Hi Tim,
After going through same issues as you, I replaced ours with a VAT gate valve and have not had to touch it now for several years.
I think this is part number….
01228-K06
Mike
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Tim Gilheart
Sent: 30 March 2021 23:13
To: Fab Network <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Cambridge/Ultratech/Veeco Savannah ALD - stop valve issues?
CAUTION: This e-mail originated outside the University of Southampton.
Greetings,
I’m hoping that several teams on this list have relevant experience to share, since I know a number of you manage Savannah ALD tools.
Our tool has presented with leakage issues through the stop valve twice in the past 6 months. We replaced the last valve at the end of Aug 2020, and have recently again experienced issues with failing to vent (due to the valve not closing completely and the vac pump still pulling on the chamber).
We have a temporary workaround in place (an external manual valve on the pump line), but this leakage through the stop valve effects process outcomes and has proven costly to address, since valve replacement seems to be the recommended solution.
Our tool typically runs Al2O3, HfO2, TiO2, and ZnO processes, sometimes ZrO2. Stop valve heating jacket is maintained at the recommended 150 C, and the heaters all seem to be working properly.
Does anyone have suggestions about maintaining these stop valves for longer? Or, failing that, a referral for refurbishing them? I am willing to consider a solution that involves swapping out valves 1-2/year and sending them out for rebuild if that’s an option for a reasonable cost.
Thanks in advance for any advice you can share,
--
Tim Gilheart, Ph.D.
Research Scientist - Nanofabrication Cleanroom Manager,
Shared Equipment Authority (SEA), Rice University
Cell: 832-341-5488 | Office: 713-348-3159 | gilheart at rice.edu<mailto:gilheart at rice.edu>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210331/364680ad/attachment.html>
More information about the labnetwork
mailing list