Hi Nagaraj,
At Nanoscribe we go through considerable length to assure the quality of the ITO coatings for cleanliness and coating thickness. However, we do not force you to use our substrates. You can certainly source your own substrates. The substrate specifications are documented in the user-accessible and free Nanoguide [0]. If you have not registered there, I wholeheartedly recommend it.
If you decide on not using our substrates, please check that the ITO surface resistance is low enough to guarantee a working interface detection. Also, if you use thicker than the standard 0.7mm samples, please talk to our support to have a custom holder registered in the software. That allows you to use substrate thicker than the usual substrates with safe interface finding. If you are an advanced user, you can also do this according to the documentation [1]. Be advised however, that misconfiguration of the NanoWrite configuration files can result in damage to the printer if hardware-dependent parameters are missing or incorrectly set by the user. If in doubt, simply reach out to our support.
Very Best,
Matthias Blaicher
[cid:image001.png at 01D74649.78FC0C20]
R&D Engineer
Phone
E-mail
Web
+49 721 981 980 720
blaicher at nanoscribe.com
www.nanoscribe.com
Nanoscribe GmbH & Co. KG
Hermann-von-Helmholtz-Platz 6
76344 Eggenstein-Leopoldshafen
Germany
Registered office: Registered office: Eggenstein-Leopoldshafen, Germany; Commercial Registry Mannheim, HRA 709547; VAT-No. DE334074592
Partner with unlimited liability: Nanoscribe Verwaltungs GmbH, CEO: Martin Hermatschweiler, CFO: Lars Tritschler; Registered Office: Eggenstein-Leopoldshafen, Commercial Registry: Mannheim, HRB 737409
Your privacy as well as the new European regulation on the protection of personal data (GDPR) are very important to us. More information can be found in the privacy policy<https://www.nanoscribe.com/en/privacy-policy> on our website.
This email and any files transmitted with it are confidential and may contain privileged or otherwise protected information. You should not disseminate, distribute or copy this email. Please notify the sender immediately by email if you have received this email by mistake and delete this email from your system.
[0] https://support.nanoscribe.com/hc/en-gb/articles/360001695714-ITO-Coated-Substrates-3D-MF-DiLL-
[1] https://support.nanoscribe.com/hc/en-gb/articles/360018530554-Editing-ini-Configuration-Files
Von: labnetwork <labnetwork-bounces at mtl.mit.edu> Im Auftrag von Nagaraj Krishna Subbaiah
Gesendet: Montag, 10. Mai 2021 19:13
An: labnetwork at mtl.mit.edu
Betreff: [labnetwork] Nanoscribe Users
Hi All,
Addressing all users of Nanoscribe. Would like to know how the users of nanoscribe are procuring their consumables. Especially the ITO coated substrates, do you purchase them from the company itself or sigma or any other resource?.
If you've used substrates from other resources, have you faced any problems with printing? And has the company turned down the support because you've used substrates bought from elsewhere?.
Your feedback is appreciated,
Thank you,
Nagaraj
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210511/04cddffa/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 3663 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210511/04cddffa/attachment.png>
More information about the labnetwork
mailing list