/louisville.edu/micronano__;!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64LdOMkVyA$>
________________________________
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> on behalf of Gheorghe Iordache <gheorghe.iordache at kaust.edu.sa<mailto:gheorghe.iordache at kaust.edu.sa>>
Sent: Monday, February 15, 2021 4:18 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu> <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: [labnetwork] lab benchmarking exercise
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Dear colleagues,
I'm running a lab benchmarking exercise and I would like to kindly ask for your feedback to the extent you will be able to share the info.
Please see the table below with the numbers for KAUST Nanofabrication Core Lab and if you will be able to help please fill in your lab numbers on the dedicated column and send it to me in confidence to gheorghe.iordache at kaust.edu.sa<mailto:gheorghe.iordache at kaust.edu.sa> .
IMPORTANT NOTE: Your input will be used by me only for the above mentioned exercise and it will not be disclosed to anyone else.
Thank you in advance and all please Stay Safe!
Question
KAUST
Your lab here
Academic or Industry?
University
Government of private?
private
user shared lab with independent management or run by faculty?
independent Core Lab in charge with equipment maintenance and training users; faculty would suggest new equipment to be purchased
cleanroom area [sq. meter]
2000
cleanroom class (ISO)
5
no. of lab staff / PhD / Engineers / Technicians
19 / 10 / 6 / 3
no. of current users
178
no. of faculty
48
no. of equipment
140
cleanroom open to users 24/7 ?
NO
do you run a cost recovery business model?
NO
the 3 most used equipment / their usage % 24h / backup equipment available?
Deposition e-beam Evaporator / 37% / YES
PPMS_2B_tf / 22% / YES
PPMS_2_tf / 21% / YES
Cleanroom Specific safety training and emergency response
YES
Training tracking system
YES / Badger
Safety Training refresher for staff and users
every 3 years
Critical Equipment Training refresher
if not used for 6 months
Equipment reservation system ?
YES / Badger
Equipment/Asset maintenance system ?
YES/FiiX
lab ISO 14644 compliant or certified ?
ISO 14644 compliant
do you have a microfluidics lab?
YES
hosting SME research or production?
NO
equipment mainenance - mostly [in-house or service contracts]
in-house
Buddy system recommended or compulsory?
recommended
Lab Control System monitored 24/7
YES
Emergency response communication
Core Labs WhatsApp on business mobile phones. Connected to campus emergency response
Emergency response team [lab internal or external]
Campus Fire Department
Toxic Gas Monitoring System
YES
All Alarm response to Fire Department
YES
Safety Walkthrough
Biweekly
Kind regards,
=======================
Gheorghe IORDACHE, PhD Physics, MBA
Director of the Nanofabrication Core Lab
KAUST
King Abdullah University of Science and Technology
Al Khawarizmi Building 1 East, Level 3, Office 3415
Thuwal 23955-6900
Kingdom of Saudi Arabia
Office: +966 (0)12 8080447
Mobile: +966 (0)540381154
Email: gheorghe.iordache at kaust.edu.sa<mailto:gheorghe.iordache at kaust.edu.sa>
Linkedin: https://www.linkedin.com/in/gheorghe-iordache-phd-physics-mba/<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Fwww.linkedin.com*2Fin*2Fgheorghe-iordache-phd-physics-mba*2F&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047921118*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=IDwNtX7p*2BksTG961jKZHfIA7wzYJNNnhX6jLcrnoY4w*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSUlJSU!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64KxxCWHsg$>
Follow the Core Labs: corelabs.kaust.edu.sa<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Fcorelabs.kaust.edu.sa*2F&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047921118*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=PIqPy6bhE9prkm*2FNNIYXF7OXYlSjVe*2BgOLV5bKqqTX4*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSUlJQ!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64KF0mJWRA$>; https://twitter.com/kaust_corelabs<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Ftwitter.com*2Fkaust_corelabs&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047931113*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=R2RQk6NKt5QhytSblCeWXTnfe3pk9anJx60IHwArTRo*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSU!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64JyyyAQ1g$>; https://www.instagram.com/kaustcorelabs/<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Fwww.instagram.com*2Fkaustcorelabs*2F&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047931113*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=MfrwhhTTIljUA7w8Xg6hV2rB*2FfswYijf32pTArtdJ*2FQ*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSUlJSU!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64I2zpj1Ew$>; https://www.linkedin.com/showcase/12179999<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Fwww.linkedin.com*2Fshowcase*2F12179999&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047941110*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=b6to2*2BQaCh*2F4xIOtwMQ96uFYjF6zEVIoZrOWmu6PVWA*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSUlJSU!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64LMCPFZug$>
Visit the Core Labs: https://corelabs.kaust.edu.sa/visitor-information<https://urldefense.com/v3/__https:/nam11.safelinks.protection.outlook.com/?url=https*3A*2F*2Fcorelabs.kaust.edu.sa*2Fvisitor-information&data=04*7C01*7Cjulia.aebersold*40louisville.edu*7C5d548483b96b4571cf7b08d8d1b76c5c*7Cdd246e4a54344e158ae391ad9797b209*7C0*7C0*7C637489933047941110*7CUnknown*7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0*3D*7C3000&sdata=OEh7pmfGvUCHCBapH85gfGOWuB2Z9v8G7dsT9hU*2FYWU*3D&reserved=0__;JSUlJSUlJSUlJSUlJSUlJSUl!!Nmw4Hv0!nkDYPNMt1joPoSGgnrgv22_m2-EjYefzu1p0NE9VVinoKbwr9qyr55xgapiTFha_64Jdiz57Sw$>
================
Please note that the weekend in Saudi Arabia is Friday and Saturday
========
What you do for yourself vanishes once you're gone.
What you do for others stays for others as your legacy.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210217/db5bd3b6/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 124773 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210217/db5bd3b6/attachment.png>
More information about the labnetwork
mailing list