[labnetwork] PR bubbles where exposed
Martin,Michael David
michael.martin at louisville.edu
Fri Nov 5 10:36:28 EDT 2021
We have used SPR 220 a lot in the past and came to the conclusion that it was just very finicky probably due to requiring just the right bake and hold times as mentioned by others. In the end, most of our users switched to AZ 4620 which is much easier to process and is a nice thick resist with a 12um nominal thickness.
Regards,
Michael
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Maduzia, Joseph Walter <jmaduzi2 at illinois.edu>
Sent: Thursday, November 4, 2021 9:59 AM
To: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [labnetwork] PR bubbles where exposed
You don't often get email from jmaduzi2 at illinois.edu. Learn why this is important<http://aka.ms/LearnAboutSenderIdentification>
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Hello All!
Thank you again for all your feedback on SiO2 etch around Al. It has been very helpful and we are moving down multiple paths suggested via the Lab Network to try to solve the issue. More to come once we solve it!
I have another issue I was hoping for feedback on. We have bubbling in our PR (SPR-220-4.5) (pos tone) that we haven’t been able to track the source of. It only bubbles during exposure and only where it is exposed. Unexposed areas are unaffected. I’ve attached some images of the bubbling where you can see the exposed (lighter) and unexposed (darker) areas. The bubbles are visible to the naked eye. The wafer is silicon w a dry thermally grown SiO2 surface. We typically expose via EV620 mask aligner with Vac+HardContact. However, even in a flood exposure with the mask just set lightly down it still bubbles. Without a mask there are also bubbles randomly distributed across the wafer, but they don’t get stuck to the mask so they don’t pop. We tried various pre-bakes, HMDS coat vs not, piranha treat vs not. In the past these bubbles show up, we trial and error to get rid of them and suddenly they disappear. Our process, although seemingly repeatable, does not yield repeatable results.
Thank You,
JOE MADUZIA
MNMS Laboratory Specialist
The Grainger College of Engineering
Mechanical Science and Engineering
2239 Sidney Lu Mechanical Engineering Bldg
1206 W. Green
Urbana, IL 61801
217.244.6302 | jmaduzi2 at illinois.edu<mailto:jmaduzi2 at illinois.edu>
https://cleanroom.mechse.illinois.edu/<https://nam11.safelinks.protection.outlook.com/?url=https%3A%2F%2Fcleanroom.mechse.illinois.edu%2F&data=04%7C01%7Cmichael.martin%40louisville.edu%7Cb438a0a763f74c04bfb708d99fa98de0%7Cdd246e4a54344e158ae391ad9797b209%7C0%7C0%7C637716372869866861%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C1000&sdata=GE7E0gAx56qcTtYJTaPL5rCwHKmLy2HeTL7rqTQ0iLM%3D&reserved=0>
[cid:image001.png at 01D7D156.50D75180]<https://nam11.safelinks.protection.outlook.com/?url=http%3A%2F%2Fillinois.edu%2F&data=04%7C01%7Cmichael.martin%40louisville.edu%7Cb438a0a763f74c04bfb708d99fa98de0%7Cdd246e4a54344e158ae391ad9797b209%7C0%7C0%7C637716372869876811%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C1000&sdata=7ges4p4pJKGWS%2BWarDREgeBzGa%2FkLEyezP9O3M3HSt0%3D&reserved=0>
Under the Illinois Freedom of Information Act any written communication to or from university employees regarding university business is a public record and may be subject to public disclosure.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20211105/865bbc3c/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 4711 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20211105/865bbc3c/attachment.png>
More information about the labnetwork
mailing list